YBa$_2$Cu$_3$$O_{7-x}$ (YBCO) films were deposited on MgO(100) and SrTiO$_3$(100) single crystal substrates by cold-wall type MOCVD method using continuous source supplying system. Under the deposition temperature of 740∼76$0^{\circ}C$, c-axis oriented YBCO films were obtained. In case of the YBCO films deposited on MgO (100) single crystal substrate, the critical temperature (T$_{c}$) was under 81 K regardless of the deposition conditions, whereas T$_{c}$ of the YBCO films deposited on SrTiO$_3$(100) single crystal substrate was 83∼84 K. The critical current (I$_{c}$) of the YBCO film deposited on SrTiO$_3$(100) single crystal substrate for 30 min was 49 A/cm-width and the critical current density (J$_{c}$) was 0.82 MA/$\textrm{cm}^2$ to film thickness of 0.6 ${\mu}{\textrm}{m}$. I$_{c}$ increased to 84.4 A/cm-width as the deposition time increased to 50 min, but J$_{c}$ decreased to 0.53 MA/$\textrm{cm}^2$ to film thickness of 1.8 ${\mu}{\textrm}{m}$.rm}{m}$.
With an aim of comparison, single grain Y-Ba-Cu-O (YBCO) bulk superconductors were fabricated using a liquid infiltration growth (LIG) process and a conventional melt growth (MTG) process with top seeding. The MTG process uses an $YBa_2Cu_3O_{7-x}$(Y123) powder as a precursor, while the LIG process uses $Y_2BaCuO_5(Y211)/Ba_3Cu_5O_8(Y035)$ pre-forms. The growth of a single Y123 domain on the top seed was successful in the both processes. Different feature between the two processes is the interior microstructure regarding the critical current density ($J_c$). The LIG-processed YBCO sample showed a lower porosity, more uniform distribution of Y211 particles and the enhanced Y211 refinement compared to the conventional MTG process. The $J_c$ improvement in the LIG process is attributed to the dispersion of finer Y211 particles as well as lower porosity within the Y123 superconducting matrix.
[ $YBa_2Cu_3O_{7-{\delta}}$ ] films have been prepared on $LaAlO_3$ (100) single-crystal substrates by the metal organic deposition using dichloroacetate precursors (DCA-MOD). DCA precursor solutions with different composition such as; Yttrium-excess(15 at%), barium-poor(25 at%), and a stoichiometric(Y:Ba:Cu=1:2:3) were prepared in order to investigate the effects of precursor composition on the properties of YBCO films prepared by DCA-MOD method. Coated films were calcined at low temperature up to $500^{\circ}C$ in flowing humid oxygen atmosphere. Conversion heat treatment was performed $800^{\circ}C$ for 2 h in flowing Ar gas containing 1000 ppm oxygen with a humidity of 9.45%. For the film prepared using excess yttrium composition, high critical current density ($J_c$) of $>2MA/cm^2$ was obtained whereas, for the films prepared using barium-poor composition, $J_c$ was lower than $1MA/cm^2$.
Bi/CNT composite and resin/CNT were chosen to improve the mechanical properties of $YBa_2Cu_3O_7$(YBCO) superconductor. In order to elucidate the effects of Bi/CNT composite and resin/CNT in YBCO superconductors, melt texture superconductor were impregnated by mixed compound of Bi and CNT into the artificial holes parallel to the c-axis, which were drilled on the YBCO superconductor. Various amount of Bi/CNT and resin/CNT were impregnated to YBCO superconductor with different holes diameters. Typical artificial holes diameters were 0.5, 0.7, and 1.0 mm respectively. Result of three-point bending test measurement, the bending strength with resin/CNT impregnation was improved up to 59.64 MPa as compared with 50.79 MPa of resin/CNT free bulk. Resin/CNT impregnation has been found to be one of the effective ways in improving the mechanical properties of bulk superconductor.
We investigated recovery in $Au/YBa_2Cu_3O_7$ (YBCO) thin film meander lines on sapphire substrates. The meander lines were fabricated by patterning YBCO films coated with gold layers. The lines were subjected to simulated AC fault current and then small current was applied for recovery measurements. The samples were immersed in liquid nitrogen during the experiment. After the fault, the resistance decreased linearly, first slowly and then fast to zero. The initial slow decrease was due to the decrease of the meander line temperature, whereas the fast decrease was originated from the transition from the normal state to the superconducting state. The recovery speed depended on the size of samples, and was faster in the smaller samples during the whole period of recovery. The experimental results were analyzed quantitatively with the concept of heat transfer within the sample and to the surrounding liquid nitrogen. A heat balance equation was solved for the initial phase of recovery, and an expression for the time dependence of resistance was obtained. The result agreed with data well.
YBCO thin films on $SiO_2$/Si substrate were fabricated by spin-coaing of an alkoxide-derived precursor and heat treatment. The structural and electrical properties of the YBCO films were investigated as functions of annealing temperature at $600{\sim}800^{\circ}C$. Although YBCO single phase was not synthesized, dense films of YBCO matrix phase and minor second phases have been successfully fabricated at the annealing temperatures of $650{\sim}800^{\circ}C$. Thickness and temperature coefficient of resistance (TCR) of YBCO thin films with annealing temperature of $750^{\circ}C$ were 0.31 ${\mu}m$ and $-2.92%/^{\circ}C$, respectively.
한국초전도학회 1999년도 High Temperature Superconductivity Vol.IX
/
pp.124-128
/
1999
We report microwave properties of high-T$_c$ superconducting (HTS) microstrip antennas without impedance matching circuits, where the impedance mismatching is obvious under the critical temperature (T$_c$). The superconducting thin films used in this report were YBa$_2Cu_3O_{7-x}$ (YBCO) films deposited on MgO substrates produced by pulse laser deposition (PLD) technique. At around T$_c$, 86 K the reflection coefficient rapidly drops, and the standing wave ratio (SWR) becomes almost unity, and the characteristic impedance based on the Smith chart is nearly 50 ${\Omega}$. The reflection coefficient and the SWR of the HTS microstrip antenna were - 62.52 dB and 1.0015, respectively, at the resonant frequency of 11.812 CHz at 86 K.
한국초전도학회 1999년도 High Temperature Superconductivity Vol.IX
/
pp.87-90
/
1999
We have studied the annealing effects of 570 (SrTiO$_3$) single crystal substrate and the I-V properties of step-edge junctions after Ar ion milling. YBa$_2Cu_3O_7$ (YBCO) thin films are fabricated on the substrates by using pulsed laser deposition (PLD) and photolithography. The surface of Ar ion milled substrate was characterized with atomic force microscope (AFM) and scanning electron microscope (SEM) images. After the substrate was damaged by milling, the critical current density of YBCO thin films deposited on the substrate was lowered. The annealing of the damaged substrate at about 1000 $^{\circ}C$ recovered the critical current density to that before the milling. Futhermore the annealing helped junction formation due to high quality film and increased the yield rate for the fabrication of high quality step-edge junction.
한국초전도학회 1999년도 High Temperature Superconductivity Vol.IX
/
pp.91-94
/
1999
A new type of high-T$_c$ superconducting Josephson junctions has been prepared by Ar ion beam etching and electron beam lithography. YBa$_2Cu_3O_{7-x}$ (YBCO) films deposited on (001) SrTiO$_3$ single crystal substrate by pulsed laser deposition were patterned by Ar ion milling with photolithography. The narrow slit with a electroresist mask, about 1000 ${\AA}$ wide, was constructed over a 3 ${\sim}$ 5 ${\mu}$m bridge of a 1200-${\AA}$-thick YBCO film by electron beam lithography. The slit was then etched by the Ar ion beam to form a damaged 600-${\AA}$-thick YBCO. Thus prepared structure forms an S-N-S (YBCO - damaged YBCO - YBCO) type Josephson junctions. Those junctions exhibit RSI-like I-V characteristics at 77 K. The properties of the Josephson junctions such as I$_c$ R$_N$, and J$_c$ were characterized.
한국초전도학회 1999년도 High Temperature Superconductivity Vol.IX
/
pp.147-151
/
1999
YBCO step-edge Josephson junction were fabricated on sapphire substrates. The steps were formed on R-plane sapphire substrates by using Ar ion milling with PR masks. The step angle was controlled in the wide range from 25$^{\circ}$ to 50$^{\circ}$ by adjusting both the Ar ion incident angle and the photoresist mask rotation angle relative to the incident Ar ion beam. CeO$_2$ buffer layer and in-situ YBa$_2Cu_3O_{7-{\delta}}$ (YBCO) thin films was deposited on the stepped R-plane sapphire substrates by pulsed laser deposition method. The YBCO film thickness was varied to obtain the ratio of film thickness to step height in the range from 0.5 to 1. The step edge junction exhibited RSJ-like behaviors with I$_cR_n$ product of 100 ${\sim}$ 300 ${\mu}$V, critical current density of 10$^3$${\sim}$ 10$^5$ A/ cm$^2$ at 77 K.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.