• 제목/요약/키워드: bioceramic materials

검색결과 46건 처리시간 0.025초

Designing Materials for Hard Tissue Replacement

  • Nath, Shekhar;Basu, Bikramjit
    • 한국세라믹학회지
    • /
    • 제45권1호
    • /
    • pp.1-29
    • /
    • 2008
  • In last two decades, an impressive progress has been recorded in terms of developing new materials or refining existing material composition/microstructure in order to obtain better performance in biomedical applications. The success of such efforts clearly demands better understanding of various concepts, e.g. biocompatibility, host response, cell-biomaterial interaction. In this article, we review the fundamental understanding that is required with respect to biomaterials development, as well as various materials and their properties, which are relevant in applications, such as hard tissue replacement. A major emphasize has been placed to present various design aspects, in terms of materials processing, of ceramics and polymer based biocomposites, Among the bioceramic composites, the research results obtained with Hydroxyapatite (HAp)-based biomaterials with metallic (Ti) or ceramic (Mullite) reinforcements as well as $SiO_2-MgO-Al_2O_3-K_2O-B_2O_3-F$ glass ceramics and stabilized $ZrO_2$ based bioinert ceramics are summarized. The physical as well as tribological properties of Polyethylene (PE) based hybrid biocomposites are discussed to illustrate the concept on how can the physical/wear properties be enhanced along with biocompatibility due to combined addition of bioinert and bioactive ceramic to a bioinert polymeric matrix. The tribological and corrosion properties of some important orthopedic metallic alloys based on Ti or Co-Cr-Mo are also illustrated. At the close, the future perspective on orthopedic biomaterials development and some unresolved issues are presented.

Characterization and Evaluation of Porous Vermiculite Containing Polyethylene Composites Film

  • Lee, Hye Sun;Chang, Jeong Ho
    • 한국세라믹학회지
    • /
    • 제55권1호
    • /
    • pp.85-89
    • /
    • 2018
  • This work reported the preparation and evaluation of a freshness-keeping film prepared by composite of a porous ceramic material such as vermiculite and polyethylene polymer. The ceramic material was pretreated physically and chemically to control the specific surface areas and particle size. A high content master-batch was prepared using the pretreated vermiculite. The master-batch, which contained 30% ceramic material, was mixed with a polymer material to prepare a film containing 3% vermiculite. The oxygen permeability and various physicochemical properties were evaluated for the prepared films. Compared to plain polyethylene film, the vermiculite loaded polyethylene film has a freshness maintenance property, indicating the creation of an improved film.

Bacterial leakage and micro-computed tomography evaluation in round-shaped canals obturated with bioceramic cone and sealer using matched single cone technique

  • Yanpiset, Kallaya;Banomyong, Danuchit;Chotvorrarak, Kanet;Srisatjaluk, Ratchapin Laovanitch
    • Restorative Dentistry and Endodontics
    • /
    • 제43권3호
    • /
    • pp.30.1-30.12
    • /
    • 2018
  • Objectives: To evaluate sealing ability of root canals obturated with bioceramic-impregnated gutta percha cone (BCC) or gutta percha (GP), with bioceramic sealer (BCS) or AH Plus (AH; Dentsply-Maillefer), in roundly-prepared canals using matched single-cone technique, based on bacterial leakage test, and to analyze obturation quality using micro-computed tomography (CT) analysis. Materials and Methods: Ninety-two distobuccal roots of maxillary molars were prepared using nickel-titanium files to apical size 40/0.06. The roots were divided into 4 groups (n = 20) that were obturated with a master cone and sealer: GP/AH, BCC/AH, GP/BCS, and BCC/BCS. Bacterial leakage model using Enterococcus faecalis was used to evaluate sealing ability for 60-day period. Obturated samples from each group (n = 4) were analyzed using micro-CT. Results: All groups showed bacterial leakage at 20%-45% of samples with mean leakage times of 42-52 days. There were no significant differences in bacterial leakage among the groups. Micro-CT showed minimal gaps and voids in all groups at less than 1%. Conclusions: In roundly-prepared canals, the single cone obturation with BCC/BCS was comparable to GP/AH for bacterial leakage at 60 days.

Comparative analysis of bond strength to root dentin and compression of bioceramic cements used in regenerative endodontic procedures

  • Maykely Naara Morais Rodrigues;Kely Firmino Bruno;Ana Helena Goncalves de Alencar;Julyana Dumas Santos Silva;Patricia Correia de Siqueira;Daniel de Almeida Decurcio;Carlos Estrela
    • Restorative Dentistry and Endodontics
    • /
    • 제46권4호
    • /
    • pp.59.1-59.14
    • /
    • 2021
  • Objectives: This study compared the Biodentine, MTA Repair HP, and Bio-C Repair bioceramics in terms of bond strength to dentin, failure mode, and compression. Materials and Methods: Fifty-four slices obtained from the cervical third of 18 single-rooted human mandibular premolars were randomly distributed (n = 18). After insertion of the bioceramic materials, the push-out test was performed. The failure mode was analyzed using stereomicroscopy. Another set of cylindrically-shaped bioceramic samples (n = 10) was prepared for compressive strength testing. The normality of data distribution was analyzed using the Shapiro-Wilk test. The Kruskal-Wallis and Friedman tests were used for the push-out test data, while compressive strength was analyzed with analysis of variance and the Tukey test, considering a significance level of 0.05. Results: Biodentine presented a higher median bond strength value (14.79 MPa) than MTA Repair HP (8.84 MPa) and Bio-C Repair (3.48 MPa), with a significant difference only between Biodentine and Bio-C Repair. In the Biodentine group, the most frequent failure mode was mixed (61%), while in the MTA Repair HP and Bio-C Repair groups, it was adhesive (94% and 72%, respectively). Biodentine showed greater resistance to compression (29.59 ± 8.47 MPa) than MTA Repair HP (18.68 ± 7.40 MPa) and Bio-C Repair (19.96 ± 3.96 MPa) (p < 0.05). Conclusions: Biodentine showed greater compressive strength than MTA Repair HP and Bio-C Repair, and greater bond strength than Bio-C Repair. The most frequent failure mode of Biodentine was mixed, while that of MTA Repair HP and Bio-C Repair was adhesive.

Investigations on the effects of mouthrinses on the colour stability and surface roughness of different dental bioceramics

  • Soygun, Koray;Varol, Osman;Ozer, Ali;Bolayir, Giray
    • The Journal of Advanced Prosthodontics
    • /
    • 제9권3호
    • /
    • pp.200-207
    • /
    • 2017
  • PURPOSE. In this study, three bioceramic materials, [IPS Empress CAD (Ivoclar), IPS e.max CAD (Ivoclar), and Lava Ultimate CAD (3M ESPE)] were treated with three commercial mouthrinses [Listerine, Tantum Verde, and Klorhex]; and changes in colour reflectance and surface roughness values were then quantitatively assessed. MATERIALS AND METHODS. One hundred and twenty ceramic samples, with dimensions of $2{\times}12{\times}14mm$, were prepared and divided into nine sample groups, except three control samples. The samples were immersed in the mouthrinse solutions for 120 hrs, and changes in colour reflectance and surface roughness values were measured by UV light spectrophotometry (Vita Easyshade; VITA Zahnfabrik) and by profilometer device (MitutoyoSurftest SJ-301), respectively. The change of surface roughness was inspected by Scanning Electron Microscopy (SEM) and Atomic Force Microscopy (AFM). RESULTS. There was a positive correlation between the ${\Delta}E$ and increase in the surface roughness. Two of the ceramic materials, IPS Empress and Lava Ultimate, were affected significantly by the treatment of the mouthrinse solutions (P<.05). The most affecting solution was Tantum Verde and the most affected material was Lava Ultimate. As expected, the most resistant material to ${\Delta}E$ and chemical corrosion was IPS e max CAD among the materials used. CONCLUSION. This work implied that mouthrinse with lower alcohol content had less deteriorating effect on colour and on the surface morphology of the bioceramic materials.

Nanostructured Hydroxyapatite for Biomedical Applications: From Powder to Bioceramic

  • Eslami, Hossein;Tahriri, Mohammadreza;Moztarzadeh, Fathollah;Bader, Rizwan;Tayebi, Lobat
    • 한국세라믹학회지
    • /
    • 제55권6호
    • /
    • pp.597-607
    • /
    • 2018
  • In this study, a wet chemical method was used to synthesize nanostructured hydroxyapatite for biomedical applications. Diammonium hydrogen phosphate and calcium nitrate 4-hydrate were used as starting materials with a sodium hydroxide solution as an agent for pH adjustment. Scanning electron microscopy, transmission electron microscopy, Fourier-transform infrared spectroscopy, differential thermal analysis, thermal gravimetric analysis, atomic absorption spectroscopy, and ethylenediaminetetraacetic acid (EDTA) titration analysis were used to characterize the synthesized powders. Having been uniaxially pressed, the powders formed a disk-like shape. The sinterability and electrical properties of the samples were examined, and the three-point bending test allowed for the measurement of their mechanical properties. Sedimentation analysis was used to analyze the slurry ability of hydroxyapatite. As in-vitro biological properties of the samples, biocompatibility and cytotoxicity were assessed using osteoblast-like cells and the L929 cell line, respectively. Solubility was assessed by employing a simulated body fluid.

무균돼지뼈를 이용한 복합 골지지체의 제조와 생체적합성 평가 (Preparation and Biocompatibility of Composite Bone Scaffolds Using Gnotobiotic Pig Bones)

  • 임애리;정종훈;임기택;정필훈;홍지향
    • Journal of Biosystems Engineering
    • /
    • 제32권1호
    • /
    • pp.50-56
    • /
    • 2007
  • Highly porous composite bioceramic bone scaffolds were developed using sintered gnotobiotic pig bones. These scaffolds consisted of poly-D,L-lactic acid (P(D,L)LA) and bioceramic materials of pig bone powder. The bone scaffolds were able to promote biocompatibility and possess interconnected pores that would support cell adhesion and proliferation adequately. The composite scaffolds were tested with dental pulp stem cells for cytotoxicity test. Cells seeded on the composite scaffolds were readily attached, well proliferated, as confirmed by cytotoxicity test, and cell adhesion assessment. The composite bone scaffold had no toxicity in cytotoxicity test on the extract of 0.013 g scaffold to 2 ml culture medium. The cells on the composite bone scaffold proliferated better than cells on the P(D,L)LA scaffolds.

A micro-computed tomographic study of remaining filling materials of two bioceramic sealers and epoxy resin sealer after retreatment

  • Kim, KyungJae;Kim, Da Vin;Kim, Sin-Young;Yang, SungEun
    • Restorative Dentistry and Endodontics
    • /
    • 제44권2호
    • /
    • pp.18.1-18.9
    • /
    • 2019
  • Objective: This study evaluated the presence of residual root canal filling material after retreatment using micro-computed tomography (micro-CT). Materials and Methods: Extracted human teeth (single- and double-rooted, n = 21/each; C-shaped, n = 15) were prepared with ProFile and randomly assigned to three subgroups for obturation with gutta-percha and three different sealers (EndoSeal MTA, EndoSequence BC sealer, and AH Plus). After 10 days, the filling material was removed and the root canals were instrumented one size up from the previous master apical file size. The teeth were scanned using micro-CT before and after retreatment. The percentage of remaining filling material after retreatment was calculated at the coronal, middle, and apical thirds. Data were analyzed using the Kruskal-Wallis test and Mann-Whitney U test with Bonferroni post hoc correction. Results: The tested sealers showed no significant differences in the percentage of remaining filling material in single- and double-rooted teeth, although EndoSeal MTA showed the highest value in C-shaped roots (p < 0.05). The percentage of remaining filling material of AH Plus and EndoSeal MTA was significantly higher in C-shaped roots than in single- or double-roots (p < 0.05), while that of BC sealer was similar across all root types. EndoSeal MTA showed the highest values at the apical thirds of single- and double-roots (p < 0.05); otherwise, no significant differences were observed among the coronal, middle, and apical thirds. Conclusions: Within the limitations of this study, a large amount of EndoSeal MTA remained after retreatment, especially in C-shaped root canals.

Synthesis and Densification of Nanostructured $Al_2O_3-(Zro_2+3%Mol\;Y_2O_3)$ Bioceramics by High-Frequency Induction Heat Sintering

  • Kim, Sug-Won;Khalil, Khalil Abdel-razek
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.527-528
    • /
    • 2006
  • Nanostructured Alumina - 20 vol% 3YSZ composites powder were synthesized by wet-milling technique. The starting materials were a mixture of Alumina micro-powder and 3YSZ nano-powders. Nano-crystalline grains were obtained after 24 h milling time. The nano-structured powder compacts were then processed to full density at different temperatures by high-frequency induction heat sintering (HFIHS). Effects of temperature on the mechanical and microstructure properties have been studied. $Al_2O_3-3YSZ$ composites with higher mechanical properties and small grain size were successfully developed at relatively low temperatures through this technique.

  • PDF