• Title/Summary/Keyword: artificial saliva

Search Result 156, Processing Time 0.022 seconds

Effectiveness of caries-preventing agents on initial carious lesions within the scope of orthodontic therapy

  • Park, Kyung-Jin;Kroker, Tessa;Gross, Uwe;Zimmermann, Ortrud;Krause, Felix;Haak, Rainer;Ziebolz, Dirk
    • The korean journal of orthodontics
    • /
    • v.49 no.4
    • /
    • pp.246-253
    • /
    • 2019
  • Objective: To evaluate the effectiveness of three different caries-preventing agents on artificial caries in a Streptococcus mutans-based caries model. Methods: Sixty-five caries-free human molar enamel blocks were treated with a demineralization solution and a remineralization solution. The specimens were assigned to the following groups according to the caries-protective product applied: group A, chlorhexidine varnish; group B, fluoride-releasing chemically cured sealant; group C, fluoride-releasing lightcured sealant; group D, positive control (specimens that were subjected to de- and remineralization cycles without treatment with any caries-protective agents); and group E, negative control (specimens that were not subjected to de- and remineralization cycles). Samples in groups A-D were stored in demineralization solution with S. mutans and thereafter in artificial saliva. This procedure was performed for 30 days. Average fluorescence loss (${\Delta}F$) and surface size of the lesions were measured using quantitative light-induced fluorescence at baseline and on the 7th, 14th, and 30th days. Results: After 30 days, group A demonstrated a significant increase in ΔF and the surface size of the lesions, no significant difference in comparison with the positive control group, and a significant difference in comparison with the negative control group. Group B showed no significant changes in both parameters at any of the measurement points. While group C showed increased ${\Delta}F$ after 14 days, no significant fluorescence change was observed after 30 days. Conclusions: Both fluoride-releasing sealants (chemically or light-cured) show anti-cariogenic effects, but the use of chlorhexidine varnish for the purpose of caries protection needs to be reconsidered.

Effect of Cobalt Contents on the Biocompatibility and Corrosion Properties of Fe-31Cr-27Ni-1.6Mo-1.5W-0.26N Alloy (Fe-31Cr-27Ni-1.6Mo-1.5W-0.26N계 초내식성 스테인리스강의 생체적합성 및 부식특성에 미치는 Co함량의 영향)

  • Jang, Soon Geun;Yoo, Young Ran;Nam, Hee Soo;Shim, Gyu Tae;Kim, Jung Gu;Kim, Young Sik
    • Korean Journal of Metals and Materials
    • /
    • v.46 no.4
    • /
    • pp.209-216
    • /
    • 2008
  • Super austenitic stainless steels shows the high PRE (Pitting Resistance Equivalent) number and the good corrosion resistance. This work controlled the Co contents in Fe-31Cr-1.7Mo-27Ni-0.25N alloys to elucidate the effect of cobalt contents on the biocompatibility and corrosion resistance. Increasing Co contents, the hardness of the annealed alloys tends to be reduced. In aged alloys, cobalt decreased the increments of hardness by aging treatment. Cobalt decreased the critical pitting temperature (CPT) in 6% $FeCl_3$ + 1% HCl solution, but improved the anodic polarization behavior in Hanks' balanced salt solution and artificial saliva solution. Repassivation rate in artificial body solutions was improved by increasing cobalt contents, but didn't show the linear relationship to PRE number of the alloys. The experimental alloys showed the non-cytotoxicity because of its high corrosion resistance.

Colorimetric Based Analysis Using Clustered Superparamagnetic Iron Oxide Nanoparticles for Glucose Detection (클러스터 초상자성체 산화철 나노입자를 이용한 색채학적 해석 기반 당 측정)

  • Choi, Wonseok;Key, Jaehong
    • Journal of Biomedical Engineering Research
    • /
    • v.41 no.6
    • /
    • pp.228-234
    • /
    • 2020
  • Superparamagnetic iron oxide nanoparticles (SPIONs) are approved by the Food and Drug Administration (FDA) in the United States. SPIONs are used in magnetic resonance imaging (MRI) as contrast agents and targeted delivery in nanomedicine using external magnet sources. SPIONs act as an artificial peroxidase (i.e., nanozyme), and these reactions were highly stable in various pH conditions and temperatures. In this study, we report a nanozyme ability of the clustered SPIONs (CSPIONs) synthesized by the oil-in-water (O/W) method and coated with biocompatible poly(lactic-co-glycolic acid) (PLGA). We hypothesize that the CSPIONs can have high sensitivity toward H2O2 derived from the reaction between a fixed amount of glucose and glucose oxidase (GOX). As a result, CSPIONs oxidized a 2,2'-azino-bis(3-ethylbenzthiazoline-6-sulfonic acid) diammonium salt (ABTS) commonly used as a substrate for hydrogen peroxidase in the presence of H2O2, leading to a change in the color of the substrate. We also utilized a colorimetric assay at 417 nm using various glucose concentrations from 5 mM to 1.25 μM to validate β-D-glucose detection. This study demonstrated that the absorbance value increases along with increasing the glucose level. The results were highly repeated at concentrations below 5 mM (all standard deviations < 0.03). Moreover, the sensitivity and limit of detection were 1.50 and 5.44 μM, respectively, in which CSPIONs are more responsive to glucose than SPIONs. In conclusion, this study suggests that CSPIONs have the potential to be used for glucose detection in diabetic patients using a physiological fluid such as ocular, saliva, and urine.

Changes in the composition of artificial cariogenic biofilms over time (인공 우식 유발성 biofilm 구성성분의 시간 흐름에 따른 변화)

  • Oh, Chul;Pandit, Santosh;Jeon, Jae-Gyu
    • Journal of Korean Academy of Oral Health
    • /
    • v.43 no.3
    • /
    • pp.118-123
    • /
    • 2019
  • Objectives: The purpose of this study was to investigate changes in the composition of artificial cariogenic biofilms using a Streptococcus mutans biofilm model over a period of time. Methods: We analyzed the dry weight, colony forming unit (CFU) number, extracellular polysaccharide (EPS) biovolume, and acid production rate of S. mutans biofilms formed on saliva-coated hydroxyapatite discs after 26 h, 50 h, 74 h, 98 h, 171 h, and 195 h. In addition, we performed a laser scanning confocal fluorescence microscopy to determine the bacterial volume, EPS biovolume, and biofilm thickness. We calculated the biofilm density using dry weight and EPS biovolume. Results: Over a period of time, there was no change in the CFU number and acid production rate of S. mutans biofilms, but there was an increase in the dry weight and EPS biovolume of S. mutans biofilms. The bacterial volume, EPS biovolume, and biofilm thickness only increased in the 50-h-old biofilm; however, no change was observed in 50-195-h-old biofilms. In addition, an increase in the biofilm density was observed over time. Conclusions: These results suggest that the acid production ability of cariogenic biofilms does not change, but the biofilm density increases over time. However, due to scientific information, further research needs to be conducted in the field of dentistry to get further insights on the progression of cariogenic biofilms over time.

Electrochemical Behaviors of Binary Ti-Zr Alloys

  • Oh, M.Y.;Kim, W.G.;Choe, H.C.;Ko, Y.M.
    • Corrosion Science and Technology
    • /
    • v.8 no.2
    • /
    • pp.89-92
    • /
    • 2009
  • Pure Ti as well as Ti-6Al-4V alloy exhibit excellent properties for dental implant applications. However, for a better biocompatibility it seems important to avoid in the composition the presence of V due to the toxic effects of V ion release. Thus Al and V free and composed of non-toxic element such as Nb, Zr alloys as biomaterials have been developed. Especially, Zr contains to same family in periodic table as Ti. The addition of Zr to Ti alloy has an excellent mechanical properties, good corrosion resistance, and biocompatibility. In this study, the electrochemical characteristics of Ti-Zr alloys for biomaterials have been investigated using by electrochemical methods. Methods: Ti-Zr(10, 20, 30 and 40 wt%) alloys were prepared by arc melting and homogenized for 24 hr at $1000^{\circ}C$ in argon atmosphere. Phase constitutions and microstructure of the specimens were characterized by XRD, OM and SEM. The corrosion properties of the specimens were examined through potentiodynamic test (potential range of -1500 ~ 2000 mV), potentiostatic test (const. potential of 300 mV) in artificial saliva solution by potentiostat (EG&G Co, PARSTAT 2273. USA).

Tarnish Behavior of Palladium-Indium-Silver alloy (Pd-In-Ag 합금의 변색거동에 관한 연구)

  • Kim, Hwa-Soo;Kim, Seong-Yun;Lee, Kyu-Hwan;Shin, Myung-Chul;Dzo, Man Hyung
    • Analytical Science and Technology
    • /
    • v.11 no.2
    • /
    • pp.125-129
    • /
    • 1998
  • The purpose of this study was to give a quantitative analysis for assessing the tarnish resistance of alloys at the artificial saliva, 0.9% NaCI solution and Ringer's solution. In light of development in low-nobility alloys, it is important that tarnish test is standardized to analyse the tarnish properties of the compositions. There are concerns with the long term chemical stability of these alloys and the resistance to tarnish. Chemical stability is a complex problem involving alloy composition, nobility, microstructure and environment.

  • PDF

CPP-ACP of artificially demineralized enamel surface and remineralization of material containing nano-sized carbonated apatite (인공 탈회된 법랑질 표면의 CPP-ACP와 nano-sized carbonated apatite 함유물질의 재광화효과)

  • Kim, Young-Sook
    • Journal of Korean society of Dental Hygiene
    • /
    • v.8 no.1
    • /
    • pp.13-22
    • /
    • 2008
  • This study compared tooth's remineralization using enamel surface artificially demineralized with 0.1M lactate and HCL solution using Vicker's Hardness Number(VHN) to compare CPP-ACP and remineralization of nano-sized Carbonate Apatite's initial caries. Using pH circulation models divided into 0% nano-CA, 5% nano-CA, 10% nano-CA, 10% CPP-ACP and D.W. they were treated for 5 minutes, three times a day for 14 days to get the following results. 1. There were no significant differences among the initial surface hardness of samples demineralized surface of front tooth in 5 groups. and all 5 groups' surface hardness reduced significantly after demineralization of enamel. 2. When inquiring into hardness changes through pH circulation model, the highest hardness change was in 5% nano-CA group. Also. 10% nano-CA and 10% CPP-ACP groups increased significantly. but there was no significant difference statistically. In generalizing the above experiment results, nano-sized Carbonate Apatite showed remineralization, and compared to 10% CPP-ACP group, 5% nano-CA had remineralization to artificial caries. thus implies that when we develop method to contact with tooth of nano-CA in the future, it is expected to gain synergy effect on function of saliva, a natural remineralization material.

  • PDF

A Study on the Color Stability of Temporary Resins according to Polymerizing Methods and Staining (온성 방법에 따른 수종의 임시 수복용 레진의 착색시의 색 안정성에 관한 연구)

  • Park, Sung-Ho;Cho, In-Ho
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.16 no.1
    • /
    • pp.1-11
    • /
    • 2000
  • Dental temporary resin should have adequate strength and similar esthetics as natural teeth. Recently esthetics has become a high priority in clinical dentistry. Thus the evaluation of color stability of dental temporary resin has become an important part in dental research. The purpose of this study was to evaluate the difference in color stability of 3 resins($Snap^{(R)}$, Temporary bridge $resin^{(R)}$, Trim $II^{(R)}$) according to polymerizing methods and stainning. The resins were divided into groups by 2 types of polymerizing methods ( air or pressure and heat curing) The resins were dyed with coffee, chlorhexidine and artificial saliva and then the color stability was evaluated with a spectrophotometer(CM-503i, Minolta, Japan). The results were as follows ; 1. In the color stability according to polymerizing method, pressure and heat polymerizing method was higher than air polymerizing method. 2. The color stability according to staining fluid decreased in the order of I, II, III group, there was significant difference among the groups of staining fluid. 3. The color stability according to resins decreased in the order of $Snap^{(R)}$, Trim $II^{(R)}$, Temporary Bridge $resin^{(R)}$, The $Snap^{(R)}$ resin was highest color stability, there was significant difference among the 3 resins.

  • PDF

A Case Report of Spinal Pharmacopuncture and Herb Medicine for Dry Mouth (구강건조증 환자에 대한 척추 약침 및 한약 치료 1례)

  • Jin, Joon-soo;Min, Baek-ki;Lee, Do-eun;Seo, Ho-seok;Kim, Jin-won
    • The Journal of Internal Korean Medicine
    • /
    • v.40 no.2
    • /
    • pp.262-269
    • /
    • 2019
  • Xerostomia is a symptom of subjective complaints due to decreased salivary secretion or various other causes, which is common in about 30% of elderly people. Parasympathetic stimulants or artificial saliva are used as remedies, but this has side effects, and there are limitations in completely resolving symptoms. In this study, an 88-year-old woman with subjective dry mouth syndrome for the previous two to three years was treated with spinal pharmacopuncture and herbal medicine (Yookmigihwang-tang). The patient received pharmacopuncture at the thoracic 3rd, 6th, and 10th level twice a day and took herbal medicine three times daily for seven days. Both the degree of oral dryness and behavior were improved after treatment of Korean medicine, especially in the case of pharmacopuncture for inner core muscles.

A Study on Corrosion according to Distance between Amalgam and Dissimilar Metals (아말감과 이종(異種)금속의 거리에 따른 부식에 대한 고찰)

  • Kim, Ju-won;Jeong, Eun-gyeong
    • Journal of dental hygiene science
    • /
    • v.4 no.3
    • /
    • pp.103-109
    • /
    • 2004
  • The present study prepared 72 test samples - 24 made of amalgam alloy, 24 of Verabond (Ni-Cr alloy) for crown and 24 of Talladium $^{TM}alloy$ for denture - according to the manufacturers' manuals and general method in consideration of the width of the mesial-distal dental crown of the lower $1^{st}$ molar and MOD cavity in clinics, put them in a 200 ml beaker containing 80 ml of artificial saliva, and measured their galvanic corrosion at distances of 0 mm, 7 mm and 40 mm after 7 days. Isolated metals in the electrolyte such as Cu, Ag, Ni, Cr, Sn, Zn and Hg were quantitatively analyzed with Inductively Coupled Plasma - Atomic Emission Spectrometer (ICP-AES, JY-50P, VG Elemental Co. France), and from the results were drawn conclusions as follows. First, Cu, Sn, Ag, Hg and Zn were highly advantageous when amalgam contacted gold alloy compared to Ni-Cr alloy for crown and Talladium alloy for denture. In addition, although gold alloy was finest in terms of oral tissue and biocompatibility, it was most disadvantageous when it was with amalgam. Second, when amalgam contacted gold alloy, heavy metals such as Ni and Cr were not isolated at all because gold alloy did not contain such elements but Sn was isolated as much as $227.1{\pm}18.0035{\mu}g/cm^2$ although it was not included in the composition either. Hg was also isolated. These elements are assumed to have been isolated from amalgam itself. Third, when amalgam alloy was apart from gold alloy 0 mm, 7 mm and 40 mm, Cu and Ag showed significance but Hg did not. This suggests that gold alloy must not be used together with amalgam, and must not be used between dissimilar prostheses regardless of distance. Fourth, when amalgam alloy contacted Ni-Cr alloy for crown, Ag was not isolated from the amalgam, but Zn, Ni, Sn, Hg and Cu were isolated in order of quantity. Significance was observed according to distance - 0 mm, 7 mm and 40 mm. Hg was not isolated but heavy metals Ni and Cr were isolated. If amalgam alloy was in the opposite arch or it was apart from Ni-Cr alloy for crown, the isolation Hg was less than that when amalgam alloy contacted Ni-Cr alloy for crown. Fifth, when amalgam alloy contacted Talladium alloy for denture, significance was observed at distances of 0mm, 7 mm and 40 mm. Hg was not isolated but heavy metals Ni and Cr were isolated. If amalgam alloy was in the opposite arch or it was apart from Talladium alloy for denture, the isolation Hg was less than that when amalgam alloy contacted Talladium alloy for denture. Sixth, according to the result of ICPES test on Cu, Sn, Ag, Hg, Zn, Ni and Cr of amalgam alloy, gold ally, Verabond and Talladium alloy when these alloys contacted artificial saliva, significance was observed in Cu and Hg. Seventh, when amalgam alloy contracted two non-precious metals Ni-Cr alloy for crown and Talladium alloy for denture in artificial saliva, significance was observed in the isolated by-products of Hg, Ni and Cr according to distance.

  • PDF