• Title/Summary/Keyword: chemical and morphological changes

Search Result 128, Processing Time 0.02 seconds

Relationship between morphology and viscosity of the main culture broth of Cephalosporium acremonium M25

  • Kim Jong Chae;Lim Jung Soo;Kim Jung Mo;Kim Chongyoup;Kim Seung Wook
    • Korea-Australia Rheology Journal
    • /
    • v.17 no.1
    • /
    • pp.15-20
    • /
    • 2005
  • In this study, the relationship between morphology and viscosity of the main culture broth of Cephalosporium acremonium M25 was investigated in a 2.5 L bioreactor. The differentiation of C. acremonium M25 showed a complex pattern during the main culture. The morphological changes of C. acremonium M25 were related to the rheological properties of the culture broth and it was well agreed with the power law model. As a result of rheology study, it was found that rheological properties of the main culture broths of C. acremonium M25 in bioreactor were closely related to morphological changes. Also, fractal dimension fairly predicted morphological and rheological changes in the main culture broth.

Effect of Structural and Morphological Changes on the Conductivity of Stretched PANI-DBSA/HIPS Film

  • Lee, Jong-Hyeok;Kim, Eun-Ok
    • Bulletin of the Korean Chemical Society
    • /
    • v.32 no.8
    • /
    • pp.2661-2665
    • /
    • 2011
  • We studied the effect of structural and morphological changes on the conductivity of a stretched conducting polymer film. To improve the poor processability of polyaniline, we used dodecylbenzenesulfonic acid as both a surfactant and a dopant during emulsion polymerization, followed by blending with high-impact polystyrene. UV-Vis/NIR spectra were obtained to observe conformational changes, and SEM and AFM were used to investigate morphological changes. FT-IR dichroism was applied to determine the microscopic orientation, and XRD patterns were obtained for quantitative crystallinity analysis. The electrical conductivity (${\sigma}_{\parallel}/{\sigma}_{\perp}$) was measured as a function of draw ratio. We found a clear correlation between morphological changes and (${\sigma}_{\parallel}/{\sigma}_{\perp}$), especially at the stretching limit. The conductivity of the films can be modified according to the desired application by controlling their structure and morphology.

The Effect of Electron Beam Irradiation on Chemical and Morphological Properties of Hansan Ramie Fibers

  • Lee, Jung Soon
    • Fashion & Textile Research Journal
    • /
    • v.15 no.3
    • /
    • pp.430-436
    • /
    • 2013
  • The purpose of this study investigates the effects of electron beam(EB) irradiation on the chemical and morphological properties of Hansan ramie fiber. Hansan ramie fibers were irradiated with electron beam doses of 0, 1, 3, 5 and 10kGy. The effect of electron beam irradiation on the chemical components of fibers as well as the surface chemical and morphological properties were investigated using chemical component analysis methods based on TAPPI standards, XPS, and SEM. The results indicate that the surface layers can be removed under suitable EB irradiation doses. Alcohol-benzene extraction and lignin content increases gradually with an increase in EB irradiation and reaching a maximum at an EB dose of 3kGy, and decreases at 10kGy. The surface chemical changes measured by XPS corresponded to the chemical composition analysis results. The C1 peak and the O/C ratio decreased with the removal of the multi-layer and primary layer by EB irradiation. The SEM images show the inter-fibrillar structure etched by EB irradiation up to 5kGy. At 10kGy, the surface structure of the ramie fiber shows highly aligned and distinctive striations in a longitudinal direction. The removal of these exterior layers of the fiber was confirmed by changes in surface morphology as observed in SEM images.

Morphological and rheological properties of culture broth of Cephalosporium acremonium M25

  • Lim, Jung-Soo;Kim, Jin-Hee;Kim, Chongyoup;Kim, Seung-Wook
    • Korea-Australia Rheology Journal
    • /
    • v.14 no.1
    • /
    • pp.11-16
    • /
    • 2002
  • Cephalosporium acremonium is a filamentous microorganism producing cephalosporin C. The morphological differentiation of C. acremonium in submerged culture is closely related with the rheological properties of culture broth and production of cephalosporin C. In this study, the rheological and morphological properties of culture broth of C. acremonium were investigated. In the seed broths of shake-flask and fermenter culture, the Herschel-Berkley equation was in excellent agreement with experimental results in the whole range of shear rate. In the seed broths of shake-flask culture, morphological differentiation into arthrospores affected to changes of apparent viscosity. But results in the fermenter culture, morphological factors such as mean hyphal thickness and the number of tips gave more effect on changes of apparent vitacosity than differentiation into arthrospores. Overall, it suggested that the morphological parameters measured by image analysis can be used as a good parameter to indicate the rheological properties of culture broth of C. acremonium M25.

Relationship Between Fractal Dimension and Morphological Features of Cephalosporium acremonium M25 in a 30-1 Bioreactor Culture

  • Lim Jung-Soo;Kim Jung-Mo;Kim Jong-Chae;Kim Chang-Ho;Yang Dae-Ryook;Chang Hyo-Ihl;Kim Seung-Wook
    • Journal of Microbiology and Biotechnology
    • /
    • v.15 no.5
    • /
    • pp.971-976
    • /
    • 2005
  • In a 30-1 bioreactor culture, whole differentiation occurred from 48 h, and then proceeded rapidly. As swollen hyphal fragments and arthrospores increased, cephalosporin C (CPC) production increased exponentially to $1.85\;g/1^{-1}$ at 72 h. To explain the morphological changes of Cephalosporium acremonium M25 more quantitatively, specific differentiation rates and fractal analysis were employed. Specific differentiation rates of morphological factors varied greatly during the period of culture time from 48 h to 72 h, when CPC production increased significantly. Changes of fractal dimensions showed a pattern similar to that of the specific rate of arthrospores. Furthermore, it was inversely related to the specific rate of tips. Overall, it was suggested that the fractal dimension had potential for a new morphological parameter of fungal morphology, showing complex differentiation patterns.

Analysis of Chemical and Morphological Changes of Phenol Formaldehyde-based Photoresist Surface caused by O2 Plasma

  • Shutov, D.A.;Kang, Seung-Youl;Baek, Kyu-Ha;Suh, Kyung-Soo;Min, Nam-Ki;Kwon, Kwang-Ho
    • Transactions on Electrical and Electronic Materials
    • /
    • v.8 no.5
    • /
    • pp.211-214
    • /
    • 2007
  • Chemical and morphological changes of phenol formaldehyde-based photoresist after $O_2$ radiofrequency(RF) plasma treatment depending on exposure time and source power were investigated. It was found that etch rate of photoresist sharply increased after discharge turn on and reached a limit with increase in plasma exposure time. Contact angle measurements and X-ray photoelectron spectroscopy(XPS) analysis showed that the surface chemical structure become nearly constant after 15 sec of the treatment. Atomic force microprobe(AFM) measurements were shown that surface roughness was increased with plasma exposure time.

Effects of Kneading Treatment on the Properties of Various Pulp Fibers (Kneading 처리가 다양한 펄프 섬유들의 특성에 미치는 영향)

  • Kim, Ah-Ram;Choi, Kyoung-Hwa;Cho, Byoung-Uk
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.47 no.3
    • /
    • pp.47-54
    • /
    • 2015
  • In this study, effects of kneading treatment on the properties of hardwood bleached kraft pulp (HwBKP), softwood bleached kraft pulp (SwBKP) and hardwood bleached chemi-thermo-mechanical pulp (HwBCTMP) were elucidated with a laboratory two-shaft kneader. Kneading treatment was performed at 30% (w/w) of pulp concentration and the number of passes through the kneader was adjusted from 0 to 10 passes. Then, changes in properties of pulp fibers were evaluated. It was found that fiber characteristics were influenced by kneading treatment. Fiber length was decreased with kneading while other morphological properties such as fiber width, curl and kink became increased as the number of passes through the kneader increased from 0 to 5 passes. The magnitude of changes in the morphological properties of softwood chemical pulp was the largest, followed by hardwood chemical pulp. The morphological properties of HwBCTMP were little influenced by kneading treatment. Swelling of fiber measured by WRV was increased with kneading except of HwBCTMP.

Chemical and micromorphological changes of archaeological waterlogged wood degraded in marine situations. (해양에서 열화된 완도선 수침고목재의 화학적.미시형태적 변화)

  • Kim, Ik-Joo
    • 보존과학연구
    • /
    • s.11
    • /
    • pp.87-105
    • /
    • 1990
  • Chemical and micro morphological changes of archaeological waterlogged woods from shipwrecked materials in marine situations were investigated which were submerged in seabed for over 900 years. Tested Wood species were Pinusdensiflora, Zelkova serrata, Quercus acutissima and Camellia japonica. The obtained results were summarized as follows; Chemical analysis showed that lignin content was increased, whereas the amout of holocellulose was heavily decreased in the degraded archaeological lwoods(DAW), when compared to the recent woods. The amount of alkalineextractives in the DAW was extremley high. IR spectra showed that disappearance of absortion band at $1,730㎝^-1$ intensity increase at 1,600, 1,500 and $1,270㎝^-1$ and the emergence of single band around $1,050㎝^-1$.Microscopic investigation showed that cell wall of latewood tracheids and fiber in the DAW were severely degraded while, early wood tracheids less degraded. Degradation in the cell wall was mainley occurred in $S_2$layer, while the middle lamella was the least degraded. The micro morphological characteristics of DAW were separation of secondary wall from middle lamella, cavities aligned with micro fibril angle in $S_2$layer and granular appearance of secondary wall by the bacterial attack.

  • PDF

The Synthesis and Electrochemical Properties of Lithium Manganese Oxide (Li2MnO3)

  • Seo, Hyo-Ree;Lee, Eun-Ah;Yi, Cheol-Woo;Kim, Ke-On
    • Journal of Electrochemical Science and Technology
    • /
    • v.2 no.3
    • /
    • pp.180-185
    • /
    • 2011
  • The layered lithium-manganese oxide ($Li_2MnO_3$) as a cathode material of lithium ion secondary batteries was prepared and characterized the physico-chemical and electrochemical properties. The morphological and structural changes of MnO(OH) and $Li_2MnO_3$ are closely connected to the changes of electrochemical properties. The crystallinity of $Li_2MnO_3$ is enhanced as the annealing temperature increase, but its capacity is reduced due to the easier structural changes of less crystalline $Li_2MnO_3$ than highly crystalline one. Moreover, the addition of buffer material such as MnO(OH) into cathode causes to reduce the morphological and structural changes of layered $Li_2MnO_3$ and increase the discharge capacity and cycleability.

Spherulitic Morphologies of Poly(ethylene terephthalate), Poly(ethylene 2,6-naphthalate), and Their Blend

  • Lee, Jong-Kwan;Lee, Kwang-Hee;Jin, Byung-Suk
    • Macromolecular Research
    • /
    • v.10 no.1
    • /
    • pp.44-48
    • /
    • 2002
  • The supermolecular structures of poly(ethylene terephthalate) (PET), poly(ethylene 2,6-naphthalate) (PEN), and their blend were investigated with optical microscopy and small angle light scattering. With increasing the crystallization temperature, incomplete spherulitic texture was developed for the PET samples. At a high crystallization temperature of 220 $^{\circ}C$, the light scattering pattern represented a random collection of uncorrelated lamellae. The general morphological appearances for the PEN samples were similar to that of the PET. A notable feature was that the spherulites of the PEN formed at 200 $^{\circ}C$ showed regular concentric bands arising from a regular twist in the radiating lamellae. The spherulitic morphology of the PET/PEN blend was largely influenced by the changes of the sequence distribution in polymer chains determined by the level of transesterifcation. The increased sequential irregularity in the polymer chains via transesterification caused a morphological transition from a regular folded crystallite to a tilted lamellar crystallite.