• 제목/요약/키워드: acicular

검색결과 207건 처리시간 0.024초

순 Ti GTA 용접부의 미세조직과 경도에 미치는 Ar-N2 보호가스 중 질소량의 영향 (Effect of Nitrogen Volume in Ar-N2 Shielding Gas on Microstructure and Hardness of GTA Welded Pure Ti)

  • 안현준;전애정;홍재근;정보영;이종섭;강정윤
    • Journal of Welding and Joining
    • /
    • 제30권2호
    • /
    • pp.70-75
    • /
    • 2012
  • In this study, effect of nitrogen volume in the shielding gas of Ar-$N_2$ mixing gas on the bead shape, hardness and microstructure of GTA welds of 3mm thick Commercial Pure Ti was investigated. As the nitrogen volume increased, the welding current for full penetration was reduced and hardness in the fusion zone significantly increased compared with that of the base metal, but there is no difference in the hardness of HAZ. Microstructure in the fusion zone with pure Ar gas changed from equiaxed alpha of the base metal to serrated alpha. On the other hand, microstructure using Ar-$N_2$ mixing gas changed to acicular alpha. With the increasing of nitrogen content, the amount of acicular alpha increased and the size of that was fine.

Microstructure and CTOD (crack tip opening displacement) of Deposit Weld Metal in 30 mm Thick Plate

  • Lee Hae-Woo;Kim Hyok-Ju;Park Jeong-Ung;Kang Chang-Yong;Sung Jang-Hyun
    • 한국재료학회지
    • /
    • 제14권9호
    • /
    • pp.642-648
    • /
    • 2004
  • The microstructure and crack tip opening displacement (CTOD) of deposit weld metal were investigated for a 30 mm- thick plate welded with flux cored arc welding (FCAW) and submerged arc welding (SAW) processes. The CTOD test was carried out both as welded condition and as stress-relieved specimen by local compression. The crack growth rates in FCAW were faster than those in a SAW, and the acicular ferrite content by the SAW process was increased relatively more than that by the FCAW process. The fatigue crack growth rate in a welded specimen was faster than that in locally compressed specimen. The CTOD value of locally compressed specimens was lower than that of as welded specimen. Furthermore, the CTOD value tested with the SAW process was higher than that tested with the FCAW process.

티타늄 주조체 냉각방법이 표면반응층에 미치는 영향 (The Effect of Cooling method on the Surface Reaction Zone of CP Titanium Casting Body)

  • 문수;최석순;문일
    • 대한치과기공학회지
    • /
    • 제23권2호
    • /
    • pp.203-210
    • /
    • 2002
  • This test is to conduct applied research the reaction area of the Ti-cast metal body which is made use of Dental Phosphate-silica alumina bonded investment material selling at a market, and the cooling method is how to effect on the acicular. The experimentation is as followings, 1. Experimental specimens After invest with Dental Phosphate-silica alumina bonded investment material, the $10{\times}10{\times}1.0mm^3$ wax pattern was casted by Dental high vacuum argon centrifugal casting machine. 2. Test We can analyze SEM/EDS, XRD utilize the fractography(an optical microscope). 3. Conclusion The pure cast metal body constituted of reaction products layer, stability layer and contamination layer. This pure cast have no connection with the cooling condition. The pure Titanium shows difference in a component distribution according to the cooling condition. Through this experimentation we can establish that acicular in the pure Ti-cast metal is consist of Hexagonal structure a=2.9505$\AA$, c=4.6826$\AA$.

  • PDF

리드프레임/EMC 계면의 파괴 인성치 (Fracture Toughness of Leadframe/EMC Interface)

  • 이호영;유진
    • 한국표면공학회지
    • /
    • 제32권6호
    • /
    • pp.647-657
    • /
    • 1999
  • Due to the inherently poor adhesion strength of Cu-based leadframe/EMC (Epoxy Molding Compound) interface, popcorn cracking of thin plastic packages frequently occurs during the solder reflow process. In the present work, in order to enhance the adhesion strength of Cu-based leadframe/EMC interface, black-oxide layer was formed on the leadframe surface by chemical oxidation of leadframe, and then oxidized leadframe sheets were molded with EMC and machined to form SDCB (Sandwiched Double-Cantilever Beam) and SBN (Sandwiched Brazil-Nut) specimens. SDCB and SBN specimens were designed to measure the adhesion strength between leadframe and EMC in terms of critical energy-release rate under quasi-Mode I ($G_{IC}$ ) and mixed Mode loading ($G_{C}$ /) conditions, respectively. Results showed that black-oxide treatment of Cu-based leadframe initially introduced pebble-like X$C_2$O crystals with smooth facets on its surface, and after the full growth of $Cu_2$O layer, acicular CuO crystals were formed atop of the $Cu_2$O layer. According to the result of SDCB test, $Cu_2$O crystals on the leadframe surface did not increase ($G_{IC}$), however, acicular CuO crystals on the $Cu_2$O layer enhanced $G_{IC}$ considerably. The main reason for the adhesion improvement seems to be associated with the adhesion of CuO to EMC by mechanical interlocking mechanism. On the other hand, as the Mode II component increased, $G_{C}$ was increased, and when the phase angle was -34$^{\circ}$, crack Kinking into EMC was occured.d.

  • PDF

TiO2 성분 플럭스충진와이어에 따른 S500강의 GMA 용접부 특성 (Characteristics of GMA Weld Zone on TiO2 Different Component Flux Cored Wire for S500 Grade Steel)

  • 유철;고영봉;박경채
    • 한국표면공학회지
    • /
    • 제48권6호
    • /
    • pp.335-342
    • /
    • 2015
  • Recently, the production of oil and gas at the arctic ocean and offshore has been growing. Accordingly, S500 steel with the high tensile strength and excellent toughness has been used and flux cored wire that can be welded to the S500 has been required. In this study, we carried out observation of microstructures, mechanical properties and CTOD (crack tip openning displacement) in the weld zone that GMA (gas metal arc) welded with different component of $TiO_2$ flux core wire (the main components, rutile or Ti-slag) for S500 steel. Weld zone produced with Ti-slag flux cored wire has formed a enough acicular ferrite and shown excellent impact toughness at $-40^{\circ}C$, tensile strength at room temperature and CTOD at $-20^{\circ}C$. As a result, the developed flux cored wire was suitable for S500 steel.

Microstructure and Mechanical Properties of Solution Treatment and Sr-Modification of Al-12%Si-1.5%Cu Alloy

  • Surin, Prayoon;Wong on, Jessada;Eidhed, Krittee
    • International Journal of Advanced Culture Technology
    • /
    • 제3권2호
    • /
    • pp.132-137
    • /
    • 2015
  • The purpose of this paper was to investigate the effects of solution treatment time and Sr-modification on the microstructure and property of the Al-Si piston alloy. It was found that as-cast microstructures of unmodified and Sr-modified Al-Si alloys consisted of a coarse acicular plate of eutectic Si, $Cu_3NiAl_6$ and $Mg_2Si$ phases in the ${\alpha}$-Al matrix but different in size and morphology. Both size and inter-particle spacing of Si particles were significantly changed by increasing of the solution treatment time. After a short solution treatment, the coarse acicular plate of the eutectic Si appears to be fragmented. Fully modified microstructure of Sr-modified alloy can reduce the solution treatment time to shorter compared to unmodified alloy. The maximum of a peak hardness value is found in the very short solution treatment of both Al-Si piston alloys. Compared to 10 h solution treatment, the solution treatment of 2-4 h is sufficient to achieve appropriate microstructures and hardness. The short solution treatment is very useful to increase the productivity and to reduce the manufacturing cost of the Al-Si piston alloys.

오스템퍼링한 구상점연주철의 부식환경중의 마멸특성에 관한 연구 (A Study on the Wear Characteristics of Austempered Ductile Cast Iron in Corrosive Environments)

  • 강명순;전태옥;박흥식;진동규
    • 한국해양공학회지
    • /
    • 제2권2호
    • /
    • pp.87-95
    • /
    • 1988
  • This paper is studied to know corrowive wear characteristics of austempered ductile cast ironin corrosive environments against mating SM45C hardened two test pieces in distilled water and NaCl aqueous solution. The corrosive wear mechanism was investigated by scanning electron microscopy and retained austenite volume fraction was investigated by X-ray diffractometer. The experimental result show that the corrosive wear characteristics depend largely on the $\textrm{Fe(OH)}_{3}$which is influenced by the critical sliding distance $L_{cr}$ and $L_{cr}$ shorted with increasing NaCl concentration. It was found that the carbides in matrix have a significant effect on their corrosive wear resisance and the fine acicular bainite showed corrosive wear resistance stronger than that of the coarse acicular and platelet bainite. From above results the model of corrosive wear mechanism in corrosive environments is proposed.

  • PDF

다층용접한 저합금 용접금속의 강도와 인성에 미치는 입열량 및 예열/패스간 온도의 영향 (Effects of Heat Input and Preheat/interpass Temperature on Strength and Impact Toughness of Multipass Welded Low Alloy Steel Weld Metal)

  • 방국수;정호신;박찬
    • 한국해양공학회지
    • /
    • 제29권6호
    • /
    • pp.481-487
    • /
    • 2015
  • The effects of the heat input and preheat/interpass temperatures on the tensile strength and impact toughness of multipass welded weld metal were investigated and interpreted in terms of the recovery of the alloying elements and microstructure. Increases in both the heat input and preheat/interpass temperatures decreased the tensile strength of the weld metal. A lower recovery of alloying elements, especially Mn and Si, and smaller area fraction of acicular ferrite in the weld metal were observed in higher heat input welding, resulting in a lower tensile strength. In contrast, only a microstructure difference was observed at a higher preheat/interpass temperature. The impact toughness of the weld metal gradually increased with an increase in the heat input because of the lower tensile strength. However, it decreased again when the heat input was larger than 45 kJ/cm because of the much smaller area fraction of acicular ferrite. No effect of the preheat/interpass temperature on the impact toughness was observed. The formation of a weld metal heat-affect zone showed little effect on the impact toughness of the weld metal in this experiment.

Brown Oxide 형성이 리드프레임/EMC 계면의 파괴인성치에 미치는 영향 (Effect of Brown Oxide Formation on the Fracture Toughness of Leadframe/EMC Interface)

  • 이호영;유진
    • 한국표면공학회지
    • /
    • 제32권4호
    • /
    • pp.531-537
    • /
    • 1999
  • A copper based leadframe was oxidized in brown-oxide forming solution, then the growth characteristics of brown oxide and the effect of brown-oxide formation on the adhesion strength of leadframe to epoxy molding compound (EMC) were studied by using sandwiched double cantilever beam (SDCB) specimens. The brown oxide is composed of fine acicular CuO, and its thickness increased up to ~150 nm within 2 minutes and saturated. Bare leadframe showed alomost no adhesion to EMC, while once the brown-oxide layer formed on the Surface of leadframe, the adhesion strength increased up to ~80 J/$\m^2$ within 2 minutes. Correlation between oxide thickness, $\delta$ and the adhesion strength in terms of interfacial fracture toughness, $G_{c}$ was linear. Considering the above results, we might conclude that the main adhesion mechanism of brown-oxide treated leadframe to EMC is mechanical interlocking, in which fine acicular CuO plays a major role.e.

  • PDF