• Title/Summary/Keyword: ammonium rejection

Search Result 2, Processing Time 0.015 seconds

Development of sulfonated polysulfone composite membranes for ammonium rejection

  • Bastos, Edna T.R.;Barbosa, Celina C.R.;Silva, Jaciara C.;Queiroz, Vanessa B.C.;Vaitsman, Delmo S.
    • Membrane and Water Treatment
    • /
    • v.4 no.2
    • /
    • pp.83-93
    • /
    • 2013
  • In the present investigation, were synthesized composite membranes prepared by simultaneous casting of two polymer solutions using the technique of phase inversion by immersion / precipitation. The support layer was prepared using polyethersulfone and polysulfone as base polymer and for the top layer was used sulfonated polysulfone (SPSU) with 50% sulfonation degree. The morphology of the resulting membranes were characterized by scanning electron microscopy (SEM). The final results showed that it is possible to prepare composite membranes by simultaneous casting of two polymer solutions with adherence between the two layers. Regarding the permeation tests, the developed membranes presented values of hydraulic permeability within the range of commercial nanofiltration (NF) membranes. Values rejection of 80% ammonium ions can be increased by using a SPSU with a greater degree of sulfonation.

Preparation and Application of Pore-filled PVDF ion Exchange Membranes (Pore-filled PVDF 이온교환막의 제조 및 응용)

  • 변홍식;박병규;홍병표;여광수;윤무홍;강남주
    • Membrane Journal
    • /
    • v.14 no.2
    • /
    • pp.108-116
    • /
    • 2004
  • In this study, the pore-filled ion-exchange membranes were prepared by using the asymmetric PVDF membrane as a nascent membrane. First, the solution of PVBCI having the chlorornethylate aryl ring of 80 percents and DABCO was made with the mixed solvent of THF and DU (8:2). These mixed solution was then, filled in the pores of PVDF membrane, and left for a day to complete the gelation. Finally the pore-filled anion-exchange membrane is obtained fallowed by the amination of the remaining chloromethyl groups with trimethylamine (TMA, 40 wt% in water) forming the positive ammonium ion sites. This 2 step procedure enabled us to produce the pore-filled membranes without change of size, and to control the properties of final membrane with various degree of cross-linking. The results of SEM and AFM showed the polyelectrolyte existed in the pores of nascent membrane as a certain configuration. From the investigation of the solvent affecting much to the permeability and rejection, it was found that the membranes using mixed solvent of THE and DMF (8:2) showed better performances than the membranes produced by THF only. The result of an investigation for the water permeability of the final membrane at low pressure (100 Kpa) showed a typical ultrafiltration membrane's permeability (8 ∼ 10 kg/$m^2$hr) and good values of rejection (55∼60 percent).