  • Background Several bone grafting materials have been used in sinus augmentation procedures. Macroporous Biphasic Calcium Phosphate($MBCP^{TM}$) consists of the mixture of 60% HA and 40% ${\beta}-TCP$. Therefore, it can provide good scaffold for the new bone to grow owing to HA, in the other hand, it can have bioactivity for bone remodeling owing to ${\beta}-TCP$. The purpose of this study was to evaluate bone formation following maxillary sinus augmentation using $MBCP^{TM}$ by means of histologic analysis. Material and Method $MBCP^{TM}$ was placed as a primary bone substitute for maxillary sinus augmentation. Three patients were selected after evalaution of their medical dental examination. $MBCP^{TM}$ only, $MBCP^{TM}$ combined with Irradicated cancellous bone and $MBCP^{TM}$ combined with autogenous bone were used for each patient. After about eight months, bone biopsies were harvested for histologic evaluation and fixtures installed. Results Eight months after surgery we observed new vital bone surrounding $MBCP^{TM}$ particle and the amount of new bone was about 30% even though there were discrepancies between specimens. This case report documents that $MBCP^{TM}$ when used as a grafting material for sinus floor augmentation whether combined other bone graft material or not, may lead to the predictable results for dental implants on posterior maxillary area with insufficient vertical height for fixture installation.

Analysis of Organic Components and Osteoinductivity in Autogenous Tooth Bone Graft Material

  • Kim, Young-Kyun;Lee, Junho;Kim, Kyung-Wook;Um, In-Woong;Murata, Masaru;Ito, Katsutoshi
    • Maxillofacial Plastic and Reconstructive Surgery
    • /
    • 제35권6호
    • /
    • pp.353-359
    • /
    • 2013
  • Purpose: Extensive research is actively ongoing for development of an ideal bone substitute that meets the gold standard. Tooth was selected as a donor site for evaluation of potentials in bone substitutes based on its similar chemical compositions to alveolar bone. Previous studies have evaluated inorganic components of autogenous tooth bone graft material (AutoBT) and osteoconductivity. In continuation from the previous studies, the current study was conducted for analysis of organic components and evaluation of osteoinductivity of AutoBT. Methods: Forty-six extracted teeth were collected from actual patients (Korea Tooth Bank, R&D Institute). Extracted teeth were processed into AutoBT and implanted in dorsal subcutaneous muscular tissues of 15 athymic mice. Biopsy samples were harvested at two, five, and eight weeks. The Bradford assay, sodium dodecyl sulphate polyacrylamide gradient gel, and western blotting were performed for investigation of organic contents of AutoBT. Results: Histology analyses showed signs of new bone formation as early as two weeks. Results of the Bradford assay indicated the existence of noncollagenous proteins (NCP). 0.29% (2.89 mg/g) of proteins were extracted by weight in the root portion of AutoBT; 0.02% (0.029 mg/g) and 1.79% (17.93 mg/g) of proteins were measured by weight in crown and block-form of AutoBT, respectively. However, recombinant human bone morphogenetic protein-2 was not observed in AutoBT. Conclusion: Within the limitation of the current study, AutoBT induced new bone formation by NCP embedded in dentin.

Bone Healing Capacity of Demineralized Dentin Matrix Materials in a Mini-pig Cranium Defect

  • Kim, Jong-Yub;Kim, Kyung-Wook;Um, In-Woong;Kim, Young-Kyun;Lee, Jeong-Keun
    • Journal of Korean Dental Science
    • /
    • 제5권1호
    • /
    • pp.21-28
    • /
    • 2012
  • Purpose: In this study the bone healing ability of autogenous tooth bone graft material as a substitute material was evaluated in a mini-pig cranial defect model through histologic examinations and osteonectin reverse transcription polymerase chain reaction (RT-PCR) quantitative analysis. Materials and Methods: A defect was generated in the cranium of mini-pigs and those without a defect were used as controls. In the experimental group, teeth extracted from the mini-pig were manufactured into autogenous tooth bone graft material and grafted to the defect. The mini-pigs were sacrificed at 4, 8, and 12 weeks to histologically evaluate bone healing ability and observe the osteonectin gene expression pattern with RT-PCR. Result: At 4 weeks, the inside of the bur hole showed fibrosis and there was no sign of bone formation in the control group. On the other hand, bone formation surrounding the tooth powder granule was observed at 4 weeks in the experimental group where the bur hole was filled with tooth powder. Osteonectin gene expression; there was nearly no osteonectin expression in the control group while active osteonectin expression was observed from 4 to 12 weeks in the experimental group. Conclusion: We believe this material will show better results when applied in a clinical setting.

탄산아파타이트로 된 인공골과 소뼈에서 유래한 무기질 골의 초기 골전도에 대한 연구 (A STUDY ABOUT EARLY OSTEOCONDUCTIVITY OF POROUS ALLOPLASTIC CARBONAPATITE AND ANORGANIC BOVINE XENOGRAFT IN CANINE MAIXLLIARY AUGMENTATION MODEL)

  • 김도균;조태형;송윤미;판휘;이수연;진임건;김인숙;홍국선;황순정
    • Maxillofacial Plastic and Reconstructive Surgery
    • /
    • 제29권6호
    • /
    • pp.485-493
    • /
    • 2007
  • Introduction: Although several types of calcium-phosphate coumpound have been frequently applied to osseous defects at maxillofacial area for many years, there is a controversy about its efficiency on bone conductivity comprared to xenograft bone substitute. Alloplastic carbonapatite has been introduced to improve disadvantages of hydroxyapatite and to mimic natural bone containing carbon elements. However, a preclinical study about its efficiency of osteoconductivity has not been reported. This study was performed to evaluate the early osteoconductive potential of synthetic carbonapatite with multiple pores relative to anorganic bovine xenograft. Materials and methods: Total 5 beagle dogs were used for maxillary augmentation model. The control (anorganic bovine xenograft) and experimental groups (synthetic carbonapatite) were randomly distributed in the mouth split design. After bone graft, all animals were sacrificed 4 weeks after surgery. Histological specimens with Masson Trichrome staining were made and histomorphometrically analysed with image analyser. The statistical analysis was performed using paired t-test. Results: In both groups, all animals had no complications. The experimental group showed relatively much new bone formation around and along the bone substitutes, whereas it was clearly reduced in the control group. The ratios of new bone area to total area, to material area and to the residual area excluding materials were higher in the experimental group ($0.13{\pm}0.03,\;0.40{\pm}0.13,\;0.20{\pm}0.06$ respectively) than in the control group ($0.01{\pm}0.01,\;0.03{\pm}0.02,\;0.03{\pm}0.03$, respectively). And the differences between both groups were statistically significant (p<0.001, <0.01, <0.01, respectively), while the ratio of material area to total area in two groups was not significant. Conclusion: Carbonapatite showed a high osteoconductivity in the early stage of bone healing compared to bovine derived anorganic bone substitute. This study suggests that this bone materials can be applied as a reliable bone substitute in the clinical treatment.

가토의 두개골에 이식한 진피 아교기질(AlloDerm®)이 골 재생에 미치는 효과 (The Effects of Bone Regeneration of the Dermal Collagen Matrix(AlloDerm®) Graft in the Rabbit Calvarium)

  • 박상우;이경석;김준식
    • Archives of Plastic Surgery
    • /
    • 제32권3호
    • /
    • pp.335-342
    • /
    • 2005
  • This study was undertaken to investigate possibility of the allogenic type I collagen inducing osteoinduction or osteoconduction at critical sized bone defect in the rabbit. Twenty Newzealand white rabbit, weighted from 2.8 kg to 3.5 kg, were used in this study. The skull was exposed and two bony defects were created with diameter of 10 mm. Group I(n=10), the bony defects was grafted from the other side bone. Group II(n=10), the bony defects was grafted by the allogenic type I collagen with bone morphogenic protein(BMP). Group III(n=10), the bony defects was grafted by the allogenic type I collagen only. Group IV(n=10), the bony defects was lefted with no grafts. The grafted bones and allogenic type I collagen were investigated with radiologic densitometry, histologic analysis and immunohistochemistry after 12 weeks. No major difference was observed in the gross finding between Group I, II, III, but dura mater was exposed in bony defect,the Group IV. The radiologic study demonstrated more bony opacity in the Group I, but the other groups did not demonstrate a significant difference. In the histologic study, grafted bone edge was completely consolidated with original bone in group I and new bone ingrew into the grafted allogenic type I collagen(group II, III),but there is no bone regeneration from the original bony edge in the group IV. The percent of the new bone formation by cross-sectional area was considered statistically significant at a p value of less than 0.05(p<0.05). In the immunohistochemistry study about BMP antibodies, the group IV demonstrated osteogenic activity in front of advancing original bone edge, in which the osteoblast stained strongly for BMP antibodies, but other group does not demonstrated any osteoblastic expression. There was no immunologic rejection. In conclusion, this results do not demonstrate that the allogenic type I collagen is useful for bone substitute, but the characters of the collagen, such as pliability, easy-handling, sponge-like structure, are useful in interpositional bone graft substitutes. The further evaluation of long term results about the resorption, immunologic tissue reaction, response of applied tissue growth factor to the allogenic collagen is needed.

The effects of hard and soft tissue grafting and individualization of healing abutments at immediate implants: an experimental study in dogs

  • Thoma, Daniel S.;Jung, Ui-Won;Gil, Alfonso;Kim, Myong Ji;Paeng, Kyeong-Won;Jung, Ronald E.;Fickl, Stefan
    • Journal of Periodontal and Implant Science
    • /
    • 제49권3호
    • /
    • pp.171-184
    • /
    • 2019
  • Purpose: To evaluate the effects of intra-alveolar socket grafting, subepithelial connective tissue grafts, and individualized abutments on peri-implant hard and soft tissue outcomes following immediate implant placement. Methods: This randomized experimental study employed 5 mongrel dogs, with 4 sites per dog (total of 20 sites). The mesial roots of P3 and P4 were extracted in each hemimandible and immediate dental implants were placed. Each site was randomly assigned to 1 of 4 different treatment groups: standardized healing abutment (control group), alloplastic bone substitute material (BSS) + standardized healing abutment (SA group), BSS + individualized healing abutment (IA group), and BSS + individualized healing abutment + a subepithelial connective tissue graft (IAG group). Clinical, histological, and profilometric analyses were performed. The intergroup differences were calculated using the Bonferroni test, setting statistical significance at P<0.05. Results: Clinically, the control and SA groups demonstrated a coronal shift in the buccal height of the mucosa ($0.88{\pm}0.48mm$ and $0.37{\pm}1.1mm$, respectively). The IA and IAG groups exhibited an apical shift of the mucosa ($-0.7{\pm}1.15mm$ and $-1.1{\pm}0.96mm$, respectively). Histologically, the SA and control groups demonstrated marginal mucosa heights of $4.1{\pm}0.28mm$ and $4.0{\pm}0.53mm$ relative to the implant shoulder, respectively. The IA and IAG groups, in contrast, only showed a height of 2.6mm. In addition, the height of the mucosa in relation to the most coronal buccal bone crest or bone substitute particles was not significantly different among the groups. Volumetrically, the IA group ($-0.73{\pm}0.46mm$) lost less volume on the buccal side than the control ($-0.93{\pm}0.44mm$), SA ($-0.97{\pm}0.73mm$), and IAG ($-0.88{\pm}0.45mm$) groups. Conclusions: The control group demonstrated the most favorable change of height of the margo mucosae and the largest dimensions of the peri-implant soft tissues. However, the addition of a bone substitute material and an individualized healing abutment resulted in slightly better preservation of the peri-implant soft tissue contour.

In vitro assay for osteoinductive activity of different demineralized freeze-dried bone allograft

  • Vaziri, Shahram;Vahabi, Surena;Torshabi, Maryam;Hematzadeh, Somayeh
    • Journal of Periodontal and Implant Science
    • /
    • 제42권6호
    • /
    • pp.224-230
    • /
    • 2012
  • Purpose: Various bone graft materials have been used for periodontal tissue regeneration. Demineralized freeze-dried bone allograft (DFDBA) is a widely used bone substitute. The current widespread use of DFDBA is based on its potential osteoinductive ability. Due to the lack of verifiable data, the purpose of this study was to assess the osteoinductive activity of different DFDBAs in vitro. Methods: Sarcoma osteogenic (SaOS-2) cells (human osteoblast-like cells) were exposed to 8 mg/mL and 16 mg/mL concentrations of three commercial types of DFDBA: Osseo+, AlloOss, and Cenobone. The effect of these materials on cell proliferation was determined using the 3-[4,5-dimethylthiazol-2-yl]-2,5-diphenyltetrazolium bromide assay. The osteoinductive ability was evaluated using alizarin red staining, and the results were confirmed by evaluating osteogenic gene expression using reverse transcription polymerase chain reaction (RT-PCR). Results: In the SaOS-2 cells, an 8 mg/mL concentration of Osseo+ and Cenobone significantly increased cell proliferation in 48 hours after exposure (P<0.001); however, in these two bone materials, the proliferation of cells was significantly decreased after 48 hours of exposure with a 16 mg/mL concentration (P<0.001). The alizarin red staining results demonstrated that the 16 mg/mL concentration of all three tested DFDBA induced complete morphologic differentiation and mineralized nodule production of the SaOS-2 cells. The RT-PCR results revealed osteopontin gene expression at a 16 mg/mL concentration of all three test groups, but not at an 8 mg/mL concentration. Conclusions: These commercial types of DFDBA are capable of decreasing proliferation and increasing osteogenic differentiation of the SaOS-2 cell line and have osteoinductive activity in vitro.

마이크로웨이브법에 의해 제조된 HAp 및 BCP 분말이 뼈모세포 및 파골세포의 활성에 미치는 영향 (The Effects of HAp and BCP Nano Powders Synthesized by Microwave-Assisted Synthesis on the Activation of Osteoblast and Osteoclast)

  • 송호연;민영기;양훈모;맹주양
    • 한국재료학회지
    • /
    • 제17권12호
    • /
    • pp.669-675
    • /
    • 2007
  • Hydroxyapatite (HAp) and biphasic calcium phosphate (BCP) nano powders were synthesized using the microwave-assisted synthesis process dependent on pH and microwave irradiation time. The average size of a powder was less than 100 nm in diameter. Through in-vitro cytotoxicity tests by an extract dilution method, the HAp and BCP nano powders have shown to be cytocompatible for L-929 fibroblast cells, osteoblastlike MG-63 cells and osteoclast-like Raw 264.7 cells. The activation of osteoblast was estimated by alkaline phosphatase (ALP) activity. When the HAp and BCP were treated to MG-63 cells, alkaline phosphatase activities increased on day 3, compared with those of the untreated cells. Also, the collagen fibers increased when the HAp and BCP powders suspension were treated to MG-63 cells, compared to those of the untreated cells. Quantitative alizarin red S mineralization assays showed a trend toward increasing mineralization in osteoblast cultured with powder suspension. In conclusion, hydroxyapatite and biphasic calcium phosphate appeared to be a bone graft substitute material with optimal biocompatibility and could be further applied to clinical use as an artificial bone graft substitute.

뼈 충진재용 생분해성 다공질 Calcium Phosphate 세라믹스의 제조 (Preparation of Biodegradable Porous Calcium Phosphate Ceramics for Bone Fillers)

  • 이중환;김석영
    • 대한의용생체공학회:학술대회논문집
    • /
    • 대한의용생체공학회 1996년도 춘계학술대회
    • /
    • pp.130-132
    • /
    • 1996
  • It is well known when porous calcium phosphate ceramics are used as a bone graft substitute, new tissues or blood vessels are grown into the porous implant due to their excellent biocompatibility. In this study, the ${\beta}$-crystalline form of calcium metaphosphate, $Ca(PO_{3})_{2}$ is prepared by the controlled thermolysis of monocalcium phosphate, $Ca(H_{2}PO_{4})_{2}$. The diameter of cylindrical pores formed during cooling was controlled by a holding time at the melting point of a monocalcium phosphate and by the change of a recrystallization temperature, to obtained the most appropriate size (about $200{\mu}m$) of pores. It was observed that the increasing holding time at the melting point of monocalcium phosphate results in the decreases of pore sizes.