• Title/Summary/Keyword: Zirliner

Search Result 3, Processing Time 0.025 seconds

The Influence of Surface Treatments on Shear Bond Strength between Zirconia Core and Heat Press Ceramic Interface (지르코니아 코어의 표면처리방법이 열 가압 세라믹과의 전단결합강도에 미치는 영향)

  • Park, Hang-Min;Chung, In-Sung
    • Journal of Technologic Dentistry
    • /
    • v.31 no.2
    • /
    • pp.23-30
    • /
    • 2009
  • All-ceramic restorations have gained acceptance among clinicians and patients because of their superior esthetics. Most all-ceramic systems have a 2-layer structure, using a weak veneering ceramic over a strong supporting core. often, failure of all-ceramic restorations occurs when the veneering ceramic fractures, exposing the core material. The purpose of this study was to compare the shear bond strength of heat press ceramic system (Zirpress) to zirconia core with various surface treatments. 10 metal cores and 50 zirconia cores were fabricated and divided into six groups according to surface treatment such as Zirliner application, aluminium oxide blasting, and 9.5% HF etching. Sixty specimens were prepared using Zirpress, veneered 8mm height and 3mm in diameter, over the zirconia cores (n=10). The shear bond strength test was performed in a universal testing machine with a crosshead speed of 1/min. Ultimate shear bond strength data were analyzed with One-way ANOVA and the Scheffe's test (p=.05). Within the limits of this study, the following conclusions were drawn: The mean shear bond strengths (MPa) were: 12.93 for $110{\mu}m$ aluminium oxide blasting/Rexillium III/IPS e.Max Zirpress; 14.92 for $50{\mu}m$ aluminium oxide blasting ${\pm}9.5%$ HF etching/Zirconis core/IPS e.Max Zirpress; 16.37 for $110{\mu}$ aluminium oxide blasting + 9.5% HF etching/Zirconis core/IPS e.Max Zirpress; 12.89 for $200{\mu}$ aluminium oxide blasting + 9.5% HF etching/Zirconis core/IPS e.Max Zirpress; 19.30 for 9.5% HF etching/Zirconis core/IPS e.Max Zirpress; 19.55 for Zirliner/Zirconis core/IPS e.Max Zirpress. The mean shear bond strength for ZNTZH (Zirliner/Zirconis core) and ZNTEH (9.5% HF etching/Zirconis core) were significantly superior to MS110H ($110{\mu}$ aluminium oxide blasting/Rexillium III) and ZS200EH ($200{\mu}$ aluminium oxide blasting + 9.5% HF etching/Zirconis core) (p<0.05).

  • PDF

Effect of Application of ZirLiner® and Blasting Treatments on Shear Bond Strength of Zirconia-Veneered Porcelain Interface (지르코니아-전장도재 계면의 전단결합강도에 대한 ZirLiner® 적용과 분사처리의 영향에 관한 연구)

  • Shin, Young-Ho;Lee, Yu-Na;Lee, Hae-Hyoung;Dong, Jin-Keun;Oh, Sang-Chun
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.24 no.1
    • /
    • pp.113-127
    • /
    • 2008
  • The purpose of this study was to evaluate effect of application of $ZirLiner^{(R)}$ and blasting treatments on shear bond strength of zirconia-veneered porcelain interface. 60 uncolored zirconia plates and 30 colored zirconia plates were fabricated and divided into nine groups of 10 according to blasting treatment such as as-ground, glass blasting and alumina blasting and zirliner application. Veneering porcelains were built up over the center of the treated zirconia ceramic surface using jig and fired according to the manufacturers' instructions. Each specimen was completely embedded in acrylic resin. The specimens were placed in a mounting jig and subjected to shear force by a universal testing machine. Load was applied at a crosshead speed of 0.5㎜/min until failure. Average shear strengths were analyzed with two-way analysis of variance and one-way analysis of variance and the Duncan's post-hoc test. The fracture surfaces of the failed specimens were examined by SEM. The obtained results were as follows: 1. Depending on surface treatment by blasting, the degree of roughness is revealed in the order of Glass-blasted, As-ground, and Alumnia-blasted. The roughness average of uncolored and colored zirconia ceramic were not significantly different from blasting treatments. 2. In uncolored zirconia ceramic, the shear bond strength were not significantly different from blasting treatments. However, the shear bond strength were significantly different from Zirliner application. 3. Used ZirLiner, mean shear bond strength of colored zirconia was lower than uncolored zirconia. Especially, mean shear bond strength of colored zirconia was quite low with alumina-blasting treatment. 4. SEM analysis showed that veneered porcelain failed in zirconia ceramic interface and there was no cohesive failure.

Effect of surface treatmet on the shear bond strength of a zirconia core to veneering ceramic (지르코니아 코어의 표면처리가 비니어링 세라믹과의 전단결합강도에 미치는 영향)

  • Choi, Mi-Sun;Kim, Young-Soo;Suh, Kyu-Won;Ryu, Jae-Jun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.47 no.2
    • /
    • pp.199-205
    • /
    • 2009
  • Purpose: The purpose of this research was to evaluate the shear bond strength between zirconia core and veneer ceramic after surface treatment. Material and methods: Zirconia cores(N=40, n=10, $10mm{\times}10mm{\times}3mm$) were fabricated according to the manufacturers' instructions and ultrasonically cleaned. The veneering ceramics(thickness 3 mm) were built and fired onto the zirconia core materials. Four groups of specimens with different surface treatment were prepared. Group I: without any pre-treatment, Group II: treated with sandblasting, Group III: treated with liner, Group IV: treated with sandblasting and liner. The shear bond strength was tested in a universal testing machine. Data were compared with an ANOVA and $Scheff{\acute{e}}$ post hoc test(P=.05). Results: The shear bond strength of group VI was significantly higher than the other groups. Conclusion: Both mechanically and chemically treated simultaneously on zirconia core surface influenced the shear bond strength between the core and veneering ceramic in all-ceramic systems.