Journal of Korea Technical Association of The Pulp and Paper Industry
/
v.37
no.5
s.113
/
pp.1-7
/
2005
The objective of this work was to investigate the effect of spreading behavior of the sizing agents (AKD or dialkyl ketone) on the sizing development of AKD-sized paper. There was a direct relationship between the spreading behavior of the sizing agents and their melting points. Both AKD and dialkyl ketone showed no substantial spreading until the temperature reaches to their melting points. Consequently, dialkyl ketone did not provide sizing development when the paper was heat-treated below $75^{\circ}C$, while AKD provided sizing effect even the paper heated at $50^{\circ}C$. The ketone, however, provided rather higher sizing effect than that of AKD, when the paper was heat-treated over $100^{\circ}C$. This result means that the ketone also gives sizing development to paper, moreover the ketone could give higher sizing effect to paper than AKD when it was melted and well spreaded on the fiber surface. While the ketone introduced to papers from hydrolyzed AKD emulsion could not contribute to sizing development.
Journal of Korea Technical Association of The Pulp and Paper Industry
/
v.39
no.1
s.119
/
pp.16-24
/
2007
This study was performed to investigate the reaction between alkylketene dimer(AKD) and cellulose molecules in AKD-sized paper sheet. AKD was added to highly beaten($80{\pm}3^{\circ}SR$) SwBKP(ca. 0.8% on pulp) in order to have much AKD retention in the paper sheet. This AKD-sized paper sheet was aged at different temperatures, $60^{\circ}C,\;80^{\circ}C,\;105^{\circ}C\;and\;125^{\circ}C$. Changes in FT-IR spectra of AKD in paper sheet during the ageing were measured. In addition, sizing degrees of the AKD-sized paper sheet pretreated for 30 sec. at $105^{\circ}C$ were measured by HST size tester during the storage at different temperature. IR spectra of AKD-sized paper sheet preheated at $105^{\circ}C$ for 30 sec. showed unchanged spectra two absorption bands at $1849cm^{-1}\;and\;1722cm^{-1}$ which refer to the typical AKD IR bands. However, these typical AKD bands were gradually reduced with increasing ageing, completely disappeared after 6 hrs. and formed new absorption band at $1706cm^{-1}$, which refers to carbonyl stretching vibration of dialkylktone. Eventually the AKD molecule was hydrolyzed to diakylketone without formation of ${\beta}$-ketoester with cellulose in paper sheet. After 6 days ageing, a little amount of ${\beta}$-ketoester bands was identified in 6 or 7 days ageing, because of the absence of water due to long-term heating. The same tendency was observed at different ageing conditions. At the practical papermaking process, AKD reacts prevailing with water, and mostly seems to be hydrolyzed to dialkylketene. Concerned to the sizing development, AKD-sized paper sheet was shown no sizing development at the initial stage of ageing at $60^{\circ}C$ after heating treatment at $105^{\circ}C$ for 30 sec., and gradually increased the sizing degree with increasing ageing, such as Hercules Sizing Tester (HST) 130 see for 12 hr, HST 300 sec. for 3 days and HST 400 sec. for 5 days. It was concluded that hydrolyzed AKD could contributed to the sizing development of the paper sheet.
Journal of Korea Technical Association of The Pulp and Paper Industry
/
v.34
no.1
/
pp.1-6
/
2002
Alkaline sizing characteristics of TMP (thermomechanical pulp) handsheets with AKD (alkylketene dimer) were studied under various conditions. The sizing degree of TMP handsheet was much lower than that of chemical pulp. Especially, the sized TMP handsheet dried at $20^{\circ}C$ showed no sizing features, but sizing degree of TMP handsheet was clearly Increased by heat treatment at $105^{\circ}C$. The sizing effect of TMP was also improved by addition of $CaCO_3$, but it was not affected by pH. Therefore, sizing effect of TMP with AKD can be improved to some extent by controlling stock condition and heat treatment of handsheet.
Proceedings of the Korea Technical Association of the Pulp and Paper Industry Conference
/
2000.11a
/
pp.83-83
/
2000
Alkylketene dimer was known as a cellulose reactive or alkaline size because it does not require to fix to the fiber as do the traditional rosin sizes. A proposed sizing mechanism of AKD was the formation of P -ketoester bond between AKD and cellulose which provides the permanent attachment and the orientation of the hydrophobic alkylchains outward. However, some questions about the reaction had arisen and thus, the sizing mechanism of AKD has been a subject of controversy for several decades. The major concern of the controversy is that AKD is really reactive with cellulose or not in the papermaking conditions. In this study, reaction between AKD and pulp fiber was investigated, in order to find out whether AKD forms P-ketoester with pulp fiber during aging under no catalyzed neutral condition with obvious spectroscopic evidence. In addition, effect of aging treatment on the sizing development was studied. It has been disclosed that, in absence of water, AKD reacted with cellulose to form P -ketoester linkage under no catalyzed neutral condition, while, in presence of water, most of AKD was hydrolyzed to a dialkyl ketone or P -ketoacid. In addition, during the aging treatment of AKD-sized paper, its typical IR spectra bands gradually were reduced, completely disappeared after 6hr aging, and formed new absorption bands at 1707cm-' and shoulder peak at 1700cm-' which refer to the typical dialkylketone absorption bands. Therefore, the formation of P -ketoester between AKD and pulp fiber is impossible in the practical papermaking process. It could be suggested that the sizing development of AKD-sized paper is obtained by next two mechanism: 1) formation of a thin-layer of AKD on the fiber surface through melting and spreading of AKD emulsion particles by heat and 2) the hydrolysis of AKD to dialkyl ketone which has higher melting point, during drying and storage of AKD sized papers.
Journal of Korea Technical Association of The Pulp and Paper Industry
/
v.32
no.5
/
pp.1-7
/
2000
Alkaline Sizing behavior and mechanism of handsheets, which were prepared from thermomechanical pulp (TMP) with alkylketene dimer (AKD), were studied in terms of the conditions of the handsheet-making. AKD content in the TMP handsheets was increased with increasing of AKD addition level and the addition of a polyamideamine-epichlorohydrin resin (PAE) clearly enhanced AKD retention as well as the resultant sizing performance of TMP handsheets. Although drying of the AKD sized TMP webs at $20^{\circ}C$ led to no or quite low sizing level, but TMP handsheets sized with AKD had higher sizing degrees with increasing of the temperature of heat treatment. Scanning electron microscopic observations of the AKD-sized TMP handsheets showed that AKD emulsion particles were present on pulp fiber surfaces independently without coagulation in the TMP handsheets dried at $20^{\circ}C$. Heat treatment of the AKD-sized handsheets resulted in disappearance of the AKD emulsion particles because of their melting and spreading. The addition of calcium carbonate filler to the TMP suspensions did not influence on AKD content in the TMP handsheets. Nevertheless, their sizing degrees clearly increased by the addition of $CaCO_3$filler. Probably, AKD molecules adsorbed on the $CaCO_3$filler particles contribute to the enhancement of sizing performance. Thus, AKD can give sizing features effectively to the TMP handsheets, when they are made under suitable conditions.
Proceedings of the Korea Technical Association of the Pulp and Paper Industry Conference
/
1999.11b
/
pp.50-55
/
1999
Sizing development of AKD-sized paper by beta-ketoester formation has been debated until recent years because of absence of its obvious and direct spectroscopic evidence. In this study, reaction between AKD and cellulose was investigated to disclose the possibility of beta-ketoester formation between two components under no catalyzed neutral condition. In absence of water, AKD reacted with cellulose to form beta-ketoester linkage under no catalyzed neutral condition, while, in presence of water, most of AKD was hydrolyzed to a dialkyl ketone or beta-ketoacid. Therefore, the main mechanism of AKD sizing would not be the formation of beta-ketoester between AKD and cellulose in the papermaking process. It could be suggested that the sizing development of AKD-sized paper is obtained by next two mechanisms: 1) formation of a thin-layer of AKD on the fiber surface through melting and spreading of AKD emulsion particles by heat, and 2) the formation of ketone by the hydrolysis of AKD during drying and storage of AKD-sized papers.
To use the agricultural residues as the raw material of molded packaging material, the packaging trays were manufactured from rice-straw pulp. The physical properties were measured to compare non-treated trays with the addition trays, such as the addition of starch, rosin size, carboxymethyl cellulose(CMC), polyethylene glycol(PEG), alkylketene dimer(AKD), polyacryl amide(PAM). The results were as follows : 1. In the addition of starch, air permeability at addition of 5% was highest. Bursting strength and tensile strength were smaller than non-treated trays. 2. In the addition of rosin size, air permeability, bursting strength and tensile strength were smaller than non-treated trays. 3. In the addition of CMC, air permeability was higher than non-treated trays. Bursting strength and tensile strength were similar to non-treated trays. 4. In the addition of PEG, air permeability was higher than non-treated trays. Bursting strength at addition of 3% was the highest and tensile strength was smaller than non-treated trays. 5. In the addition of AKD, air permeability at addition of 1% and 5% was higher than non-treated trays. Bursting strength and tensile strength were smaller than non-treated trays. 6. In the addition of PAM, air permeability at addition of 0.01% was the highest. Tensile strength at addition of 0.01% were higher than non-treated trays. 7. The water absorption of the trays decreased with increasing adding of natural additives.
Journal of Korea Technical Association of The Pulp and Paper Industry
/
v.30
no.2
/
pp.24-29
/
1998
This study was carried out in order to elucidate the deterioration mechanism of paper according to various sizing chemicals. No additive paper and four kinds of papers containing rosin-alum, alum only, alkylketene dimer(AKD)-cation polymer and cation polymer only were treated by UV light to study changes of water-resistant, optical and mechanical properties from the view points of natural deterioration of paper. Since rosin chemicals have UV absorption at the relatively long wavelength region, rosins are degraded to form hydrophilic groups such as carboxylic acid from their double bonds by UV treatments. These phenomena caused the decreasing of sizing degree and wetting time in case of rosin-sized paper, while the UV treatments brought about the slight increase of wetting time in rosin-free papers such as no additive, alum and kymene only paper owing to the auto-sizing effect. Optical properties were primarily influenced by sizing chemicals. Rosin-sized paper showed lower brightness after UV and near UV treatment because of its UV instability.
The objective of this study was to investigate the influence of the water repellents' treatment on the water absorptivity and the dimensional stability of Korean red pine wood(Pinus densiflora). The alkylketene dimer(AKD), fluororesin emulsion(Wood-seal, WS), and paraffin wax emulsions(PW25, PW40, and PW1200) were used as water repellents. PW40 and WS were proved as excellent water repellents for pine wood, because the samples treated with these agents showed high contact angles and large reduction in water absorptivities. Also, the dimensional stability(antiswelling efficiency) of pine wood was considerably improved by water repellents treatments, such as PW40 and WS at the pressure of 2MPa. The water repellent treated woods with WS, PW40, and PW1200 at the pressure of 2MPa were relatively stable to the wet-dry cyclic leaching test.
This study was conducted to determine the properties of seedling plate papers currently used in commercial production, then to get basic information for manufacturing new seedling plate paper. Imported seedling plate paper had high wet tensile and burst strengths in its usage circumstances. Wet tensile strength was very high with 38.7% of dry tensile strength. Wet burst strength was also very high with 62.4% of dry burst strength. The seedling plate paper contained about 30% of synthetic fibers. It had 10 Gurley sec. in air permeability indicating effective movement of air. Seedling plate papers were' made in laboratory scale. For sufficient sizing degree, the addition of 0.5% AKD (alkylketene dimer) by weight was good enough. Additional amount of AKD more than 0.5% by weight caused strength loss even though improving sizing effect. The addition of wet strength reagent such as Finex-B 2% by weight resulted in good strength and air permeability.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.