알루미늄 합금표면에 코팅된 세라믹재의 마찰마멸 특성 (Friction and Wear at Ceramic Coated Surfaces of Aluminum Alloy)

  • 공호성;권오관;김형선
    • 대한기계학회논문집
    • /
    • 제17권12호
    • /
    • pp.3083-3093
    • /
    • 1993
  • Friction and wear at ceramic coated surfaces of aluminum alloy were experimentally studied using a Ring-on-Block wear test machine. Ceramic materials coated on aluminum alloy surfaces were WC, CrC, $Al_{2}O_{3}$ by a plasma spray; and $Al_{2}O_{3}$,$Al_{2}SiO_{5}$, $Na_{2}B_{4}O_{7}$,$Na_{4}P_{2}O_{7}$, and $Al_{2}O_{3}-ZrO_{2}$ composite coating by an Anodic Spark Depositon. They were tested under the sliding wet contact and compared with aluminum alloys and steels. Test results showed that ceramic coated surfaces, in general, have better anti-wear property than those of aluminum alloys due to increase in the surface hardness ; however, they also showed higher coefficients of friction and changes in wear mechanisms, resulting in brittle fractures.

Ti 및 TiAl 주조재의 ${\alpha}$-case 형성에 미치는 공정변수에 대한 영향 (Effects of Process Parameter on Alpha-Case Formation of Ti and TiAl castings)

  • 이상화;김명균;성시영;김영직
    • 한국주조공학회지
    • /
    • 제23권3호
    • /
    • pp.137-146
    • /
    • 2003
  • The main purpose of this study is to investigate the effects of process parameter on alpha-case formation of Ti and TiAl castings. The previous studies showed that the molten titanium is excessively reactive to the refractory oxide mold, resulting in alpha-caes of the titanium castings regardless of composition of titanium alloys. However, the behavior of the alpha-case formation of TiAl alloy is not consistent with conventional titanium alloy. In order to investigate the alpha-case formation of Ti and TiAl castings with process parameter, especially the associated factors of investment mold such as mold material, binder and mold preheating temperature. An attempt has been made to characterize the alpha-case of titanium casting by using optical microscope, EDS, XRD, EMPA and hardness profiles. The formation of the alpha-case on the surface of pure titanium during investment casting was rather by that of solid solution with metallic element from mold material. The required mold strength was obtained with $CaZrO_3$ because of the possibility of using water soluble binder. However, the separation phenomenon between facing and back-up mold materials should be considered. The interfacial reaction of TiAl alloy showed different behavior from that of pure titanium and $Al_2O_3$ was best mold materials. The effect of binder as well as mold material on the formation of alpha-case was significant.

베릴륨(Be)이 미 첨가된 치과도재소부용 Ni-Cr-Mo계 합금의 미세조직 및 기계적 성질 특성 (Microstructures and Mechanical Properties of Beryllium(Be)-free Ni-Cr-Mo based Alloys for Metal-Ceramic Crown)

  • 송경우;고은경;이정환;정종현;노학;한재익
    • 대한치과기공학회지
    • /
    • 제28권2호
    • /
    • pp.321-329
    • /
    • 2006
  • The popularity of Ni-Cr-Mo based metal alloys for metal-ceramic crown have increased recently because of low price, superior yield strength and rigidity. the use of these alloys give them the potential advantage of thinner copping with the required rigidity for long span bridges. The purpose of this study was to assess the microstructures and mechanical properties of Ni-Cr-Mo-(Si,Al,Nb,Zr,Ti.Cu,Mm) based Alloys not containing beryllium(Be) related toxic effects. The abtained results indicated that as-cast these specimen alloys showed compositional and microstructural differences, and mechanical properties values of Ni69Cr20Mo5Si2Al4 alloy among these specimen alloys was found to be superior to those of commercial Ni-Cr based alloy using in market place today.

  • PDF

Fe-30Al-5Cr 합금의 미세조직 및 $D0_3{\leftrightarrow}B2$ 천이온도에 미치는 Ti, Hf 및 Zr의 첨가효과 (Effects of Titanium, Hafnium and Zircornium Alloying Elements on Microstructures and $D0_3{\leftrightarrow}B2$ Transition Temperature of Fe-30Al-5Cr Alloys)

  • 김성수;주성민;오선훈;김관휴;최답천
    • 한국주조공학회지
    • /
    • 제21권1호
    • /
    • pp.15-23
    • /
    • 2001
  • The changes in the microstructures and $D0_3{\leftrightarrow}B2$ transition temperature were investigated for Fe-30at.%AI-5at.%Cr alloy with the ordered $D0_3$, structure when Ti, Hf and Zr were added respectively. The addition of Cr has no effect on the microstructure. However, as the amount of Ti addition increased, the grain size became smaller. Addition of Ti+Hf, Ti+Zr and Ti+Hf+Zr also showed the similar effect. When 20at.% of Ti was added, the second phase precipitates on the substrate. The addition of Cr, Hf and Zr alone has no effect on $D0_3{\leftrightarrow}B2$ transition temperature. However, as the amount of Ti addition increased by 5, 10, 15 and 20at.%, the transition temperatures showed 929, 930, 960 and $930^{\circ}C$ respectively.

  • PDF

초고진공계재료 (UHV Materials)

  • 박동수
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 1998년도 제14회 학술발표회 논문개요집
    • /
    • pp.24-24
    • /
    • 1998
  • 반도체장비를 포함하는 초고진공장비의 園훌化가 급속히 그리고 절실히 요구되고 있는 것이 현실정이다. 當面해서 실현할 국산진공장비의 대상은 廣範圍하다. 즉, 각종 진공 pump ( (rotary, dry, diffusion, cryo, ion, turbo melecular pump), 진공 chamber, 진공 line, gate valve 를 위 시 한 진공 V머ve, flange, gasket, fl않d야lU, mainpulater 퉁 진공 部品이 다. 진공계 의 핵심 은 適切하고 優良한 진공재료의 선태파 사용이다. 진공장비는 사용자가 원하는 진공도를 원하 는 시간 동안 륨空度를 유지해 주어야 한다. 진공재료 선태의 기준사항은:(1) 기체의 透過성 (2) 薰했훌 (3) 혔體放出특성 - -outgassing과 degassing- (4) 機械的 량훌度 (5) 온도 의존성 (6) 化學톡성 (7) 加I성 및 鎔接 성 (8) 課電특성 (9) 磁氣특성 (10) 高速함子 및 放射線 특성 (11) 經濟성 및 調達생 둥이 다. 우량한 초고진공계재료는 풍부하게 개발되어 왔고, 또 新材料들이 개발되고 있다. 여기에서는 주로 초고진공 내지는 극고진공계의 構造材料, 機能材料, 部品材料 일반파 몇가지 신재료의 특 성에 관해서 記述한다. M Mild SteeHSAE, 1112, 1010, 1020, 1022, etc)., S Stainless SteeHAlSI, 304, 304L, 310, 316, 321, 347): 구조재료, chamber, fl하1ges A Aluminum과 Alloys (1060, 1100, 2014, 4032, 6(뻐1): 구조재료, chamber, flanges, gaskets A AI, Al 떠loy는 SS에 代替하는 역 할올 시 작하고 있다. C Copper, Copper Alloys(C11$\alpha$)0, C26800, C61400, Cl7200): 내장인자, gasket, cryopanel, tubing T Titanium, Ziriconium, Haf띠um 및 Alloys: 특히 Ti은 10n pump 용 getter material 이 외 에 U UHV,XHV용 chamber계로서 관심올 끌고 있다. N Nickel, Nickel Alloys (200, 204, 211, monel, nichrome): 부식 방지 , 전자장치 , 자기 장치 귀 금속(Ag, Au, Pt, Pd, Rh, Ir, Os, Ru): 보조부품, gasket, filament, coating, thermocouple, 접 합부위 T TiC, SiC, zrC, HfC, TaC 둥의 탄화물과, BN, TiN, AlN 동의 질화물, 붕화물이 둥장하고 었 다. 유리: Soda Lime, Borosilicate, Potash Soda Lead: View Port, Chamber envelope C Ceramics: AlZ03, BeO, MgO, zrOz, SiOz, MgOzSiOz, 3Alz032SiOz, Z$textsc{k}$hSiOz S상N4: e electrical, thermal insulators, crucibles, boats, single crystals, sepctr려 windows 저자는 최근 저자들이 발견한 Zr-Ti-Cu-Ni-Be amorphous alloys coated cham뾰r가 radiation p proof로 이용될 수 있는 사실을 점검하고 었다 .. Z.Y. Hua 들은 Cs3Sb를 새로운 photocathode 재료로 보고하고 있다.

  • PDF

황동합금의 미세조직과 내산화성에 미치는 미량 합금원소의 영향

  • 문재진;이동복
    • 한국신뢰성학회:학술대회논문집
    • /
    • 한국신뢰성학회 2002년도 정기학술대회
    • /
    • pp.117-120
    • /
    • 2002
  • The addition of minor alloying elements such as Al, Si, Mg, Cr, Zr, and Sn changed the microstructure and the oxidation characteristics of the Cu-40%Zn alloys. Detailed microstructure, scale morphology and the oxidation mechanism were described.

  • PDF

크롬동합금의 도전율과 경도에 미치는 용체화처리와 시효처리의 영향 (The Effects of Solution Heat Treatment and Aging Treatment on the Electrical Conductivity and Hardness of Cu-Cr Alloys)

  • 김신우
    • 열처리공학회지
    • /
    • 제15권1호
    • /
    • pp.21-24
    • /
    • 2002
  • The electrode materials for welding machine in automobile industry such as Cu-Cr, Cu-Zr and Cu-$Al_2O_3$ require the high electrical conductivity and the proper hardness. Therefore the effects of solution heat treatment and aging treatment on the electrical conductivity and hardness of Cu-0.8wt%Cr and Cu-1.2wt%Cr alloys have been investigated. Cu-0.8wt%Cr alloy showed the higher electrical conductivity and hardness than Cu-1.2wt%Cr alloy and both alloys showed the better electrical conductivity at $930^{\circ}C$ among 930, 980 and $1030^{\circ}C$ solution heat treatment temperatures. The electrical conductivity and hardness in both alloys were not affected by aging treatment but remarkably affected by solution heat treatment temperature. The final drawing process reduced electrical conductivity and increased hardness more in Cu-1.2wt%Cr alloy.

플라즈마질화처리에 의한 13Cr 스테인리스강의 표면경화특성에 미치는 질화물형성원소첨가의 영향 (Effects of Alloying Elements on Hardening of 13Cr Stainless Steels Using Plasma Nitriding Process)

  • 박화순;조희정;박봉규;강정윤
    • Journal of Welding and Joining
    • /
    • 제16권1호
    • /
    • pp.88-97
    • /
    • 1998
  • The surface characteristics of 13Cr stainless steel systems by plasma nitriding were investigated. The plasma nitriding for the 13Cr steels, in which the nitriding forming elements such as Ti, V, W, Nb, Al, Zr and Si were added about 2~3wt.%, respectively, was performed. In all nitrided specimens, .epsilon.-F $e_{2-3}$N, UPSILON.'-F $e_{4}$N and CrN were detected as the nitrides with the a-Fe in the nitrided layer. VN and .betha.- $W_{2}$N were also detected in 13Cr-3V and 13Cr-3W alloys. The growth of the nitrided layer was controlled by the diffusion process. The thickness of the nitrided layer was similar in the 13Cr-2Nb and 3Zr specimens to that of 13Cr(BM) specimen, while the others exhibited the thinner layer. The activation energy for the growth of the nitrided layer in the temperature range of 773-873K was about 130kJ/mol in 13Cr(BM), 13Cr-2Ti, 3W, 3Al, 3Zr and 3Si alloys. The hardness of the nitrided specimens was significantly increased above Hv1000, comparing to the non-nitrided specimen. The specimens with the nitrided forming elements revealed much higher hardness values and, especially, 13Cr-3Al, 3V and 3Si specimens were significantly hardened up to Hv1300.v1300.0.

  • PDF

비정질 합금의 조성분리가 소성에 미치는 영향: 변형국부화 관점에서의 해석 (Effect of the Compositional Modulation on the Plasticity of Amorphous Alloys: Shear Localization Viewpoint Interpretation)

  • 이미림;박경원;사현제;이재철
    • 대한금속재료학회지
    • /
    • 제47권11호
    • /
    • pp.687-693
    • /
    • 2009
  • Experiments have demonstrated that a moderate amount of Be added to $Zr_{57.5}Cu_{38.3}Al_{4.2}$ amorphous alloy enhances the plasticity of the alloy. In particular, $Zr_{54}Cu_{36}Al_{4}Be_{6}$ alloy exhibited 19% of strain to fracture along with a strength exceeding 2 GPa. Energy dispersive x-ray spectroscopy conducted on the $Zr_{54}Cu_{36}Al_{4}Be_{6}$ alloy exhibited the presence of compositional modulation, indicating that nm-scale phase separation had occurred at local regions. In this study, the role played by the nm-scale phase separation on the plasticity was investigated in terms of structural disordering, structural softening and shear localization in order to better understand the structural origin of the enhanced plasticity shown by the developed alloy.

Magnetoresistance Characteristics of Magnetic Tunnel Junctions Consisting of Amorphous CoNbZr Alloys for Under and Capping Layers

  • Chun, Byong Sun;Lee, Seong-Rae;Kim, Young Keun
    • Journal of Magnetics
    • /
    • 제9권1호
    • /
    • pp.13-16
    • /
    • 2004
  • Magnetic tunnel junctions (MTJs) comprising amorphous CoNbZr layers have been investigated. $Co_{85.5}Nb_8Zr_{6.5}$(in at. %) layers were employed to substitute the traditionally used Ta layers with an emphasis given on under-standing underlayer effect. The typical junction structure was $SiO_2/CoNbZr$ or Ta 2/CoFe 8/IrMn 7.5/CoFe 3/Al 1.6 + oxidation/CoFe 3/CoNbZr or Ta 2 (nm). For both as-deposited state and after annealing, the CoNbZr-underlayered structure showed superior surface smoothness up to the tunnel barrier than Ta-underlayerd one (rms roughness of 0.16 vs. 0.34 nm). CoNbZr-based MTJs was proven beneficial for increasing thermal stability and increasing $V_h$ (the bias voltage where MR ratio becomes half) characteristics than Ta-based MTJs. This is because the CoNbZr-based junctions offer smoother interface structure than the Ta-based one.