전부도재관용 레진시멘트의 생체적합성에 관한 연구 (A STUDY ON BlOCOMPATABILITY OF RESIN CEMENTS FOR ALL-CERAMIC CROWN)

  • 김광준;김성훈;진태호
    • 대한치과보철학회지
    • /
    • 제41권2호
    • /
    • pp.111-127
    • /
    • 2003
  • Statement of problem : Resin cements were used widely on all ceramic crowns, but the influence of resin cements on biocells was not understood clearly. Purpose : This study was investigated to evaluate the biocompatibility of resin cements for all-ceramic crowns. Material and Method : The resin cements used in this study were Panavia F (Kuraray Co., Ltd. Japan), Variolink II (Vivadent Ets., Schann / Liechtenstein), and Bistite II (Bistite dual cure resin cement-clear Tokuyama Soda Co. Japan). The viability of normal human oral keratocytes, gingival fibroblast, and gingival fibroblast immortalized by Human Papilloma virus 16 was measured in vitro for evaluation of cytotoxicity on resin cements, and the response of pulp tissue was analyzed and evaluated with light microscope after application of cements at cutting edge of incisors. Results : The normal human oral keratocytes was the most sensitive to toxicity of resin cement, and toxicity of cements was higher in Bistite II than in Variolink II. The cell viability of immortalized gingival fibroblast did not affected by type of cement and cultivation period, but there was a tendency that cytotoxicity in Bistite II was higher than in Variolink II. The cell viability of gingival fibroblast was similar to that of immortalized gingival fibroblast regardless of cement type, but Bistite II showed more toxic than others after 5 days cultivation. The responses of pulp tissue according to cement type were similar after 2 days cultivation, but revealed high toxicity in Bistite II after 10 days cultivation. Conclusion : Variolink II was more biocompatible than any other resin cements used in this study.

코발트-크롬 합금으로 제작된 금속-도재관의 적합도 평가 (Evaluation of fitness of metal-ceramic crown fabricated by cobalt-chrome alloy)

  • 김재홍;김원수;김기백
    • 한국치위생학회지
    • /
    • 제13권2호
    • /
    • pp.361-368
    • /
    • 2013
  • Objectives : The purpose of this in vitro study was to evaluate the effect of firing cycles on the marginal and internal fit of metal ceramic crown. Methods : Ten same cases of stone models (abutment teeth 11) were manufactured. Ten cobalt-chrome cores were made per each models and the marginal and internal fit was evaluated through a silicone replica technique. The marginal and internal fit of specimens was measured twice. The first measurement was done after manufacturing cobalt-chrome alloy core and the second measurement was done after porcelain firing. T-test of paired sample for statistical analysis was executed with SPSS 12.0K for Windows (${\alpha}$=0.05). Results : Mean(SD) marginal and internal fit were 77.1(23.3) ${\mu}m$ for the cobalt-chrome alloy core group and 84.4(21.9) ${\mu}m$ for the metal-ceramic crown group. They were statistically significant differences between groups for marginal and internal fit (p<.05). Conclusions : All metal ceramic crowns showed marginal and internal fit ranged within the current clinical recommendations.

도재와 상아질의 표면 처리가 도재의 파절 강도에 미치는 영향 (THE EFFECT OF SURFACE TREATMENT ON FRACTURE STRENGTH OF DENTAL CERAMICS)

  • 이신원;이선형;양재호;정헌영
    • 대한치과보철학회지
    • /
    • 제37권5호
    • /
    • pp.658-671
    • /
    • 1999
  • The major influencing factors on the strength of all-ceramic crowns are types of dental ceramics, fabrication techniques, methods of abutment preparation and cementation modes of all-ceramic restorations. Zinc phosphate cement and glass-ionomer cement were used as an early lot-ing media for all-ceramic crowns. Recently many studies have reported that resin cements have more advantages in increasing the fracture strength of restorations comparing with zincphosphate cement and glass-ionomer cement. The purpose of this study is to investigate the effect of etching, silane treatment, sandblasting and dentin bonding agents on fracture strengths of dental ceramics. 40 flat dentin specimens and 40 ceramic discs of 1.5mm thickness and 8mm diameter were fabricated, and divided into 4 groups according to surface treatments. Surface treatments before cementation were as follows Group I : (ceramic) : HF etching - silane treatment - application of bonding resin (dentin) : application of dentin bonding agent Group II : (ceramic) : sandblasting - application of bonding resin (dentin) : application of dentin bonding agent Group III : (ceramic) : application of bonding resin (dentin) : application of dentin bonding agent Group IV : (ceramic) : HF etching - silane treatment - application of bonding resin (dentin) : no dentin bonding procedure Dentin specimens and ceramic discs were cemented with dual cure resin cement, and went through thermocycling. Compressive stress es were loaded on the centers of ceramic discs with Instron test-ing machine, and fracture strengths resistance for catastrophic fracture were measured The results were as follows. 1. The group I showed the highest fracture resistance. The next was group II And group III, IV followed. 2. There was a significant difference in the mean value of fracture strengths between group I and group III (p<0.05), but no significant differences between group I and group II, and group II and group III (p>0.05). 3. There was a significant difference in the mean value of fracture strengths between group I and group IV (p<0.05).

  • PDF

다른 특성을 가지는 도재가 반복소성에 따라 색조변화에 미치는 영향 (The Effect of Repeated Firing on the Color Difference of a Metal-Ceramic System with Different Porcelain Powder)

  • 황재선
    • 대한치과기공학회지
    • /
    • 제31권1호
    • /
    • pp.23-36
    • /
    • 2009
  • The goal of esthetic restoration is to achieve morphologic, optical, and biologic acceptance. Creation of a natural looking ceramic restoration, which blends harmoniously with surrounding dentition, is not always achieved. A successful color match is an important aspect of any esthetic dental restoration. Since natural enamel has inherent translucency, it is important that ceramic restorations reproduce the translucency and color of the natural teeth. However, the final color match of porcelain crowns to adjacent natural dentition remains some problem. Difficulties related to color matching arise from the structural differences that exist between metal ceramic crowns and natural teeth, the limited range of available ceramic shades, inadequate shade guides, different types of metal alloys, repeated firing, the condensation technique, and varying compositions of ceramic materials. Many factors contribute to the esthetic success of dental restoration: optical properties such as color and its elements of hue, value, and chroma; translucency and opacity; light transmission and scattering; and metamerism and fluorescence. The purpose of this study was to determine the color changes of metal-ceramic system with different veneering porcelain powder after repeated firing. The objectives of this in vitro study were to measure the lightness($L^*$), chromaticity($a^*$), chromaticity($b^*$), chroma($C^*$), hue(h), reflectance(%), color difference(${\Delta}E$). The following conclusions were obtained: 1. An increase in the number of firings resulted in decrease in lightness($L^*$) but increase in chromacticity($a^*$) with all porcelain. After the second sintering resulted in decrease in chromacticity($b^*$) with opaque-dentin porcelain and dentin porcelain but in increase with enamel porcelain and translucency porcelain. And after the second sintering resulted in decrease in chroma($C^*$) with opaque-dentin porcelain and dentin porcelain, but on the whole side in decrease with enamel porcelain and translucency porcelain. 2. After the second firing, a increase in the number of firings resulted in decrease reflectance(%) in all wavelength. 3. There were noticeable color differences(${\Delta}E$) between first sintering and multiple firings(dentin porcelain: 5.29~8.15, opaque-dentin porcelain: 4.83~8.2, enamel porcelain: 8.93~13.15, translucency porcelain: 9.37~12.91), but the color difference(${\Delta}E$) after second sintering were down to 4.87 in all porcelain. 4. Given the NBS Criteria, a 'trace' was not found this study but a 'slight' was found 2-3, 3-5 in dentin porcelain, 2-3 in opaque-dentin porcelain, 3-5, 5-10 in enamel porcelain and translucency porcelain, a 'noticeable' was 2-5, 3-10, 5-10 in dentin porcelain and opaque-dentin porcelain, 2-3, 2-5, 3-10 in enamel porcelain 2-3, 3-10 in translucency porcelain, an 'appreciable' was 1-2, 1-3, 2-10 in dentin porcelain 1-2, 1-3, 2-10, 3-10 in opaque-dentin porcelain, 2-10 in enamel porcelain, 2-5, 2-10 in translucency porcelain, a 'much' was 1-5, 1-10 in dentin porcelain and opaque-dentin porcelain, 1-2, 1-3, 1-5 in enamel porcelain 1-2, 1-3, 1-5, 1-10 in translucency porcelain, a 'very much' was 1-10 in enamel porcelain.

  • PDF

전부도재관의 변연 적합도 비교평가 (Comparative study in marginal accuracy of several all ceramic crowns)

  • 김정미;정수하
    • 대한치과기공학회지
    • /
    • 제30권2호
    • /
    • pp.87-92
    • /
    • 2008
  • Purpose: In this study, we tried to compare marginal accuracy when produce ceramic crown using all ceramic materials and existent metal-ceramic system. Material and methods: All-ceramic systems were E-max (Ivoclar/Vivadent, Lichtenstein), Lava(3M, U.S.A.) and Wol-ceram(Teamziereis, Germany). Metal-ceramic system(PFG) was composed of Au-Pt alloy (Metalor, Switzerlandand) and overlying ceramic(D-sign, Ivoclar/Vivadent, Lichtenstein). We fabricated metal master die with upper diameter of 7.95mm, bottom diameter of 9.00mm, height of 5.00mm, and taper of $6^{\circ}$. All ceramic system used 0.5mm thickness ceramic coping, while metalceramic system used 0.3 thickness metal coping. By adding dentin and enamel ceramics on each coping, a crown with a proximal thickness of 1.0 mm and occlusal thickness of 2.0mm was fabricated. Pressure of 2kg was applied for 10 seconds on each crown with static load compressor. Before and after cementation, we measured the marginal gap at 4 points of each crown using optical microscope. The data was analyzed using a Student's t test and repeated-measures of analyses of variance(ANOVA) followed by a Bonferroni test. A p value<0.05 was considered significant. Results: As experiment results, marginal accuracy of wol-ceram and Lava is no good when compared with marginal accuracy of PFG. But marginal accuracy of E.max is good when compared with PFG. This result showed not significant. The marginal accuracy of E.max is good when compared with marginal accuracy of wol-ceram and Lava. Conclusion: The marginal accuracy of E.max is very good when compared with marginal accuracy of another group.

  • PDF

수종의 post와 IPS-Empress Ingot 두께가 전부 도재 수복물 최종색조에 미치는 영향 (INFLUENCE OF SEVERAL POSTS AND IPS-EMPRESS INGOT THICKNESS ON THE FINAL SHADE OF ALL-CERAMIC CROWNS)

  • 복원미;최근배;박찬운;안승근
    • 대한치과보철학회지
    • /
    • 제42권5호
    • /
    • pp.514-523
    • /
    • 2004
  • Statement of problem: All-ceramic restorations have been advocated for superior esthetics. Various post and core systems have been used to improve the strength of damaged teeth, but it is unclear whether they affect the final shade of finished all-ceramic restorations. Purpose: The influence of different types of post and core systems on light transmission through all-ceramic crowns was assessed by spectrophotometric analysis. Also the masking effect of different thickness of ceramic ingot was evaluated. Material and Methods : Forty-five sample disks (15mm in diameter) at several thickness(1.0, 1.5, 2.0mm) and value(shade 100, 200, 300) were made in heat pressed ceramic(IPS-Empress). Background specimens simulating gold-alloy cast posts(Type III casting gold alloy), metal posts(Ni-Cr casting alloy) and ceramic posts(CosmoPost) were fabrica-ted. Resin composite(Z250, A3 shade) was used as a tooth substrate reference. For each combination, the change in color was measured with a spectrophotometer. Readings were performed for 2 conditions (1) ability of ceramic to mask the core in relation to its thickness(1.0, 1.5, or 2.0mm) ; (2) influence of post and core types on the final color of the ceramic. Data were recorded according to the CIE $L^*a^*b^*$ systems and color difference($\Delta$E) was calculated. Results: 100 shade ingot: when ceramic thickness was 1.0mm, $\Delta$E value for ceramic post larger than 1 but $\Delta$E value for metal and gold post was larger than 2. For ceramic thickness of 1.5mm, only $\Delta$E value for metal was larger than 2, and the other samples' $\Delta$E value was smaller than 2. For ceramic thickness of 2.0mm, $\Delta$E values for all specimens was smaller than 2. 200 shade ingot: when ceramic thickness was 1.0mm, $\Delta$E value for ceramic post was smaller than 1 but $\Delta$E value for metal and gold post was larger than 2. For ceramic thickness of 1.5 mm, only the $\Delta$E value for metal was larger than 2, and the other samples' $\Delta$E value was smaller than 2. For ceramic thickness of 2.0mm, $\Delta$E values for all specimens was smaller than 1. 300 shade ingot: when ceramic thickness was 1.0mm, only $\Delta$E value for metal was larger than 2 and the other samples' $\Delta$E value was smaller than 2. For ceramic thickness of 1.5mm, $\Delta$E values for all specimens was smaller than 1. For ceramic thickness of 2.0mm, $\Delta$E values for all specimens was smaller than 1. Conclusion: The final esthetic result of the IPS-Empress glass-ceramic restoration was not affected by the presence of different core materials when the thickness was more than 2.0 mm. When ceramic thickness decreases to 1.5mm, it is advised to take the substrate aspects into consideration. If the ceramic thickness is less than 1.0mm, using the tooth color matched substrate is strongly recommended.

Survival rate of modern all-ceramic FPDs during an observation period from 2011 to 2016

  • Pott, Philipp-Cornelius;Eisenburger, Michael;Stiesch, Meike
    • The Journal of Advanced Prosthodontics
    • /
    • 제10권1호
    • /
    • pp.18-24
    • /
    • 2018
  • PURPOSE. In literature, many studies compare survival rates of different types of FPDs. Most of them compared restorations, which originated from one university, but from different clinicians. Data about restoration survival rates by only one experienced dentist are very rare. The aim of this study was to evaluate the survival rate of all-ceramic FPDs without the blurring effects of different clinicians. MATERIALS AND METHODS. 153 veneered-zirconia FPDs were observed for follow-up. 22 patients received 131 single crowns and 22 bridges. Because of the different bridge lengths, one unit was defined as a restored or replaced tooth. In total, 201 units were included. Only the restorations performed by the same clinician and produced in the same dental laboratory from 2011 to 2016 were included. Considered factors were defined as "type of unit", "type of abutment", "intraoral region", and "vitality". Modified UHPHS criteria were used for evaluation. Statistical analysis was performed using cox-regression. RESULTS. 189 units (94.0%) showed no kind of failure. 5 chippings (2.4%) could be corrected by intraoral polishing. 4 units (1.9%) exhibited spontaneous decementation. These polishable and recementable restorations are still in clinical use. Chippings or decementations, which lead to total failure, did not occur. One unit was completely fractured (0.5 %). Biological failures (caries, periodontitis or periimplantitis) did not occur. The statistical analysis of the factors did not reveal any significant differences. CONCLUSION. Modern all-ceramic FPDs seem to be an appropriate therapy not only for single restorations but for complex occlusal rehabilitations.

리튬 디실리케이트 최종 결정화 과정이 CAD/CAM으로 제조된 수복물의 적합도에 미치는 영향 (Influence of final crystallization process on precision of fit of monolithic CAD/CAM-generated restorations by lithium disilicate: A comparative study)

  • 김재홍;김기백
    • 대한치과기공학회지
    • /
    • 제41권4호
    • /
    • pp.271-278
    • /
    • 2019
  • Purpose: To quantify the effect of the crystallization process on lithium disilicate ceramic crowns that are fabricated using a computer-aided design/computer-aided manufacturing(CAD/CAM) system, and to determine whether they are clinically acceptable by comparing values before and after the crystallization process. Methods: The maxillary first molar was selected as the abutment for the experiments. Ten working models were prepared. Marginal and internal gap of 4 groups of lithium disilicate crowns(n=10) fabricated with conventional method. Comparison was performed using the silicone replica technique and 3D superimposition analysis. The marginal and internal gaps of the restoration were measured before and after the crystallization process of this prosthesis. The average value of each part(the average of values measured before and after the crystallization) was statistically analyzed using paired t-test(α=0.05). Results: The results from the second phase of this research, which compared the average value of the gap between the marginal and internal fits of the lithium disilicate single crown before and after the crystallization process, indicated that the marginal gap was larger and the internal gap was smaller after the crystallization process, and this difference was statistically significant (P<0.05) in all the parts evaluated. Conclusion: While the shrinkage that occurs during crystallization does affect the marginal and internal fit of the prosthesis, it cannot be concluded to be a major effect because the resultant distortion was within the clinically acceptable range.

IPS-Empress system을 이용한 상악 중절치의 치관복제술 (Crown Duplication Technique of Upper Central Incisor using IPS-Empress system)

  • 오상천;신영호
    • 구강회복응용과학지
    • /
    • 제22권3호
    • /
    • pp.243-250
    • /
    • 2006
  • Due to high esthetic demands from patients, we are driven to fabricate natural-looking(form and color) restorations. In the past decade, the glass-ceramic in dentistry has been used as a material with variable crystals that affects the appearance, characteristics, and mechanical properties of metal-free fixed restoration. The conventional IPS Empress glass-ceramic is a heat-pressed, leucite reinforced material using the "lost wax" principle. This glass-ceramic has been successfully used for esthetic restorations such as all-ceramic crowns, inlays/onlays, and veneers for about 15 years. This article presents that the form and surface texture of clinical crown are duplicated by IPS-Empress system using "lost-wax technique".

Fracture resistances of zirconia, cast Ni-Cr, and fiber-glass composite posts under all-ceramic crowns in endodontically treated premolars

  • Habibzadeh, Sareh;Rajati, Hamid Reza;Hajmiragha, Habib;Esmailzadeh, Shima;Kharazifard, Mohamadjavad
    • The Journal of Advanced Prosthodontics
    • /
    • 제9권3호
    • /
    • pp.170-175
    • /
    • 2017
  • PURPOSE. The aim of the present study was to evaluate the fracture resistances of zirconia, cast nickel-chromium alloy (Ni-Cr), and fiber-composite post systems under all-ceramic crowns in endodontically treated mandibular first premolars. MATERIALS AND METHODS. A total of 36 extracted human mandibular premolars were selected, subjected to standard endodontic treatment, and divided into three groups (n=12) as follows: cast Ni-Cr post-and-core, one-piece custom-milled zirconia post-and-core, and prefabricated fiber-glass post with composite resin core. Each specimen had an all-ceramic crown with zirconia coping and was then loaded to failure using a universal testing machine at a cross-head speed of 0.5 mm/min, at an angle of 45 degrees to the long axis of the roots. Fracture resistance and modes of failure were analyzed. The significance of the results was assessed using analysis of variance (ANOVA) and Tukey honest significance difference (HSD) tests (${\alpha}=.05$). RESULTS. Fiber-glass posts with composite cores showed the highest fracture resistance values ($915.70{\pm}323N$), and the zirconia post system showed the lowest resistance ($435.34{\pm}220N$). The corresponding mean value for the Ni-Cr casting post and cores was reported as $780.59{\pm}270N$. The differences among the groups were statistically significant (P<.05) for the zirconia group, as tested by ANOVA and Tukey HSD tests. CONCLUSION. The fracture resistance of zirconia post-and-core systems was found to be significantly lower than those of fiber-glass and cast Ni-Cr post systems. Moreover, catastrophic and non-restorable fractures were more prevalent in teeth restored by zirconia posts.