Rashad, M.;Tekin, H.O.;Zakaly, Hesham MH.;Pyshkina, Mariia;Issa, Shams A.M.;Susoy, G.
Nuclear Engineering and Technology
/
제52권9호
/
pp.2078-2084
/
2020
Magnesium oxide (MgO) and Zinc oxide (ZnO) nanoparticles (NPs) have been successfully synthesized by solid-solid reaction method. The structural properties of ZnO and MgO NPs were studied using X-ray diffraction (XRD) and scanning electron microscopy (SEM). XRD results indicated a formation of pure MgO and ZnO NPs. The mean diameter values of the agglomerated particles were around to be 70 and 50 nm for MgO and ZnO NPs, respectively using SEM analysis. Further, a wide-range of nuclear radiation shielding investigation for gamma-ray and fast neutrons have been studied for Magnesium oxide (MgO) and Zinc oxide (ZnO) samples. FLUKA and Microshield codes have been employed for the determination of mass attenuation coefficients (μm) and transmission factors (TF) of Magnesium oxide (MgO) and Zinc oxide (ZnO) samples. The calculated values for mass attenuation coefficients (μm) were utilized to determine other vital shielding properties against gamma-ray radiation. Moreover, the results showed that Zinc oxide (ZnO) nanoparticles with the lowest diameter value as 50 nm had a satisfactory capacity in nuclear radiation shielding.
암모니아수와 zinc acetate로부터 액상 수열합성법에 의한 ZnO의 제조에 있어 반응온도, 반응물의 농도와 혼합방법, 용액의 pH 등 반응조건에 따른 ZnO 입자의 형상과 입자분포 등 제조특성을 고찰하고, UV 조사하에 tartrazine의 광분해를 측정하여 합성된 ZnO의 광촉매로서의 성능을 확인하였다. 반응용액의 pH가 높을수록 ZnO 입자의 평균 크기는 증가하였고, zinc acetate의 농도가 증가할수록 그리고 반응온도가 증가할수록 입자의 크기는 감소하였다. 반응용액의 혼합시 암모니아수 주입 후에 zinc acetate를 첨가하였을 경우 더 작은 입자를 얻을 수 있었다. 최소 크기의 ZnO 입자의 생성을 위한 최적 조건은 용액의 pH 11.2, zinc acetate의 농도 0.6 M, 반응온도 $90^{\circ}C$였으며, 입자 평균크기는 3.133 ${\mu}$m이었다. 합성온도 $80^{\circ}C$, zinc acetate 농도 1.0M 및 반응용액의 pH 11.2의 조건에서 합성된 ZnO에 의한 tartrazine의 광촉매 분해는 분해시간 60분에서 약 97%의 분해율을 보였다.
Zinc oxide micro rods were fabricated using as chemical bath deposition ok photolithography. Vertically aligned Zinc Oxide rod array as grown by chemical bath deposition method on Zinc Oxide template layer. The ZnO template layer was deposited on glass and the pattering was made by standard photolithography technique. The selective growth of ZnO micro rods were achieved with the masked ZnO template layer substrate. The fabricated ZnO micro rods were found to be single crystalline and have grown along hexagonal c-axis direction of (0002) which is same as the preferred growth orientation of ZnO template layer. The ZnO micro-rod array structure was implemented as a window layer in Cu(InGa)Se2 solar cell and its effect on photovoltaic efficiency was examined.
The highly c-axis oriented zinc oxide thin films were deposited on Sapphire(0001) substrates by reactive RF magnetron sputtering. The characteristics of zinc oxide thin films on RF power, substrate-target distance, and substrate temperature were investigated by XRD, SEM and EDX analyses. The physical characteristics of zinc oxide thin films changed with various deposition conditions. The higher substrate temperatures were, The better crystallinity of zinc oxide thin films. The highly c-axis oriented zinc oxide thin films were obtained at sputter pressure 5mTorr, rf power 200W, substrate temperature 350.deg. C, substrate-target distance 5.5cm. In these conditions, the resistivity of zinc oxide thin films deposited on pt/sapphire was 12.196*10$^{9}$ [.ohm.cm].
ZnO는 반도전성과 초전도성을 나타내며 광학적으로도 독특한 재료로 가스센서, 태양전지, 광학도파관 등 여러 방면에 널리 활용되고 있다. 본 논문에서는 이러한 ZnO에 Al을 첨가함에 따라 광학적 특성에 어떠한 영향을 미치는지 알아보기 위하여 ZnO에 Al 첨가량 변화에 따른 나노구조체를 제작하여 특성을 비교하였다. ZnO 용액은 PVP, ethanol, zinc acetate를 이용하여 Sol의 형태로 제작하였으며, Al첨가용액을 넣어 Al이 첨가된 ZnO Sol을 제작하였다. 제작된 Sol을 전기 방사법을 이용하여 나노구조체를 제조하였다. 제조된 섬유들을 각각 300, 500, $700^{\circ}C$로 열처리 한 후 나노 구조체를 XRD, XPS, SEM을 이용하여 분석하였다. 또한 TGA, DSC를 이용하여 온도변화에 따른 질량 및 열량의 변화를 측정하였다. UVvis를 이용하여 ZnO와 Al이 첨가된 ZnO의 흡광도를 측정 비교하였다.
Zinc oxide (ZnO) is a unique semiconductor material that exhibits numerous useful properties for dye-sensitized solar cells (DSSCs) and other applications. Various thin-film growth techniques have been used to produce nanowires, nanorods, nanotubes, nanotips, nanosheets, nanobelts and terapods of ZnO. These unique nanostructures unambiguously demonstrate that ZnO probably has the richest family of nanostructures among all materials, both in structures and in properties. The nanostructures could have novel applications in solar cells, optoelectronics, sensors, transducers and biomedical sciences. This article reviews the various nanostructures of ZnO grown by various techniques and their application in DSSCs. The application of ZnO nanowires, nanorods in DSSCs became outstanding, providing a direct pathway to the anode for photo-generated electrons thereby suppressing carrier recombination. This is a novel characteristic which increases the efficiency of ZnO based dye-sensitized solar cells.
In this paper, aluminum doped zinc oxide (ZnO:Al) thin films on plastic substrate such as poly carbonate (PC), polyethylene terephthalate (PET) were prepared by RF magnetron sputtering method for flexible solar cell applications. Effects of the sputter pressure on the structural, electrical and optical properties were investigated. The crystallinity and the degree of the (002) orientation were deteriorated with increasing the sputter pressure. When the sputter pressure was higher, the conductivity of ZnO:Al films was improved because of the high carrier concentration and the Hall mobility. High quality ZnO:Al films with resistivity as low as $1.9{\times}10^{-3}{\Omega}-cm$ and the optical transmittance over 80 % in the visible region have been obtained on PC substrate at 2 mTorr.
Ja-Seon Yoon;Sang Yoon Nam;Beom Jun Lee;Hyun Jik Lee
Journal of Veterinary Science
/
제24권1호
/
pp.3.1-3.13
/
2023
Background: Zinc (Zn) is an essential cofactor for physiological homeostasis in the body. Zn oxide (ZnO), an inorganic compound that supplies Zn, exists in various sizes, and its bioavailability may vary depending on the size in vivo. However, comparative studies on the nutritional effects of micro-sized ZnO (M-ZnO) and nano-sized ZnO (N-ZnO) supplementation on Zn deficiency (ZnD) animal models have not been reported. Objectives: This study investigated the nutritional bioavailability of N-ZnO and M-ZnO particles in dietary-induced ZnD mice. Methods: Animals were divided into six experimental groups: normal group, ZnD control group, and four ZnO treatment groups (Nano-Low, Nano-High, Micro-Low, and MicroHigh). After ZnD induction, N-ZnO or M-ZnO was administered orally every day for 4 weeks. Results: ZnD-associated clinical signs almost disappeared 7 days after N-ZnO or M-ZnO administration. Serum Zn concentrations were higher in the Nano-High group than in the ZnD and M-ZnO groups on day 7 of ZnO treatment. In the liver and testis, Nano-Low and Nano-High groups showed significantly higher Zn concentrations than the other groups after 14-day treatment. ZnO supplementation increased Mt-1 mRNA expression in the liver and testis and Mt-2 mRNA expression in the liver. Based on hematoxylin-and-eosin staining results, N-ZnO supplementation alleviated histological damage induced by ZnD in the testis and liver. Conclusions: This study suggested that N-ZnO can be utilized faster than M-ZnO for nutritional restoration at the early stage of ZnD condition and presented Mt-1 as an indicator of Zn status in the serum, liver, and testis.
Due to the high surface-to-volume ratio, the 3-dimensional(3D) nanostructures of metal oxides are regarded as the best candidate materials for the chemical gas sensors. Here we have synthesised flower-like 3D zinc oxide nanostructures through a simple hydrothermal route. Specific surface area of the 3D zinc oxide nanostructures synthesised in different pH values from 9.0 to 12.0 were evaluated by using a BET analyzer and the results were compared with that of a zinc oxide thin film fabricated by rf sputtering. Using interdigitated electrodes, superior CO gas sensing properties of the 3D zinc oxide nanostructures on the ZnO thin film to those of the ZnO thin film were demonstrated.
In this study, an environment-friendly synthetic strategy to process zinc oxide nanocrystals is reported. The biosynthesis method used in this study is simple and cost-effective, with reduced solvent waste via the use of fruit peel extract as a natural ligation agent. The formation of ZnO nanocrystals using a rambutan peel extract was observed in this study. Rambutan peels has the ability to ligate zinc ions as a natural ligation agent, resulting in ZnO nanochain formation due to the presence of an extended polyphenolic system over the whole incubation period. Via transmission electron microscopy, successful formation of zinc oxide nanochains was confirmed. TEM observation revealed that the bioinspired ZnO nanocrystals were spherical and/or hexagonal particles with sizes between 50 and 100 nm.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.