This study presents the mechanical characteristics, such as the permanent deformation and the crack, of the large stone asphalt mixtures. The large stone mixture was studied by Kandhal at NCAT(National Center for Asphalt Technology) in 1989. Japan and Arabian countries adopted the large stone mixture for the pavement construction. The experience and the study results showed that the interlocking of the aggregate system of the large stone mixtures is stable and less dependent on the binder characteristics in high temperature. These properties are known as the rutting resistant parameters. However, the mechanical test results should be supported to prove the benefits of the large stone mixtures. The creep test, resilient modulus tests on three different temperature, wheel tracking test and ravelling tests were conducted to evaluate the performance of the large stone mixtures in this study. The test results were compared with the conventional mixtures and modified asphalt concrete mixtures. The large stone mixtures showed better rutting resistance performance.
This study was carried out to select most efficient bonding methods of geogrid at the interface of old concrete pavement before placing asphalt overlay layer for reflection cracking retardation. Three bonding methods, a RSC-4 emulsified asphalt, a compound and an unsaturated polyester resin (UPR) were compared in this study. Three types of asphalt mixture (AC 60-80, RLDPE 8%, PG 76-22) and a dense-graded aggregate were used for overlay asphalt pavement. A reinforcing material which consists of a woven fabric underneath a glass fiber grid was used. An expedite test method which is for simulating mixed mode (mode I and II) fracture test was performed using a wheel tracker in laboratory. Cracking development by load repetition was measured as fatigue life (number of load cycle) and expansion of specimen body were measured for each test specimen. The results showed that UPR was the best and RSC-4 the next. But considering field applicability, RSC-4 was considered as an appropriate choice for bonding reinforcing material.
Journal of the Korean Society of Hazard Mitigation
/
v.8
no.5
/
pp.65-70
/
2008
Asphalt concrete pavements are susceptible to deformation and failure compared to cement concrete pavements. Epoxy is commonly used to enhance the bonding and durability of structures. Based on this concept, an epoxy and ceramics combined mixture was developed and applied to the field to estimate the pavement performance, Laboratory and field performance tests were conducted to observe the applicability of epoxy and ceramics composite materials compared to the conventional one. In this research, the epoxy and ceramics composite mixturewas used in two ways. 7 mm and 15 mm of thin surface layers using the mixture were constructed on cement and asphalt concrete pavements, respectively, after surface treatment. 12 months of field performance surveys were conducted to observe the resistances to the crack and deformation. According to the field performance tests, epoxy and ceramics combined mixture showed better bonding and field performances than the conventional one.
KSCE Journal of Civil and Environmental Engineering Research
/
v.3
no.1
/
pp.43-51
/
1983
The fatigue failure envelopes for the prediction of the fatigue life of asphalt pavements were obtained from the results of laboratory fatigue test for asphalt mixture. The envelopes did not depend on the experimental temperature and the number of loading, and varied with the types of asphalts. In the case of dense graded asphalt concrete, the envelopes formed a single curve regardless of the penetration of the asphalt. On the other hand, the method for the fatigue life prediction was presented based on the envelopes obtained and the triple layered elastic theory developed by Burmister.
This study was performed to evaluate the effect of various joint sealant on reducing the reflection cracking of asphalt concrete overlay on cement concrete pavement. The test method used was an accelerated reflection cracking test in shear mode, which was developed for evaluation of reflection cracking resistance of overlaid asphalt concrete in laboratory. The test results showed that use of joint sealants resulted in a significant reduction of reflection cracking. When sealant E was used, the fatigue life was the highest, with relatively larger horizontal deformation. When Sealant B was used, the dynamic stability was the highest with the smallest horizontal deformation. In general, the greater the tensile strength of sealant, the better the crack resistance of the mixture.
This study was Performed to evaluate applicability of color flexible pavement concrete (CFPC) for motorway pavement. Color flexible pavement has been applied to non-motorway pavements, such as pedestrian and bicycle road. Two polymers were used to modify the binder and to strengthen the stiffness of pavement mixture. Waste paper was used to prevent the asphalt of gap-grade mixture from draining. Marshall properties, indirect tensile strength(ITS), tensile strength ratio(TSR) before and after freezing-and-thawing treatment and artificial aging, permanent deformation and fatigue life were measured. Color bituminous concrete mixtures used this study had nearly the same quality in mechanical properties when compared with conventional asphalt concrete mixtures manufactured with AP-3 and all mixtures satisfied with domestic specification for motorway pavement. Therefore, it is proved that the color bituminous concrete used this study can be applied for motorway pavement.
Journal of the Korean Society of Hazard Mitigation
/
v.9
no.1
/
pp.57-64
/
2009
This study intends to evaluate of the characteristics of pavement deformation and develop the model for prediction model in the asphalt layer using a regression analysis. In test, there are two different asphalt binders and 5 different aggregate types. The air voids of hot mix asphalt are 6% and 10% for target value. Repeated triaxial compression test with 3 different confining pressures was used for test at 3 different test temperatures. It is going to verify the main parameters for permanent deformation of HMA and to develop the distress model. This paper is to figure out the factor affecting the pavement deformation, and then to develop model the pavement deformation for asphalt mixture. Also, the reliability of prediction model has been studied. The permanent deformation prediction model for asphalt mixtures with temperature, loading time, and air voids has been developed and the proposed permanent deformation prediction model has been validated by using the multiple regression approach which is called Statistical Package for the Social Sciences(SPSS).
Journal of the Korean Recycled Construction Resources Institute
/
v.7
no.3
/
pp.224-234
/
2019
Waterproof layers are installed in civil engineering structures and bridge construction is commonly finished by applying a layer of regular or asphalt concrete above the waterproof layer. However, asphalt materials are susceptible to melting at high temperature due to its superior temperature sensitivity, and this causes the waterproofing material to melt due to the high temperature of the asphalt concrete, thereby increasing the defect occurrence rate due to the thickness reduction. In this study, tensile strength and elongation of hard and soft type of MMA(Methyl Methacrylate) applied to bridges were compared in accordance to standard performance criteria based on different mixture ratios. Results of comparative testing showed that hard MMA resin can display a satisfactory tensile strength, and soft MMA resin displays satisfactory elongation properties, but as the two resin types are separately used, neither types are able to satisfy the standard requirements outlined in KS F 4932. When the amount of the powder exceeds 56.25% of the total amount, voids are generated on the surface after curing and self leveling was impossible and a heterogeneous surface is formed. Furthermore, when the hard resin: soft resin: powder mixture ratio was set to 15g: 85g: 150g. the tensile strength was $1.5N/mm^2$ and the elongation percentage was 133% which satisfy the tensile performance of KS F 4932.
The Construction policy of government ever since 1970s have brought the economical growth, but has been causing environmental problems. Most roads were paved either asphalt concrete or portland cement concrete. These types of pavements has caused to rise temperature by making local heat islands in urban during summer time. Recently the wet-mixing solidified soil pavement, a kind of soil-cement, has developed and has been applied to the environment-oriented pavement. The solidified soil wet-mixed is placed on the subgrade along with asphalt concrete and portland cement concrete. Thermistors are laid in these field test pavements. The temperature gradients of these pavements are automatically measured with time. As the results of this test, the equation estimating surface temperature of pavement is proposed by analyzing measured temperature data. It is shown that the temperature change within the surface layer due to the change of air temperature is the greatest in the asphalt mixture and the least in the solidified soil mixture. Since it is proven that this wet-mixing solidified soil pavement emit less radiant heat than other existed pavements. Therefore this type of pavement can be successfully applied to the roads, such as walks, parkways, and bikeways, which are required to be human-friendly and environment-oriented.
Kim, Kwang-Woo;Yim, Sung-Bin;Doh, Young-Soo;Rhee, Suk-Keun
International Journal of Highway Engineering
/
v.1
no.1
/
pp.97-106
/
1999
This study was conducted to develop a test system for evaluating resistance against reflection cracking in shear mode caused by wheel load in asphalt concrete overlaid on the deteriorated cement concrete pavement. Reflection cracking resistance of selected polymer modified asphalt(PMA) mixtures with and without reinforcement was evaluated using this test system. It was shown that the test results accounted for the effectiveness of materials and reinforcement characteristics in terms of the difference in the resistance against reflection cracking. A shear failure life of a certain mixture was estimated with a high coefficient of determination. when the test results were used in a well known prediction model. Therefore, it seemed to be possible to use this technique for predicting a relative service life of on overlay.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.