Transparent, photocatalytic, and self-cleaning TiO2 thin film is developed by TiO2 sol-gel coating on glass and polycarbonate (PC) substrates. Acetyl acetone (AcAc) suppresses the precipitation of TiO2 by forming a yellowish (complex) transparent sol-gel. XPS analysis confirms the presence of Ti2p and O1s in the thin films on glass and PC substrates. The TiO2-sol is prepared by stabilizing titanium (IV) isopropoxide (TTIP) with diethylamine and methyl alcohol. The addition of AcAcsilane coupling solution to the TiO2-sol instantaneously turns to yellowish color owing to the complexing of titanium with AcAc. The AcAc solution substantially improves the photocatalytic property of the TiO2 coating layer in MB solutions. The coated TiO2 film exhibits super hydrophilicity without and with light irradiation. The TiO2 thin film stabilized by adding 8.7 wt% AcAc shows the highest photo-degradation for methylene blue (MB) solution under UV light irradiation. Also, the optimum photocatalytic activity is obtained for the 8.7 wt% AcAc-stabilized TiO2 coating layer calcined at 450 ℃. The thin-films on glass exhibit fast self-cleaning from oleic acid contamination within 45 min of UV-light irradiation. The appropriate curing time at 140 ℃ improves the anti-fogging and thermal stability of the TiO2 film coated on PC substrate. The watermark-free PC substrate is particularly beneficial to combat fogging problems of transparent substrates.
Ferroelectric PZT(30/70)/PZT(70/30) heterolayered thin films were fabricated by spin-coating method on the $Pt/Ti/SiO_2Si$ substrate alternately using(30/70) and PZT(70/30) alkoxide solutions prepared by sol-coating method. The coating and heating procedure was repeated six times to form PZT heterolayered films, and thickness of the film obtained by one-times drying/sintering process was about 40-50 nm. All PZT heterolayered films, showed dense and homogeneous structure without the presence of rosette sturctrue. The relative dielectric constant, remanent polarization and leakage current density of PZT heterolayered films were superior to those of single composition PZT(30/70) and PZT(70/30) films, and those values for the PZT-6 film were 975, $21 \muC/cm^2\; and\; 8\times10^{-9}\; A/cm^2$, respectively. And the PZT-6 heterolayered film showed fairly good fatigue characteristics of remanent polarization and coercive field after application of $10^8$ switching cycles.
Valinasab, Behzad;Rukosuyev, Maxym;Lee, Jason;Ko, Junghyuk;Jun, Martin B.G.
한국생산제조학회지
/
제24권1호
/
pp.23-30
/
2015
The scanning quality can be influenced by reflective abilities of a surface. Transparency and glossiness of a surface can highly limit the scanning results. Various techniques have been developed to solve problems of reflective and transparent surfaces. As one of the most feasible and convenient solutions, a thin layer of coating with proper specifications is sprayed on surface for eliminating the problems of the surfaces. As the main goal is to keep the object geometry unchanged, then it is important to coat the surface with layers less than one micrometer in thickness. For this purpose, a newly designed atomization-based spray system has been developed and tested in sets of experiments to study its efficiency on scanning results while objects with the surface are in use. This paper presents the spray design process and then studies and compares the 3D scanning results of the surfaces coated with atomization-based and aerosol sprays.
The phosphate coating on the $(Fe_{0.97}Cr_{0.03})_{76}(Si_{0.5}B_{0.5})_{22}C_2$ amorphous powders with an average size of 10 ${\mu}m$ in diameter has been carried out in aqueous 1.0-2.0 wt% $H_3PO_4$ solutions, and the consolidation behavior and magnetic properties of their compressed powder cores has been investigated. The phosphate coating could provide efficient electrical insulation between amorphous powders and improved consolidation ability at room temperature. Especially when the powders were treated in more concentrated phosphoric acid solution, enhanced phosphate covering and higher frequency/dc-bias stability were achieved. The powder cores phosphate-coated in 2.0 wt% $H_3PO_4$ solution exhibited constant permeability of 21 up to 10 MHz, 110 of the quality factor at 0.9 MHz, 610 mW/cm3 core loss at 100 kHz/0.1 T and 89 of percent permeability at 100 kHz.
A method of preparation of synthetic ignorgaic coating on copper (patina) has been presented . An Eh--pH diagram was constructed for the present Cu-H2O-SO$_4$ system using the most recently available thermodynamic data. In the path of the patination at room temperature the general behaviour of copper in acidic copper sulfate solutions with potassium chlorate as an oxidizing agent appeared to follow those predictable in this Eh-pH diagram. In the presence 0.05 molar cupric sulfate at a temperature of about 28$^{\circ}C$ a green brochantite (CuSO$_4$$.$3Cu(OH)$_2$) layer was formed on copper sheet in 20 days. In a solution having an initial pH of 3.5 the development of a brochantite coating has been observed to take place in two stages. In the first, a layer of cuprous oxide formed on the copper at a relatively rapid rate. In the ensuing step the outer layer of cuptrite was oxidized at much slower rate to form brochantite. The syntetic coatings appeared to consist of crystal-lites of brochanitite growing perpendicular to the cuprose oxide surface. The outer tips of the -crystallites were reasily broken off and gave to the layer a rather chalky character. Underneath, at the brochantite Cu$_2$O interface, however, the green layers were firmely attached. The effect of reagent concentration , solution agitation , and moderate temperature increase were investigated to improve the quality of coating. So also in a qualitative way were the effect of light.
Jo, Du-Hwan;Yun, Sang-Man;Park, Kee-Cheol;Kim, Myung-Soo;Kim, Jong-Sang
Corrosion Science and Technology
/
제18권1호
/
pp.16-23
/
2019
Steels for automotive fuel tank require unique properties such as corrosion resistance for fuel, welding for joining, forming for press, and painting for exterior. Recently, automakers have been requiring excellent seam weldable steels to enhance manufacturing productivity of fuel tank. Thus, POSCO developed a new type of functional steels coated with nano-composite thin layer on Zn-Ni plating steels. The nano-composite coating solution was prepared by mechanical fine dispersion of solutions consisting of polymeric resin and nano-composite materials in aqueous media. The composite solution was coated on the plating steel surface by using roll coater and cured through induction furnace. These new developed plating steels were evaluated for quality performances such as seam and spot weldability, press formability, and corrosion resistance. These new functional steels coated with nano-composite layer exhibited excellent seam weldability and press formability. Detailed discussion of coating solution and experimental results suggest that nano-sized composite dispersion as coating layer plays a key role in enhancing the quality performance.
This paper studies the experimental method that uses the homogeneous precipitation method to prepare mica flakes coated with anatase-type titania pearlescent pigment with urea as precipitant. The optimum technology parameters, the chemical composition, the microstructure, and the color property of resulting pigments are discussed. The coating principle of mica coated titania with various coating thickness is analyzed by X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy(TEM) and tested by spectrophotometer analysis. The colored nanocrystalline pigments with different morphology and coating thickness 45-170 nm were prepared by homogeneous precipitation treatment of $TiOSO_4$(titanum oxysulfate) aqueous solutions. Characterizations on the pigments show that the pearlescent effects of the pigments depend mainly on mica size, thickness of the metal oxide deposit, its chemical composition, and crystal structure.
International Journal of Computer Science & Network Security
/
제21권1호
/
pp.49-54
/
2021
Relative to the outer surface of the mastic coating, the reliability of the available waterproofing resource is determined by the ability to stabilize the structural characteristics in difficult climatic conditions. Organic components of mastic as a result of solar radiation, elevated temperatures and their alternating change, atmospheric oxidants, especially in industrial areas, have a tendency to self-polymerization and loss of low molecular weight components. This is the gradual loss of deformability and the transition to brittleness with its tendency to crack as the reasons for the gradual transition from normal to emergency operating condition.The presented mechanism of functioning of the coating surface indicates the expediency of increasing its components, able to stabilize the structure and prevent changes in deformability.Durability, hydrophobicity, water displacement, water absorption are accepted as estimating indicators. The main dependences of the influence of the lost additional components of mastic on the operational properties of the formed coating characterize the ability to provide successful resistance to environmental influences and longer stability. As a result, mastic acquires additional service life.
International Journal of Concrete Structures and Materials
/
제2권1호
/
pp.21-25
/
2008
Surface treatments act as a barrier between the environment and the concrete, preventing or retarding the entry of harmful substances and cutting off the transportation path into concrete. The effectiveness of a surface protection preventing the permeation depends on how close and strongly connected are the resin molecules. This work intends to contribute to a better understanding of the performance of protected concrete in chemically aggressive environments, by presenting results of ion diffusion and resistance to aggressive solutions of several hydrophobic agents and coatings used to protect concrete. Three different types of surface protections were tested: silicone hydrophobic agent, acrylic and epoxy coatings. The obtained results indicate that the overall performance of epoxy resin was better than the other selected types of protections.
The water permeation in protective coatings, which may greatly influence the corrosion protective property of these coatings, was studied using the electrochemical impedance spectroscopy technique. During the absorption of water in protective coatings immersed in electrolyte solution, the change of coating capacitance with concentration of electrolyte was determined from impedance measurements. When water absorption or desorption of coatings occured by exposing the coatings to electrolyte solutions of different concentration, increase in impedance caused by desorption of water was found to be higher in the case of thicker film. The amount of water absorbed in coatings changed with concentration of electrolyte. The water taken up in coatings from the solution of lower electrolyte concentration was deserted by contact with the solution of higher concentration. The uptake of water in protective coatings varied depending on the type of coating ingredient especially binder.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.