Min, Su Ryun;Lee, Jang Woo;Cho, Han Na;Chung, Chee Won
Applied Chemistry for Engineering
/
v.18
no.1
/
pp.24-28
/
2007
The etching of zinc oxide (ZnO) thin films has been studied using a high density plasma in a $Cl_2/Ar$ gas. The etch characteristics of ZnO thin films were systematically investigated on varying $Cl_2$ concentration, coil rf power, dc-bias voltage, and gas pressure. With increasing $Cl_2$ concentration, the etch rate of ZnO thin film increased, the redeposition around the etched patterns decreased but the sidewall slope of the etched patterns slanted. As the coil rf power and dc-bias voltage increased, the etch rates of ZnO thin films increased and etch profiles of ZnO thin films were improved. With increasing gas pressure, the etch rate of ZnO thin films slightly increased but little change in etch profile was observed. Based on these results, the optimal etching conditions of ZnO thin film were selected. Finally, the etching of ZnO thin films with a high degree of anisotropy of approximately $75^{\circ}{\sim}80^{\circ}$ without the redepositions and residues was successfully achieved at the etching conditions of 20% $Cl_2$ concentration, coil rf power of 1000 W, dc-bias voltage of 400 V, and gas pressure of 5 mTorr.
Proceedings of the Korean Institute of Surface Engineering Conference
/
2009.10a
/
pp.223-224
/
2009
본 연구에서는 $Cl_2$/Ar 기반의 플라즈마 식각에 $N_2$가스를 첨가하여 ZnO 박막을 식각 하였을 때 관찰된 ZnO 박막의 식각 특성에 관하여 연구 하였다. ZnO 박막 식각 실험은 RF 800 W, bias power 400 W, 공정 압력 15 mTorr를 기준으로 하였으며 가스 혼합 비율로는 최적의 식각률을 보여주는 $Cl_2$/Ar=8:2 비율에서 실행하였다. 연구의 목적인 첨가 가스 $N_2$를 $Cl_2$ (80%)/Ar (20)%에 5 sccm 씩 첨가하여 20 sccm 까지 증가 시켜 실험 하였다. $N_2$ 가스가 15 sccm 첨가되었을 때 식각률 95.9 nm/min로 기존 $Cl_2$/Ar 기반의 플라즈마 식각보다 높은 식각률을 보여 주었으며 $N_2$ 가스 흐름 조절 외에도 공정 압력, RF power, bias power를 변경하며 실험하였다. 식각된 ZnO 박막의 표면은 최대 식각률을 보이는 공정 조건을 찾기 위해 surface profiler ($\alpha$-step)을 이용하여 식각률을 측정하였으며 ZnO 박막 표면의 화학적인 변화를 조사하기 위해 x-ray photoelectron spectroscopy (XPS)를 사용하였다. XPS 분석 결과 Zn $2p_{3/2}$ peak 가낮은 binding energy 쪽으로 이동한 것을 관찰 할 수 있었다. 또한 O 1s 의 스펙트럼을 분석한 결과 N-O bond와 O-H bond가 존재함이 밝혀졌다.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.23
no.10
/
pp.747-751
/
2010
In the study, the characteristics of the etched Zinc oxide (ZnO) thin films surface, the etch rate of ZnO thin film in $Cl_2/BCl_3/Ar$ plasma was investigated. The maximum ZnO etch rate of 53 nm/min was obtained for $Cl_2/BCl_3/Ar$=3:16:4 sccm gas mixture. According to the x-ray diffraction (XRD) and atomic force microscopy (AFM), the etched ZnO thin film was investigated to the chemical reaction of the ZnO surface in $Cl_2/BCl_3/Ar$ plasma. The field emission auger electron spectroscopy (FE-AES) analysis showed an elemental analysis from the etched surfaces. According to the etching time, the ZnO thin film of etched was obtained to The AES depth-profile analysis. We used to atomic force microscopy to determine the roughness of the surface. So, the root mean square of ZnO thin film was 17.02 in $Cl_2/BCl_3/Ar$ plasma. Based on these data, the ion-assisted chemical reaction was proposed as the main etch mechanism for the plasmas.
Cathodoluminescence(CL) properties of ZnO:Zn green phosphor were investigated. ZnO:Zn phosphor was synthesized by varying reducing agents and firing temperatures. ZnS, charcoal and 5% H2 gas mixed with 95% N2 gas(5H2-95N2) were used as the reducing agent and atmosphere. The highest CL intensity of ZnO:Zn phosphor was observed under the condition of 5H2-95N2 atmosphere and firing temperature of 90$0^{\circ}C$ for 1h. Charocal and ZnO as reducing agents in the syntehsis of ZnO:Zn phosphor exhibited about 60% and 40%, respectively, of the CL intensity obtained with 5H2-95N2 atmosphere.
Transactions on Electrical and Electronic Materials
/
v.11
no.3
/
pp.116-119
/
2010
The etching characteristics of zinc oxide (ZnO) were investigated, including the etch rate and the selectivity of ZnO in a $Cl_2/BCl_3$/Ar plasma. It was found that the ZnO etch rate, the RF power, and the gas pressure showed non-monotonic behaviors with an increasing Cl2 fraction in the $Cl_2/BCl_3$/Ar plasma, a gas mixture of $Cl_2$(3 sccm)/$BCl_3$(16 sccm)/Ar (4 sccm) resulted in a maximum ZnO etch rate of 53 nm/min and a maximum etch selectivity of 0.89 for ZnO/$SiO_2$. We used atomic force microscopy to determine the roughness of the surface. Based on these data, the ion-assisted chemical reaction was proposed as the main etch mechanism for the plasmas. Due to the relatively low volatility of the by-products formed during etching with $Cl_2/BCl_3$/Ar plasma, ion bombardment and physical sputtering were required to obtain the high ZnO etch rate. The chemical states of the etched surfaces were investigated using X-ray photoelectron spectroscopy (XPS). This data suggested that the ZnO etch mechanism was due to ion enhanced chemical etching.
The purpose of this study is to investigate effects of several zinc solutions including Artemisia asiatica-containing zinc solution on concentration of oral volatile sulfur compounds(VSCs). We determined the VSCs concentration of breath of human subjects before and after use of zinc solutions(O.25% $ZnF_2$ Artemisia asiatica-containing 0.25% $ZnCl_2$ and Artemisia asiatica-containing 0.25% $ZnCl_2$ solutions) The results were as follows : 1. 0.25% $ZnCl_2$ solution was more effective than 0.25% $ZnF_2$ solution in reducing the concentration of oral VSCs and the maintenance duration of effectiveness. 2. Artemisia asiatica-containing 0.25% $ZnCl_2$ solution was more effective than Artemisia asiatica-containing 0.25% $ZnF_2$ solution in reducing the concentration of oral VSCs and the maintenance duration of effectiveness. 3. Artemisia asiatica-containing 0.25% $ZnF_2$ solution and 0.25% $ZnF_2$ solution showed no significant difference in reducing the concentration of oral VSCs and the maintenance duration of effectiveness but, Artemisia asiatica-containing 0.25% $ZnF_2$ solution was slightly more effective. 4. Artemisia asiatica-containing 0.25% $ZnCl_2$ solution and 0.25% $ZnCl_2$ solution showed no significant difference in reducing the concentration of oral VSCs and the maintenance duration of effectiveness but, Artemisia asiatica-containing 0.25% $ZnF_2$ solution was slightly more effective.
In the flux used in the batch galvanizing process, the effect of the component ratio of NH4Cl to ZnCl2 on the microstructure, coating adhesion, and corrosion resistance of Zn-Mg-Al ternary alloy-coated steel is evaluated. Many defects such as cracks and bare spots are formed inside the Zn-Mg-Al coating layer during treatment with the flux composition generally used for Zn coating. Deterioration of the coating property is due to the formation of AlClx mixture generated by the reaction of Al element and chloride in the flux. The coatability of the Zn-Mg-Al alloy coating is improved by increasing the content of ZnCl2 in the flux to reduce the amount of chlorine reacting with Al while maintaining the flux effect and the coating adhesion is improved as the component ratio of NH4Cl to ZnCl2 decreases. Zn-Mg-Al alloy-coated steel products treated with the optimized flux composition of NH4Cl·3ZnCl2 show superior corrosion resistance compared to Zn-coated steel products, even with a coating weight of 60 %.
Journal of the Korean Crystal Growth and Crystal Technology
/
v.7
no.2
/
pp.271-275
/
1997
We have successfully grown Cl-doped ZnSe epitaxial layers on GaAs(100) sub-strates by HWE using $ZnCl_2$ as a doping source. The Cl-doped ZnSe layers showed mirrorlike morphology and good crystallinity. It has been found that the layer exhibited an n-type conduction with low resistivity. The carrier concentration is, obtained about $10^{16}\textrm {cm}^{-3}$, where a resistivity reached 10 $\Omega \textrm {cm}$. The layer with an appropriate doping level exhibited blue photoluminescence at room temperature. The strong blue PL was obtained at the hall mobility of $100^2\textrm {cm}$/Vㆍsec.
Park, Yong-Kyu;Sung, Hyun-Ho;Cho, Whang-Sin;Lee, Jong-Chan;Park, Dae-Hee
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2000.04b
/
pp.22-25
/
2000
ZnS:Cu,Cl 형광체의 여기 및 발광 스펙트럼 측정 결과 주게인 $Cl^-$ 이온과 받게인 $Cu^+$ 이온 사이의 흡수와 발광에 기인하는 peak과 국소화된 발광 중심인 $(CU_2)^{2+}$ 이온의 흡수와 발광에 기인하는 peak이 관측되었다. CuCl의 첨가량이 증가함에 따라 $Cu^+$ 이온의 농도가 증가하게 되어 $(Cu_2)^{2+}$ 이온에 기안하는 발광으로부터 공명 에너지 전달 (Resonant Energy Transfer)의 확률이 높아지기 때문에 513 nm를 중심으로 하는 발광의 세기가 증가하게 된다. 자체 제작한 ZnS:Cu,Cl 형광체를 이용하여 제작한 소자의 휘도 측정결과 400 Hz, 100 V 에서 CuCl 의 첨가량이 0.2 mole% 일 때 휘도가 최대였고, 진동수가 증가함에 따라 휘도가 포화되는 현상이 나타났다. CuCl의 첨가량이 증가함에 따라 513 nm를 중심으로 하는 발광이 강해지고 CIE 좌표값이 녹색영역으로 이동하게 된다. 진동수가 증가하면 인가된 전압의 유지 시간이 짧아지게 되어 발광의 감쇄시간이 긴 513 nm를 중심으로 하는 발광보다 감쇄시간이 짧은 458 nm를 중심으로 하는 발광이 강해지게 되고, CIE 좌표값이 청색영역으로 이동하게 된다.
Journal of the Korea Academia-Industrial cooperation Society
/
v.7
no.4
/
pp.733-737
/
2006
In this paper, we report the coordination state and structure of $Zn(cyclam)Cl_{2})$ complex that was studied by the Raman spectrum and conductivity method. The complex of zinc(II) ion with 1,4,8,11-tetraazacyclotetradecane(cyclam) ligand is formed in aqueous solution. According to the Raman spectrum of $Zn(cyclam)Cl_{2})$ complex, $H_{2}O$ molecule and $Cl^{-}$ ion compete for the trans coordination site of zinc(II) ion. We also have investigated the competition effect of $H_{2}O$ molecule and $Cl^{-}$ ion by the conductivity method. On addition of 1,4,8,11-tetraazacyclotetradecane(cyclam) ligand to the aqueous $ZnCl_{2}$ solution, 2: 1 electrolyte is changed to 1:1 electrolyte. We suggest the possibility of elimination of heavy metal because of the affinity effect of macrocyclic polyamine(1,4,8.11-tetraazacyclotetradecane) for the heavy metal,.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.