Control of Particle Size and Luminescence Property in Zn$_2$SiO$_4$:Mn Green Phosphor (Zn$_2$SiO$_4$:Mn 녹색형광체의 입도제어 및 발광특성)

  • Seong, Bu-Yong;Jeong, Ha-Gyun;Park, Hui-Dong
    • Korean Journal of Materials Research
    • /
    • v.11 no.8
    • /
    • pp.636-640
    • /
    • 2001
  • In order to improve the optical Performance of green emitting phosphor for plasma display panel (PDP) application, the wet chemical method for preparing $Zn_{2-x}$ $SiO_4$:xMn (xi=0.02. 0.08) phosphor was designed. The spherical phosphor particles were obtained and the size can be between 0.5$\mu\textrm{m}$ and 2$\mu\textrm{m}$. The formation of phosphor, which had the willemite structure, was completed at relatively low temperature of 108$0^{\circ}C$. Also, photoluminescence Properties of the phosphors prepared were investigated under vacuum ultraviolet excitation. In particular, the emission intensity of Zn$_2$SiO$_4$:0.08Mn phosphor having the 1$\mu\textrm{m}$ of particle size was higher than that of commercial phosphor by 40%. The decay time of zinc silicate powder prepared as containing 8 mole% of manganese has been measured as 7.8ms.

  • PDF

Control of Particle Size and Luminescence Property in Zn$_2$SiO$_4$:Mn Green Phosphor (Zn$_2$SiO$_4$:Mn 녹색형광체의 입도제어 및 발광특성)

  • 성부용;정하균;박희동
    • Korean Journal of Materials Research
    • /
    • v.11 no.8
    • /
    • pp.363-363
    • /
    • 2001
  • In order to improve the optical Performance of green emitting phosphor for plasma display panel (PDP) application, the wet chemical method for preparing $Zn_{2-x}$ $SiO_4$:xMn (xi=0.02. 0.08) phosphor was designed. The spherical phosphor particles were obtained and the size can be between 0.5$\mu\textrm{m}$ and 2$\mu\textrm{m}$. The formation of phosphor, which had the willemite structure, was completed at relatively low temperature of 108$0^{\circ}C$. Also, photoluminescence Properties of the phosphors prepared were investigated under vacuum ultraviolet excitation. In particular, the emission intensity of Zn$_2$SiO$_4$:0.08Mn phosphor having the 1$\mu\textrm{m}$ of particle size was higher than that of commercial phosphor by 40%. The decay time of zinc silicate powder prepared as containing 8 mole% of manganese has been measured as 7.8ms.

The Effect of Liquid Medium on Silicon Grinding and Oxidation during Wet Grinding Process (습식분쇄공정에서 액상매체가 실리콘 분쇄 및 산화특성에 미치는 영향)

  • Kwon, Woo Teck;Kim, Soo Ryong;Kim, Young Hee;Lee, Yoon Joo;Shin, Dong Geun;Won, Ji Yeon;Oh, Sea Cheon
    • Journal of the Korean Ceramic Society
    • /
    • v.51 no.2
    • /
    • pp.121-126
    • /
    • 2014
  • The influence of a liquid medium duringa wet-milling process in the grinding and oxidation of silicon powder was investigated. Distilled water, dehydrated ethanol and diethylene glycol were used as the liquid media. The applied grinding times were 0.5, 3, and 12 h. Ground silicon powder samples were characterized by means of aparticle size analysis, scanning electron microscopy(SEM), x-ray powder diffraction (XRD), FT-IR spectroscopy and by a chemical composition analysis. From the results of the characterization process, we found that diethylene glycol is the most efficient liquid medium when silicon powder is ground using a wet-milling process. The FT-IR results show that the Si-O band intensity in an unground silicon powder is quite strongbecause oxygen becomes incorporated with silicon to form $SiO_2$ in air. By applying deionized water as a liquid medium for the grinding of silicon, the $SiO_2$ content increased from 4.12% to 31.7%. However, in the cases of dehydrated ethanol and diethylene glycol, it was found that the $SiO_2$ contents after grinding only changed insignificantly, from 4.12% to 5.91% and 5.28%, respectively.

Influence of KOH Solution on the Passivation of Al2O3 Grown by Atomic Layer Depostion on Silicon Solar Cell

  • Jo, Yeong-Jun;Jang, Hyo-Sik
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2013.08a
    • /
    • pp.299.2-299.2
    • /
    • 2013
  • We investigated the potassium remaining on a crystalline silicon solar cell after potassium hydroxide (KOH) etching and its effect on the lifetime of the solar cell. KOH etching is generally used to remove the saw damage caused by cutting a Si ingot; it can also be used to etch the rear side of a textured crystalline silicon solar cell before atomic layer-deposited Al2O3 growth. However, the potassium remaining after KOH etching is known to be detrimental to the efficiency of Si solar cells. In this study, we etched a crystalline silicon solar cell in three ways in order to determine the effect of the potassium remnant on the efficiency of Si solar cells. After KOH etching, KOH and tetramethylammonium hydroxide (TMAH) were used to etch the rear side of a crystalline silicon solar cell. To passivate the rear side, an Al2O3 layer was deposited by atomic layer deposition (ALD). After ALD Al2O3 growth on the KOH-etched Si surface, we measured the lifetime of the solar cell by quasi steady-state photoconductance (QSSPC, Sinton WCT-120) to analyze how effectively the Al2O3 layer passivated the interface of the Al2O3 layer and the Si surface. Secondary ion mass spectroscopy (SIMS) was also used to measure how much potassium remained on the surface of the Si wafer and at the interface of the Al2O3 layer and the Si surface after KOH etching and wet cleaning.

  • PDF

Sol- Gel Synthesis and Luminescent Properties of ${Y_2}{SiO_5}:Ce$ Blue Phosphors (${Y_2}{SiO_5}:Ce$ 청색 형광체의 졸-겔 합성 및 발광특성)

  • Lee, Jun;Han, Cheong-Hwa;Park, Hee-Dong;Yun, Sock-Sung
    • Korean Journal of Materials Research
    • /
    • v.11 no.9
    • /
    • pp.740-744
    • /
    • 2001
  • The $Y_2SiO_5:Ce$ phosphors were synthesized by sol-gel technique in order to improve the performance of blue emitting phosphors for field emission display(FED). The resulted$Y_2SiO_5:Ce$ phosphors enhanced the emission intensity. In addition, calcination temperature of sol-gel technique(1300~140$0^{\circ}C$) was lower than that of the solid state reaction(>1$600^{\circ}C$). Under 365 nm and low voltage electron excitations. $Ce^{3+}$ -activated $Y_2SiO_5$phosphors showed blue emission band with a range of 400~ 430nm. Especially, 2mol% $Ce^{3+}$ doped $Y_2SiO_5:Ce$phosphors showed the maximum emission intensity. We have also controlled drying temperature of wet gel, pH, and $H_2O$/TEOS molar ratio for the optimum condition of TEOS hydrolysis.

  • PDF

Passivation properties of SiNx and SiO2 thin films for the application of crystalline Si solar cells (결정질 실리콘 태양전지 응용을 위한 SiNx 및 SiO2 박막의 패시베이션 특성 연구)

  • Jeong, Myung-Il;Choi, Chel-Jong
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.24 no.1
    • /
    • pp.41-45
    • /
    • 2014
  • We have investigated the passivation property of $SiN_x$ and $SiO_2$ thin films formed using various process conditions for the application of crystalline Si solar cells. An increase in the thickness of $SiN_x$ deposited using plasma enhanced chemical vapor deposition (PECVD) led to the improvement of passivation quality. This could be associated with the passivation of Si dangling bonds by hydrogen atoms which were supplied during PECVD deposition. The $SiO_2$ thin films grown using dry oxidation process exhibited better passivation behavior than those using wet oxidation process, implying the dry oxidation process was more effective in the formation of high quality $SiO_2$ thin films. The relative effective life time gradually decreased with increasing dry oxidation temperature. Such a degradation of passivation behavior could be attributed to the increase in interface trap density caused by thermal damages.

Characteristics of HfO2 Thin Films Using Wet Etching (습식식각을 이용한 HfO2 박막의 식각특성)

  • Yang, Jeung-Ryoul;Kwak, Noh-Seok;Lim, Jung-Hun;Choi, Yong-Jae;Hwang, Taek-Sung
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.24 no.9
    • /
    • pp.687-692
    • /
    • 2011
  • Hafnium oxide ($HfO_2$) was very advantageous for substitute material of gate on existing transistor. $HfO_2$ has been widely studied due to high contact with polysilicon and thermal stability and also, it is easily etched by using HF solution. In this study, $HfO_2$ and thermal oxide films were etched by wet etch method using chemical etchant. Etch rate of $HfO_2$ and thermal oxide was linearly increased with increasing concentration of HF and temperature but etch rate of $HfO_2$ was higher than thermal oxide due to $H^+$, $F^-$, and $HF_2^-$ ions at below 0.5% concentration of HF. And also, etch selectivity was improved by adding Hydrazine as additive.

Sintering Characteristics of Zircon Nanopowders Fabricated by High Energy Milling Process (고 에너지 밀링 공정으로 제조된 지르콘 나노분말의 소결특성에 관한 연구)

  • Lee, Ju Seong;Kang, Jong Bong
    • Korean Journal of Materials Research
    • /
    • v.26 no.2
    • /
    • pp.95-99
    • /
    • 2016
  • In this study, 5 um sized $ZrSiO_4$ was ground to 1.9 um, 0.3 um, and 0.1 um sized powders by wet high energy milling process, and the sintering characteristics were observed. Pure $ZrSiO_4$ itself can-not be sintered to these levels of theoretical density, but it was possible to sinter $ZrSiO_4$ powder of nano-scale size of, -0.1 um to the theoretical density and to lower the sintering temperature for full density. Also, the decomposition of $ZrSiO_4$ with a size in the micron range resulted in the formation of monoclinic $ZrO_2$; however, in the nano sized range, the decomposition resulted in the tetragonal phase of $ZrO_2$. So, it was possible to improve the sintering characteristics of nano-sized $ZrSiO_4$ powders.

Fabrication and Network Strengthening of Monolithic Silica Aerogels Using Water Glass (물유리를 이용한 모노리스 실리카 에어로젤의 제조 및 구조강화)

  • Han, In-Sub;Park, Jong-Chul;Kim, Se-Young;Hong, Ki-Seog;Hwang, Hae-Jin
    • Journal of the Korean Ceramic Society
    • /
    • v.44 no.3 s.298
    • /
    • pp.162-168
    • /
    • 2007
  • Silica wet gels were prepared ken water glass ($29\;wt%\;SiO_{2}$) by using Amberlite as a ion exchange resin. After washing in distilled water, the wet gels were further aged in a solution of TEOS/EtOH to strengthen of 3-dimensional network structure. As increase TEOS content in aging solution, BET surface area and porosity of the ambient dried silica aerogels were significantly decreased, and average pore diameter was also decreased 30 nm to -10 nm. Also, higher density and compressive strength were obtained in case of higher TEOS content. This is due to precipitation of $SiO_{2}$ nano particles by TEOS. Hence, TEOS addition plays an important role of both strengthening and stiffness of silica wet gel network. By adding over 30 vol% TEOS, a crack-free monolithic silica aerogel tiles were obtained and its density, compressive strength, and thermal conductivity were shown $0.232g/cm^{3}$, 7.3 MPa, and 0.029 W/mk, respectivly.