• 제목/요약/키워드: Weld-zone

검색결과 659건 처리시간 0.024초

구조용강 용접부 CGHAZ의 상변태 예측 Modeling에 관한 연구 (A Study on the Prediction Modeling of Phase Transformation in the CGHAZ of Structural Steel Weld)

  • 조일영;이경종;이창희
    • Journal of Welding and Joining
    • /
    • 제16권3호
    • /
    • pp.74-84
    • /
    • 1998
  • The microstructures of the HAZ (Heat Affected Zone) are generally different from the base metal due to rapid thermal cycle during welding process. Particuraly, CGHAZ (Coarsened Grain Heat Affected Zone) near the fusion line is the most concerned region in which many metallurgical and mechanical discontinuities have been normally generated. A computer program by the numerical formularization of phase transformation during cooling with different rates was developed to generate the CCT diagram, and to predict microstructural (phase) changes in the CGHAZ. In order to verify simulated results, isothermal and continuous cooling transformation experiments were conducted. The simulated and experimental results showed that the developed computer model could successfully predict the room temperature microstructural changes (changes in volume fraction of phases) under various welding conditions (heat input & cooling rate $(Δt_{8/5})$).

  • PDF

Modeling of the Bainite Transformation kinetics in C-Mn-Mo-Ni Steel weld CGBAZ

  • Uhm, S.;Lee, C.;Kim, J.;Hong, J.
    • International Journal of Korean Welding Society
    • /
    • 제2권1호
    • /
    • pp.11-14
    • /
    • 2002
  • A metallurgical model for bainite transformation kinetics in the coarse-grained heat affected zone(CGHAZ) on the basis of an Avrami-type equation was studied. Isothermal transformation tests were carried out to obtain the empirical equations for incubation time and Avrami kinetic constants for C-Mn-Mo-Ni steel. The effect of prior austenite grain size(PAGS) on the reaction rate of bainite was also investigated. Compared with experimental transformation behavior of bainite, the predicted behavior was in good agreement. It was also found that a smaller grain size retard the bainite reaction rate, contrary to the classical grain size effect and this is considered to be caused by constraint of grain size to bainite growth.

  • PDF

Microstructure and Hardness of Surface Melting Hardened Zone of Mold Steel, SM45C using Yb:YAG Disk Laser

  • Lee, Kwang-Hyeon;Choi, Seong-Won;Yoon, Tae-Jin;Kang, Chung-Yun
    • Journal of Welding and Joining
    • /
    • 제34권1호
    • /
    • pp.75-81
    • /
    • 2016
  • This study applied laser surface melting process using CW(Continuous wave) Yb:YAG laser and cold-work die steel SM45C and investigated microstructure and hardness. Laser beam speed, power and beam interval are fixed at 70 mm/sec, 2.8 kW and $800{\mu}m$ respectively. Depth of Hardening layer(Melting zone) was a minimum of 0.8 mm and a maximum of 1.0 mm that exceeds the limit of minimum depth 0.5 mm applying trimming die. In all weld zone, macrostructure was dendrite structure. At the dendrite boundary, Mn, Al, S and O was segregated and MnS and Al oxide existed. However, this inclusion didn't observe in the heat-affected zone (HAZ). As a result of interpreting phase transformation of binary diagram, MnS crystallizes from liquid. Also, it estimated that Al oxide forms by reacting with oxygen in the atmosphere. The hardness of the melting zone was from 650 Hv to 660 Hv regardless of the location that higher 60 Hv than the hardness of the HAZ that had maximum 600 Hv. In comparison with the size of microstructure using electron backscatter diffraction(EBSD), the size of microstructure in the melting zone was smaller than HAZ. Because it estimated that cooling rate of laser surface melting process is faster than water quenching.

Ni-Cr-Fe 및 Ni-Fe-Cr-Mo계 합금의 용접부 균열특성에 관한 연구 Part I : 용착금속의 응고균열 (A Study on the Cracking Behavior in the Welds of Ni-Cr-Fe and Ni-Fe-Cr-Mo Alloys Part I : Solidification Cracking in the Fusion Zone)

  • 김희봉;이창희
    • Journal of Welding and Joining
    • /
    • 제15권4호
    • /
    • pp.78-89
    • /
    • 1997
  • This study has evaluated the weld metal solidification cracking behavior of several Ni base superalloys (Incoloy 825, Inconel 718 and Inconel 600). Austenitic stainless steels(304, 310S) were also included for comparison. In addition, a possible mechanism of solidification cracking in the fusion zone was suggested based on the extensive microstructural examinations with SEM, EDAX, TEM, SADP and AEM. The solidification cracking resistance of Ni base superalloys was found to be far inferior to that of austenitic stainless steels. The solidification cracking of Incoloy 825 and Inconel 718 was believel to be closely related with the Laves-austenite (Ti rich in 825 and Nb rich in 718) and MC-austenite eutectic phases formed along the grain boundaries during solidification. Cracking in Inconel 600 was always found along the grain boundaries which were enriched with Ti and P. Further, solidifidcation cracking resistance was dependent not only upon the type of love melting phases but also on the amount of the phases along the solidification grain boundaries.

  • PDF

LNG 저장탱크 내조용 9% Ni강의 SAW 용접열영향부내 파괴인성 변화 평가 (Change in Fracture Toughness within Heat-Affected Zone of SA-Welded 9% Ni Steel)

  • 장재일;이정석;이백우;주장복;권동일;김우식
    • 대한기계학회논문집A
    • /
    • 제26권3호
    • /
    • pp.528-536
    • /
    • 2002
  • As one step for the safety performance of LNG storage tank, the change in fracture toughness within the X-grooved weld heat-affected zone (HAZ) of newly developed 9% Ni steel, which was submerged arc (SA)-welded, was investigated. Both crack initiation fracture toughness and crack arrest fracture toughness were evaluated by the crack tip opening displacement (CTOD) tests and compact crack arrest (CCA) tests. As the evaluated region approached the fusion line, each test result shorted different tendency, that is, crack initiation toughness decreased while crack arrest toughness increased. The results were discussed through the observation of the microstructural change.

AH36-TMCP강의 용접후열처리 효과에 관한 연구 (A Study on Effect of PWHT in AH36-TMCP Steel)

  • 유효선;장원상;안병국;정세희
    • Journal of Welding and Joining
    • /
    • 제16권6호
    • /
    • pp.44-51
    • /
    • 1998
  • It is well known that the fine bainitic microstructure obtained by TMCP(thermo-mechanical control process) secures the high toughness of base metal. Besides, TMCP steel is very suitable for high heat input in welding as it has low carbon equivalent. In HAZ, however, the accelerated cooling effect imparted on the matrix by the weld thermal cycles is relieved and thus the weldment of TMCP steel has softening zone which shows low fracture toughness compared with base metal. Therefore, PHWT of weldment is carried out to improve the fracture toughness in weldment of TMCP steel which has softening zone. In this study, the effects of PWHT on the weldment of AH36-TMCP steel are investigated by the small punch (SP) test. From the several results such as SP energy and displacement at room temperature, the behavior of transition curves, the fracture strength at -196$^{\circ}C$, distribution of (DBTT)sp and (DBTT)sp, the PWHT condition of A.C. after 85$0^{\circ}C$-1 sec W.C. was suitable condition for recovering a softening zone of HAZ as welded.

  • PDF

박판 알루미늄 도금강판의 플라즈마 용접성에 미치는 용접조건 및 롤러의 영향 (Effect of Welding Condition and Roller on Weldability of Al Coated Steel Sheet using Plasma Arc Welding)

  • 이태우;박철호;강남현;김명덕
    • Journal of Welding and Joining
    • /
    • 제30권2호
    • /
    • pp.54-58
    • /
    • 2012
  • Al-coated steel sheets with excellent heat and corrosion resistance are widely used in various applications. In welding of thin plate, some defects such as unmelted zone and metal-through occur easily in the beginning and ending of welding line. In the study, the welding defects in Al-coated steel sheets were investigated with respect to plasma arc current, height between Cu block and base metals, and using a roller to align the height of the base metal. Full penetration and voids free welds were obtained with a plasma arc current 52A and weld speed 2.3m/min. An unmelted zone increased and Ericshen rate decreased as the height between Cu block and base metal increased from 0 to 0.6mm. Using a roller moving ahead of the plasma arc, the length of unmelted zone decreased from 1.7mm to 0.5mm.

겹치기 마찰교반접합된 Invar 42/SS 400 합금의 미세조직과 기계적 특성 발달 (Development of Microstructure and Mechanical Properties of Friction Stir Lap Jointed Invar 42/SS 400)

  • 송국현
    • Journal of Welding and Joining
    • /
    • 제30권5호
    • /
    • pp.34-39
    • /
    • 2012
  • This study was conducted to investigate the microstructure and mechanical properties of friction stir lap joints. Invar 42 and SS 400 were selected as the experimental materials, and friction stir welding was carried out at a tool rotation speed of 200 rpm and welding speed of 100 mm/min. The application of friction stir welding to Invar 42 effectively reduced the grain size in the stir zone; the average grain size of Invar 42 was reduced from $11.5{\mu}m$ in the base material to $6.4{\mu}m$ in the stir zone, which resulted in an improvement in the mechanical properties of the stir zone. The joint interface between Invar 42 and SS 400 showed a relatively sound weld without voids and cracks, and the intermetallic compounds with $L1_2$ type in lap jointed interface were partially formed with size of 100 nm. Moreover, the hook in the advancing side of Invar 42 was formed from SS 400, which contributed to maintenance of the tensile strength. The evolution of microstructures and mechanical properties of friction stir lap jointed Invar 42 and SS 400 are also discussed herein.

선급용 고장력강 FSW접합부의 미세조직 및 기계적 성질 (Microstructures and Mechanical Properties of Friction Stir Welded High Strength Steels far Shipbuilding)

  • 장웅성;최기용
    • Journal of Welding and Joining
    • /
    • 제20권3호
    • /
    • pp.67-73
    • /
    • 2002
  • In an attempt to evaluate the feasibility of friction stir welding(FSW) for joining carbon steels, microstructures and mechanical properties of friction stir welded carbon steels with different grain structures were investigated. In comparison of O-type stir zone(SZ) appeared in various aluminium alloys, configuration of SZ in friction stir welded carbon steels displayed U-type. Plastically deformed pearlite band structure was identified to surround the SZ, indicating the existence of so-called thermo-mechanically affected zone(TMAZ). However, the TMAZ of carbon steels was much narrower than that of Al alloys. The microstructures of both stir zone and TMAZ revealed bainite matrix in a conventional carbon steel for shipbuilding, while, in the same region, ferrite matrix microstructures were formed in a low carbon fine grained steel. The conventional carbon steel showed superior stirring workability to that of the fine grained carbon steel. The yield and tensile strength of the friction stir welded joints were comparable to those of the base metals, and the elongation in welded joints demonstrated excellent ductility. Absorbed energy in SZ of the fine grained carbon steel was ten times higher than that obtained from conventional submerged arc weld metal of the same steel. Based on these results, the application FSW to carbon steels was found to be feasible.

페라이트계 스테인리스강의 마찰교반접합 (Friction Stir Welding of Ferritice Stainless Steel)

  • 안병욱;최돈현;연윤모;정승부
    • Journal of Welding and Joining
    • /
    • 제32권2호
    • /
    • pp.14-17
    • /
    • 2014
  • Ferritic stainless steels are widely used in the construction industry and in exhaust manifolds due to their low cost and relatively superior stress corrosion cracking resistance and pitting corrosion resistance compared to austenite stainless steels. Ferritic stainless steels are currently welded by various welding process including gas tungsten arc welding (GTAW), electron resistance welding (ERW) and laser beam welding. However, when these stainless steels are welded by fusion welding, some problems occur in the fusion zone (FZ) and heat affected zone (HAZ). First, the ductility of the weld is reduced due to the grain growth in the FZ and HAZ. Second, as its HAZ is frequently sensitized during welding, corrosion resistance deteriorates in this region due to the Cr depletion zone. To prevent these problems, it is recommended that ferritic stainless steels be welded with a low heat input. In this study, recent researches in the view of friction stir welded ferritic stainless steels are briefly reviewed.