Partially stabilized zirconia (PSZ) is an attractive material for thermal barrier coating. Zirconia exists in three crystallographic phases: cubic, tetragonal and monoclinic. Especially, the phase transformation of tetragonal phase to monoclinic phase accompanies significant volume expansion, so this transition generally results in cracking and contributes to the failure of the TBC system. Both the plasma sprayed ZrO$_2$-8Y$_2$O$_3$ (YSZ) coat and the ZrO$_2$,-25CeO$_2$,-2.5Y$_2$O$_3$ (CYSZ) coat are isothermally heat -treated at 130$0^{\circ}C$ and 150$0^{\circ}C$ for 100hr and cooled at different cooling rates. The monoclinic phase is not discovered in all the CYSZ annealed at 130$0^{\circ}C$ and 150$0^{\circ}C$. In the 150$0^{\circ}C$ heat-treated specimens, the YSZ contains some monoclinic phase while none exists in the 130$0^{\circ}C$ heat-treated YSZ coat. For the YSZ, the different phase transformation behaviors at the two temperatures are due to the stabilizer concentration of high temperature phases and grain growth. For the YSZ with 150$0^{\circ}C$-100hr annealing, the amount of monoclinic phase increased with the slower cooling rate. The extra oxygen vacancy, thermal stress, and c to t'phase transformation might suppress the t to m martensitic phase transformation.
Zirconia ($ZrO_2$) is a crystalline dioxide of zirconium. Dental zirconia blocks for CAD/CAM are usually fabricated with powders of tetragonal zirconia polycrystals (TZP) stabilized with 3mol% yttria. Because of its mechanical properties similar to those of metals and color similar to tooth, it is evaluated to attain the two purposes at a time, strength and aesthetic in prosthetic dentistry. The ability of transformation of Y-TZP from tetragonal to monoclinic helps to prevent crack propagation and contributes the increase of strength and fracture toughness. Two different types of blocks, soft and hard, are used to prepare the zirconia frameworks. The fuzzy-sintered block is difficult in machining, so pre-sintered soft 3Y-TZP block is usually used to mill by computer aided machining.
Sinterability, mechanical and electrical properties of yttria-stabilized zirconia(92 mole% $ZrO_{2}$+8 mole% $Y_{2}O_{3}$) doped with 0.5 mole% $SiO_{2}$ and $0{\sim}2.0 mole%{\;}Al_{2}O_{3}$ were studied as a function of $Al_{2}O_{3}$ addition. Sintered density increased with increasing $Al_{2}O_{3}$ addition up to 0.5 mole % but leveled off with further addition. Victors hardness is proportional to sintered density. The specimen with 0.5 mole% $Al_{2}O_{3}$ and 0.5 mole% $SiO_{2}$ exhibited the maximum electrical conductivity and revealed a maximum electromotive force for a given oxygen partial pressure. Experimental voltage curve of this oxygen sensor take on a sharper, more steplike transition at the stoichiometric A/F ratio than those of other commercial oxygen sensors.
Park, Jin-Seong;Kim, Si-Uk;Lee, Eun-Gu;Kim, Jae-Yeol;Lee, Hyeon-Gyu
Korean Journal of Materials Research
/
v.9
no.9
/
pp.896-899
/
1999
A carbon dioxide gas sensor was studied as a function of temperature and $CO_2$concentration in the Li$_2$ZrO$_3$ system. Lithium zirconate(Li$_2$ZrO$_3$) was synthesized by the heat-treatment of zirconia(ZrO$_2$)and Lithium carbonate(Li$_2$CO$_3$). The specimens were prepared both as bulk disk, 10mm in diameter and 1.0mm thickness, and thick films on an alumina substrate. Lithium zirconate readily responded to $CO_2$concentration from 0.1% to 100% in the range of 45$0^{\circ}C$ to $650^{\circ}C$. The sensitivity to $CO_2$ was dependent on the measuring temperature. Lithium zirconate(Li$_2$ZrO$_3$) decomposes into Li$_2$CO$_3$ and ZrO$_2$after the reaction with $CO_2$in the range of 45$0^{\circ}C$ to $650^{\circ}C$. Li$_2$CO$_3$ changes into Li$_2$O and $CO_2$ above $650^{\circ}C$. The material showed difficulty with reversibility and recovery. The optimum temperature for the highest sensitivity is around 55$0^{\circ}C$.
Kim, Gi-Dong;Sin, Dong-Geun;Jo, Yeong-A;Jeon, Jin-Seok;Choe, Dong-Su;Park, Jong-Jin
Korean Journal of Materials Research
/
v.9
no.3
/
pp.234-239
/
1999
A Abstract Yttria-stabilized zirconia(YSZ) thin films were synthesized by plasma enhanced chemical vapor deposition process. $Zr[TMHD]_4$$Y[TMHD]_3$ precursors and oxygen were used with the deposition temperature of $425^{\circ}C$ and rf power ranging 0-100 watt. Effects of the deposition parameters were studied by X-ray diffraction and thickness analysis. YSZ thin films have cubic crystal structure with (200) orientation. From the results of EDX analysis, the converte ed content of TEX>$Y_2O_3$ was determined to be 0-36%, and the film thickness was increased with bubbling temperature which is considered to be due to increasing TEX>$Y_2O_3$ flux. The depth profiles of Zr, Y and 0 appeared relatively $\infty$nstant through film thickness. Columnar grains of $1000~2000\AA$ grew vertical to the substrate surface for the case of Ar carrier gas. In case of He carrier gas, the grain size was observed to be about $1000~2000\AA$. X-ray diffraction data showed the increase of lattice constant with TEX>$Y_2O_3$ content. It was that the presence of the cracks formed during film deposition, partially released the stress generated by the increase of lattice constant.
Kim, Seong-Won;Lee, Sung-Min;Oh, Yoon-Suk;Kim, Hyung-Tae;Jang, Byung-Koog
Journal of Powder Materials
/
v.18
no.6
/
pp.568-574
/
2011
As operating temperatures of engines or turbines continually increase for higher efficiency, significant amounts of researches have been focused on finding new materials, which would be alternatives to conventional yttria-stabilized zirconia (YSZ) for thermal barrier coatings (TBCs). In this study, phase evolution and thermo-physical properties of $La_2(Zr_{1-x}Hf_x)_2O_7$ pyrochlore systems are investigated for TBC applications. $La_2(Zr_{1-x}Hf_x)_2O_7$ systems are comprised by selecting $La^{3+}$ as A-site ions and $Zr^{4+}/Hf^{4+}$ as B-site ions in $A_2B_2O_7$ pyrochlore structures. For the developed phases in $La_2(Zr_{1-x}Hf_x)_2O_7$ compositions, thermo-physical properties such as thermal conductivity, thermal expansion coefficient are examined. The potential of these $La_2(Zr_{1-x}Hf_x)_2O_7$ compositions for TBC application is also discussed.
Proceedings of the Korean Nuclear Society Conference
/
1996.05c
/
pp.39-45
/
1996
핵비확산 목적으로 원심분무방법으로 저농축 우라늄 고밀도의 U$_3$Si$_2$구형분말 분산핵연료를 개발하는 일환으로 융점이 높은 U$_3$Si$_2$원심분무용 도가니와 nozzle에 적합한 재료를 선정하고자 zirconia계 물질과 yttria물질에 대한 양립성을 시험하였다. ZrO$_2$계 세라믹은 U$_3$Si$_2$와 우수한 양립성을 나타냈는데 부분 안정화시킨 Zirconia가 Crack 발생이 없어 완전 안정화시킨 것보다 내열충격이 더 양호한 것으로 보인다. Zirconia 도가니는 흑연과 반응하여 표면에 carbide를 형성하여 박리 되는 현상이 발생되었는데 부분 안정화 zirconia가 약간 더 많이 형성됨을 나타냈다. Yttria는 180$0^{\circ}C$이상에서 흑연과 반응하여 액상으로 형성되고 U$_3$Si$_2$와도 반응하여 사용에 부적합한 것으로 판명되었다. 내열충격이 비교적 우수한 부분 안정화 zirconia로 tundish를 제조하여 U$_3$Si$_2$를 원심분무한 결과 nozzle확장되지 않아서 입도분포가 협소한 분말을 얻는데 성공하였다.
Yttria-stabilized zirconia(YSZ) films were prepared onto p-type (100) silicon wafer by a plasma-enhanced metallorganic chemical vapor deposition(PE MO CVD) processing involving the application of vapor mixture of tri(2.2.6.6-tetramethyl-3, 5-heptanate) yttrium$[Y(DPM)_3]$, zirconiumtriflouracethyla cetonate$(Zr(tfacac)_4$ and oxygen gas. The x-ray diffraction(XRD) and fourier transform infrared spectra(FT1R) results showed that the deposited YSZ films had a single cubic phase. $Y_2O_3$ content of YSZ film was analyzed by PIXE(partic1e induced x-ray emission). The experimental results by PIXE revealed that 12.lmol%, 20.4mol% and 31.6mol% $Y_2O_3$ could be obtained as the $Y(DPM)_3$ bubbling temperature varied at $160^{\circ}C, 165^{\circ}C$ and $170^{\circ}C$ respectively. The increase of $Y(DPM)_3$ bubbling temperature caused shifting flat band voltage to have a negative value.
Selvaraj, D. Edison;Vijayaraj, R.;Sugumaran, C. Pugazhendhi
Journal of Electrical Engineering and Technology
/
v.10
no.4
/
pp.1700-1711
/
2015
In the last decade it has been witnessed significant developments in the area of nano particles and nano scale fillers on electrical, thermal, and mechanical properties of polymeric materials such as resins, varnishes, enamel and bakelites. The electric and thermal properties were more important in the electrical equipments for both steady state and transient state conditions. This paper deals with the characterization of the electric and thermal properties of the pure varnish and zirconia (ZrO2) filler mixed varnish. The electric properties such as dielectric loss (tan δ), dielectric constant (ε), dielectric strength and partial discharge voltage were analyzed and detailed for different samples. It was observed that zirconia nano filler mixed varnish has the superior dielectric and thermal properties when compared to those of standard varnish. It has shown that at power frequency the 1wt% nano composite sample has the higher permittivity value when compared to other samples. It has been examined that the 1wt% sample was having higher inception and extinction voltages when compared to other samples. It has been observed that 1wt% sample has higher dielectric strength when compared with other samples. There has been an improvement of thermal property by adding few weight percent of zirconia nano fillers. There was not much variation in glass transition among the nano mixed composites. The weight loss was improved at 1wt% of the zirconia nano fillers.
Monodispersed alumina-zirconia fine powders were prepared by controlled hydrolysis of alkoxides. These powders and the sintered bodies were characterized. Aluminium alkoxide and zirconium alkoxide were dissolved into complex solvent with butanol and n-propanol, and by acetonitrile added hydrolytic solution, hydrolysis rate was controlled. The oil, as a dispersant, was added in hydrolytic solution, and then prepared powders were nano-sized and well-monodispersed. In the case of hydroxypropyl celluose (HPC) as a dispersant, it was added in complex solution with butanol and iso-propanol, sub-micrometer sized and well-monodispersed powders could be prepared. The value of relative density (R.D.) and tetragonal phase fraction of zirconia in the sintered body made by nano-meter sized powders were respectively higher than those in the case of sub-micrometer sized one.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.