Physical, Mechanical and Durability Properties of the Quartzite Units of Central Nepal Lesser Himalaya

  • Dinesh Raj Sharma;Naresh Kazi Tamrakar;Upendra Baral
    • The Journal of Engineering Geology
    • /
    • v.34 no.1
    • /
    • pp.67-105
    • /
    • 2024
  • This study compares the quartzites of four quartzite units: The Fagfog Quartzite, Dunga Quartzite (member of the Robang Formation), Pandrang Quartzite (member of the Kalitar Formation) and the Chisapani Quartzite. The analysis shows variations in flakiness and elongation, as the Fagfog Quartzite displays low flakiness whereas the Pandrang and the Chisapani have moderate and the Dunga Quartzite has shown variations. The density values of the four quartzite units remain consistent, indicating uniform physical properties and porosity levels. However, bulk density values differ among the quartzites, suggesting variations in particle arrangement, porosity, and density. Regarding strength measures, the Pandrang and the Chisapani Quartzite have higher strength characteristics as compared to the Fagfog and the Dunga Quartzites. The Pandrang Quartzite has the highest average point load strength index, classifying it as "Extremely Strong". The resistance to impact and crushing forces varies among the quartzites, with lower Aggregate Impact Value (AIV) and Aggregate Crushing Value (ACV) indicating higher strength and durability. Durability tests show that the Fagfog Quartzite has high durability against slaking, with a slight decrease observed after the fifth cycle. The Dunga Quartzite shows varying degrees of weathering, while the Pandrang and the Chisapani Quartzite have minimal weight changes, indicating strong resistance to weathering. Magnesium sulfate soundness tests indicate high durability and resistance to degradation for all four units. The Los Angeles abrasion value (LAAV) tests indicate favorable resistance to abrasion for the majority of the Fagfog, Dunga, and the Pandrang Quartzites samples, while Chisapani Quartzite shows more variability in LAAV values. The Pandrang Quartzite shows a higher proportion of elongated particles but lower flakiness index values as compared to Fagfog and Dunga Quartzites while Chisapani Quartzite stands out with a significantly higher presence of flaky particles and lower elongation index values. Mechanically, the Fagfog and Dunga Quartzite show higher strength and better resistance to abrasion and freeze and thaw. The Pandrang Quartzite shows moderate resistance to crushing and sudden effect, while the Chisapani Quartzite has variable resistance to effect. This comparative study emphasizes the diversity and complexity of quartzite rock types, showing the need for comprehensive characterization and assessment to determine their suitability for specific applications.

Characterization of Wetness Index in Western Area of Yangsan Fault, Sangbuk-myeon, Kyeongnam-do (경상남도 상북면 양산단층 서부지역에 대한 습윤지수 특성 연구)

  • Kim, Sung-Wook;Han, Ji-Young;Lee, Son-Kap;Kim, Sang-Hyun;Kim, Choon-Sik;Kim, In-Soo
    • Proceedings of the Korean Geotechical Society Conference
    • /
    • 2004.03b
    • /
    • pp.904-909
    • /
    • 2004
  • The study area adjoins with Yangsan fault in Sangbuk-myeon, Samsam-ri, Kyongsang-namdo and consist of the natural steep slope. After drawing data layer which have altitude by using digital topography data, it is converted to lattice DEM of $10m{\times}10m$ size. From this, gradient map of unit lattice, slant direction map and shadow relif map are made. Using flow apportioning algorithm, upper slope contributing area and wetness index by established lattice can be calculated. Area that have high wetness index shows lineament structure of northwest-southeast direction, and this agrees with shear fracture system. The result of electricity specific resistance survey in the study area shows that area of high wetness index has low electricity specific resistance anomaly. That is, wetness index conforms with distribution of fractured zone that accompanied chemical weathering of rock. Therefore, wetness index can be used as the method of detecting fractured zones and judging the stability of the area.

  • PDF

Material Characteristics and Deterioration Assessment of the Stone Buddhas and Shrine in Unjusa Temple, Hwasun, Korea (화순 운주사 석조불감의 재질특성과 풍화훼손도 평가)

  • Park, Sung-Mi;Lee, Myeong-Seong;Choi, Seok-Won;Lee, Chan-Hee
    • Journal of Conservation Science
    • /
    • v.24
    • /
    • pp.23-36
    • /
    • 2008
  • The stone Buddhas and Shrine of Unjusa temple (Korea Treasure No. 797) in Hwasun formed in Koryo Dynasty are unique style which the Buddha faces each other the back parts of south and north within the stone Shrine. The stone Buddhas and Shrine are highly evaluated in historical, artistic and academic respects. But, the stone properties have been exposed in the open system various aspects of degradations weathered for a long time without specific protective facilities. The rock materials of the stone Buddhas and Shrine are about 47 blocks, and total press load is about 56.6 metric ton. The host rocks composed mainly of white grey hyaline lithic tuff and rhyolitic tuff breccia. In addition, biotite granite used as part during the restoration works. The chemical index of alteration for host tuffaceous rocks and the replacement granites range from 52.1 to 59.4 and 50.0 to 51.0, respectively. Weathering types for the stone Buddhas and Shrine were largely divided with physical, chemical and biological weathering to make a synthetic deterioration map according to aspects of damage, and estimate share as compared with surface area. Whole deterioration degrees are represented that physical weathering appeared exfoliation. Chemical weathering is black coloration and biological weathering of grey lichen, which show each lighly deterioration degrees. According to deterioration degree by direction of stone Buddhas and Shrine, physical weathering mostly appeared by 39.1% on the sorthern part, and chemical weathering is 61.2% high share on the western part. Biological weathering showed 38.3% the largest distribution on the southern part. Therefore, it is necessary to try hardening for the parts with serious cracks or exfoliations, remove secondary contaminants and organisms through regular cleaning. Also necessary to make a plan to remove moisture of the ground which causes weathering, and estimate that need established and scientific processing through clinical demonstration of conservation plan that chooses suitable treatment.

  • PDF

Effect of the Degree of Weathering on the Distribution of Aggregate Particle Size and the Generation of Fine Rock Particles during Crushing of Granite (화강암 파쇄시 풍화정도가 골재 입도분포 및 미석분 발생에 미치는 영향)

  • You, Byoung-Woon;Lee, Jin-Young;Lee, Dong-kil;Cheong, Young-Wook
    • Economic and Environmental Geology
    • /
    • v.55 no.5
    • /
    • pp.429-438
    • /
    • 2022
  • This study evaluated the effect of the degree of weathering on the particle size distribution and the amount of fine particles generated in the aggregate production process during the crushing of igneous rock. Rock samples were collected from three areas with differences in strength from the Schmith hammer measurement at the aggregate quarry in Geochang, Gyeongsangbuk-do. After crushing with a jaw crusher under the same conditions in laboratory, particle size analysis, mineral analysis, chemical analysis, and weathering index were calculated. The Schmidt hammer measurements were 56, 28, and <10, and the CIA and CIW values of weathering index were also different, so the rock samples were classified into hard rock, soft rock, and weathered rock according to the weathering degree. It shows a smaller particle size distribution toward weathered rocks under the microscope, and the proportion of altered clay minerals such as sericite increased. The composition of feldspar and quartz was high for hard rock, and the ratio of muscovite and kaolinite was low. As a result of the crushing of the jaw crusher, hard rock produced a lot of coarse crushed material (13.2mm), while soft rock and weathered rock produced fine crushed material (4.75mm). The former showed the characteristics of the beta distribution curve, and the latter showed the bimodal distribution curve. The production of fine rock particles (based on 0.71mm of sieve, wt. %) increased to 13%<21%<22% in hard rock, soft rock, and weathered rock, and the greater the degree of weathering, the more fine rock particles were generated. The fine particles are recovered by the operation of the sand unit in the wet aggregate production process. Therefore, in order to minimize the amount of sludge generated in the aggregate production process, it was judged that a study on the optimal operation of cyclones could be necessary.

Estimation of Shear Wave Velocity of Weathered Granite Layer Using Nonlinear Multiple Regression Analysis; A Case Study in South Korea (비선형 다중회귀분석을 통한 국내 화강 풍화대 전단파 속도 평가에 대한 사례 연구)

  • Lee, Seung-Hwan;Baek, Sung-Ha;Chung, Choong-Ki;Kwak, Tae-Young
    • Journal of the Korean Geotechnical Society
    • /
    • v.37 no.6
    • /
    • pp.29-37
    • /
    • 2021
  • Since many geotechnical structures are constructed on a weathered granite layer, it is important to evaluate their characteristics. As a seismic design is the more important nowadays, the demands to estimate a shear wave velocity (VS) based on acceptable methods are increasing. In this study, an empirical equation predicting VS of the weathered granite layer is suggested based on the nonlinear multiple variable regression analysis whose independent variables are both SPT (Standard penetration test)-N60 and chemical weathering index. It is concluded that the accuracy of the empirical equation estimating VS of the weathered granite layer increases when it considers the chemical weathering index as an additional independent variable compared to the result of simple regression analysis using only N60.

Geological Environments and Deterioration Causes of the Sitting Buddha Carved on Rockcliff in Bukjiri, Bonghwa (봉화 북지리 마애여래좌상의 지질환경과 훼손원인)

  • Hwang, Sang-Koo;Nam, Jae-Guk
    • Economic and Environmental Geology
    • /
    • v.40 no.1 s.182
    • /
    • pp.47-66
    • /
    • 2007
  • The Sitting Buddha Carved on Rockcliff (National treasure No. 201) in Bukjiri consists of porphyritic biotite granite, which was fractured by three joint sets of NE-SW, EW and NS directions. They produced a physical weathering that broke many parts of the Buddha and background. The chemical index of alteration is 59 to 61 from the major elements in the granite that was weathered into producing kaolin minerals from alteration of feldspars and biotite. With weathering degree, major element compositions increase in $SiO_2$ and MnO, whereas decrease in $TiO_2,\;{Fe_2O_3}^t,\;MgO,\;CaO\;and\;K_2O$. Change proporations of trace elements to $Al_2O_3$ increase in all transition elements, Rb and Y, whereas decrease in Li, Sr and Ba. REE pattern increases only in HREE. Particularly, a decrease in CaO, $K_2O$, Sr and Ba results in what they are effluxed to dissolve from feldspars by groundwater. The Buddha image has been deteriorated into joints, color changes, brown rusts, granular decay, microorganic smears by the such weathering causes as deformation, moisture, temperature variation and microorganic living. The moisture, which leaks along the joints in the granite, not only dissolve to decompose minerals but also grows many microorganism and is frozen over during winter. NE-SW and NS joint sets affect to seep in water during rainy days to deteriorate the image because they extend outward.

A Study on the Chemical Weathering Characteristics of the Weathered Granite Residual Soils prone to Laterization (적황색토화된 화강암질 풍화잔적토의 화학적 풍화특성에 관한 연구)

  • 정두영;이광준
    • Geotechnical Engineering
    • /
    • v.12 no.4
    • /
    • pp.115-130
    • /
    • 1996
  • The definition of laterite or lateritic soils is discussed on a climatic condition of tropical and semitropical regions, and the weathering index is indicated by the chemical composition. The chemical composition of$(Fe_2O_3+Al_2O_3)$ of the weathered granite residual soils in tropical and the temperate regions which shelus laterization usually ranges from 0.2 to 0.5. This study shows that the chemical ratio of the Chonju Ajung site is about 0.2U, and that of the regions along the shore of the western sea of Hongsong and Taechon is about 0.33. The chemical ratio of the non-laterite is less than 0.2, and the Kyougju Pulguksa site confirmed about 0.17, The X-Ray diffraction test shows that the clay mineral of the laterite soils is made of kaolinite, this X -Ray result indicates the same characteristics compared with the wrathered granite residual soils of other sites.

  • PDF

A study on the change of chemical composition of sediment particles of terrace deposits - A case of fine sediments at Jeongdongjin area - (단구 퇴적층의 화학 조성 변화에 대한 연구 - 정동진 단구의 세립 물질을 사례로 -)

  • Kim, Jong Yeon
    • Journal of The Geomorphological Association of Korea
    • /
    • v.23 no.2
    • /
    • pp.29-45
    • /
    • 2016
  • Chemical composition of fine sediments from Jeongdongjin area are analyzed with XRF method. The results are compared with previously reported results of sandstones of the nearest Simgok port. The weight percentage of $SiO_2$ of the samples are far lower than those of sandstones of Simgok. It is supposed to be happened by the selective elution of $SiO_2$ from the sediment layer of coastal terrace, as there's no evidence of selective input or precipitation of other elements from outside. As a result of chemical alteration or weathering of sediment at coastal terrace, weight percentage of $Al_2O_3$ and $Fe_2O_3$ of samples show far higher values than those of Simgok sandstone. In addition, the relative portion of $Al_2O_3$ and $Fe_2O_3$ are decreased to upward within outcrop of terrace sediment layers. It could be caused by the chemical weathering progress with time. However Chemical Index of alteration(CIA) of sediment samples are no larger than 90 and it could be interpreted that it would take over 100ka for total weathering of sediment in this area. Meanwhile the ratio of $SiO_2/Al2O_3$ of terrace sediment showed as 3.48~6.0 and it is far smaller than those of Simgok sandstones(23.9~49.0). The ratio of $SiO_2/Fe_2O_3$ of terrace sediment(19.19~55.85) showed similar pattern with $SiO_2/Al2O_3$ (Simgok sanstone: 119.6~601.8). The ratios have a weak trend of decreasing upwards within the outcrop, there also a huge difference in value among the samples. Chemical composition of reddish brown and gray layers which suspected as the result of psudogleization reveals that reddish brown parts have higher concentration of $Fe_2O_3$ than other parts, while there was no significant difference in concentration of $Al_2O_3$ and CaO.

Lithological Characteristics and Deterioration Diagnosis of Dosolammaaebulsang (Rock-carved Buddha Statue of Dosolam) in the Seonunsa Temple, Gochang, Korea (고창 선운사 도솔암마애불의 암석학적 특성과 손상도 진단)

  • Park, Sung-Mi;Ryu, Keong-Seok;Choi, Hee-Soo;Lee, Chan-Hee
    • Journal of Conservation Science
    • /
    • v.27 no.1
    • /
    • pp.101-114
    • /
    • 2011
  • The rock-carved Buddha statue at Dosolam (Korea Treasure No. 1200) of the Seonunsa temple in Gochang is unique style sculptured on natural rock cliff of 13.0m height. The Buddha statue is composed of volcanic complex with tuff, dacitic tuff breccia, tuff bereccia and lithic tuff. Especially, the Buddha statue is characterized by hydrothermal alteration and fragmentation on the upper and lower part. As a result of damage diagnosis, exfoliation and detachment of physical weathering are high of 11.3% and 9.3%, respectively. Infrared thermography analysis, exfoliation and micro-cracks occurred in the measuring parts that have not been confirmed by naked eyes. Chemical index of alteration and weathering potential index of host rock for the Buddha statue are 55.16 to 64.01 and 6.14 to 9.92 which are represented within highly weathering degree. In surface, dark black, reddish brown and white discoloration are observed prominently in the lower. Brown discoloration 6.9% is highest. According to the P-XRF measurements, high concentration of Fe in common, in part of dark black discoloration was Mn, white and brown discoloration in part of S and Ca content were higher. Biological weathering that yellowish brown and dark gray crustoes lichenes appeared by 20.8% and 13.3%, respectively. Therefore, comprehensive deterioration rate of Buddha statue show physical damage by 21.2%, discoloration for inorganic contaminants by 10.8% and biological damage by 39.4%. Ultrasonic velocity measurement carried out of Buddha statue on the surface by 555 points. Measured value of ultrasonic velocity was about 2,273m/s(1,067 to 3,215m/s, and weathering coefficient is 0.5(0.4 to 0.8) that progress on MW(moderately weathered) to HW(highly weathered) grade of rocks.

Petrographic Characteristics and Deterioration Evaluation of the Rock-carved Seated Buddha at Bugmireugam Hermitage in Daeheungsa Temple of Haenam, Korea (해남 대흥사 북미륵암 마애여래좌상의 암석기재적 특성과 손상도 평가)

  • Cho, Ji Hyun;Lee, Chan Hee
    • Economic and Environmental Geology
    • /
    • v.52 no.6
    • /
    • pp.617-626
    • /
    • 2019
  • In this study, we investigated the petrographic characteristics and physical property of the Rock-carved Seated Buddha at Bugmireugam hermitage of Daeheungsa temple in Haenam. The Buddha Statue was carved on micrographic granite, and the rock was composed of the fine quartz encircled by orthoclase. The results of diagnosis for deterioration evaluation have shown a highly damage rate of black contaminants (8.4%) and crack index (6.6). The ultrasonic velocity have detected SW (slightly weathered) grade of weathering coefficient (mean 0.18). Various weathering factor on the surface of the Buddha Statue was affected by precious shelter, and physical property with ultrasonic was directly influenced by the structural characteristics and fissure of host rock.