• Title/Summary/Keyword: Zirconium diboride ($ZrB_2$)

Search Result 21, Processing Time 0.032 seconds

Sintering characteristics of monolithic ZrB$_{2 }$ and ZrB$_{2 }$-ZrC composit (단일상 ZrB$_{2 }$ 및 ZrB$_{2 }$- ZrC 복합체의 소결특성)

  • 김경훈;심광보
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.10 no.2
    • /
    • pp.145-151
    • /
    • 2000
  • The sintering behaviour of monolithic zirconium diboride (ZrB$_{2 }$) and ZrB$_{2 }$-based composite ZrB$_{2 }$-ZrC were studied using a pressureless sintering technique. The specimens were prepared using commercially available ZrB$_{2 }$ and ZrC powder which were pressed and subjected to pressureless sintering. The effects of lanthanum and neodymium used as sintering aids in the sintering processes were investigated. The sintered specimens were characterized using X-ray diffraction analysis and scanning electron microscopy. The ZrB$_{2 }$ specimen prepared using and addition of 1 wt% lanthanum and pressurelessly sintered at $2200^{\circ}C$ showed the maximum relative density of 96%. The ZrB$_{2 }$-ZrC composite specimen without the addition of any sintering aids exhibits the maximum sintered density but contains significantly detectable amount of secondary phase.

  • PDF

Mechanical and Electrical Properties of Hot-Pressed Silicon Carbide-Zirconium Diboride Composites (고온가압소결한 SiC-ZrB$_2$ 복합체의 기계적, 전기적 특성)

  • 신용덕
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1997.04a
    • /
    • pp.135-140
    • /
    • 1997
  • The influences of ZrB$_2$ additions to SiC on microstructural, DDM(Electrical Discharge Machining), mechanical and electrical properties were investigated. composites were prepared by adding 15, 30, 45 vol.% ZrB$_2$particles as a second phase to SiC matrix. SiC-ZrB$_2$ composites obtained by hot pressing for high temperature structural application were fully dense with the relative densities over 99%. The fracture toughness of the composites were increased with the ZrB$_2$contents. In case of composite containing 30vol.% ZrB$_2$, the flexural strength and fracture toughness showed 45% and 60% increase, respectively compared to that of monolithic SiC sample. The electrical resistivities of SiC-ZrB$_2$ composites decreased significantly with the ZrB$_2$ contents. The electrical resistivity of SiC-30vol.% ZrB$_2$ composite showed 6.50$\times$10$^{-4}$ $\Omega$.cm. Cutting velocity of EDM of SiC-ZrB$_2$ composites are directly proportional to duty factor of pulse width. Surface roughness, however, are not all proportional to pulse width. Higher-flexural strength composites show a trend toward smaller crater volumes, leaving a smoother surface; the average surface roughness of the SiC-ZrB$_2$ 15 vol.% composite with the flexural strengthe of 375㎫ was 3.2${\mu}{\textrm}{m}$, whereas the SiC-ZrB$_2$ 30.vol% composite of 457㎫ was 1.35${\mu}{\textrm}{m}$. In the SEM micrographs of the fracture surface of SiC-ZrB$_2$ composites, the SiC-ZrB$_2$ two phases are distinct; the white phase is the ZrB$_2$and the gray phase is the SiC matrix. In the SEM micrographs of the EDM surface, however, these phases are no longer distinct because of thicker recast layer of resolidified-melt-formation droplets present. It is shown that SiC-ZrB$_2$ composites are able to be machined without surface cracking.

  • PDF

Properties of SiC-$ZrB_2$ Electroconductive Ceramic Composites by Spark Plasma Sintering (방전플라즈마 소결에 의한 SiC-$ZrB_2$ 도전성 세라믹 복합체 특성)

  • Shin, Yong-Deok;Ju, Jin-Young;Jo, Sung-Man;Lee, Jung-Hoon;Kim, Cheol-Ho;Lee, Hee-Seung
    • Proceedings of the KIEE Conference
    • /
    • 2009.07a
    • /
    • pp.1252_1253
    • /
    • 2009
  • The composites were fabricated by adding 0, 15, 20, 25[vol.%] Zirconium Diboride(hereafter, $ZrB_2$) powders as a second phase to Silicon Carbide(hereafter, SiC) matrix. The physical, mechanical and electrical properties of electroconductive SiC ceramic composites by spark plasma sintering(hereafter, SPS) were examined. Reactions between $\beta$-SiC and $ZrB_2$ were not observed in the XRD analysis The relative density of mono SiC, SiC+15[vol.%]$ZrB_2$, SiC+20[vol.%]$ZrB_2$ and SiC+25[vol.%]$ZrB_2$ composites are 90.97[%], 74.62[%], 77.99[%] and 72.61[%] respectively. The XRD phase analysis of the electroconductive SiC ceramic composites reveals high of SiC and $ZrB_2$ and low of ZrO2 phase. The electrical resistivity of mono SiC, SiC+15[vol.%]$ZrB_2$, SiC+20[vol.%]$ZrB_2$ and SiC+25[vol.%]$ZrB_2$ composites are $4.57{\times}10^{-1}$, $2.13{\times}10^{-1}$, $1.53{\times}10^{-1}$ and $6.37{\times}10^{-2}[{\Omega}{\cdot}cm]$ at room temperature, respectively. The electrical resistivity of mono SiC, SiC+15[vol.%]$ZrB_2$, SiC+20[vol.%]$ZrB_2$ and SiC+25[vol.%]$ZrB_2$ are Negative Temperature Coefficient Resistance(hereafter, NTCR) in temperature ranges from 25[$^{\circ}C$] to 100[$^{\circ}C$]. It is convinced that SiC+20[vol.%]$ZrB_2$ composite by SPS can be applied for heater above 1000[$^{\circ}C$].

  • PDF

Effect of SiC and WC additon on Oxidation Behavior of Spark-Plasma-Sintered ZrB2

  • Kim, Chang-Yeoul;Choi, Jae-Seok;Choi, Sung-Churl
    • Journal of Powder Materials
    • /
    • v.26 no.6
    • /
    • pp.455-462
    • /
    • 2019
  • ZrB2 ceramic and ZrB2 ceramic composites with the addition of SiC, WC, and SiC/WC are successfully synthesized by a spark plasma sintering method. During high-temperature oxidation, SiC additive form a SiO2 amorphous outer scale layer and SiC-deplete ZrO2 scale layer, which decrease the oxidation rate. WC addition forms WO3 during the oxidation process to result in a ZrO2/WO3 liquid sintering layer, which is known to improve the anti-oxidation effect. The addition of SiC and WC to ZrB2 reduces the oxygen effective diffusivity by one-fifth of that of ZrB2. The addition of both SiC and WC shows the formation of a SiO2 outer dense glass layer and ZrO2/WO3 layer so that the anti-oxidation effect is improved three times as much as that of ZrB2. Therefore, SiC- and WC-added ZrB2 has a lower two-order oxygen effective diffusivity than ZrB2; it improves the anti-oxidation performance 3 times as much as that of ZrB2.

Densification and Properties of ZrB2-based Ceramics for Ultra-high Temperature Applications (초고온용 ZrB2-계 세라믹스의 치밀화와 물성)

  • Kim, Seong-Won;Kim, Hyung-Tae;Kim, Kyung-Ja;Seo, Won-Seon
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.29 no.3
    • /
    • pp.273-278
    • /
    • 2012
  • $ZrB_2$ has a melting temperature of $3245^{\circ}C$ and a low density of $6.1\;g/cm^3$, which makes this a candidate for application to ultra-high temperature over $2000^{\circ}C$. Beside these properties, $ZrB_2$ has excellent resistance to thermal shock and oxidation compared with other non-oxide engineering ceramics. This paper reviewed briefly 2 research examples, which are related to densification and properties of $ZrB_2$-based ceramics for ultra-high temperature applications. In the first section, the effect of $B_4C$ addition on the densification and properties of $ZrB_2$-based ceramics is shown. $ZrB_2$-20 vol.% SiC system was selected as a basic composition and $B_4C$ or C was added to this system in some extents. With sintered bodies, densification behavior and hightemperature (up to $1400^{\circ}C$) properties such as bending strength and hardness are examined. In the second section, the effect of the SiC size on the microstructures and physical properties is shown. $ZrB_2$-SiC ceramics are fabricated by using various SiC sources in order to investigate the grain-growth inhibition and the mechanical/thermal properties of $ZrB_2$-SiC.

Effects of Pressure on Properties of SiC-ZrB2 Composites through SPS (SiC-ZrB2복합체의 특성에 미치는 SPS의 압력영향)

  • Lee, Jung-Hoon;Jin, Bm-Soo;Shin, Yong-Deok
    • The Transactions of The Korean Institute of Electrical Engineers
    • /
    • v.60 no.11
    • /
    • pp.2083-2087
    • /
    • 2011
  • The SiC-$ZrB_2$ composites were produced by subjecting a 40:60 vol.% mixture of zirconium diboride($ZrB_2$) powder and ${\beta}$-silicon carbide (SiC) matrix to spark plasma sintering(SPS). Sintering was carried out for 60sec at $1400^{\circ}C$ (designation as TP145 and TP146), $1500^{\circ}C$(designation as TP155 and TP156) and uniaxial pressure 50MPa, 60MP under argon atmosphere. The physical, electrical, and mechanical properties of the SiC-$ZrB_2$ composites were examined. The relative density of TP145, TP146, TP155 and TP156 were 94.75%, 94.13%, 97.88% and 95.80%, respectively. Reactions between ${\beeta}$-SiC and $ZrB_2$ were not observed via x-ray diffraction (hereafter, XRD) analysis. The flexural strength, 306.23MPa of TP156 was higher than that, 279.42MPa of TP146 at room temperature, but lower than that, 392.30MPa of TP155. The properties of a SiC-$ZrB_2$ composites through SPS under argon atmosphere were positive temperature coefficient resistance (hereafter, PTCR) in the range from $25^{\circ}C$ to $500^{\circ}C$. The electrical resistivities of TP145, TP146, TP155 and TP156 were $6.75{\times}10^{-4}$, $7.22{\times}10^{-4}$, $6.17{\times}10^{-4}$ and $6.71{\times}10^{-4}{\Omega}{\cdot}cm$ at $25^{\circ}C$, respectively. The densification of a SiC-$ZrB_2$ composite through hot pressing depend on the sintering temperature and pressure. However, it is convinced that the densification of a SiC-$ZrB_2$ composite do not depend on sintering pressure under SPS.

The Development of an Electroconductive SiC-ZrB2 Ceramic Heater through Spark Plasma Sintering

  • Ju, Jin-Young;Kim, Cheol-Ho;Kim, Jae-Jin;Lee, Jung-Hoon;Lee, Hee-Seung;Shin, Yong-Deok
    • Journal of Electrical Engineering and Technology
    • /
    • v.4 no.4
    • /
    • pp.538-545
    • /
    • 2009
  • The SiC-$ZrB_2$ composites were fabricated by combining 30, 35, 40 and 45vol.% of Zirconium Diboride (hereafter, $ZrB_2$) powders with Silicon Carbide (hereafter, SiC) matrix. The SiC-$ZrB_2$ composites, the sintered compacts, were produced through Spark Plasma Sintering (hereafter, SPS), and its physical, electrical, and mechanical properties were examined. Also, the thermal image analysis of the SiC-$ZrB_2$ composites was examined. Reactions between $\beta$-SiC and $ZrB_2$ were not observed via X-Ray Diffractometer (hereafter, XRD) analysis. The relative density of the SiC+30vol.%$ZrB_2$, SiC+35vol.%$ZrB_2$, SiC+40vol.%$ZrB_2$, and SiC+45vol.%$ZrB_2$ composites were 88.64%, 76.80%, 79.09% and 88.12%, respectively. The XRD phase analysis of the sintered compacts demonstrated high phase of SiC and $ZrB_2$ but low phase of $ZrO_2$. Among the SiC-$ZrB_2$ composites, the SiC+35vol.%$ZrB_2$ composite had the lowest flexural strength, 148.49MPa, and the SiC+40vol.%$ZrB_2$ composite had the highest flexural strength, 204.85MPa, at room temperature. The electrical resistivities of the SiC+30vol.%$ZrB_2$, SiC+35vol.%$ZrB_2$, SiC+40vol.%$ZrB_2$ and SiC+45vol.%$ZrB_2$ composites were $6.74\times10^{-4}$, $4.56\times10^{-3}$, $1.92\times10^{-3}$, and $4.95\times10^{-3}\Omega{\cdot}cm$ at room temperature, respectively. The electrical resistivities of the SiC+30vol.%$ZrB_2$, SiC+35vol.%$ZrB_2$ SiC+40vol.%$ZrB_2$ and SiC+45[vol.%]$ZrB_2$ composites had Positive Temperature Coefficient Resistance (hereafter, PTCR) in the temperature range from $25^{\circ}C$ to $500^{\circ}C$. The V-I characteristics of the SiC+40vol.%$ZrB_2$ composite had a linear shape. Therefore, it is considered that the SiC+40vol.%$ZrB_2$ composite containing the most outstanding mechanical properties, high resistance temperature coefficient and PTCR characteristics among the sintered compacts can be used as an energy friendly ceramic heater or electrode material through SPS.

Properties of $SiC-ZrB_2$ Electroconductive Ceramic Composites by Spark Plasma Sintering (SPS 소결에 의한 $SiC-ZrB_2$ 도전성 세라믹 복합체 특성)

  • Ju, Jin-Young;Lee, Hui-Seung;Jo, Sung-Man;Lee, Jung-Hoon;Kim, Cheol-Ho;Park, Jin-Hyoung;Shin, Yong-Deok
    • The Transactions of The Korean Institute of Electrical Engineers
    • /
    • v.58 no.9
    • /
    • pp.1757-1763
    • /
    • 2009
  • The composites were fabricated by adding 0, 15, 20, 25[vol.%] Zirconium Diboride(hereafter, $ZrB_2$) powders as a second phase to Silicon Carbide(hereafter, SiC) matrix. The physical, mechanical and electrical properties of electroconductive SiC ceramic composites by Spark Plasma Sintering(hereafter, SPS) were examined. Reactions between ${\beta}-SiC$ and $ZrB_2$ were not observed in the XRD analysis. The relative density of mono SiC, SiC+15[vol.%]$ZrB_2$, SiC+20[vol.%]$ZrB_2$ and SiC+25[vol.%]$ZrB_2$ composites are 90.93[%], 74.62[%], 74.99[%] and 72.61[%], respectively. The XRD phase analysis of the electroconductive SiC ceramic composites reveals high of SiC and $ZrB_2$ and low of $ZrO_2$ phase. The lowest flexural strength, 108.79[MPa], shown in SiC+15[vol.%] $ZrB_2$ composite and the highest - 220.15[MPa] - in SiC+20[vol.%] $ZrB_2$composite at room temperature. The trend of the mechanical properties of the electroconductive SiC ceramic composites moves in accord with that of the relative density. The electrical resistivities of mono SiC, SiC+15[vol.%]$ZrB_2$, SiC+20[vol.%]$ZrB_2$ and SiC+25[vol.%]$ZrB_2$ composites are 4.57${\times}10^{-1}$, 2.13${\times}10^{-1}$, 1.53${\times}10^{-1}$ and 6.37${\times}10^{-2}$[${\Omega}$ cm] at room temperature, respectively. The electrical resistivity of mono SiC, SiC+15[vol.%]$ZrB_2$. SiC+20[vol.%]$ZrB_2$ and SiC+25[vol.%]$ZrB_2$ are Negative Temperature Coefficient Resistance(hereafter, NTCR) in temperature ranges from 25[$^{\circ}C$] to 100[$^{\circ}C$]. The declination of V-I characteristics of SiC+20[vol.%]$ZrB_2$ composite is 3.72${\times}10^{-1}$. It is convinced that SiC+20[vol.%]$ZrB_2$ composite by SPS can be applied for heater or electrode above 1000[$^{\circ}C$]

Development of Electroconductive SiC-$ZrB_2$ Ceramic Heater and Electrod by Spark Plasma Sintering (SPS에 의한 SiC-$ZrB_2$계 전도성 세라믹 발열체 및 전극 개발)

  • Shin, Yong-Deok;Ju, Jin-Young;Kim, Jae-Jin;Lee, Jung-Hoon;Kim, Cheol-Ho;Choi, Won-Seok
    • Proceedings of the KIEE Conference
    • /
    • 2009.07a
    • /
    • pp.1254_1255
    • /
    • 2009
  • The composites were fabricated by adding 30, 35, 40, 45[vol.%] Zirconium Diboride(hereafter, $ZrB_2$) powders as a second phase to Silicon Carbide(hereafter, SiC) matrix. The physical, mechanical and electrical properties of electroconductive SiC ceramic composites by Spark Plasma Sintering(hereafter, SPS) were examined. Reactions between $\beta$-SiC and $ZrB_2$ were not observed in the XRD analysis. The relative density of SiC+30[vol.%]$ZrB_2$, SiC+35[vol.%]$ZrB_2$, SiC+40[vol.%]$ZrB_2$ and SiC+45[vol.%]$ZrB_2$ composites are 88.64[%], 76.80[%], 79.09[%] and 88.12[%], respectively. The XRD phase analysis of the electroconductive SiC ceramic composites reveals high of SiC and $ZrB_2$ and low of $ZrO_2$ phase. The electrical resistivity of SiC+30[vol.%]$ZrB_2$, SiC+35[vol.%]$ZrB_2$, SiC+40[vol.%]$ZrB_2$ and SiC+45[vol.%]$ZrB_2$ composites are $6.74{\times}10^{-4}$, $4.56{\times}10^{-3}$, $1.92{\times}10^{-3}$ and $4.95{\times}10^{-3}[{\Omega}{\cdot}cm]$ at room temperature, respectively. The electrical resistivity of SiC+30[vol.%]$ZrB_2$, SiC+35[vol.%]$ZrB_2$, SiC+40[vol.%]$ZrB_2$ and SiC+45[vol.%]$ZrB_2$ are Positive Temperature Coefficient Resistance(hereafter, PTCR) in temperature ranges from 25[$^{\circ}C$] to 500[$^{\circ}C$]. It is convinced that SiC+40[vol.%]$ZrB_2$ composite by SPS can be applied for heater or electrode.

  • PDF

The Development of an Electroconductive SiC-ZrB2 Composite through Spark Plasma Sintering under Argon Atmosphere

  • Lee, Jung-Hoon;Ju, Jin-Young;Kim, Cheol-Ho;Park, Jin-Hyoung;Lee, Hee-Seung;Shin, Yong-Deok
    • Journal of Electrical Engineering and Technology
    • /
    • v.5 no.2
    • /
    • pp.342-351
    • /
    • 2010
  • The SiC-$ZrB_2$ composites were fabricated by combining 30, 35, 40, 45 and 50 vol. % of zirconium diboride ($ZrB_2$) powders with silicon carbide (SiC) matrix. The SiC-$ZrB_2$ composites and the sintered compacts were produced through spark plasma sintering (SPS) under argon atmosphere, and its physical, electrical, and mechanical properties were examined. Also, the thermal image analysis of the SiC-$ZrB_2$ composites was examined. Reactions between $\beta$-SiC and $ZrB_2$ were not observed via x-ray diffraction (XRD) analysis. The apparent porosity of the SiC+30vol.%$ZrB_2$, SiC+35vol.%$ZrB_2$, SiC+40vol.%$ZrB_2$, SiC+45vol.%$ZrB_2$ and SiC+50vol.%$ZrB_2$ composites were 7.2546, 0.8920, 0.6038, 1.0981, and 10.0108%, respectively. The XRD phase analysis of the sintered compacts demonstrated a high phase of SiC and $ZrB_2$. Among the $SiC+ZrB_2$ composites, the SiC+50vol.%$ZrB_2$ composite had the lowest flexural strength, 290.54MPa, the other composites had more than 980MPa flexural strength except the SiC+30vol.%$ZrB_2$ composite; the SiC+40vol.%$ZrB_2$ composite had the highest flexural strength, 1011.34MPa, at room temperature. The electrical properties of the SiC-$ZrB_2$ composites had positive temperature coefficient resistance (PTCR). The V-I characteristics of the SiC-$ZrB_2$ composites had a linear shape in the temperature range from room to $500^{\circ}C$. The electrical resistivities of the SiC+30vol.%$ZrB_2$, SiC+35vol.%$ZrB_2$, SiC+40vol.%$ZrB_2$ SiC+45vol.%$ZrB_2$ and SiC+50vol.%$ZrB_2$ composites were $4.573\times10^{-3}$, $1.554\times10^{-3}$, $9.365\times10^{-4}$, $6.999\times10^{-4}$, and $6.069\times10^{-4}\Omega{\cdot}cm$, respectively, at room temperature, and their resistance temperature coefficients were $1.896\times10^{-3}$, $3.064\times10^{-3}$, $3.169\times10^{-3}$, $3.097\times10^{-3}$, and $3.418\times10^{-3}/^{\circ}C$ in the temperature range from room to $500^{\circ}C$, respectively. Therefore, it is considered that among the sintered compacts the SiC+35vol.%$ZrB_2$, SiC+40vol.%$ZrB_2$ and SiC+45vol.%$ZrB_2$ composites containing the most outstanding mechanical properties as well as PTCR and V-I characteristics can be used as an energy friendly ceramic heater or ohmic-contact electrode material through SPS.