Frequency Dependent Magnetoelectric Responses in [0.948 Na0.5K0.5NbO3-0.052 LiSbO3]-[Co1-xZnxFe2O4] Particulate Composites

  • Choi, Moon Hyeok;Noh, Byung Il;Yun, Woosik;Jung, Chaewon;Yang, Su Chul
    • 한국전기전자재료학회논문지
    • /
    • 제35권3호
    • /
    • pp.303-307
    • /
    • 2022
  • Magnetoelectric (ME) properties of 3-0 type particulate composites have been investigated with respect to application features for reliable magnetic sensitivity and magnetically-induced output voltage. In order to figure out the magnetoelectric characteristics in the ME composites, frequency dependent ME responses were studied from [0.948 Na0.5K0.5NbO3-0.052 LiSbO3]-[Co1-xZnxFe2O4] (NKNLS)/Co1-xZnxFe2O4 (CZFO, x=0, 0.1, and 0.2). As a result, the maximal αME of 23.15 mV/cm·Oe was achieved from the NKNLS-CZFO (xZn = 0.1) composites at resonance frequency of 315 kHz and Hdc = 0 Oe. From the frequency dependent ME responses, it is clearly described that the self-biased ME composites can be used for applications as both magnetic sensors and energy harvesters, respectively.

추출조건(抽出條件)에 따른 인삼(人蔘)엑기스의 무기성분정량(無機成分定量)에 관(關)한 연구(硏究) (Approach to the Extraction Method on Minerals of Ginseng Extract)

  • 조한옥;이중화;조성환;최영희
    • 한국식품과학회지
    • /
    • 제8권2호
    • /
    • pp.95-106
    • /
    • 1976
  • 인삼중에는 약리학적면에서 뿐 아니라 생화학적 및 영양학적면에서 중요한 역할을 하는 무기질 및 미량원소가 다양하게 함유되어 있어서 생체를 구성하거나 각 조직의 기능을 촉진시키는 생물학적 활성물질로서의 역할을 하고 있다. 본 실험에서는 인삼 무기질의 효율적 이용을 목적으로 추출조건에 따른 엑기스의 수량과 추출된 인삼 엑기스의 무기질 및 미량원소를 미색법 및 원자흡광 분석법으로 측정하여 다음과 같은 결과를 얻었다. 1. 가장 효율적인 추출방법은 인삼원료량의 $10{\sim}20$배 되는 $60{\sim}80%$ ethanol로 60시간 이상 연속추출하는 것으로서 그 수량은 60% ethanol의 경우가 16.5%, 80%의 경우가 13.5%로서 가장 높은 값을 보였다. 2. 6년근 수삼과 백삼및 미삼의 수분함량은 각각 66.37%, 12.61%, 12.20%였으며 회분은 1.56%, 3.52%, 6.04%였고, 가용성 무질소물은 20.75%, 61.00%, 45.00%였으며 조단백질은 6.30%, 13.69%, 12.69%였고 순단백질은 2.26%, 5.94%, 5.76%였으며 조지방은 1.11%, 2.02%, 2.50%였고 조섬유는 2.41%, 8.74%, 8.87%였다. 3. 무기질 및 미량원소를 분석한 결과는 다음과 같다. 1) P함량은 미삼, 백삼, 수삼이 각각 1.318%, 1.362%, 0.713%였고 인삼엑기스의 그것은 미삼, 백삼, 수삼이 각각 0.038%, 0.063%, 0.036%로서 비교적 낮은추출율을 보이고 있다. 2) Ca함량은 미삼, 백삼, 수삼이 각각 0.147%, .238%, 0.126%이고 그 엑기스는 미삼, 백삼, 수삼이 0.023%, 0.011%, 0.016%여서 미삼은 15.6%이상이 ethanol로 추출된데 비해 백삼은 4.6%로 추출율이 극히 낮았다. 3) CI함량은 미삼 0.11%, 백삼 0.07%, 수삼 0.09%로 시료간에는 뚜렷한 함량차가 없었으며 미삼은 그 함량의 36.4%가 백삼은 67.1%가 ethanol로 추출된데 반하여 수삼은 84.4%로 가장 높은 추출수율을 보였다. 4) Fe함량은 미삼이 125.0ppm으로 가장 많고 백삼은 32.5ppm, 수삼은 20.0ppm이었는데 그 추출수율은 극히 낮아서 미삼은 1.33%, 백삼은 0.83%, 수삼은 1.08%에 불과하였다. 5) Cu, Zn 및 Mn은 미량원소로서 이중 Mn은 미삼 62.5ppm, 백삼 25.0ppm, 수삼 5.0ppm으로 비교적 많은 양이 함유되었으나 ethanol로 추출한 엑기스에서는 정량되지 않았으며 Cu는 미삼, 백삼, 수삼이 각각 15.0ppm, 20.0ppm, 5.0ppm이고 인삼 엑기스에는 7.5ppm, 6.5ppm, 4.5ppm으로서 50%, 32.5%, 90%의 추출율을 보였다. Zn은 다른 작물체에 비하여 많은 양이 함유되었고 미삼이 47.5ppm, 백삼이 27.5ppm, 수삼이 5.5ppm이고 그 인삼 엑기스에는 각각 4.5ppm, 1.25ppm, 15.0ppm의 Zn이 함유되어 있었다.

  • PDF

ZnO를 첨가한 (Na,K)$NbO_3$계 무연 압전 세라믹스의 유전 및 압전 특성에 관한 연구 (A Study on the Characteristics of Dielectric and Piezoelectric in (Na,K)$NbO_3$-system Pb-free Piezoelectric Ceramics add ZnO)

  • 류성림;김시철;이경선;이충호;류주현;김영민
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 추계학술대회 논문집 Vol.18
    • /
    • pp.218-219
    • /
    • 2005
  • In this paper, in order to develop Pb-free piezoelectric ceramics, $[Li_{0.04}(Na_{0.44}K_{0.52})-(Nb_{0.86}Ta_{0.10}Sb_{0.04})]O_3$ ceramic was fabricated with the variation of ZnO addition. Piezoelectric properties of the ceramic were varied with the amount of ZnO addition and showed the maximum kp value at 0.2 wt% ZnO addition. Qm of ZnO added ceramics showed lower values than the non-added ceramics, however, the kp was increased by the addition of ZnO up to 0.2 wt%. At the sintering temperature of 1110$^{\circ}C$ and the calcination temperature of 850$^{\circ}C$, the optimal values of density=473g/$cm^3$, kp=0.473, $\varepsilon_r$=1403 were obtained.

  • PDF

ZnO가 첨가된 (Na,K)NbO3계 세라믹스의 압전 특성 (Piezoelectric Properties in ZnO Dopped (Na,K)NbO3 Ceramics)

  • 류성림;권순용;어순철;김시철;류주현
    • 한국전기전자재료학회논문지
    • /
    • 제19권8호
    • /
    • pp.707-711
    • /
    • 2006
  • ZnO was doped up to 0.3 wt% for improving the electrical properties of lead-free $[Li_{0.04}(Na_{0.44}Ko_{0.52})-(Nb_{0.86}\;Ta_{0.10}\;Sb_{0.04})]O_3$ piezoelectric ceramics. The ceramics were fabricated with the conventional sintering processes. Crystal structure of the samples was tetragonal phase regardless of ZnO amount. However, the piezoelectric properties were varied with the ZnO amount. The electro-mechanical coupling factor $(k_p)$ was with the ZnO amount up to 0.2 wt% but decreased with the further addition. the maximum value of $k_p$ was 0.475. Density, piezoelectric charge constant and relative dielectric constant was also showed maximum value at 0.2 wt%. The maximum values are $4.75g/cm^3$, 275 pC/N, 1403, respectively. In contrast, the mechanical quality factor $(Q_m)$ was not varied with increasing the ZnO addition up to 0.2 wt% but rapidly increased at 0.3 wt%.

배전급 피뢰기용 ZnO 바리스터 소자의 미세구조 및 서지 특성에 관한 연구 (A Study on the microstructure and Surge Characteristics of ZnO varistors for distribution Arrester)

  • 김석수;조한구;박태곤;박춘현;정세영;김병규
    • 한국전기전자재료학회논문지
    • /
    • 제15권2호
    • /
    • pp.190-197
    • /
    • 2002
  • In this thesis, ZnO varistors with various formulation, such as A∼E, were fabricated according to ceramic fabrication method. The microstructure, electrical properties, and surge characteristics of ZnO varistors were investigated according to ZnO varistors with various formulation. In the microstructure, A∼E\`s ZnO varistor ceramics sintered at 1130$\^{C}$ was consisted of ZnO grain(ZnO), spinel phase (Zn$\_$2.33/Sb$\_$0.67/O$\_$4/), Bi-rich phase(Bi$_2$O$_3$) and intergranuler phase, wholly. Lightning impulse residual voltage of A, B, C and E\`s ZnO varistors suited standard characteristics, below 12kV at current of 5kA. On the contrary, D\`s ZnO varistor exhibited high residual voltage as high reference voltage. In the accelerated aging test, leakage current and watt loss of B, C and D\`s ZnO varistors increases abruptly with stress time under the first a.c. stress(115$\^{C}$/3.213kV/300h). Consequently, C varistor exhibited a thermal run away. On the contrary, leakage current and watt loss of A and C\`s ZnO varistors which show low initial leakage current exhibited constant characteristics. After high current impulse test, A\`s ZnO varistor has broken the side of varistor but impulse current flowed. On the contrary, E\`s ZnO Varistor exhibited good discharge characteristics which the appearance of varistor was not wrong such as puncture, flashover, creaking and other significant damage. After long duration impulse current test, E\`s ZnO varistor exhibited good discharge characteristics which the appearance of varistor was not wrong such as puncture, flashover, creaking and other significant damage. After high current impulse test and long duration impulse current test, E\`s ZnO varistor exhibited very good characteristics which variation rate of residual voltage is 1.4% before and after test.

전철탑재형 직류피뢰기용 ZnO 바리스터의 개발 (A Development of ZnO Varistor for Railroad Vehicle d.c. Arrester)

  • 조이곤;박춘현;정세영;송태권;김석수
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 추계학술대회 논문집 Vol.15
    • /
    • pp.552-556
    • /
    • 2002
  • The microstructure and electrical characteristics of A~C's ZnO varistors fabricated according to variable sintering condition, which sintering temperature is $1130^{\circ}C$ and speeds of pusher are A: 2mm/min, B: 4mm/min, C: 6mm/min, respectively, were investigated. In the microstructure, A~C's ZnO varist-ors fabricated variable sintering condition was consisted of ZnO grain(ZnO), spinel phase$(Zn_{2.33}Sb_{0.67}O_4)$ Bi-rich $phase(Bi_{2}O_{3})$, wholly. Varistor voltage of A~C's ZnO varistors sintered at $1130^{\circ}C$ increased in order A < B < C's ZnO varistors. C's ZnO varistor exhibited good characteristics that nonlinear exponent is 31.70. Leakage current of A~C's ZnO varistors exhibited below 2mA at rated voltage. Lightning impulse residual voltage of A's ZnO varistor suited standard characteristics, which is 3.85kV at 2.5kA, 4.4kV at 5kA and 5.16kV at 10kA. After multi lightning impulse residual voltage test of A's ZnO varistor exhibited good discharge characteristics which ZnO varistor reveals no evidence of puncture, flashover, cracking in visual examination. After high current impulse test of A's ZnO varistor exhibited good discharge characteristics, which variation rate of residual voltage is 0.4% before and after test, and revealed no evidence.

  • PDF

의성 광화대 동-연-아연-은 광상의 지화학적 연구 (Geochemistry of Cu-Pb-Zn-Ag Deposits from the Euiseong Mineralized Area)

  • 지세정;도성재;최선규;이재호
    • 자원환경지질
    • /
    • 제22권3호
    • /
    • pp.253-266
    • /
    • 1989
  • 경북 의성 퇴적분지내에는 수개조의 함 Cu-Pb-Zn-Ag 열수석영맥이 주향 N $20^{\circ}-40^{\circ}W$, 경사 $70^{\circ}-80^{\circ}NE$의 단층면을 따라 충진되어 있으며, 맥폭은 1.0m 이하이고, 약 200m 이상 연장되어 있다. 광화작용은 구조운동에 수반되어 3회 (I, II, III기)에 걸쳐 진행되었다. 주 광화시기인 제 I 광화시기에는 주로 황동석, 유비철석, 황철석, 방연석, 섬아연석과 미량의 사면동석 및 함Pb, Ag, Sb, Bi 유염 광물 등이 산출된다. 유체 포유물 연구에 의하면, 제I광화작용시 동(銅)을 위시한 광석 광물은 7.5-4.5wt.% 염상당농도를 갖는 광화유체로부터 초기 $400^{\circ}C$에서 후기 $200^{\circ}C$에 걸쳐 침전되었고, $350^{\circ}C$ 부근에서 광화유체의 비등 현상이 있었음을 확인하였다. $H_2O-NaCl$ 임계곡선에 의해 구한 광화유체의 최대 압력은 150bar이고, 이는 1.7km의 심도에 해당된다. Cu의 침전은 전 유황종(種)의 농도가 $10^{-0.5}-10^{-1.8}M$인 광화유체가 약 $350^{\circ}C$에서 $250^{\circ}C$로 감소되면서 비등작용과 함께 천수유입에 의한 냉각 작용에 의하여, 광화유체 내의 유황, 산소의 분압이 각각 $10^{-8}$, $10^{-30}atm$.에서 $10^{-12}$, $10^{-36}atm$.으로 감소되고, 한편 pH가 증가되어, Cu complex 이온의 농도가 $10^3$에서 10ppm으로 감소되면서 주로 황동석으로 침전되었다. 함 Pb, Ag, Sb, Bi 유염광물은 $250^{\circ}C$ 이하에서 유황과 산소분압이 각각 $10^{-12}$, $10^{-36}atm$. 이하인 광화유체에서 계속되는 천수유입으로 인한 냉각작용과 희석작용에 의해 침전되었다.

  • PDF

고분자 금속촉매의 합성과 유기합성 반응에의 활용에 관한 연구 (Studies on the Synthesis of Polymer Metal Complex and Its Application to Organic Reactions)

  • 황규자;김영주;이용근
    • 대한화학회지
    • /
    • 제30권5호
    • /
    • pp.449-455
    • /
    • 1986
  • 각종 무수금속염화물을 양이온 교환수지(PK 212)와 같이 이황화탄소 용매속에서 반응시켜 고분자 금속콤플렉스 ${\circled{P}}-AlC_3,\;{\circled{P}}>-FeCl_3,\;{\circled{P}}-SbCl_5,\;{\circled{P}}-SnCl_4,\;{\circled{P}}- ZnCl_2$들을 각각 합성하여 이들의 표면과 절단면을 scanning electron probe microanalyzer로 관찰하였다. 합성된 고분자 금속콤플렉스를 각종 이염기성산과 알코올의 에스테르화 반응에 촉매로 이용하여 고분자 금속콤플렉스의 촉매효과를 비교 검토한 결과 이염기성 카르복실산의 에스테르화 반응에 있어서 고분자 금속콤플렉스들은 유용한 촉매임을 확인하였다.

  • PDF

M-Zn (M = Sb, V, and Nb) Substituted Strontium Hexaferrites with Enhanced Saturation Magnetization for Permanent Magnet Applications

  • Sapoletova, Nina;Kushnir, Sergey;Ahn, Kyunghan;An, Sung Yong;Choi, Moonhee;Kim, Jae Yeong;Choi, Changhak;Wi, Sungkwon
    • Journal of Magnetics
    • /
    • 제21권3호
    • /
    • pp.315-321
    • /
    • 2016
  • M-Zn (M = Sb, V, Nb) substituted M-type strontium hexaferrites were prepared by a ceramic method. The phase composition, morphology and magnetic properties were studied by x-ray diffractometry, scanning electron microscopy and vibrating sample magnetometry. Saturation magnetization increases with a substitution up to 75.0 emu/g (2.5 % higher compared to unsubstituted hexaferrite) and then decreases with a further substitution. A coercive field of substituted hexaferrite powders with highest saturation magnetization is more than 3 kOe. Substituted strontium hexaferrite powders prepared in this work are a rare example of high $M_S$ compositions without doping rare-earth elements and would be a promising candidate for a permanent magnet application.