• 제목/요약/키워드: backlight

검색결과 533건 처리시간 0.022초

Luminous Characteristics of Transparent Field Emitters Produced by Using Ultra-thin Films of Single Walled Carbon Nanotubes

  • Jang, Eun-Soo;Goak, Jeung-Choon;Lee, Han-Sung;Lee, Seung-Ho;Lee, Nae-Sung
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2009년도 춘계학술발표대회
    • /
    • pp.31.1-31.1
    • /
    • 2009
  • Carbon nanotubes (CNTs) are attractive material because of their superior electrical, mechanical, and chemical properties. Furthermore, their geometric features such as a large aspect ratio and a small radius of curvature at tip make them ideal for low-voltage field emission devices including backlight units of liquid crystal display, lighting lamps, X-ray source, microwave amplifiers, electron microscopes, etc. In field emission devices for display applications, the phosphor anode is positioned against the CNT emitters. In most case, light generated from the phosphor by electron bombardment passes through the anode front plate to reach observers. However, light is produced in a narrow depth of the surface of the phosphor layer because phosphor particles are big as much as several micrometers, which means that it is necessary to transmit through the phosphor layer. Hence, a drop of light intensity is unavoidable during this process. In this study, we fabricated a transparent cathode back plate by depositing an ultra-thin film of single walled CNTs (SWCNTs) on an indium tin oxide (ITO)-coated glass substrate. Two types of phosphor anode plates were employed to our transparent cathode back plate: One is an ITO glass substrate with a phosphor layer and the other is a Cr-coated glass substrate with phosphor layer. For the former case, light was radiated from both the front and the back sides, where luminance on the back was ~30% higher than that on the front in our experiments. For the other case, however, light was emitted only from the cathode back side as the Cr layer on the anode glass rolled as a reflecting mirror, improving the light luminance as much as ~60% compared with that on the front of one. This study seems to be discussed about the morphologies and field emission characteristics of CNT emitters according to the experimental parameters in fabricating the lamps emitting light on the both sides or only on the cathode back side. The experimental procedures are as follows. First, a CNT aqueous solution was prepared by ultrasonically dispersing purified SWCNTs in deionized water with sodium dodecyl sulfate (SDS). A milliliter or even several tens of micro-liters of CNT solution was deposited onto a porous alumina membrane through vacuum filtration. Thereafter, the alumina membrane was solvated with the 3 M NaOH solution and the floating CNT film was easily transferred to an ITO glass substrate. It is required for CNT film to make standing CNTs up to serve as electron emitter through an adhesive roller activation.

  • PDF

유리관의 유전 특성이 외부전극 형광램프에 미치는 영향 (Influence of Glass Dielectric Property on the External Electrode Fluorescent Lamps)

  • 신명주;정종문;김정현;김가을;이미란;유동근;구제환;홍병희;최은하;조광섭
    • 한국진공학회지
    • /
    • 제16권5호
    • /
    • pp.330-337
    • /
    • 2007
  • 유전 장벽 방전이 특징인 외부전극 형광램프(External Electrode Fluorescent Lamp, EEFL)에서 유리재의 유전 특성인 유전상수 K와 유전손실 tan ${\delta}$가 램프에 미치는 영향을 조사하기 위하여 4 종류의 유리관을 사용하였다. 종래 일반적으로 사용되는 Borosilicate 유리재는 유전상수 $K=5.6{\sim}5.9$이고 유전 손실 tan ${\delta}=5.0{\times}10^{-3}{\sim}6.0{\times}10^{-3}$이다. Aluminosilicatae는 K=6.6이고 유전손실이 작은 tan ${\delta}=1{\times}10^{-4}$이다. Soda-lime 유리관은 유전상수가 큰 K=7.7이고, 유전 손실이 매우 큰 tan ${\delta}=1.37{\times}10^{-2}$이다. 유전 상수 K가 크면 외부전극 자체의 캐패시터를 크게 하여 방전 효율이 증가한다. 그러나 유전 손실이 크면 외부전극 자체의 전력 소모로 인하여 효율 저하와 핀홀 발생의 원인이 된다. 높은 유전상수 및 낮은 유전손실의 Aluminosilicate 외부전극 형광램프는 종래의 Borosilicate 외부전극 형광램프에 비하여 휘도와 효율이 $12{\sim}20%$ 증가하고, 핀홀에 매우 강하다. 유전상수와 유전손실이 큰 Soda-lime 외부전극 형광램프는 효율이 다소 낮고, 핀홀에도 매우 취약하다. 따라서 외부전극 형광램프는 유전상수 K가 크고 유전손실 tan ${\delta}$가 작은 유리관이 최적이다.

냉음극 형광램프의 표준화 계측을 위한 실험과 분석 (An Experiment and Analysis for Standardize Measurement on CCFL)

  • 김동준;정종문;정희석;김진선;이민규;김정현;구제환;권기청;강준길;최은하;조광섭
    • 한국진공학회지
    • /
    • 제17권4호
    • /
    • pp.331-340
    • /
    • 2008
  • 교류 $50{\sim}100\;kHz$의 고주파와 수 kV의 고전압으로 구동되는 냉음극 형광램프의 전류 및 전압을 계측하는 방법을 조사하였다. 고 전압 측에 설치되는 프로브 자체의 임피던스 영향으로 램프의 휘도가 변화하고 누설 전류가 발생하여 정확한 전류 및 전압의 계측이 어렵다. 따라서 프로브의 임피던스와 누설 전류를 고려한 회로 분석을 통하여 올바른 계측 방법을 제시하였다. 프로브 설치로 휘도 변화 시, 인버터에 입력되는 DC 전압을 조정하여 램프의 특정 휘도를 유지하여 계측한다. 램프 전류($I_G$)는 접지 측에서 전류 프로브나 고주파 전류계로 계측하며, 전압은 고 전압 측에 설치한 전압 프로브로 계측한다. 램프 전압($V_C$)은 고전압이 인가되는 냉음극과 안전 캐패시터 사이에서 계측하며, 인버터의 출력 전압(VI)은 안전 캐패시터와 인버터 출력단 사이에서 계측한다. 램프 전압($V_C$)과 램프 전류($I_G$)의 위상차가 없기 때문에, 램프 자체의 순수 소모 전력은 램프 전압($V_C$)와 램프 전류($I_G$)의 곱이다. 인버터의 출력 전압($V_I$)과 램프 전류($I_G$)의 위상차($\theta$)는 전압 프로브의 용량성 임피던스로 인하여 계측값이 부정확하며, 회로의 분석에서 얻어진 $cos{\theta}=V_C/V_I$로부터 위상차를 얻을 수 있다.