• Title/Summary/Keyword: W/Mo

Search Result 765, Processing Time 0.032 seconds

Impact Toughness and Fracture Behavior in Non-Heat Treating Steels Containing Bainite (베이나이트 함유 비조질강의 충격인성 및 파괴거동)

  • Cho, Ki-Sub;Kwon, Hoon
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.32 no.4
    • /
    • pp.161-167
    • /
    • 2019
  • Impact toughness and fracture behavior were studied in five kinds of non-heat treating steels containing bainite; standard(0.25C-1.5Mn-0.5Cr-0.2Mo-0.15V), high V(0.3V), Ni(0.5Mn-2Ni), W(0.4W instead of Mo), and high C-Ni(0.35C-0.5Mn-2Ni) steels. The good hardness and impact toughness balance was exhibited in the $1100^{\circ}C$-rolled condition, while the impact toughness was deteriorated due to coarse grained microstructure in the $1200^{\circ}C$-rolled condition. The impact toughness decreased with increasing the hardness in all steels studied. The fracture behavior was also basically identical, that is, the fracture area was divided into 3 zones; shear and fibrous zone, fracture transition zone with ductile dimples and cleavage cracks, where the cracks initiate and grow to critical size, unstable cleavage fracture propagation zone. The energy absorbed for the critical crack formation through the plastic deformation inside the plastic zone in front of the notch root contributed to a mostly significant portion of the total impact energy.

Comparison of Wear Amount of Surface Coating Layers on Dies for Cold-Stamped Products with MART1470 (MART1470 판재 냉간 프레스 성형용 금형 코팅층의 마모량 비교)

  • Son, M.K.;Kim, S.H.
    • Transactions of Materials Processing
    • /
    • v.31 no.1
    • /
    • pp.11-16
    • /
    • 2022
  • In this paper, wear characteristics of PVD coatings were compared on the die surface for cold stamping of MART1470 steel sheet with the finite element analysis and the pin-on-disc wear test. Three types of PVD coatings (CrN, TiAlCrN, and MoS2TiCr(W)N) were considered for the tool surface made of STD11 material. The stamping process of an auto-body part was analyzed with the finite element method. Ranges of process variables for the wear test such as contact pressure, relative speed, and sliding distance were predicted from analysis results. In order to quantitatively analyze wear characteristics of each coating, the amount of wear was measured and compared according to process variables with the pin-on-disc wear test. The influence of each process variable was investigated and the wear characteristics of the three coating layers were quantitatively compared. It was confirmed that the wear characteristics of MoS2TiCr(W)N coating were better than those of CrN and TiAlCrN. It was noted that the proposed prediction approach could predict and respond to the wear phenomenon occurring in the stamping process.

Characterization of Toxicity Symptoms of Molybden and Determination of Tissue Threshold Levels for Diagnostic Criteria in Korean Bred Strawberries (국내육성 주요 딸기 품종에서 발생하는 Mo 과잉 증상 및 영양진단을 위한 식물체 내 한계농도)

  • Choi, Jong-Myung;Nam, Min-Ho;Lee, Chi-Won W.;Chun, Jong-Pil
    • Horticultural Science & Technology
    • /
    • v.30 no.4
    • /
    • pp.392-399
    • /
    • 2012
  • This study was carried out to investigate the influence of molybden (Mo) concentrations in fertilizer solution on the growth of and nutrient uptake by domestically bred strawberries. Tissue analysis based on the dry weight was also conducted to determine the threshold levels in plants when Mo toxicity developed in strawberries. The leaf chlorophyll contents decreased lineally as Mo concentrations in the fertilizer solution were elevated. The differences among treatments in chlorophyll contents were statistically significant. The fresh and dry weights decreased significantly when the Mo concentrations in fertilizer solution were higher than 3.0 mM in 'Keumhyang' and 'Maehyang' strawberries and 1.0 mM in 'Seolhyang' strawberry. The elevation of Mo concentrations in fertilizer solution resulted in severe toxicity and crops developed the unique symptoms. The margin of older leaves became yellow and desiccated. Then, the margin of leaf blade rapidly became bronze colored and died as the symptoms spread up the plants. The interveinal area of the young leaves became yellowing. The elevation of Mo concentrations in fertilizer solution did not influence the tissue P, K, and Mg contents based on the dry weight. The tissue Ca contents were higher in 1.0 mM treatment than other treatments of 'Keumhyang' and 'Seolhyang' strawberries. The tissue Mo contents based on the dry weight of 'Keumhyang', 'Maehyang', and 'Seolyahng' strawberries were 76.5, 104.0, and 187.3 $mg{\cdot}kg^{-1}$, respectively, in the 0.25 mM treatments and 4,155, 5,367, and 2,190 $mg{\cdot}kg^{-1}$, respectively, in the 4.0 mM treatments. The contents increased lineally as Mo concentrations in fertilizer solution were elevated. When the concentration of Mo at which growth of crops were retarded by 10% is regarded as threshold level, the Mo contents based on dry weight of above ground plant tissue should be lower than 653.4, 686.2, and 589.7 $mg{\cdot}kg^{-1}$, in 'Keumhyang', 'Maehyang', and 'Seolyahng' strawberries, respectively.

Identification and Analysis of the Novel pGAPDH-w Gene Differentially Expressed in Wild Ginseng

  • Han, Young-Ju;Kwon, Ki-Rok;Kang, Won-Mo;Jeon, Eun-Yi;Jang, Jun-Hyeog
    • Journal of Pharmacopuncture
    • /
    • v.16 no.1
    • /
    • pp.30-36
    • /
    • 2013
  • Objective: Panax ginseng is one of the most medicinally used herbal medicines in the world. Wild ginseng is widely accepted to be more active than cultivated ginseng in chemoprevention. However, little has actually been reported on the differences between wild ginseng and cultivated ginseng. Method: To identify wild ginseng-specific genes, we used suppressive subtraction hybridization. Results: We report that one of the clones isolated in this screen was the GAPDH (glyceraldehyde 3-phosphate dehydrogenase) gene (designated pGAPDH-w). DNA BLAST sequence analysis revealed that this pGAPDH-w gene contained novel sequences of 94 bp. RT-PCR results showed that the expression of the pGAPDH-w gene was significantly up-regulated in the wild ginseng as compared with the cultivated ginseng. Conclusion: The pGAPDH-w gene may be one of the important markers of wild ginseng.

A clean technology development using the molybdenum dissolution reaction with hydrogen peroxide/UV/Ozone ($오존/UV/H_2O_2$를 이용한 몰리브덴(Mo) 용해 반응에 따른 청정기술 개발에 관한 연구)

  • 김재우;홍종순;신대윤
    • Journal of environmental and Sanitary engineering
    • /
    • v.14 no.4
    • /
    • pp.143-149
    • /
    • 1999
  • In the tungsten industry as light source material, tungsten filament which used as light source material could form after molybdenumwire which used as the center supporter for coil shape tungsten wire was removed. This process uses hydrogen peroxide, Ozone and UV(Ultraviolet)Lamp, for the quantity of hydrogen peroxide decrease. The results were as follows : 1. An incandescent electric Lamp type : FL(FL-20) type : A standard of commodity (P.W.: $19{\pm}1.0mg$, $C.R:4.5{\pm}0.3{\Omega}$) 1) Only hydrogen peroxide treated ; Reaction Time : 65Min., P.W.: 18.60mg, $C.R.:4.60{\Omega}$ 2) Ozone/Ultraviolet/70% of hydrogen peroxide; Reaction Time : 64Min., P.W.: 18.61mg, C.R.: $4.61{\Omega}$ 2. A Fluorescent Lamp Type : GLS(GLS-40) Type : A standard of commodity(P.W.: $11.8{\pm}0.2mg$$65{\pm}1.5{\Omega}$) 1) Only hydrogen peroxide treated ; Reaction Time: 72Min, P.W.:11.88mg, C.R.: $65.62\Omega$ 2) Ozone/Ultraviolet/70% of hydrogen peroxide;Reaction Time:71Min., P.W.:11.88mg, C.R.: $65.63\Omega$

  • PDF

Magnetic Properties and Magnetocaloric Effect in Ordered Double Perovskites Sr1.8Pr0.2FeMo1-xWxO6

  • Hussain, Imad;Anwar, Mohammad Shafique;Khan, Saima Naz;Lee, Chan Gyu;Koo, Bon Heun
    • Korean Journal of Materials Research
    • /
    • v.28 no.8
    • /
    • pp.445-451
    • /
    • 2018
  • We report the structural, magnetic and magnetocaloric properties of $Sr_{1.8}Pr_{0.2}FeMo_{1-x}W_xO_6$($0.0{\leq}x{\leq}0.4$) samples prepared by the conventional solid state reaction method. The X-ray diffraction analysis confirms the formation of the tetragonal double perovskite structure with a I4/mmm space group in all the synthesized samples. The temperature dependent magnetization measurements reveal that all the samples go through a ferromagnetic to paramagnetic phase transition with an increasing temperature. The Arrott plot obtained for each synthesized sample demonstrates the second order nature of the magnetic phase transition. A magnetic entropy change is obtained from the magnetic isotherms. The values of maximum magnetic entropy change and relative cooling power at an applied field of 2.5 T are found to be $0.40Jkg^{-1}K^{-1}$ and $69Jkg^{-1}$ respectively for the $Sr_{1.8}Pr_{0.2}FeMoO_6$ sample. The tunability of magnetization and excellent magnetocaloric features at low applied magnetic field make these materials attractive for use in magnetic refrigeration technology.

Effect of Cobalt Contents on the Biocompatibility and Corrosion Properties of Fe-31Cr-27Ni-1.6Mo-1.5W-0.26N Alloy (Fe-31Cr-27Ni-1.6Mo-1.5W-0.26N계 초내식성 스테인리스강의 생체적합성 및 부식특성에 미치는 Co함량의 영향)

  • Jang, Soon Geun;Yoo, Young Ran;Nam, Hee Soo;Shim, Gyu Tae;Kim, Jung Gu;Kim, Young Sik
    • Korean Journal of Metals and Materials
    • /
    • v.46 no.4
    • /
    • pp.209-216
    • /
    • 2008
  • Super austenitic stainless steels shows the high PRE (Pitting Resistance Equivalent) number and the good corrosion resistance. This work controlled the Co contents in Fe-31Cr-1.7Mo-27Ni-0.25N alloys to elucidate the effect of cobalt contents on the biocompatibility and corrosion resistance. Increasing Co contents, the hardness of the annealed alloys tends to be reduced. In aged alloys, cobalt decreased the increments of hardness by aging treatment. Cobalt decreased the critical pitting temperature (CPT) in 6% $FeCl_3$ + 1% HCl solution, but improved the anodic polarization behavior in Hanks' balanced salt solution and artificial saliva solution. Repassivation rate in artificial body solutions was improved by increasing cobalt contents, but didn't show the linear relationship to PRE number of the alloys. The experimental alloys showed the non-cytotoxicity because of its high corrosion resistance.

Dehydration Reaction of Fructose to 5-Hydroxymethylfurfural over Various Keggin-type Heteropolyacids (Keggin형 헤테로폴리산에 의한 과당의 5-하이드록시메틸퍼퓨랄로의 전환을 위한 탈수반응)

  • Baek, Ja-Yeon;Yun, Hyeong-Jin;Kim, Nam-Dong;Choi, Young-Bo;Yi, Jong-Heop
    • Clean Technology
    • /
    • v.16 no.3
    • /
    • pp.220-228
    • /
    • 2010
  • Four Keggin-type heteropolyacids, $H_nXM_{12}O_{40}$(X = P and Si, M = W and Mo) that were substituted with heteroatom and polyatom were applied to the dehydration reaction of fructose to 5-hydroxymethylfurfural (HMF). The results showed that the acid became stronger when the heteroatom and polyatom were substituted with P and W than the cases of Si and Mo, respectively. However, the amount of acidic sites increased with the decrease in the acid strength, resulting in the change of the catalytic activity of heteropolyacids in the dehydration reaction. The experimental results revealed that four different heteropolyacids produced similar amounts of HMF via the dehydration reaction of fructose due to the counterbalancing effect between the amount of active sites, which is related to the catalytic activity of heteropolyacids, and the softness of polyanion. In addition, it was observed that the prepared heteropolyacids showed good structural stability after heat treatment at $200^{\circ}C$.

Evolution of Hydrothermal Fluids at Daehwa Mo-W Deposit (대화 Mo-W 열수 맥상 광상의 유체 진화 특성)

  • Jo, Jin Hee;Choi, Sang Hoon
    • Economic and Environmental Geology
    • /
    • v.46 no.1
    • /
    • pp.11-19
    • /
    • 2013
  • The Daehwa Mo-W deposit is located within the Gyeonggi massif. Quartz and calcite vein mineralization occurred in the Precambrian gneiss and Jurassic granites. Three main types (Type I: liquid-rich $H_2O$ type, Type II: vapor-rich $H_2O$ type, Type III: $CO_2-H_2O$ type) of fluid inclusions were observed and are classified herein based on their phase relations at room temperature. Within ore shoots, type III fluid inclusions have been classified into four subtypes (type IIIa, IIIb, IIIc and IIId) based on their volume percent of aqueous and carbonaceous ($CO_2$) phase at room temperatures combined with their total homogenization behavior and homogenization behavior of $CO_2$ phase. Homogenization temperatures of primary type I fluid inclusions in the quartz range from $374^{\circ}C$ to $161^{\circ}C$ with salinities between 13.6 and 0.5 equiv. wt.% NaCl. Homogenization temperatures of primary type III fluid inclusions in quartz of main generation, are in the range of $303^{\circ}C$ to $251^{\circ}C$. Clathrate melting temperatures of the type III fluid inclusions were 7.3 to $9.5^{\circ}C$, corresponding to salinities of 5.2 to 1.0 equiv. wt. % NaCl. Melting and homogenization temperatures of $CO_2$ phase of type III fluid inclusions were -57.4 to $-56.6^{\circ}C$ and 29.0 to $30.8^{\circ}C$, respectively. Fluid inclusion data indicate a complex geochemical evolution of hydrothermal fluids. The Daehwa early hydrothermal system is characterized by $H_2O-CO_2$-NaCl fluid at about $400^{\circ}C$. The main mineralization occurred by $CO_2$ immiscibility at temperatures of about 300 to $250^{\circ}C$. At the late base-metal mineralization aqueous fluid formed by mixing with cooler and less saline meteoric groundwater.

Trends in Technology for High-speed RFID and Beamforming (고속 RFID 및 빔포밍 기술 동향)

  • Cho, K.S.;Jung, J.Y.;Choi, W.K.;Kim, H.S.;Mo, S.H.;Han, K.W.;Park, C.W.
    • Electronics and Telecommunications Trends
    • /
    • v.29 no.5
    • /
    • pp.40-50
    • /
    • 2014
  • 최근에 RFID(Radio Frequency Identification) 기술은 사물인터넷의 기반 기술로 다양한 애플리케이션의 개발과 함께 산업화/정보화에 크게 기여하고 있다. 그러나 산업에서 요구하는 RFID 태그, 리더의 요구사항이 단순한 인식뿐만 아니라 다양한 정보를 장기간 저장하고 관리할 목적으로 태그 메모리 크기가 확장되고 있으며, 해당 정보를 태그에 읽고 쓰기 위하여 간섭 잡음에 강한 신뢰성 있는 성능 향상 무선통신기술이 연구되고 있다. 본고에서는 RFID 태그-리더 간 고속으로 통신하는 기술과 다량의 태그 밀집 환경에서 RFID 인식률 향상을 위한 빔포밍 기술에 대하여 기술한다.

  • PDF