분자 동역학 계산을 통한 결정질 실리콘 태양전지 기판에 콜드 스프레이 전극 형성 시 발생되는 비정질 구리상에 대한 용융 온도 변화 연구 (Melting Point of Amorphous Copper Phase on Crystalline Silicon Solar Cells During Cold Spray using Molecular Dynamics Calculations)

  • 김수민;강병준;정수정;강윤묵;이해석;김동환
    • Current Photovoltaic Research
    • /
    • 제3권2호
    • /
    • pp.61-64
    • /
    • 2015
  • In solar industry, numerous researchers reported about cold spray method among various electrode formation technic, but there are no known a bonding mechanism of metal powder. In this study, a cross-section of copper electrode formed by cold spray method was observed and heterogeneous phase between silicon substrate and copper electrode was analyzed using morphology observation technic. SEM and TEM analysis were performed to analyze a crystallinity and distribution shape of heterogeneous copper phase. Molecular dynamics simulation was performed to calculate glass transition temperature of copper metal. In the result, amorphous copper phase was observed near interface between silicon substrate and metal electrode. The results of the molecular dynamics simulation show that an amorphous copper phase could be formed at a temperature below the melting point of copper because cold spraying resulted in a lower glass transition temperature.

Ursodeoxycholic acid의 무정형 초미립자제제들의 CC4 유도 간손상 생쥐에 대한 보호 효과 (Hepatoprotective Effects of Amorphous and Nnno-Particle Pyeparations of Ursodeoxycholic Acid in CC4-Induced Mice : Effects of Three Types of Fine Grinding Mills)

  • 정한영;곽신성;김현일;최우식;이지현;김애라;박태현;정해영;김유정
    • Biomolecules & Therapeutics
    • /
    • 제10권1호
    • /
    • pp.1-6
    • /
    • 2002
  • The particle size of medicinal materials is an Important physical property that affects the phar-maceutical behaviors such as dissolution, chemical stability, and bioavailability of solid dosage forms. The size reduction of raw medicinal powder is needed to formulate insoluble drugs or slightly soluble medicines and to improve the pharmaceutical properties such as the solubility, the pharmaceutical mixing, and the dispersion. The objective of the present study is to evaluate physiological activity of amorphous and nano-particle prep-arations of insoluble drug, ursodeoxycholic acid (UDCA), which were made by three types of fine grinding mills. The change of physical properties of ground UDCA was conformed by Mastersiger microplus and X-ray diffraction. We have investigated hepatoprotective effects of the nano-particle preparations of UDCA by plan-etary mill, vibration rod mill and jet mill in $CCI_4$-induced oxidatively injured mouse liver. The results showed that nano-particle preparations of UDCA all decreased reactive oxygen sepecies generation and lipid peroxi-dation in $CCI_4$-induced oxidative stress mice. Among them, nano-particle preparations by vibration rod mill and jet mill showed more significantly hepatoprotective effects compared to intact UDCA and planetary mill-ground UDCA. These results suggest that ground UDCA with vibration rod mill and jet mill shows a high amorphous state and the improved dissolution.

습식법에 의한 형광체 제조용 비정질 탄산칼슘 전구체 분말의 합성에 관한 연구 (A study on the powder synthesis of the amorphous calcium carbonate precursor for phosphors by wet chemical method)

  • 최종건;김판채;이충효
    • 한국결정성장학회지
    • /
    • 제10권4호
    • /
    • pp.302-308
    • /
    • 2000
  • 탄산칼슘을 모재로 한 형광체 제조를 위하여 비정질 탄산칼슘 전구체를 합성할 때 용액의 농도, 반응온도, 유지시간 및 모액의 pH의 영향을 조사함으로써 안정한 비정질 탄산칼슘을 합성할 수 있었으며, 물 속에 침적하여 결정화 조건을 달리하여 줌으로써 calcite, aragonite, vaterite의 결정 상을 얻을 수 있었다. 또한 활성원소로서 Sn을 첨가하여 비정질 탄산칼슘을 합성하고, 이를 결정화시켜 각 결정형에 따른 형광특성을 조사하였다. 결정형에 따른 발광강도는 calcite가 가장 우수하였으며, 발광중 심파장은 순수한 청색을 나타내는 464 nm였다. calcite의 발광강도는 여기파장 255 nm에서 최대가 되었으며, 형광램프용의 형광체로 사용하기 적합한 것으로 기대된다.

  • PDF

다중압출공정을 이용한 Cu-Ni-Zr-Ti 비정질 복합재의 미세조직제어 (Microstructure Control of Cu-Ni-Zr-Ti Metallic Glass Composites by Multi-Pass Extrusion Process)

  • 김택수;이진규
    • 소성∙가공
    • /
    • 제16권5호통권95호
    • /
    • pp.386-390
    • /
    • 2007
  • In order to, simultaneously, synthesize and control the size of microstructure of amorphous/crystalline composites, a repeated extrusion process was performed using the gas atomized $Cu_{54}Ni_6Zr_{22}Ti_{18}$ metallic glass powders and the crystalline brasses. The size of microstructure in the resultant composites was varied depending on the pass of extrusion as well as on the area reduction ratio. The microstructure could be estimated using an equation of $r_n=r_{n-1}/R^{1/2}$, where R is reduction ratio and $r_n$ is the resultant radius of the extruded bar after n pass. Theory of microstructural refinement as well as the relationship between the resultant microstructures and mechanical properties was discussed.

Eutectic Nanocomposites for Thermophotovoltaic Application

  • Han, Young-Hwan;Lee, Jae-Hyung;Kakegawa, Kazuyuki
    • Transactions on Electrical and Electronic Materials
    • /
    • 제11권6호
    • /
    • pp.249-252
    • /
    • 2010
  • The ground amorphous powder was consolidated into a dense sintered body with a typical ultrafine $Al_2O_3-GdAlO_3$ eutectic structure by spark plasma sintering (SPS). Sintered material with ultrafine and dense eutectic structure was obtained by an appropriate combination of rapid quenching and SPS at lower temperature and more quickly than by conventional sintering. The $Al_2O_3$-based rare earth eutectic ceramics for solar cell emitters are believed to have a higher efficiency and the $Al_2O_3$ based eutectic ceramics with ultrafine grains will be one of the promising materials showing excellent selective emitter characteristics.

Effect of Surface Morphology on Dimerization of tert-Butyl Mercaptan on the Surface of Amorphous Aluminosilicate Impregnated with Mn and Cu

  • Kweon, Jeong-Eun;Joo, Hyun-ha;Park, Dong-Gon
    • Bulletin of the Korean Chemical Society
    • /
    • 제27권1호
    • /
    • pp.53-58
    • /
    • 2006
  • A powder of destructive adsorbent was prepared by impregnating Mn and Cu on the surface of amorphous aluminosilicate. It catalytically dimerized tert-butyl mercaptan into di-tert-butyl disulfide on its surface. Turnover of the dimerization was strongly dependent on the surface morphology of the adsorbent, which could be altered by modification of aluminosilicate support. During the process of impregnation, which involved heat treatment at 500 ${^{\circ}C}$, the shape of the pore was preserved, though large fraction of micropores were eliminated. The reactive sites on the surface were poisoned as dimerization products strongly adhered on them. Therefore, high surface area was not always desirable. When the surface was heavily populated with “inkbottled” pores with a narrow entrance in uniform size, heavy poisoning of the reactive sites turned the destructive adsorbents almost useless.

기상반응에 의한 $Si_3N_4$ 미세분말의 합성 (Synthesis of Ultrafine Silicon Nitride Powders by the Vapor Phase Reaction)

  • 유용호;어경훈;소명기
    • 한국세라믹학회지
    • /
    • 제37권1호
    • /
    • pp.44-49
    • /
    • 2000
  • Silicon nitride powders, were synthesized by the vapor phase reaction using SiH4-NH3 gaseous mixture. The reaction temperature, ratio of NH3 to SiH4 gas and the overall gas quantity were varied. The synthesized powders were characterized using X-ray, TEM, FT-IR and EA. The synthesized silicon nitride powders were in amorphous state, and the average particle size was about 100nm. TEM analysis revealed that the particle size decreased with increasing reaction temperature and gas flow quantity. As-received amorphous powders were annealed in nitrogen atmosphere at 140$0^{\circ}C$ for 2h, then the powders were completely crystallized at 0.2 ratio of NH3 to SiH4.

  • PDF

초임계 유체를 이용한 나노크기 $TiO_2$ 분말제조 및 소결특성 (Preparation and Sinterability of Nano-Size $TiO_2$ Powders Using Supercritical Fluids)

  • 송정환;이정석;박인석;임대영
    • 한국세라믹학회지
    • /
    • 제37권7호
    • /
    • pp.625-631
    • /
    • 2000
  • In this study, the characteristics and sinterablities of TiO2 powders which were fabricated on sol-gel process and supercritical fluid process were examined. The powders fabricated on sol-gel process were amorphous. The particle size and shape were changed with the amount of water used for hydrolysis of titanium ethoxide. The powders were changed from amorphous to crystalline by heating at 400℃. The crystalline anatase TiO2 powders were directly prepared in ethanol supercritical fluid condition that temperature was 270±3℃ and pressure was 7.3 MPa. It's primary crystalline size was 20 nm and agglomerated as spherical shape whose size was 0.7∼1㎛. The powders prepared on sol-gel process were not sintered densely at 900℃ because of abnormal grain growth. However, the powders which prepared on supercritical fluid process were sintered densely at the comparatively low temperature of 800℃ by ideal growth of grain, which are fired at 900℃.

  • PDF

기계적 합금화 방법에 의한 $Nb_3Sn$합금 제조 (The synthesis of $Nb_3Sn$ alloy powders by mechanical alloying)

  • 이성만
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1996년도 추계학술대회 논문집 학회본부
    • /
    • pp.464-467
    • /
    • 1996
  • The microstructural evolution during mechanical alloying of Nb and Sn powders, of average composition Nb3Sn, has been investigated by X-ray diffraction(XRD) and scanning electron microscopy(SEM). Observations by SEM showed a progressive change of milling time. From the XRD studies, the structural development with milling time depends on the ball size for a given powder/ball ratio. Using a larger ball of 9.5mm diameter, the elemental powders initially alloy mechanically to form an A15 structure phase, and then amorphised with continued milling. However, in case of milling with a smaller ball of 3.968mm diameter, an amorphous phase is first formed. These results can be understood by considering the dependence of the milling energy on the ball size. The homogeneous stoichiometric $Nb_3Sn$ phase could be easily obtained by heat treatment of a supersaturated solid solution produced by MA. Heat treatment of an amorphous phase formed by MA resulted in the mixture of the $Nb_3Sn$ and $Nb_6Sn_5$ phases.

  • PDF

Epoxy/Annealing $SiO_2$ Composites의 충진함량에 대한 저 유전특성 (Low Dielectric Properties of Epoxy/Annealing $SiO_2$ Composites for Filler Contents Variation)

  • 박재준;안준오;윤종현
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 추계학술대회 논문집
    • /
    • pp.224-225
    • /
    • 2007
  • The Low dielectric properties of epoxy/Annealing $SiO_2$ composites using Annealing new material of nanosized amorphous particles were investigated as function frequency, temperature and filler contents composition. The dielectric constant decrease with increasing frequency and also increase with increasing ambient temperature. The dielectric constant decrease with increase annealing filler contents for epoxy base. The result of x-ray diffraction could obtained single crystal of annealing $SiO_2$ from 500nm amorphous $SiO_2$ powder.