• 제목/요약/키워드: activation energy for decomposition

검색결과 128건 처리시간 0.023초

Thermogravimetric Analysis of Rice Husk Flour for a New Raw Material of Lignocellulosic Fiber-Thermoplastic Polymer Composites

  • Kim, Hyun-Joong;Eom, Young-Guen
    • Journal of the Korean Wood Science and Technology
    • /
    • 제29권3호
    • /
    • pp.59-67
    • /
    • 2001
  • Rice husk flours were analyzed by chemical composition and thermogravimetric methods in nitrogen atmosphere to discuss its feasibility as a raw material for manufacturing agricultural lignocellulosic fiber-thermoplastic polymer composite. It was revealed in the chemical composition analysis that rice husk flour was composed of moisture, 5.0%; lignin, 21.6%; holocellulose, 60.8%; ash, 12.6%. In the thermogravimetric analysis (TGA), thermal decomposition behavior of rice husk flour from room temperature to $350^{\circ}C$ was similar to that of wood flour, but rice husk flour was more thermally stable from 350 to $800^{\circ}C$ than wood flour because of higher silica content in the rice husk flour and smaller particle size of rice husk flour. The activation energy of thermal decomposition was evaluated using Flynn & Wall expression. As the thermal decomposition proceeded in rice husk flour, the activation energy of thermal decomposition appeared almost constant up to ${\alpha}=0.25$, but thereafter increased. Activation energy of thermal decomposition in wood flour, however, decreased steeply up to ${\alpha}=0.3$, but thereafter remained almost constant. From the results, rice husk flour was thought be a substitute for wood flour in manufacturing agricultural lignocellulosic fiber-thermoplastic polymer composite in the aspect of thermal decomposition.

  • PDF

고무용 카본블랙 촉매를 이용하는 메탄분해에 의한 수소 생산 (Hydrogen Production by Catalytic Decomposition of Methane over Rubber-Grade Carbon Blacks)

  • 윤기준;류보현;이상엽;한귀영
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 한국신재생에너지학회 2005년도 춘계학술대회
    • /
    • pp.223-226
    • /
    • 2005
  • For $CO_2-free$ hydrogen production and better utilization of the produced carbon, catalytic decomposition of methane over rubber-grade carbon blacks manufactured from coal tar was carried out. The catalytic activities of several domestic carbon blacks were compared. A pelletized carbon black exhibited considerably lower activity and activation energy than the fluffy( loose) carbon black of the same grade. This difference is considered due to the binder that was added during pelletization. For pelletized carbon blacks, a tendency was observed that the activity per unit mass of catalyst increased with the specific surface area of the carbon black. Another tendency was also observed that the activation energy increased with the primary particle size or decrease of the specific surface area.

  • PDF

Comparison Study of Thermal Decomposition Characteristics of Wattle & Pine Tannin-based Adhesives

  • Kim, Sumin;Lee, Young-kyu;Kim, Hyun-Joong;Eom, Young Geun
    • Journal of the Korean Wood Science and Technology
    • /
    • 제30권3호
    • /
    • pp.34-41
    • /
    • 2002
  • This study investigated the thermogravimetric analysis of two types of cured tannin-based adhesives from wattle and pine, with three hardeners of paraformaldehyde, hexamethylenetetramine and TN (tris(hydroxyl)nitromethan), at a temperature of 170℃ and a heating rate of 5, 10, 20 and 40℃/min for 10 minutes. The 5 minutes cured wattle tannin-based adhesive with each hardener at 170℃ was also tested to compare the degree of curing. It was found that thermogravimetric analysis could be used to measure the degree of curing of a thermosetting adhesive. The TG-DTG curves of all the adhesive systems were similar and showed three steps in a similar way to a phenolic resin. This means that each adhesive system is well cross-linked. However, a high thermal decomposition rate was shown at 150 to 400℃ in the case of the pine tannin sample with TN (tris(hydroxyl)nitromethan). The Flynn & Wall expression was used to evaluate the activation energy for thermal decomposition. As the level of conversion (𝛼) increased, the activation energy of each system increased. The activation energy of the wattle tannin-based adhesive with paraformaldehyde was higher than the others.

결정화에 의한 4성분계 에너지 복합체 제조 및 열분해 특성 (Preparation of Quaternary Energetic Composites by Crystallization and Their Thermal Decomposition Characteristics)

  • 김병수;김재경;안익성;김현수;구기갑
    • 공업화학
    • /
    • 제30권2호
    • /
    • pp.178-185
    • /
    • 2019
  • 결정화/응집 공정을 이용하여 금속/금속산화물/분자화약/산화제로 구성된 구형 4성분계 복합체 3종을 제조하였다. 열중량 분석(TGA) 및 시차주사열량법(DSC)에 의한 열 특성 분석 결과 복합체를 이룬 분자화약의 분해 구간이 단축됨을 관찰하였고, ammonium perchlorate(AP) 분해 생성물인 HCl 및 $ClO_2$에 의한 자가 촉매 반응에 의한 것으로 해석된다. 활성화 에너지 분석 결과 분자화약 분해 종료 구간에서 급격하게 활성화 에너지가 감소함을 확인할 수 있었으며, 이는 분자화약 분해 생성물 중 공통으로 발생하는 $HNO_2$에 의한 것으로 판단된다. 본 연구에서 복합체 열분해 분석 결과로부터 Distributed Activation Energy Model (DAEM)에 의해 모사된 활성화 에너지가 model-fitting 분석법인 Kissinger-Akahira-Sunose와 Flynn-Wall-Ozawa model에 의한 모사치보다 정확도가 대단히 우수함을 알 수 있었다.

초음파를 적용한 PET 직물의 알칼리 가수분해에 관한 연구(I) - 분해속도상수와 활성화 에너지- (A Study on the Alkali Hydrolysis of PET fabric with Ultrasonic Application(I) - Decomposition Rate Constant and Activation Energy -)

  • 서말용;조호현;김삼수;전재우;이승구
    • 한국염색가공학회지
    • /
    • 제14권4호
    • /
    • pp.214-222
    • /
    • 2002
  • In order to give a silk-like touch to PET fabrics, the PET fabrics were treated with NaOH alkaline solution in various conditions. In alkaline treatment, the liquor flow type pilot weight reduction apparatus with magnetostrictive ultrasonic transducer was used for the study. The weight loss of PET fabrics hydrolyzed in 4% and 6% NaOH solution, at $95^\circ{C}$ and $99^\circ{C}$ for 60min. with ultrasonic application showed 3.7~4.6% higher than that of treated fabric without ultrasonic application. From the difference of specific weight loss, the treatment condition of the maximum of hydrolyzation effect appeared at $95^\circ{C}$ in $4^\circ{C}$ and at $90^\circ{C}$ in 6% NaOH solution, respectively. During the alkali hydrolysis of PET fabrics, the decomposition rate constant(k) increased exponentially with the treatment temperature and were not related with ultrasonic cavitation. The activation energy$(E_a)$ in decomposition of PET fabrics were 21.06kcal/mol with ultrasonic application and 21.10kcal/mol without ultrasonic application. The ultrasonic application gave a little higher value of the activation entropy$(\Delta{S}^\neq)$ and a little lower value of Gibbs free energy$(\Delta{S}^\neq)$ compared with not used ultrasonic apparatus.

양이온 개시제를 이용한 열경화성 액정 에폭시의 열분해 활성화에너지 (Thermal Decomposition Activation Energy of Liquid Crystalline Epoxy using Cationic Initiator)

  • 정예지;현하늘;조승현
    • Composites Research
    • /
    • 제34권3호
    • /
    • pp.180-185
    • /
    • 2021
  • 기존 아민계 경화제를 사용해 액정 에폭시를 경화할 경우, 랜덤 한 3차원 네트워크 구조의 생성으로 인해 phonon의 산란이 많이 발생하기 때문에 열전도도가 낮게 나타났다. 이러한 문제를 mesogen그룹을 적층된 구조로 형성하는 양이온 개시제를 이용하여 해결하기 위해 본 연구에서는 아민계 경화제와 양이온 개시제를 사용한 에폭시의 TGA분석(Thermogravimetric Analysis)을 통해 등온 열분해 활성화에너지를 조사하여 열적안정성을 비교하였다. 양이온 개시제를 이용한 에폭시의 경우 활성화가 에너지가 높았으며 기존 실험과 비교했을 때, 열적안정성은 열전도도와 비슷한 양상을 보인다.

밀가루의 열분해 특성과 활성화 에너지에 관한 연구 (A Study on the Activation Energy and Characteristics of the Heat Decomposition of Flour)

  • 권승렬;최재욱;이동훈;최재진
    • 한국안전학회지
    • /
    • 제24권6호
    • /
    • pp.55-62
    • /
    • 2009
  • After examining the characteristics of the heat decomposition of the 80~120mesh flour using the Mini cup pressure vessel test and determining the apparent activation energy in a spontaneous combustion, the conclusion is as follows. The heat decomposition of flour occurs at around $100^{\circ}C$ and the peak for the maximum rise in pressure appears at around $290^{\circ}C$. The decomposition pressure against various temperature in the vessel shows the maximum value of $4.7kg/cm^2$ approximately at $440^{\circ}C$. When the thickness of the sample is 3cm, the maximum temperature and the critical temperature of ignition are $398^{\circ}C$ and $204.5^{\circ}C$, respectively; the critical temperature is $194.5^{\circ}C$ when the thickness of the sample is 5cm, and $182.5^{\circ}C$ when the sample is 7cm. In addition, the apparent velocity calculated using the method of least squares is 35.0407Kcal/mol.

Thermal Decomposition Kinetics of Polyurethane Elastomers Prepared with Different Dianiline Chain Extenders

  • Ahn, WonSool
    • Elastomers and Composites
    • /
    • 제51권2호
    • /
    • pp.122-127
    • /
    • 2016
  • Thermal decomposition kinetics for two different types of polyurethane elastomers prepared with 2,2'-dichloro-4,4'-methylenedianiline (MOCA) and 3,5-dimethyl-thiotoluenediamine (Ethacure-300), based on PTMG/TDI isocyanate prepolymer, were studied using non-isothermal thermogravimetric analysis (TGA). Thermograms were obtained and analyzed using Friedman (FR) and Kissinger-Akahira-Sunose (KAS) methods for activation energy, $E_a$. The results obtained showed that decomposition reaction of both samples was observed similarly to occur through three different stages, i.e., initial stage with vaporization of low molecular weight materials, second stage of urethane linkage decompositions, and later stage of polyol segment decompositions. However, activation energy values at each stage for the sample cured with Ethacure-300 was much lower than those for the sample with MOCA, exhibiting relatively lower thermal stability for the sample with Ethacure-300 than that with MOCA.

PS/SAN/ABS의 열분해특성과 생성물의 독성에 관한 연구 (A Study of Thermal Decomposition Characteristics and Toxicity of Product on PS/SAN/ABS)

  • 강윤진;이내우;설수덕
    • 한국가스학회지
    • /
    • 제4권1호
    • /
    • pp.16-25
    • /
    • 2000
  • 스틸렌 공중합체의 열적특성과 독성인자를 평가하기 위하여 활성화 에너지, 물리적 특성 및 마취성 기체와 같은 독성물질의 발생가능성에 대하여 조사하였다 고온 분해시에 Kissinger법과 DSC법에 의해 계산된 활성화 에너지는 25${\~}$50 Kcal/mol이었다. 이것은 화재발생가능성에 대하여 좋은 정보가 될 것이다 FED계산으로부터 PS, SAN 및 ABS에 대한 $LC_{50}$의 값은 8,580, 265 및 308 $mg/m^3$이 되었다. FT-IR에 의해 분석한 열분해 반응의 메카니즘은 측쇄반응이 아니고 주쇄반응이었다.

  • PDF

PVAc 라텍스 접착제의 열적 안정성에 대한 고찰 (A Consideration on Thermal Stability of the PVAc Latex Adhesive)

  • 권재범;이내우;설수덕
    • 한국안전학회지
    • /
    • 제18권3호
    • /
    • pp.81-87
    • /
    • 2003
  • Latex polymers are widely used for adhesive, binder, paint etc. Especially the PVAc(Polyvinyl acetate) latex which manufactured by vinyl acetate and vinyl alcohol as protective colloid is a useful environmentally friendly adhesive. To increase useful property of PVAc latex, this study was carried out for checking thermal characteristics and physical condition of PVAc latex by DSC, FT-IR, Pyrolyzer GC-MS. The activation energies of thermal decomposition for 40, 48, 56, 64% solid content of PVAc latex were found as 28.1-36.0kcal/mol by Kissinger's method and 17.2-22.0kcal/mol by DSC method. Actually, reasonable solid content could be consiered as 56% because of activation energy and adhesive characteristics. According to the effect of protective colloid for 4, 10, 15, 20wt%, the activation energy shows same tendency to both method and in case of l5wt% has been found as the highest activation energy. The mechanism of thermal decomposition was mainly estimated by main chain scission, not by side group on FT-IR analysis. Main component of Pyrolzer GC-MS result were consisted of $CH_3COOH$, $CH_3$, $H_2O$ and light gases(CO, $CO_2$, $CH_4$ etc).