• 제목/요약/키워드: butt joint

검색결과 269건 처리시간 0.023초

조선 적용을 위한 하이브리드 레이저 용접 캐리지 개발 (Development of the Hybrid Laser Welding Carriage for Shipbuilding)

  • 신정현;이윤식;류상훈;성희준
    • 한국레이저가공학회지
    • /
    • 제11권3호
    • /
    • pp.21-24
    • /
    • 2008
  • Hybrid laser welding technology is a good process to reduce a thermal distortion and increase the productivity. However, it requires a high investment and a massive modification of the fabrication line such as a gantry system, milling machine for the edge preparation, high power laser system and weld machine. Therefore the development of an economical laser welding system is a crucial point to apply this system in shipbuilding yard. In this study, a portable hybrid laser welding carriage was developed for I-butt joint without edge milling. It is expected that the carriage type system could reduce investment cost.

  • PDF

레일 용접부의 경도와 마멸특성에 관한 실험적 연구 (Experimental Study on Hardness and Wear Characteristics of Welded Rails)

  • 김청균;황준태;나성훈;민경주
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1998년도 제28회 추계학술대회
    • /
    • pp.234-243
    • /
    • 1998
  • In this paper, thermite and gas pressure weldings have been used to join rails in-track and analyzed as functions of hardness and wear characteristics. The wear rate of thermite welded rail is low compared with that of gas pressure welded rail, which is tested in a pin-on-disk wear tester. The hardness of thermite welded materials is relatively high and narrow distributed between three zones, welded part, thermally affected zone, and a base matrix. Wear of a welded rail may be a major factor in railroad maintenance costs and failures at the rail-rail butt joint.

  • PDF

용접공정 및 용접형상 변화에 따른 소구경 분기배관 용접부의 피로특성 (Fatigue Properties of the Small Diameter Branch Welded Pipe Joint with variation of Welding Procedures and Welding Shapes.)

  • 백종현;김철만;김우식
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2003년도 추계학술발표대회 개요집
    • /
    • pp.191-193
    • /
    • 2003
  • S-N fatigue tests were conducted to investigate the fatigue strength of the small diameter socket and butt welded joints of carbon steels. Experimental parameters were pipe diameter, throat depth, shape of socket welds and welding procedure. Filler metals used in SMAW and GTAW procedure were E9016-G with diameter of 4.0 mm and ER70S-G with diameter of 2.4 m. API 5L Gr.B pipes were adopted as a small diameter branch pipes. All socket fittings were machined from ASTM A105 carbon steel. Fatigue strength in socket weld joints increased with increasing pipe diameter, area of weld metal and weld leg length of pipe side.

  • PDF

잔류응력 완화를 고려한 공칭응력 기반 용접재의 피로수명 평가 모델 (Fatigue Life Evaluation Model for Welded feints Based on Nominal Stress and Residual Stress Relaxation)

  • 구병춘;양승용;정흥채;최성규
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2004년도 춘계 학술발표대회 개요집
    • /
    • pp.249-251
    • /
    • 2004
  • According to our fatigue tests carried out at 20 ㎐, R=0.1 on transversely butt-welded joints, fatigue strengths of as-welded specimens, that is, specimens having residual stress are higher than those of annealed specimens in short hie range, but vice verse in long life range. This behavior seems to be concerned mainly with residual stress relaxation by applied loading. After analyzing the welding process, we conducted finite element analysis to quantify the degree of residual stress relaxation. By taking into account residual stress relaxation, modified Goodman diagram, and nominal stress, we evaluated the fatigue life of the welded joint from the S-N curve for the parent material. The estimated results are in a good agreement with the experimental results.

  • PDF

An in-vitro investigation of microleakage of sandwich restorations with flow able liner in class II cavaties with cervical margins in dentine

  • Lee, Kang;Hong, Chan-Ui
    • 대한치과보존학회:학술대회논문집
    • /
    • 대한치과보존학회 2001년도 추계학술대회(제116회) 및 13회 Workshop 제3회 한ㆍ일 치과보존학회 공동학술대회 초록집
    • /
    • pp.586.1-586
    • /
    • 2001
  • Large butt-joint box typed class II cavites with cervical margins 1mm below the cemento-enamel junction were cut into 70 extracted human molars. The cavities(7 groups, n=10) were filled using a closed/open sandwich restoration or total bond restoration technique with materials according to the manufacturer's recommandation using the single-component bonding agent for each system. Teeth were thermocycled 500 times between $5^{\circ}C$ and $55^{\circ}C$ with 30-second dwell times.(omitted)

  • PDF

마찰교반접합한 알루미늄 합금과 스테인리스 강 이종접합부 계면 조직 및 접합부 강도 (Interface Analysis and Mechanical Properties of Friction Stir Welded Dissimilar joints between Stainless steel and AI alloy)

  • 이원배;이창용;연윤모;정승부
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2005년도 추계학술발표대회 개요집
    • /
    • pp.189-191
    • /
    • 2005
  • Dissimilar joining of AI 6013-T4 alloys and austenite stainless steel was carried out using friction stir welding technique. Microstructures near the weld zone and mechanical properties of the joint have been investigated. Microstructures in the stainless steel side and AI alloy were depended on the thermo-mechanical condition which they received. TEM micrographs revealed that the interface region was composed of the mixed layers of elongated stainless steel and ultra-fine grained AI alloy and intermetallic compound layer which was identified as the $Al_{4}Fe$ with hexagonal close packed structure. Mechanical properties were lower than those of 6013 AI alloy base metal, because tool inserting location was deviated to AI alloy from the butt line, which resulted in the lack of the stirring.

  • PDF

로봇 레이저용접을 위한 캐드캠 인터페이싱에 관한 연구 (Study on CAD/CAM Interfacing for Robot based Laser Welding)

  • 강희신;서정;김정오;박경택;조택동
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2007년 추계학술발표대회 개요집
    • /
    • pp.67-69
    • /
    • 2007
  • Laser welding technology for automobile body is studied. Laser system, robot and seam tracking system are used for 3D laser welding system. The laser system is used 4kW Nd:YAG laser(HL4006D) of Trumpf and the robot system is used IRB6400R of ABB. The seam tracking system is SMRT-20LS of ServoRobot. The welding joints of steel plate are butt and lap joint. The 3 dimensional laser welding for non-linear pipe welding line is performed.

  • PDF

304 스테인레스 스틸의 마찰교반접합 (Friciton stir welding of type 304 stainless steel)

  • 이창용;최돈현;표성은;이원배;이종봉;연윤모;정승부
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2007년 추계학술발표대회 개요집
    • /
    • pp.158-160
    • /
    • 2007
  • The butt and lap configurational friction stir welding of type 304 stainless steel was conducted in this study. The sound joints were obtained by WC tool. As the welding distance increased, tool deformation gradually increased at the pin edge. The discoloration by oxidation was observed at the top surface of the joint, a sufficient heat-input was required to avoid the welding defect owing to the lack of stirring at the welding start point. Very fine grains were observed in the stir zone, and the grain coarsening was not observed in the heat affected zone.

  • PDF

Computer Simulation에 의한 비정질 변압기의 코어 형상 설계 (Core design of amorphous transformer by computer simulation)

  • 우병철;정순종;송재성;최형식;황시돌;신판석
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1994년도 하계학술대회 논문집 A
    • /
    • pp.57-59
    • /
    • 1994
  • The transformer core using amorphous Fe-B-Si ribbon were designed by magnetostatic software. The basic model of core is Butt-Lap-Step type, non-culled typo and stair type core joint. And the variables are the number of ribbons for on step, flux density and core shape.

  • PDF

후육 고강도 Al 2519합금의 FSW 접합기술 및 접합부 특성(II) (FSW Process Optimization for Al 2519 Alloys and Its Joint Characteristics(II))

  • 김흥주;장웅성;양광하;방한서
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2005년도 춘계학술발표대회 개요집
    • /
    • pp.174-176
    • /
    • 2005
  • On the basis of successful experiences and data from author's past experimental results of friction stir welding on thin aluminum plates, thick aluminum plate of high strength 2000 series has been carried out in this study. For various combination of rotating speed, welding speed and tool (RIWRC38-C) shape, the butt welded specimens has been prepared to check the metallurgical characteristics, hardness distributions and defects. From the results, feasible welding conditions have been obtained as 450 rpm rotating speed and 5 mm/min welding speed. Using these optimum welding parameters, 38.1mm-thickness A2519-T87 plates have been FSWelded in single pass. A good weld surface appearance and defects free weld zone has been observed in X-ray inspection. Softened region has been generated by dissolution of precipitates and coarsened microstructure in the stir zone after FSWeld.

  • PDF