Study on the Effects of Single Fiber Tensile Properties on Bundle Tensile Properties through Estimation of HVI Bundle Modulus and Toughness

  • Koo, Hyun-Jin;Jeong, Sung Hoon;Suh, Moon W.
    • Fibers and Polymers
    • /
    • 제2권1호
    • /
    • pp.144-147
    • /
    • 2001
  • The HVI properites and Mantis single fiber tensile properties were analyzed to evaluate the relationship between fiber and bundle tensile properties. For this study, a new method has been developed for estimating the modulus and toughness of cotton fiber bundles directly from the HVI tenacity-elongation curves. The single fiber tensile properties were shown to be translated well into the bundle tensile properties. The single fiber breaking elongation was found to be the most significant contributing factor to bundle tensile properties. The bundle breaking elongation and toughness were shown to increase as the single fiber breaking elongation increased. The bundle modulus increased as the single fiber breaking elongation and/or standard deviation of single fiber breaking elongation decreased.

  • PDF

링 정방공정에서 단사제조에 의한 공정특성 분석 (Analysis of Process Characteristics by Single Yarn Production in Ring Spinning)

  • Lee, Choon-Gil;Oh, Bong-Hyo;Park, Sung-Diuk
    • 한국염색가공학회지
    • /
    • 제9권5호
    • /
    • pp.1-9
    • /
    • 1997
  • In the single yarn spinning process by the ring spinning system, the finer the fineness of yarn and the lower the twist coefficient, the lower the breaking strength and breaking elongation. The change of yarn specific volume to yarn number agreed with Peirce's formula in the range of Ne 50 to 70, but above that range the values of the experiment are higher than that of the formula. The change of diameter of yarn to the reciprocal of the square root of yarn number agreed with Peirce's formula in the range of under 0.14, but above that value the values of the experiment are higher than that of the formula. In breaking strength variation according to twist constant of single yarn, as the twist coefficient increased, breaking strength increased. At 5.8∼6.0 of twist coefficient the maximum breaking strength was shown, but above that value breaking strength decreased. Breaking elongation also showed a similar tendency. But at 6.0∼6.5 of twist coefficient the maximum breaking elongation was shown. Also spinning tension increased as twist coefficient increased. Twist coefficient, breaking strength and breaking elongation according to the number of coils stayed almost the same. Yarn spinning tension according to the number of coils at the maximum of diameter was the lowest value. The speed of the traveller at the maximum of diameter was the highest value.

  • PDF

견사의 탄성적성질에 관한 연구 II. 인장속도 및 팽윤에 따른 파괴강신도의 변화 (Reological Studies on Cocoon Filament II. Changes of strength and elongation at breaking related to the stretching speed and swelling degree)

  • 남중희
    • 한국잠사곤충학회지
    • /
    • 제14권2호
    • /
    • pp.105-112
    • /
    • 1972
  • 팽윤견사를 수중에서 인장시킬 경우, 인장속도 및 팽윤정도의 차이가 견사의 하중신장곡선에 미치는 영향을 조사하였다. 인장시험은 Tensilon을 사용하였고, 절단시 강도, 신도 및 인장저항도를 조사한바 다음과 같은 결과를 얻었다. 1. 팽윤견사의 절단강도는 인장속도의 증가와 더부러 높아지나 절단신도는 감소하였다. 2. 견사를 팽윤(90$^{\circ}$, 15분)시켜 저속(4mm/분)으로 인장하면 견사의 macrofibril의 분리절단상태가 chart 상에 기록되었다. 3. 9$0^{\circ}C$로 장시간 팽윤처리(60분)하면 절단강도는 현저히 감소하고, 절단신도는 증가의 경향을 보였다. 4. 초기인장저항도는 인장속도 및 팽윤정도의 차이에 의하여 영향된다. 즉 고속인장은 초기인장저항도를 높이지만 팽윤도의 증가는 감소시켰다.

  • PDF

옥외 노출시험에 의한 PBS 단일섬유 망사의 내구성 변화 (The Durability of Polybutylene Succinate Monofilament for Fishing Net Twines by Outdoor Exposure Test)

  • 박성욱;김성훈;임지현;최혜선
    • 수산해양교육연구
    • /
    • 제25권4호
    • /
    • pp.766-774
    • /
    • 2013
  • Biodegradable polybutylene succinate(PBS) is a kind of environmentally friendly plastics for fisheries, because it can mitigate the ghost fishing problem caused by gill-net and trap fisheries. To evaluate durability of PBS monofilament, each of different diameter 3 types of monofilaments were spun and exposed to 56 month outdoor and then their gravity, modification of surface, breaking strength, and elongation were analysed. The gravity of PBS monofilament was estimated to be approximately 1.24 when spinning ratio from 4.8 to 6.1. PBS monofilaments did not show any crack after 56 month exposed to outdoor and load-elastic elongation curve was showed sigmoid type. Decreasing ratio of elongation was appeared in the thinnest monofilament 0.2mm diameter and breaking strength was in the thickest monofilament 0.4mm diameter. Breaking strength and elongation at break were decreased rapidly after 48 month exposed to outdoor. Breaking strength reduced linearly after 48 month exposure, while no such linear relationship was found in the case of elongation at break. In results, it was investigated that the durability of PBS monofilament nets for gillnet and trap were 24, 50 month when keep to land, respectively.

생체내 이식된 흡수성 봉합사들의 물리적 성질 변화와 조직 소견에 관한 연구 (The Mechanical Appearances and Microscopic Tissue Reactions of the Suture Materials in vivo)

  • 김남중;김명철
    • 한국임상수의학회지
    • /
    • 제13권2호
    • /
    • pp.184-194
    • /
    • 1996
  • A comparative study of three absorbable suture materials of chromic catgut, Dexon II (a polyglycolic acid suture with a polycaprolate coating system) and Coated Vicryl (a polyglactin 910 suture with a glycolide-lactide-calcium stearate coating system) was undertaken in terms of tensile strength, breaking elongation, appearances of the suture materials in the subcutaneous layer of rats and of tissue reaction in the intramuscular layer of rats. The initial tensile strength of chromic catgut and the tensile strength after 21 days were about 1.55 kg and 0.19 kg, respectively. Those of Dexon II were about 2.01 kg and 0. 20 kg, respectively. Those of Coated Vicryl were about 2.39 kg and 0.48 kg, respectively. Coated Vicryl showed the highest tensile strength among the three materials during the whole period. On the other hand, Dexon II showed the highest breaking elongation among the three materials during the first week. But the breaking elongation of Dexon II rapidly continuously decreased during the whole period. The appearances of the suture materials in the subcutaneous layer of rats showed that chromic catgut was the fastest among the three materials, whereas it formed comparatively much connective tissue. The intramuscular absorption rate and tissue reaction of Dexon II were similar to those of Coated Vicryl. The intramuscular absorption rate of these was fairly late when compared with chromic catgut. And the tissue reaction appearance of these showed the formation of a granuloma with foreign body giant cells, macrothages and epitheloid cells by the 28th day in the experimental period.

  • PDF

A Study on the Mechanical Change of Emulsion-Treated Hair by Color

  • Ko, Hee-Ja;Park, Jang-Soon
    • 한국염색가공학회지
    • /
    • 제34권2호
    • /
    • pp.127-133
    • /
    • 2022
  • With the increasing interest in the expression of individuality and appearance of modern people, it is time to conduct research and development of novel hair coloring from various angles. Therefore, taking into account the order of discoloration of hair pigments, we selected a creative and novel emulsion as a novel material for hair coloring, rather than a cosmetic material such as hot water extract using natural products dealt with in previous studies, commercially available hair manicure, and oxidation hair dye for hair. Thus, the change in tensile strength and elongation of hair samples by color was studied. As a result of the study, hair with green emulsion paint had a significantly higher maximum load, maximum stress, maximum elongation and breaking load, breaking stress, breaking elongation values are shown. Maximum in terms of modulus, green emulsion applied hair and the control group were higher in the 0-15s strain and 15-145s sections, respectively, and the tangential modulus value was much higher in the control group than the experimental group hairs in all the 0-145s sections. This study, which analyzes the dynamic changes of hair samples that extend the daily color gamut, will greatly contribute to the development of innovative hair coloring materials in the research and production of hair beauty works, and it is judged that it will also contribute to the development of the beauty industry.

용융방사에 의한 생분해성 PBS/PBAT 블랜드 모노 필라멘트 제조 및 물리적 특성 (Preparation and physical properties of biodegradable polybutylene succinate/polybutylene adipate-co-terephthalate blend monofilament by melt spinning)

  • 박성욱;김성훈;최혜선;조현혹
    • 수산해양기술연구
    • /
    • 제46권3호
    • /
    • pp.257-264
    • /
    • 2010
  • In order to improve the breaking strength and elongation of Polybutylene succinate (PBS) monofilament, the monofilament was produced by blending PBS and Polybutlyne adipate-co-terephthalate (PBAT). The PBS/PBAT blend monofilament was prepared by the melt spinning system, and the weight ratios of the compositions of PBS/PBAT was 100/0, 95/5, 90/10 and 85/15, respectively. The breaking strength, elongation, softness and crystallization of PBS/PBAT blend monofilament were analyzed by using a tensionmeter, softness measurement, X-ray diffractometer in the both dry and wet conditions. The PBS/PBAT blend monofilaments were spun in the take-up velocity of 1.19m/sec under the drawing ratio of 6.8:1 condition. The production volumes of PBS/PBAT blend monofilaments showed 20% less than that of Nylon. The breaking strength of PBS/PBAT blend monofilaments were decreased as PBAT contents increased, while elongation and softness were increased. In case of PBAT content were over 5%, the breaking strength, elongation and softness of PBS/PBAT blend monofilaments were not shown to increase in spite of increasing in PBAT contents. Based on these results, it was possible to make the monofilaments with the maximized physical properties when the PBAT contents at 5%.

미류나무 잎절편체 조직배양을 통한 식물체 재분화에 미치는 요인 (Factors influencing Adventitious Shoot induction from Leaves of Populus deltoides Bartr)

  • 신동일;설일환
    • 생명과학회지
    • /
    • 제7권2호
    • /
    • pp.134-141
    • /
    • 1997
  • 미류나무 잎절편 조직배양에 의한 식물체 재분화에 관한 여러 가지 여인을 조사한 결과를 요약하면 다음과 같다. 1. 5가지 각기 다른 농도를 가진 培地에 줅,절편을 치상하여 側牙의 발달을 유기시킨 결과, WPM이 MS배지 보다 더 좋은 반응을 보였고 또한 배지내의 NH$_{4}$NO$_{3}$의 양은 측아 증식에 큰 영향을 미치지 않는 것으로 관찰되었다. 2. 기내에서 증식된 잎을 3부분으로9윗, 중간 그리고 및) 절단하여 2종류의 식물성장 절물질(TDZ와NAA)의 16가지의 농도배합을 사용하여 배양한 결과 TDZ0.01mg/1와 NAA 0.02 mg/1에서 가장 높은 부정줄기 형성체들이 생성되었다. 또한 잎의 윗 부분 보다는 중간과 밑부분에서 높은 부정줄기 형성체들이 생성되었는 것을 관찰하였다. 3. 3가지 탄수화물을 사용하여 부정줄기의 유기를 관찰한 바, sucrose 나 glucose보다 fructose를 첨가한 배지에서 좋은 반응을 보여 주었다.

  • PDF

백모(白毛) 커버(cover)용 화학염모제 처리 모발의 미용학적 분석 (For white Hair Cover for Chemical Hair Dye Treated Hair Cosmetic Analysis)

  • 오정선;박장순
    • 한국융합학회논문지
    • /
    • 제10권6호
    • /
    • pp.281-286
    • /
    • 2019
  • 현대인에게 외모는 경쟁력의 수단이며 이러한 현대인의 욕구에 위해요소로 작용하는 요인 중 하나는 백모(白毛)이다. 백모를 커버하여 타인에게 아름다운 외모를 표출해야 하는 현대인을 위하여 백모 염모제 시술 후 모발분석을 실시하였다. 실험결과 1N-3N 화학염모제의 control 대조군과 1N부터 3N 실험군 간에 최대하중, 최대 인장 강도, 최대 신장률, 파단하중, 파단강도, 파단 신장률, 평가구간에 따른 최대 모듈러스 및 tangential modulus가 대체적으로 유의적인 차이를 보였다. 최대 하중과 최대 인장강도, 파단 하중과 파단 강도가 대조군에 비해 커다란 경향을 보인 반면 최대 신장률과 파단 신장률은 대조군이 가장 큰 값으로 실험군 처리에 따라 신장률이 감소하였다. 평가구간에 따른 최대 모듈러스와 tangential modulus는 대조군에 비해 1N-3N 실험군들이 0~0.15와 0.15~2.5 등 모든 strain 구간에서 대체적으로 높게 나타났다. 백모 커버용 산화염모제의 시술 전후 모발의 미용학적 변화에 대한 연구를 바탕으로 올바른 화학염모제 제품의 선택, 적당한 도포량 및 방치시간 등을 효과적으로 선택할 수 있는 기초자료로 활용되리라 사료된다.

Solo-spun 방적에서 섬유의 거동과 사의 물리적 성질(1) (The Fiber Behavior in Yarn Formation and the Physical Properties of Solo-spun Yarn(1))

  • 박수현;김승진
    • 한국염색가공학회지
    • /
    • 제13권5호
    • /
    • pp.58-58
    • /
    • 2001
  • This study surveys the fiber behavior in yarn formation and the physical properties of Solo-spun yarn. The specimens were made by six types of Solo-spun rollers with fixed twist multiplier. The physical properties such as yarn count, evenness, strength, and breaking elongation of these yarns were compared with the properties of ring spun yarns and analysed with the mechanism of Solo-spun yarn formation. The grooves on the surface of Solo-spun roller divide the web and interfere the twist propagation. These phenomena cause the uneven draft and the fly of fiber, so the Solo-spun yarn becomes finer than fing-spun yarn and the yarn breaking strength and elongation deteriorate, but these demerits can be improved with rounding the protruded edge of Solo-spun roller grooves.