Development of the Carbide Reinforced Ni-Grain Roll (탄화물 강화 Ni-Grain Roll개발)

  • Suh Y. C.;Chung B. H.;Lee H. C.;Kim Y. K.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2004.08a
    • /
    • pp.223-230
    • /
    • 2004
  • In order to improve the productivity and quality of the hot rolled products, many morden mills have continuously required advanced roll materials. The introduction of HSS rolls in early stands of the Hot Strip Mill brought the excellent performance in wear resistance and surface roughness. Ni-grain rolls used in the later stands was needed to improve the roll performance. Therefore, the carbide reinforced Ni-grain roll was developed. The present paper will describe the development of carbide reinforced rolls made by INI STEEL and the results of mill tests. The wear resistance was increased upto $40\%$ and the anti-accident ablility was remarkably improved compared to the normal Ni-rain roll.

  • PDF

Mechanical Behavior of Indentation Stress in Carbon Fiber Reinforced Silicon Carbide Composites with Different Densities (서로 다른 밀도를 갖는 탄소섬유강화 탄화규소 복합재료의 압흔응력에 의한 기계적 거동)

  • Lee, Kee-Sung;Kim, Il-Kyum;Kim, Tae-Woo;Kim, Se-Young;Han, In-Sub;Woo, Sang-Kuk
    • Journal of the Korean Ceramic Society
    • /
    • v.48 no.4
    • /
    • pp.288-292
    • /
    • 2011
  • In this study, we investigated the mechanical behavior of carbon fiber reinforced silicon carbide composites by indentation stress. Relatively porous and dense fiber reinforced ceramic composites were fabricated by liquid silicon infiltration (LSI) process. Densification of fiber composite was controlled by hardening temperature of preform and consecutive LSI process. Load-displacement curves were obtained during indentation of WC sphere on the carbon fiber reinforced silicon carbide composites. The indentation damages at various loads were observed, and the elastic modulus were predicted from unloading curve of load-displacement curve.

Development of a Drill Tool for CFRP Machining and Evaluation of Drilling Processing (탄소섬유 강화 복합재 가공용 드릴 공구 개발 및 홀 가공성 평가)

  • Sa, Min-Woo
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.19 no.3
    • /
    • pp.8-13
    • /
    • 2020
  • Carbon fiber-reinforced plastics (CFRPs) are extremely strong and light fiber-reinforced plastics containing carbon fibers. CFRPs can be expensive to produce, but are commonly used wherever high strength-to-weight ratio and rigidity are required, such as in the aerospace, automotive, and ship superstructure industries. In CFRP drilling, the tool performance greatly varies depending on the tool shapes, cutting conditions, and diamond coating. This study developed a new type of tungsten carbide drill with multi-blade edges to evaluate the surface quality of CFRP materials according to the coating thickness of diamond-coated drills. Experiments on tool wear, surface roughness, and burr formation were conducted. The bore exit quality of a 12 mμ -coated drill was better than that of a 6 mμ -coated drill. The superior effects of the 12 mμ -coated drill and the good surface quality of CFRP were also demonstrated.

Preparation of Self-reinforced Silicon Carbide Ceramics by Hot Pressing (가압소결에 의한 자체강화 탄화규소 세라믹스의 제조)

  • Park, Jong-Gon;Lee, Jong-Kook;Seo, Dong-Seok;Kim, Min-Jeong;Lee, Eun-Gu;Kim, Hwan
    • Journal of the Korean Ceramic Society
    • /
    • v.36 no.12
    • /
    • pp.1356-1363
    • /
    • 1999
  • Self-reinforced silicon carbide was prepared by hot pressing and the control of starting phases of raw materials and its microstructural characteristics was investigated. The specimens with self-reinforced microstructure were obtained from the compacts with mixed compositions of ${\alpha}$-and ${\beta}$-SiC powders. Self-reinforced microstructure which is composed of large dispersed grains with rod-like shape and matrix with small equiaxed grains was formed by the transformation to the ${\alpha}$-SiC with 4H polytype for ${\beta}$-SiC and anisotropic grain growth during the heat treatment. Of all speimens the values of volume fraction maximum length and aspect ratio for large grains with rode-like types were the highest at the specimen with 50 vol% ${\beta}$-SiC in the starting SiC powder and therefore this specimen showed the highest fracture toughness due to the crack deflection by rod-like grains during crack propagation.

  • PDF

Effects of Interface Boundary Strength on Wear and Wear Transition during Sliding in Silicon Carbide Ceramics (탄화규소계 세라믹스에서 미끄럼시의 마모 및 마모천이에 미치는 계면강도의 영향)

  • Kim, Dong-Jin;Park, Seong-Khil;Ryu, Hyun;Um, Chang-Do;Cho, Seong-Jai;Kim, Seock-Sam
    • Tribology and Lubricants
    • /
    • v.11 no.4
    • /
    • pp.21-27
    • /
    • 1995
  • The effects of interface boundary strength on wear and wear transition during sliding have been investigated in silicon carbide ceramics. Three different microstructures, i.e., solid state sintered silicon carbide, liquid phase sintered silicon carbide and liquid phase sintered silicon carbide composite reinforced with TiB$_{2}$ particulates, were designed by hot pressing. Examinations of crack patterns and fracture modes indicated that interface boundaries were relatively strong between silicon carbide grains in the solid state sintered silicon carbide, intermediate in the liquid phase sintered silicon carbide and weak between silicon carbide grains and TiB$_{2}$ particles in the composite. Wear data and examinations of worn surfaces revealed that the wear behavior of these silicon carbide ceramics could be significantly affected by the interface strength. In the solid state sintered silicon carbide, the wear occurred by a grooving process. In the liquid phase sintered silicon carbide and composite, on the other hand, an abrupt transition in wear mechanism from initial grooving to grain pull-out process occurred during the test. The transition occurred significantly earlier in the composite than in the carbide.

Abrasion Wear Behavior of Recycled Tungsten Carbide Reinforced Metal Matrix Composite (재생 초경합금 분말을 활용한 금속기지 복합재료의 Abrasion 마모거동)

  • Kang, Nam-Hyun;Chae, Hyun-Byung;Kim, Jun-Ki;Choi, Jong-Ha;Kim, Jeong-Han
    • Korean Journal of Materials Research
    • /
    • v.13 no.12
    • /
    • pp.850-854
    • /
    • 2003
  • The abrasion wear behavior on the hardfacing weld was investigated by performing abrasion wear, hardness, and microstructural tests. The gas metal arc(GMA) weld was produced by using the cored wire which was filled with the hard metal, i.e., the recycled tungsten carbide (WC) reinforced metal matrix composite. For 30% addition of the hard metal, the abrasion wear resistance was significantly improved comparing with that for 20% addition of the hard metal. Above 30% addition of the hard metal, however, there was no significant improvement of the wear resistance. The improvement of the wear resistance was due to the increased amount of eutectic carbides(W$_{6}$C) which was formed during GMA welding. For the weld in which the hard metal was added to 30-40%, an optimum level of abrasion wear resistance was performed.

Preparation and Application of Fiber Composites made of Carbon Nanofibers and Carbide Nanofibers (나노탄소섬유와 나노카바이드섬유를 이용한 복합재의 제조와 활용에 관한 연구)

  • 임연수;김기덕;이재춘;김명수;김성수
    • Journal of the Korean Ceramic Society
    • /
    • v.37 no.6
    • /
    • pp.569-575
    • /
    • 2000
  • Fabrication of carbon fiber reinforced composites was carried out by hand lay-up method. Carbon nanofibers and SiC nanofibers were used as filler in the composites fabrication. Carbon nanofibers, one of the new carbon materials, have 5∼500 nm in diameter and 5-10 nm in length. SiC nanofibers were modified by silicon monoxide vapor with carbon nanofibers. The composites were carbonized at 1000$^{\circ}C$ in a nitrogen atmosphere, and then densified by molten pitches impregnated in vacuum. Multiple cycles of liquid pitch impregnation and carbonization were carried out to obtain a desired density. The composites were characterized by density, microstructure. The inter-laminar shear strength (ILSS) test was performed for mechanical properties. For the new application, the microwave reflective proeprty of composites was investigated. Dielectric constant and permeability spectrum were measured in 12∼18 GHz frequency ranges. On the basis of the wave propagation theory in a lossy media, the reflection loss from the composite inter-layer was predict as a function of frequency.

  • PDF

Comparison of TiAlN DLC and PCD Tool Wear in CFRP Drilling (CFRP 드릴링에서 TiAlN DLC 코팅과 PCD의 공구마모 비교)

  • Baek, Jong-Hyun;Kim, Su-Jin
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.21 no.5
    • /
    • pp.77-83
    • /
    • 2022
  • A high-hardness tool material is required to reduce extreme abrasive wear when drilling carbon fiber reinforced plastic (CFRP). Single-crystal diamond is the hardest material in the world, but it is very expensive to be used as a cutting tool. Polycrystalline diamond (PCD) is a diamond grit fused at a high temperature and pressure, and diamond-like carbon (DLC) is an amorphous carbon with high hardness. This study compares DLC coatings and PCD inserts to conventional TiAlN-coated tungsten carbide drills. In fiberglass and carbon fiber reinforced polymer drilling, the tool wear of DLC-coated carbide was approximately half that of TiAlN-coated tools, and slight tool wear occurred in the case of PCD insert end drills.

Studies on Effects of Deposition Parameters in Manufacturing of C/Sic composites by Pulse-CVI (C/SiC 복합재료 제조시 Pulse-CVI에서 증착변수의 영향 연구)

  • 김용탁;김영준;정귀영
    • Proceedings of the Korean Society For Composite Materials Conference
    • /
    • 2001.10a
    • /
    • pp.141-143
    • /
    • 2001
  • Ceramic fiber-reinforced composites have good mechanical properties in hardness and durability. In this study, we studied the formation of SiC/C composites from methyltrichlorosilane and hydrogen by the Pulse-chemical vapor infiltration(PCVI) to deposit silicon carbide around the changes of the amount of deposit. SiC/C composites formed at $950^{\circ}C$, 20torr, Pulse-times (5s/60s). SEM of the cross sectional area of semple showed deposited silicon carbide around fibers.

  • PDF

The Effect of Heat Treatment on the Microstructures and Mechanical Properties of Inconel 713C Alloy Vacuum Investment Castings (진공 정밀주조한 Inconel 713C 합금의 조직과 기계적 성질에 미치는 열처리의 영향)

  • Yoo, Byung-Ki;Choi, Hak-Kyu;Park, Heung-Il;Jeong, Hae-Yong
    • Journal of Korea Foundry Society
    • /
    • v.40 no.2
    • /
    • pp.16-24
    • /
    • 2020
  • The effect of a heat treatment on the microstructure and mechanical properties of Inconel 713C alloy vacuum investment castings were investigated. The microstructure of the as-cast state was observed, showing well-developed dendrite structures and distributed carbide particles and solidified massive precipitates in the grain or grain boundary during solidification, in this case the γ′ phase and MC particles. During a heat treatment, the γ phase matrix was reinforced by solid solution elements, carbide particles from the film morphology precipitated along the grain boundary, and many micro-precipitates of second γ′ phases 0.2 ㎛~2 ㎛ in size were newly formed in the γ phase matrix according to SEM-EDS analysis results. The tensile strength at a high temperature (850℃) decreased slightly becoming comparable with the room-temperature result, while the hardness value of the specimen after the vacuum heat treatment increased by approximately 19%, becoming similar to that of the as-cast condition. However, the impact values at room temperature and low temperature (-196℃) were approximated; this alloy was mostly not affected by an impact at a low temperature. In the observations of the fracture surface morphologies of the specimens after the tensile tests, the fractures at room temperature were a mix of brittle and ductile fractures, and an intergranular fracture in the inter-dendrite structure and some dimples in the matrix were observed, whereas the fractures at high temperatures were ductile fractures, with many dimples arising due to precipitation. It was found that a reinforced matrix and precipitates of carbide and the γ′ phase due to the heat treatment had significant effects, contributing greatly to the excellent mechanical properties.