• 제목/요약/키워드: Welding Line

검색결과 518건 처리시간 0.027초

저온 압력용기용 SA516강의 응력비에 따른 피로크랙 전파특성에 관한 연구 (A Study of Stress ratio on the Fatigue Crack Growth Characteristics of Pressure Vessel SA516 Street at Low Temperature)

  • 박경동;하경준
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2001년도 춘계학술발표대회 개요집
    • /
    • pp.220-223
    • /
    • 2001
  • In this study, CT specimens were prepared hem ASTM SA516 which was used for pressure vessel plates for room and low temperature service. And we got the following characteristics from fatigue crack growth test carried out in the environment of room and low temperature at $25^{\circ}C$, -3$0^{\circ}C$, -6$0^{\circ}C$, -8$0^{\circ}C$, -l$0^{\circ}C$ and -l2$0^{\circ}C$ and in the range of stress ratio of 0.1, 0.3 by means of opening mode displacement. At the constant stress ratio, the threshold stress intensity factor range ΔK$_{th}$ in the early stage of fatigue crack growth ( Region I ) and stress intensity factor range ΔK in the stable of fatigue crack growth ( Region II) was increased in proportion to descend temperature. It assumed that the fatigue resistance characteristics and fracture strength at low temperature is considerable higher than that of room temperature in the early stage and stable of fatigue crack growth region. The straight line slope relation of logarithm da/dN - ΔK in Region II, that is, the fatigue crack growth exponent m increased with descending temperature at the constant stress ratio. It assumed that the fatigue crack growth rate da/dN is rapid in proportion to descend temperature in Region H and the cryogenic-brittleness greatly affect a material with decreasing temperature.e.greatly affect a material with decreasing temperature.

  • PDF

박판 점 곡직 시 변형 특성에 관한 연구 (Study on the Deformation Behavior by Spot Heating for thin plate)

  • 장경복;박중구;조시훈;장태원
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2005년도 춘계학술발표대회 개요집
    • /
    • pp.285-287
    • /
    • 2005
  • During fabrication of deck house block in passenger ships, the problem of unexpected large deformation and distortion frequently occurs. In this case, line and spot heating method were widely used to correct the distortion of thin plate structure. Spot heating was especially used for the case under 5mm thickness. Few papers are available on the working conditions of spot heating method but only little information on deformation control. In this study, evaluation was carried out on the temperature distribution of spot heating methods using FEA and practical experiments for various heating time. IIn FEA, heat input model was established using Tsuji's double Gaussian heat input mode (Tsuji, I., 1988). This model was verified by comparing with experimental data. Also radial shrinkage and angular distortion due to spot heating were determined and compared with experimental results. Thermo elasto-plastic analysis was performed using commercial FE code, MSC/MARC. Radial shrinkage and angular distortion were measured using 3D measuring apparatus. Based on these results, simplified analysis model for deformation by spot heating was established.

  • PDF

선체 박판구조의 용접변형 제어에 관한 연구(I) (On the Weld-Induced Deformation Control of Ship's Thin Plate Block (I))

  • 이주성;김철호
    • 대한조선학회논문집
    • /
    • 제44권5호
    • /
    • pp.496-503
    • /
    • 2007
  • Although weld-induced deformation is inevitable in shipbuilding, it is important to reduce it as low as possible during fabrication for a more efficient production of ships' blocks. The weld-induced deformation is more serious in thin plates than in thick plates because heat affect zone of thin plates is wider than that of thick plates, and in addition internal and external constraints much more influence upon weld-induced deformation of thin plates. This paper deals with the application of the mechanical tensioning method to butt weld of thin plates to reduce the transverse and longitudinal deformation. in order to investigate the quantitative effect of tensioning method upon the reduction of angular deformation and shrinkage in longitudinal and transverse direction of weld line, butt welding test have been carried out for several thin plate specimens with varying plate thickness and magnitude of tensile load. Numerical simulation has been also carried out to compare the weld-induced deformation and residual stress. From the present study, it has been found that the tensioning method is very effective on reduction of weld-induced residual stress as well as weld-induced deformation.

장력법을 적용한 선체 박판블록의 변형감소 방안에 관한 실험연구 (On the Deformation Control of Ship's Thin Plate Block by Applying the Tensioning Method)

  • 이주성;김철호
    • 한국해양공학회지
    • /
    • 제20권3호
    • /
    • pp.103-108
    • /
    • 2006
  • It has been well appreciated that reducing weld-induced deformation as law as possible is important during fabrication for a more efficient production of blocks. The weld-induced deformation is more serious in thin plates than in thick plates because heat affect zone of thin plates is wider than that of thick plates and in addition internal and external constraints much more influence upon weld-induced deformation of thin plates. This paper deals with the application of the mechanical tensioning method to butt weld of thin plates to reduce the weld-induced deformation. In order to investigate the quantitative effect of tensioning method upon the reduction of angular deformation and shrinkage in longitudinal and transverse direction of weld line, butt welding test have been carried out for several thin plate specimens with varying plate thickness and magnitude of tensile load. From the present experimental study, it has been found that the tensioning method is very effective on reduction of weld-induced residual stress as well as weld-induced deformation.

직렬공진 PWM인버터를 이용한 전자간절유도가열 열유체 에너지시스템과 그 성능평가 (Electromagnetic Indirect Induction Fluid Heating System using Series Resonant PWM Inverter and Its Performance Evaluations)

  • 김용주;김기환;신대철
    • 전력전자학회논문지
    • /
    • 제7권1호
    • /
    • pp.48-54
    • /
    • 2002
  • 본 논문에서는 간접 유도가열 되는 DPH시스템과 주파수 범위가 20kHz에서 50kHz사이에서 작동되는 전압형 직렬공진 고주파인버터를 이용하여 열 기체를 발생시키는 전압형 공진형 인버터에 관하여 설명하였다. 얇은 스텐레스 판재가 서로 스폿 용접되어 연결되어 있고 미세한 많은 구멍을 갖고있는 적층형 충진발열테로 특수하게 설계된 유도 가열기는 외부에 워크 코일로 감겨져 있는 불소수지계의 절연용기 안에 삽입되어 있다. 이 워크 코일은 공진형 인버터와 연결되어 있으며 유도가열기를 통해 흐르는 관 유체를 1단가열부에서 저압의 포화증기를 2단가열부에서 열방사성 증발유체를 생성하는 본 DPH시스템의 성능 및 효용성을 실용적인 측면에서 논의하고 평가 할 것이다.

Effects of sizes and mechanical properties of fuel coupon on the rolling simulation results of monolithic fuel plate blanks

  • Kong, Xiangzhe;Ding, Shurong;Yang, Hongyan;Peng, Xiaoming
    • Nuclear Engineering and Technology
    • /
    • 제50권8호
    • /
    • pp.1330-1338
    • /
    • 2018
  • High-density UMo/Zr monolithic nuclear fuel plates have a promising application prospect in high flux research and test reactors. The solid state welding method called co-rolling is used for their fabrication. Hot co-rolling simulations for the composite blanks of UMo/Zr monolithic nuclear fuel plates are performed. The effects of coupon sizes and mechanical property parameters on the contact pressures between the to-be-bonded surfaces are investigated and analyzed. The numerical simulation results indicate that 1) the maximum contact pressures between the fuel coupon and the Zircaloy cover exist near the central line along the plate length direction; as a whole the contact pressures decrease toward the edges in the plate width direction; and lower contact pressures appear at a large zone near the coupon corner, where de-bonding is easy to take place in the in-pile irradiation environments; 2) the maximum contact pressures between the fuel coupon and the Zircaloy parts increase with the initial coupon thickness; after reaching a certain thickness value, the contact pressures hardly change, which was mainly induced by the complex deformation mechanism and special mechanical constitutive relation of fuel coupon; 3) softer fuel coupon will result in lower contact pressures and form interfaces being more out-of-flatness.

LNG 저장탱크 내조용 강 용접부의 파괴인성 평가 (Evaluation of Fracture Toughness in Steel Weldment for Inner Wall of LNG Storage Tank)

  • 장재일;주장복;양영철;김우식;홍성호;권동일
    • 한국가스학회지
    • /
    • 제2권1호
    • /
    • pp.7-13
    • /
    • 1998
  • 본 연구에서는 LNG 저장탱크의 안전성을 확보하기 위한 연구의 일환으로서, 실제 탱크의 건설에서와 같은 조건으로 SMAW(Shielded Metal Arc Welding) 방식으로 용접된 $9\%$ Ni강의 X-개선 후판용접부내의 파괴인성의 변화를 평가하고 미세조직을 분석하였다. 이때 파괴인성의 평가는 본 연구자들이 제안한 '개선한 CTOD(crack tip opening displacement) 시험법'으로 행하였으며 열영향부내의 미세조직 및 파면은 광학현미경, 주사전자현미경 및 X-선 회절 분석기로 관찰하였다. 결과로부터 열영향부 내의 CTOD 값은, 평가위치가 용융선(Fusion Line-F.L.)으로 접근할수록 감소하는 경향을 나타내었다. 이는 잔류 오스테나이트의 양이 줄어들고 결정립 미세화 효과가 없어지는 영역인 결정립 조대화영역이 열영향 부내에서 차지하는 분율이 증가함에 따른 것이다. 한편, 잔류 오스테나이트의 열적 안정성이 상대적으로 감소하게 되는 F.L.${\~}$F.L.+3mm에서 온도감소에 따른 인성감소의 정도가 F.L.+5mm${\~}$F.L.+7mm보다 상대적으로 매우 큼을 알 수 있었다.

  • PDF

조선업의 작업환경측정결과를 이용한 노출평가의 문제점과 해결방향 - 유사노출군을 중심으로 - (Recommendation and current status in exposure assessment using monitoring data in ship building industry - focused on the similar exposure group(SEG))

  • 노영만;임현우;김석일;박효만;정재열;박숙경;김현욱;정치경;이원철;김정만;김수근;고상백;;김은아;최정근
    • 한국산업보건학회지
    • /
    • 제11권2호
    • /
    • pp.126-134
    • /
    • 2001
  • Statistical approaches for analysis of data from the limited number of samples in ship building industry(SBI) collected by an industrial hygienist for checking compliance to an occupational standard were considered. Sampling for compliance usually has been guided by judgment selection, rather than true randomness, resulting in the creation of compliance samples which approximate a censored sample from the upper tail of the exposure distribution. Similar exposure groups(SEGs) including welding and painting process were established to assess representative values in each groups after reviewing the whole production line in SBI. For the convenient statistical approaches, the code has assigned to each SEGs. The descriptive statistics and probability plotting were used to yield the representative values in each SEGs. In the first step, SEGs of 558 were established from 5 ship building companies. The 38 SEGs showed the uncertainty are divided into each 5 companies and assessed the representative values again. The 44 SEGs in each companies was not showed the normal and lognormal distribution was analyzed each data. And also, recommendation was suggested to resolve the uncertainty in each groups.

  • PDF

Effect of Induction Heat Bending Process on the Properties of ASME SA106 Gr. C Carbon Steel Pipes

  • Kim, Ki Tae;Kim, Young Sik;Chang, Hyun Young;Oh, Young Jin;Sung, Gi Ho
    • Corrosion Science and Technology
    • /
    • 제14권2호
    • /
    • pp.47-53
    • /
    • 2015
  • Recently, the bending process is greatly applied to fabricate the pipe line. Bending process can reduce welding joints and then decrease the number of inspection. Thus, the maintenance cost will be reduced. Induction heat bending process is composed of bending deformation by repeated local heat and cooling. By this thermal process, corrosion properties and microstructure can be affected. This work focused on the effect of induction heating bending process on the properties of ASME SA106 Gr. C low carbon steel pipes. Microstructure analysis, hardness measurements, and immersion corrosion test were performed for base metal and bended area including extrados, intrados, crown up, and down parts. Microstructure was analyzed using an optical microscope and SEM. Hardness was measured using a Rockwell B scale. Induction heat bending process has influenced upon the size and distribution of ferrite and pearlite phases which were transformed into finer structure than those of base metal. Even though the fine microstructure, every bent area showed a little lower hardness than that of base metal. It is considered that softening by the bending process may be arisen. Except of I2, intrados area, the others showed a similar corrosion rate to that of base metal. But even relatively high rate of intrados area was very low and acceptable. Therefore, it is judged that induction heat bending process didn't affect boric acid corrosion behaviour of carbon steel.

황동제 온간단조용 금형제작과 환경친화형 작업장 개선에 관한 연구 (A Research on the improvement scheme for manufacturing bronze warm forging die through environment-friendly workshop)

  • 김세환
    • 한국산학기술학회논문지
    • /
    • 제11권2호
    • /
    • pp.420-425
    • /
    • 2010
  • 온간단조(warm forging) 가공은 가공소재(Billet)를 $800^{\circ}C$ 정도로 가열하여 금형의 다이블록 임프레션(impression) 상면(上面)에 위치결정 시켜 단조하고 있는데, 이 단조가공 과정에서 산화스케일의 비산에 따른 작업자의 화상에 대한 위험도와 산화스케일이 다이블록의 임프레이션에 부착 되거나 열처리기술 미흡으로 금형수명(die life)을 단축시키며 다이블록 안에 분무하는 이형제는 유해먼지, 유해증기, 미스트, 퓸, 악취 등을 발생시켜 작업장 환경을 오염시킴으로써 직무기피 직종으로 분리되기 때문에 생산량 목표 달성에 큰 문제점으로 대두 되고 있다. 더욱이 다이블록의 임프레이션 마멸부위를 수리보수하기 위한 재생공법의 미흡으로 납기지연, 금형비 상승의 요인으로 나타나므로 이에 대한 재생공법 개선과 작업장의 공해물 제거장치의 개발이 요망되고 있다. 본 연구에서는 황동제 관 이음쇠의 온간단조가공에서 도출된 빌릿가열시 문제점, 금형재생 보수시 문제점, 제조원가의 상승요인 등을 외국의 기술과 비교하여 온간단조 금형제작방법개선, 금형재생보수공법 개선, 유해가스 제거장치를 도입하여 환경친화형 작업장 개선 등으로 문제점을 해결 하고자 하였다.