Proceedings of the Korean Society for Technology of Plasticity Conference
/
1997.10a
/
pp.89-92
/
1997
Design of a weld line in a tailor welded blank is indispensable for good manufacturing of stamped parts as assigned, since the intial weld line is distorted severely with forming. The initial weld line has to be determined such that desired weld line in a formed part can be obtained. The initial weld line was predicted by inverse finite element analysis from the desired weld line in a formed part. The inverse approach is applied to the cylindrical and square cup drawing with tailor welded blanks. The applications demonstrates that the approach is useful for design of weld line of tailor welded blank.
Kim, Young-Mo;Park, Yeong-Min;Jang, Min-Kyu;Jeong, Yeong-Deug
Design & Manufacturing
/
v.6
no.2
/
pp.1-5
/
2012
Weld line in injection molded part is one of the defects in injection molding process. Weld line deteriorates not only appearance quality but mechanical property. In this study, ABS and PP were used as experimental materials. And weld line length, depth and strength have been examined according to the injection molding conditions. As the results of experimental studies, weld line length increased as flow rate increases for all materials. And the flow rate is most influenced to the creation of weld line length. Also weld line strength increased, as flow rate and melt temperature increase for all materials. The whole experiment results was similar to CAE analysis results.
Kim, Young-Mo;Park, Yeong-Min;Jang, Min-Kyu;Jeong, Yeong-Deug
한국금형공학회:학술대회논문집
/
2008.06a
/
pp.115-119
/
2008
Weld line in injection molded part is one of the defects in injection molding process. Weld line deteriorates not only appearance quality but mechanical property. In this study, ABS and PP were used as experimental materials. And weld line length, depth and strength have been examined according to the injection molding conditions. As the results of experimental studies, weld line length increased as flow rate increases for all materials. And the flow rate is most influenced to the creation of weld line length. Also weld line strength increased, as flow rate and melt temperature increase for all materials. The whole experiment results was similar to CAE analysis results.
Hydroforming is a forming process enabling circular metal tubes to be produced in complex cross sections along curved axial paths. This forming process is widely used to manufacture parts in automotive industry. This paper presents bending and forming results to following angle of weld line positions. These compare to good bending, bad bending and without weld line model case. And then this result of after forming compare to each forming cases. The purpose of this paper is found that adaptive weld line position for bended final shape.
Proceedings of the Korean Society for Technology of Plasticity Conference
/
2003.10a
/
pp.211-216
/
2003
Weld line in injection molded part is one of the defect in injection molding process. Weld line deteriorates not only appearance quality but mechanical property. In this study weld line strength has been examined according to the injection operational conditions, materials and mold designs. PC and PP were used, and four different specimens were used in this experiment. Weld line strength decreased as injection temperature increases for PC. It was more dependent on mold temperature than injection temperature for PP Among the four different specimens, uneven thickness specimen showed the highest weld line strength.
Transactions of the Korean Society of Machine Tool Engineers
/
v.10
no.2
/
pp.64-72
/
2001
Weld line is one of serious troubles which are observed in a plastic part manufactured by a injection molding process. This is caused by many process factors, which are molding pressure, temperature, velocity, location of a injection gate, mold geometry and material properties. investigation on the effects of these process factors to the appearance of a weld line was carried out using a finite element method. Filling and packing analyses were carried out by modifying both the configuration of the injection gates and cavity thickness. Proper locations of the injection gates could be determined by considering molding pressure, temperature, velocity and frozen layer, and whereby the weld line was controled. In order to make a weak appearance of the weld line, flow velocity and flow front in a cavity were also investigated by modifying a cavity thickness. As a result, flow front was extended around the corner in the cavity by changing the flow velocity and hence the appearance of the weld line was much weakened.
Journal of the Korean Society of Manufacturing Technology Engineers
/
v.9
no.3
/
pp.160-168
/
2000
Hydroforming is a metal forming process that enables circular metal tubes to be formed in to the parts with the complex cross section along the curved axial direction. Recently this hydroforming process is largely used for the production of the automotive parts. This paper presents the results of tube bending and hydroforming simulations in cases of the varying weld line positions of the tube. Ten cases of prebending and hydroforming simulations are carried out to find the optiaml weld line position.
Proceedings of the Korean Society for Technology of Plasticity Conference
/
1997.03a
/
pp.19-24
/
1997
The weld line location and the weld line movement in stamping with laser-tailor welded blanks(TWB) were investigated through square cup deep drawing tests. The step blank holder was introduced to form TWB of different thicknesses without wrinkling, and the non-uniform blank holding force(BHF) was enforced to control weld line movement. Test results of the blanks with shifted weld lines showed that the large portion of the thinner area could result in a large weld line movement. Careful selection of the weld line location and the BHF control should be adapted in TWB design to avoid failures and to ensure its formability.
A CCD camera with a laser stripe was applied to realize the automatic weld seam tracking in GMAW. It takes relatively long time to process image on-line control using the basic Hough transformation, but it has a tendency of robustness over the noises such as spatter and arc light. For this reason. it was complemented with adaptive Hough transformation to have an on-line processing ability for scanning specific weld points. The adaptive Hough transformation was used to extract laser stripes and to obtain specific weld points. The 3-dimensional information obtained from the vision system made it possible to generate the weld torch path and to obtain the information such as width and depth of weld line. We controled the wire feeding rate using informations of weld line.
In injection molding, many kinds of defects have occurred because of a characteristic of plastics injection molding. Weld line is one of the defects is formed when separated melt fronts recombine together during the mold filling stage. That is one of problems in injection molding. Weld lines in the appearance of plastics parts can deteriorate visible quality. And most importantly, the local mechanical strength in the weld line area can be significantly weaker. It could be one of the most problems for structural applications. In this study, the mold available two-shot-molding of same polymers have been designed, and a series of experiment about tensile strength in weld line area has been conducted using Taguchi's design of experiment to optimize injection molding conditions decreasing of weld strength and find out a factors affected weld strength in two-shot- molding.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.