  • The physical, electrical and piezoresitive characteristics of CrN(chromiun nitride) thin-films on silicon substrates have been investigated for use as strain gauges. The thin-film depositions have been carried out by DC reactive magnetron sputtering in an argon-nitrogen atmosphere(Ar-(5~25 %)$N_2$). The deposited CrN thin-films with thickness of $3500{\AA}$nd annealing conditions($300^{\circ}C$, 48 hr) in Ar-10 % $N_2$ deposition atmosphere have been selected as the ideal piezoresistive material for the strain gauges. Under optimum conditions, the CrN thin-films for the strain gauges is obtained a high electrical resistivity, $\rho=1147.65\;{\mu}{\Omega}cm$, a low temperature coefficient of resistance, TCR=-186 ppm/$^{\circ}C$ and a high temporal stability with a good longitudinal gauge factor, GF=11.17.

  • PDF

Fabrication of High-sensitivity Thin-film Type Strain-guges (고감도 박막형 스트레인 게이지의 제작)

  • Chung, Gwiy-Sang;Seo, Jeong-Hwan
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.05b
    • /
    • pp.135-141
    • /
    • 2000
  • The physical, electrical and piezoresitive characteristics of CrN(chromiun nitride) thin-films on silicon substrates have been investigated for use as strain gauges. The thin-film depositions have been carried out by OC reactive magnetron sputtering in an argon-nitrogen atmosphere(Ar-(5~25 %)$N_2$). The deposited CrN thin-films with thickness of $3500{\AA}$ and annealing conditions($300^{\circ}C$, 48 hr) in Ar-10 % $N_2$ deposition atmosphere have been selected as the ideal piezoresistive material for the strain gauges. Under optimum conditions, the CrN thin-films for the strain gauges is obtained a high electrical resistivity, $\rho=1147.65\;{\mu}{\Omega}cm$, a low temperature coefficient of resistance, TCR=-186 ppm/$^{\circ}C$ and a high temporal stability with a good longitudinal gauge factor, GF=11.17.

  • PDF

Ceramic Pressure Sensors Based on CrN Thin-films (CrN박막 세라믹 압력센서)

  • Chung, Gwiy-Sang;Seo, Jeong-Hwan;Ryu, Gl-kyu
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.07a
    • /
    • pp.573-576
    • /
    • 2000
  • The physical, electrical and piezoresitive characteristics of CrN(chromium nitride) thin-films on silicon substrates have been investigated for use as strain gauges. The thin-film depositions have been carried out by DC reactive magnetron sputtering in an argon-nitrogen atmosphere(Ar-(5∼25 %)Na$_2$). The deposited CrN thin-films with thickness of 3577${\AA}$ and annealing conditions(300$^{\circ}C$, 48 hr) in Ar-10 % N$_2$deposition atmosphere have been selected as the ideal piezoresistive material for the strain gauges. Under optimum conditions, the CrN thin-films for the strain gauges is obtained a high electrical resistivity, $\rho$=1147.65 ${\mu}$$\Omega$cm, a low temperature coefficient of resistance, TCR=-186 ppm/$^{\circ}C$ and a high temporal stability with a good longitudinal gauge factor, GF=11.17.

  • PDF

The Annealing Characteristics of Chromiun Nitride Thin-Film Strain Gauges (크롬질화박막형 스트레인 게이지의 열처리 특성)

  • 서정환;박정도;김인규;정귀상
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1999.05a
    • /
    • pp.692-695
    • /
    • 1999
  • This paper presents annealing characteristics of CrN thin-film strain gauges, which were deposited on glass by DC reactive magnetron sputtering in an argon-nitrogen atmosphere)Ar-(5-~25%)$N_2$. The physical and electrical characteristics of these films investigated with the thickness range 3500$\AA$ of CrN thin films, annealing temperature (100~30$0^{\circ}C$) and annealing time (24-72hr) . The optimized condition of CrN thin-film strain gauges were thickness range of 3500$\AA$ and annealing condition(30$0^{\circ}C$ , 48hr) in Ar-10%$N_2$ deposition atmosphere. Under optimum conditions, the CrN thin-films for strain gauge is obtained a high resistivity, $\rho$=1147.65$\Omega$cm a low temperature coefficient of 11.17. And change in resistance after annealing for the CrN thin film were quitely linear and stable.

  • PDF

The Characteristics of Chromiun Nitride Thin-Film Strain Gauges (크롬질화박막형 스트레인 게이지의 특성)

  • Seo, Jeong-Hwan;Kim, Il-Myung;Lee, Chae-Bong;Kim, Sun-Cheol;Chung, Gwiy-Sang
    • Proceedings of the KIEE Conference
    • /
    • 1999.07d
    • /
    • pp.1989-1991
    • /
    • 1999
  • This paper presents characteristics of CrN thin-film strain gauges, which were deposited on glass by DC reactive magnetron sputtering in an argon-nitrogen atmosphere(Ar-$(5{\sim}25%)N_2$). The physical and electrical characteristics of these films investigated with the thickness range $3500{\AA}$ of CrN thin films, annealing temperature $(100{\sim}300^{\circ}C)$ and annealing $(24{\sim}72hr)$. The optimized condition of CrN thin-film strain gauges were thickness range of $3500{\AA}$ and annealing condition($300^{\circ}C$, 48 hr) in Ar-10 %$N_2$ deposition atmosphere. Under optimum conditions, the CrN thin-films for strain gauge is obtained a high resistivity, ${\rho}=1147.65{\mu}{\Omega}cm$, a low temperature coefficient of resistance, TCR=$-186ppm/^{\circ}C$ and a high temporal stability with a good longitudinal, 11.17. And change in resistance after annealing for the CrN thin-films were quitely linear and stable.

  • PDF