In this study, we compared and analyzed the flame retardancy and mechanical properties of three different rigid polyurethane foams (RPUF) containing noble non-halogen phosphorus flame retardant (BHP-RPUF) or halogen-phosphorus flame retardant (TCPP-RPUF) or no flame retardant material (Pure-RPUF). The noble phosphorus-based flame retardant, bis(3-(3-hydroxypropoxy)propyl) phenyl phosphate (BHP), was synthesized by the reaction between disodium phenyl phosphate and 3-chloro-1-propanol. Through universal testing machine (UTM) experiments, the compressive strength of BHP-RPUF was similar to that of TCPP-RPUF. From the result of foam morphology analysis, it was confirmed that BHP-RPUF has the lowest thermal conductivity of $0.023W/m{\cdot}K$. We also measured the size of air bubbles using reaction velocity and SEM, and analyzed how they affect the thermal conductivity. In addition, the heat-resisting property was investigated through TGA analysis. The limited oxygen index (LOI) test confirmed that BHP had the ability to increase the flame retardancy of RPUF.
PURPOSE. This study evaluated the effect of chemical surface treatment using methyl formate-methyl acetate (MF-MA) solution on the tensile bond strength between acrylic denture teeth and auto-polymerized acrylic resin. MATERIALS AND METHODS. Seventy maxillary central incisor acrylic denture teeth for each of three different brands (Yamahachi New Ace; Major Dent; Cosmo HXL) were embedded with incisal edge downwards in auto-polymerized resin in polyethylene pipes and ground with silicone carbide paper on their ridge lap surfaces. The teeth of each brand were divided into seven groups (n=10): no surface treatment (control group), MF-MA solution at a ratio of 25:75 (v/v) for 15 seconds, 30 seconds, 60 seconds, 120 seconds, 180 seconds, and MMA for 180 seconds. Auto-polymerized acrylic resin (Unifast Trad) was applied to the ground surface and polymerized in a pressure cooker. A tensile strength test was performed with a universal testing machine. Statistical analysis of the results was performed using two-way analysis of variance (ANOVA) and post-hoc Dunnett T3 test (${\alpha}$=.05). RESULTS. The surface treatment groups had significantly higher mean tensile bond strengths compared with the control group (P<.05) when compared within the same brand. Among the surface treatment groups of each brand, there were no significantly different tensile bond strengths between the MF-MA groups and the MMA 180 second group (P>.05), except for the Yamahachi New Ace MF-MA 180-second group (P<.05). CONCLUSION. 15-second MF-MA solution can be an alternative chemical surface treatment for repairing a denture base and rebonding acrylic denture teeth with auto-polymerized acrylic resin, for both conventional and cross-linked teeth.
In general, most physical properties of wood/polyvinyl chloride (PVC) composites are lower than those of corresponding neat PVC resin because of poor interfacial adhesion between the hydrophilic wood flour and hydrophobic PVC. Therefore, in this study, we treated wood flour with three aminosilanes to improve wood/PVC interfacial adhesion strength, and eco-friendly wood/PVC/nanoclay composites were prepared by melt blending the aminosilane-treated wood flour, a heavy metal free PVC compound, and a type of nanoclay. The effects of treating wood flour with the aminosilanes and adding the nanoclay on the mechanical properties of the composites were investigated. Mechanical properties of the composites were investigated by universal testing machine (UTM), izod impact tester, dynamic mechanical analyzer (DMA), and thermomechanical analyzer (TMA). The tensile properties of the composites with the aminosilane-treated wood flour were considerably higher than those of the composites with neat wood flour. Furthermore, a small amount of the nanoclay improved mechanical properties of the composites. The performance of the wood/PVC composites was considerably improved by using the aminosilane-treated wood flour and the nanoclay.
Journal of the Society of Cosmetic Scientists of Korea
/
v.22
no.2
/
pp.201-210
/
1996
Predictive tests for the identification of contact sensitizing chemicals have been developed. We measured the sensitization potential with three predictive tests, the in vitro and the in vivo Local Lymph Node Assay(LLNA), ELISA to detect interferon-gamma(IFN-${\gamma}$) from supernatant and flow cytometry to detect change of cell surface proteins, using draining lymph nodes of mice. BALB/c mice were exposed to various chemicals or vehicles on the ears daily for 3 consecutive days in all experiments. With some exceptions of propyl paraben, neomycin sulfate, the in vivo LLNA was able to detect the sensitizing capacity of test chemicals and was more sensitive than the in vitro LLNA for chemicals used in the present study. In another experiment, contact sensitivity was assessed by the ELISA to detect IFN-Υ from the supernatants of the cultured LNCs after sensitization with chemicals. There was a good correlation between the LLNA and the IFN-Υ production for test chemicals. We also examined the change of cell surface proteins on LNCs after sensitization by flow cytometry for some cell adhesion molecules(ICAM-1, E-cadherine, B7 molecule), T cell markers(CD3, CD4, CD8, T$\alpha$$\beta$,T${\gamma}$$\delta$) and B cell markers(LR1, CD45R, I-Ad). The number of ICAM-1 positive cells and B cells in LNCs were increased after sensitization with DNCB, TNCB, isoeugenol and 25%, 50% cinnamic aldehyde compared with that of vehicle as a control. In conclusion, the in vivo LLNA could provide more sensitive screening test for moderate to strong sensitizers and some weak sensitizers including cosmetic raw materials than the in vitro LLNA. The production of IFN-Υ by allergen-activated LNCs might be a values indicators without radioisotopes for the identification of contact allergens. Detection of allergens by testing the increase of ICAM-1 positive cells and B cells in LNCs by flow cytometry might be used as a test method to detect allergens.
Polymer/wood flour composites are recently attracting a lot of interest because they are economic and ecofriendly. In this study, the effects of wood flour size on the thermal and mechanical properties of a polypropylene/wood flour composite were investigated. Mechanical properties of the composite samples prepared by melt-mixing and compression molding were tested by UTM and an izod impact tester, and thermal properties of them were measured by TGA, DMA, DSC and TMA. The best coupling agent was selected by testing three kinds of maleic anhydride modified polypropylene coupling agents, and under the same condition, the effects of wood flour size on the physical properties of the composite were investigated. According to the test results for four different wood flour sizes of 600, 250, 180 and $150{\mu}m$, flexural strength, flexural modulus, crystallinity and water-resistivity of the composite increased with decreasing wood flour size.
In order to improve the specific capacitance of amorphous hydrous manganese oxide ($MnO_2$) for supercapacitors, it is made into composites with vapour-grown carbon nanofibers (VGCF) having the VGCF ratio as 40 wt% in the composites. The electrochemical properties of these composites are investigated in 1.0 M $Na_2SO_4$ by cyclic voltammetry (CV), impedance measurements and chronopotentiometric charger/discharger. The composite with 40 wt% VGCF shows the superior electrochemical performance, whose specific capacitance (based on the mass of $MnO_2$, $0.8mg/cm^2$) is 380 F/g at 20 mV/s and 230 F/g at 500 mV/s. Also, the cycle-life testing of this electrode carried out for 3,000 charge/discharge cycles at $2.0mA/cm^2$ shows 97% capacitance retention.
Kim, Myung Sook;Kwak, Han Kang;Kim, Yoo Hak;Kang, Seong Soo;Gong, Myung Suk;Zhang, Yong Seon;Yoon, Hong Bae;Lee, Chang Hoon
Korean Journal of Soil Science and Fertilizer
/
v.46
no.3
/
pp.153-162
/
2013
Most test methods for plant available soil phosphate are based on the extraction with a chemical solution. The objective of this study is to evaluate available phosphate of various tests at different soil phosphate levels. Two experiments were conducted as follows: i) Extracting capacities of soil phosphate tests - Mehlich III, Mehlich II, Bray I, Olsen, Kelowna, and Modified Lancaster(Mod. Lancaster) - were compared with that of Lancaster test for the soils collected from 32 paddy and 27 upland fields with various soil chemical properties. ii) Field trials on comparing to phosphate uptake by plant were accomplished by cultivating rice and corn plants in the pots filled with the soils. Available phosphate of Lancaster test was significantly correlated with those of Mehlich III, Mehlich II, Bray I, Olsen, Kelowna, and Mod. Lancaster. In upland soils, available phosphates of all the tests were curvilinearly regressed with phosphate uptake by corn. The determination coefficients ($R^2$) of the regression equation between available phosphate in soils and phosphate uptake by plants were ranged from 0.861 (Mehlich III) to 0.741 (Olsen). In paddy soils, the available phosphate measured by Mehlich III and Lancaster was significantly correlated with phosphate uptake by rice. In conclusion, Lancaster and Mehlich III tests could be used for predicting available phosphate in upland and paddy soils.
Nicotine is the main component of environmental tobacco smoke, and its presence in indoor air is widely used as a secondhand-smoke indicator. Environmental tobacco smoke is a major source of indoor air pollution, but sufficient investigation of the uncertainty of its measurement, which mirrors the reliability of nicotine measurement, has not been performed. We calculated the uncertainty of measurement of indoor air nicotine concentration at low, medium, and high concentrations of 11.3798, 10.1977, $98.3768{\mu}g/m^3$, respectively, and we employed the Guide to the Expression of Uncertainty in Measurements (GUM), proposed by the International Organization for Standardization (ISO). The factors considered in determining the uncertainty were uncertainty of the calibration curve (calibration curve and repeated measurements), desorption efficiency, extraction volume, and sampling airflow (accuracy and acceptable limits of flowmeter). The measurement uncertainty was highest at low concentrations; the expanded measurement uncertainty is $0.9435{\mu}g/m^3$ and is represented as a relative uncertainty of 63.38%. At medium and high (concentrations, the relative uncertainty was 13.1% and 9.1%, respectively. The uncertainty of the calibration curve was largest for low indoor nicotine concentrations. To increase reliability of measurement in assessing the effect of secondhand smoke, measures such as increasing the sample injection rate ($1{\mu}L$ or more), increasing sampling volume to increase collected nicotine, and using gas chromatography-mass spectrometry (GC/MS) or GC/MS/MS, which has a lower quantitation threshold, rather than gas chromatography with nitrogen phosphorous detector, should be considered.
The adhesive mechanisms on the metal-ceramic restorations have been reported to be mechanical interlocking, chemical bonding, compressive force, and Van der Waal's force, etc. Of these, the mechanical interlocking and chemical bonding forces are thought to affect the adhesive force between Ni-Cr alloy and porcelain. This study investigates the adhesion of Ni-Cr alloy to porcelain according to surface treatment. For this purpose, the following experiments were made; The compositions of Ni-Cr alloy as cast by emission spectrograph, and the oxides produced on Ni-Cr alloy during degassing at $1850^{\circ}F$ for 30 minutes in air and in vacuum were analyzed by X-ray diffractograph. The metal phases of Ni-Cr alloy were observed according to porcelain-baking cyclic heat treatment by photo microscope and the distribution and the shift of elements of Ni-Cr alloy and porcelain and the failure phases between Ni-Cr alloy and porcelain by scanning electron microscope. The adhesive force between Ni-Cr alloy and porcelain was measured according to surface treatment with oxidization and roughening by Instron Universal Testing Machine. Results were as follows; 1. The metal phases of Ni-Cr alloy as cast and degassing state showed the enlarged and fused core, but when subjected to porcelain-baking cyclic heat treatment, showed a dendrite growing. 2. The kinds of metal oxides produced on Ni-Cr alloy during degassing were found to be NiO and $Cr_2O_3$. 3. The distribution of elements at the interface of Ni-Cr alloy and porcelain in degassing state showed demarcation line, but in roughening state, showed mechanical interlocking phase. 4. The shift of elements at the interface occurred in both states, but the shift amount was found to be larger in roughening than in degassing. 5. The adhesive force between Ni-Cr alloy and porcelain was found to be $3.45{\pm}0.93kg/mm^2$, in degassing and $3.82{\pm}0.99kg/mm^2$, in roughening. 6. The failure phase between Ni-Cr alloy and porcelain showed the mixed type failure.
Fading of Chlorantine Fast Red 5B (C.I. Direct Red 81) on cotton fabric exposed to carbon are light was examined. It was observed that the dye had anomaly in CF curve slope, while normal in CFG one. Auther considered that the reason for discrepancy of the one with the other curve slope might be appeared from Weber-Fechner law, and derived following equation $F_v=[logC_0-log(C_0-C_0F_t/100)]{\times}100/(logC_0+b)$ where $F_t$; the proportion of dye faded after t hour exposure. $F_v$; the proportion of dye faded after t hour exposure, when a pattern is judged by visual method $C_0$; initial dye concentration. b; constant. also, the reason for increasing lightfastness with dye concentration was discussed on view of the above equation.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.