• Title/Summary/Keyword: White Jabon

Search Result 2, Processing Time 0.026 seconds

Comparison of Anatomical Characteristics of White Jabon and Red Jabon Grown in Indonesia (인도네시아산 White Jabon과 Red Jabon의 해부학적 특성 비교)

  • Kim, Jong-Ho;Jang, Jae-Hyuk;Ryu, Jae-Yun;Hwang, Won-Joung;Febrianto, Fauzi;Kim, Nam-Hun
    • Journal of the Korean Wood Science and Technology
    • /
    • v.41 no.4
    • /
    • pp.327-336
    • /
    • 2013
  • Anatomical characteristics of White Jabon (Arthocephalus cadamba) and Red Jabon (Arthocephalus macrophyllus) were investigated by IAWA hardwood feature list. Both species were diffuse-porous, and radial multiple pore with 2~3 rows was mostly observed. Tangential diameter of vessel lumina was 100 to $200{\mu}m$, and vessels per square millimeter were 5 to 20. White Jabon has more vessels than Red Jabon. The number of solitary pore per square millimeter in both species was similar, but more pore multiple was observed in White Jabon. Axial parenchyma diffuse was observed in both species, but axial parenchyma of White Jabon was hardly identified on the cross section. Rays were classified into "body ray cells procumbent with over 4 rows of upright/square marginal cells" type and partly "all ray cells upright and/or square" type on radial section. Ray width 1 to 3 cells and 1 to 2 cells observed in White Jabon and Red Jabon, respectively. Ray height of White Jabon was $420{\mu}m$ and Red Jabon $474{\mu}m$. Fiber length was the range of 900 to $1,600{\mu}m$ in both species, and it showed a tendency to increase from pith to bark. Consequently, it is considered that pore multiple, ray width and axial parenchyma are to be suggested the keys for identification of both species.

Effect of Tree Age and Active Alkali on Kraft Pulping of White Jabon

  • Wistara, Nyoman J.;Carolina, Anne;Pulungan, Widya S.;Emil, Nadrah;Lee, Seung-Hwan;Kim, Nam-Hun
    • Journal of the Korean Wood Science and Technology
    • /
    • v.43 no.5
    • /
    • pp.566-577
    • /
    • 2015
  • White Jabon (Anthocephalus cadamba Miq.) is one of the fast growing species in Indonesia and has the potential as the raw material for pulp and paper. In this research, 3, 5, and 7 years old White Jabon woods were pulped under different active alkali charge of 15%, 18%, 21%, 24%, and 27%, and its effect on delignification degree, kappa number, pulp yield, pulp viscosity, brightness, unbeaten freeness, and delignification selectivity was investigated. The results showed that tree age and active alkali concentration influenced the quality of pulp and pulping properties, except for that of unbeaten freeness. Delignification degree increased with increasing active alkali charge, and this brought about the decrease of pulp kappa number. The pulping yield tended to decrease below the Klason lignin of approximately 4%. Even though the 3 years old wood resulted in the highest brightness and highest delignification selectivity, the highest pulp viscosity was obtained with the 5 years old wood. The dominant fiber length of all wood ages was in the range of 1.2 - 2.0 mm. The 3 years old wood was considered to be the most promising raw material for kraft pulping in the view point of pulping properties, pulp quality and harvesting rotation.