3%C-10%Cr-5%Mo-5%W 백주철에 있어서 열처리가 현미경조직, 경도 및 내마모성에 미치는 영향 (Effects of Heat Treatments on Microstructure , Hardness and Abrasive Wear Resistance in 3%C-10%Cr-5%Mo-5%W White Cast Iron)

  • 류성곤
    • 한국주조공학회지
    • /
    • 제19권1호
    • /
    • pp.33-37
    • /
    • 1999
  • White cast iron of 3%C-10%Cr-5%Mo-5%W was casted, and then heat treated with three different methods such as homogenizing, austenitizing and tempering to observe its effects on the microstructure, hardness and abrasive wear resistance. In uni-directional soldification, bamboo tree-like $M_7C_3$ carbide grew along with the heat flow direction, and fishbone-like $M_6C$ carbide was dispersed randomly among $M_7C_3$ carbides. While almost pearlitic structures were observed in the as-cast specimen, those of the heat treated specimens consisted of secondary carbide, retained austenite and tempered martensite. In austenitized specimen, the amounts of retained austenite were 60.88% due to the higher cooling rate encountered in forced air cooling. On the other hand, the amounts of retained austenite were reduced from 60.88% to 23.85% in tempered specimen due to the transformation of austenite into tempered martensite. The hardness of tempered specimen showed the highest value, and then decreased in the order of austenitized, as-cast and homogenized specimens. But, the abrasive wear resistance of austenitized specimen was the highest, and then decreased in the order of tempered, as-cast and homogenized specimens.

  • PDF

25Cr-7Ni-2Mo-4W 슈퍼 2상 스테인리스강의 기계적 성질에 미치는 R상의 영향 (Effect of R Phase Formation on the Mechanical Properties of 25Cr-7Ni-2Mo-4W Super Duplex Stainless Steel)

  • 이병찬;강창룡
    • 한국재료학회지
    • /
    • 제24권8호
    • /
    • pp.401-406
    • /
    • 2014
  • In this study, we investigated the precipitation behavior of the R-phase precipitated at the initial stage of aging and its effects on the mechanical properties of 25%Cr-7%Ni-2%Mo-4%W super duplex stainless steel. The R-phase was mainly precipitated at the interface of ferrite/austenite phases and inside of the ferrite phase during the initial stage of aging. It was transformed into the ${\sigma}$-phase with an increase of the aging time. The ferrite phase was decomposed into a new austenite(${\gamma}_2$)phase and the ${\sigma}$-phase by an aging treatment. The R phase was an intermetallic compound showing higher molybdenum and tungsten concentrations than the matrix and also showed higher molybdenum and tungsten concentrations than the ${\sigma}$ phase. In the initial stage of aging, precipitation of the R-phase did not change the hardness, the strength and the elongation. The hardness and the strength increased upon a longer aging time, but the elongation rapidly decreased. These results show that the R-phase did not significantly affect the hardness and the strength, though it did influence the elongation.

공구강의 고온 변형 거동 예측을 위한 모델 비교 연구 (Comparison Study of Prediction Models for Hot Deformation Behavior of Tool Steel)

  • 김근학;박동성;전중환;이민하;이석재
    • 열처리공학회지
    • /
    • 제31권4호
    • /
    • pp.180-186
    • /
    • 2018
  • High temperature flow behaviors of Fe-Cr-Mo-V-W-C tool steel were investigated using isothermal compression tests on a Gleeble simulator. The compressive test temperature was varied from 850 to $1,150^{\circ}C$ with the strain rate ranges of 0.05 and $10s^{-1}$. The maximum height reduction was 45%. The dynamic softening related to the dynamic recrystallization was observed during hot deformation. The constitutive model based on Arrhenius-typed equation with the Zener-Hollomon parameter was proposed to simulate the hot deformation behavior of Fe-Cr-Mo-V-W-C steel. An artificial neural network (ANN) model was also developed to compare with the constitutive model. It was concluded that the ANN model showed more accurate prediction compared with the constitutive model for describing the hot compressive behavior of Fe-Cr-Mo-V-W-C steel.

아크롤레인 선택 산화반응에서 Mo-V-O와 금속산화물의 상간협동 (Phase Cooperation Between Mo-V-O and Metal Oxide in Selective Oxidation of Acrolein)

  • 박대원;나석은;김경훈;이원호;정종식
    • 공업화학
    • /
    • 제5권2호
    • /
    • pp.327-336
    • /
    • 1994
  • 본 연구는 아크롤레인의 선택산화반응에서 Mo-V-O와 금속산화물의 기계적 혼합촉매에 대한 synergy 효과를 고찰한 것으로 금속산화물로는 $SnO_2$, ${\alpha}-Sb_2O_4$, $WO_3$, ${\alpha}-Al_2O_3$, CuO, $MnO_2$, $Cu_2O$, MgO, CoO 그리고 ZnO 등을 사용하였다. $SnO_2$${\alpha}-Sb_2O_4$와 Mo-V-O의 혼합물 촉매는 Mo-V-O보다 높은 전화율과 수율을 나타내었는데 이것은 이들이 산소 빈자리에 해리 홉착된 산소를 형성하여 Mo-V-O에 전달하는 상간협동에 의한 것으로 판단된다 그러나 $Cu_2O$, MgO, CuO, $MnO_2$와 Mo-V-O의 혼합물 촉매의 경우 전화율은 증가하였으나 수율은 감소하였고, CoO와 ZnO는 Mo-V-O의 촉매성능을 억제하였다. 각 금속산화물의 역할이 서로 다른 점을 그들의 산화-환원 특성으로 설명하였다.

  • PDF

Fe-l7Cr-2M(M=Si, Nb, Mo)합금 분말 소결체의 교류 자기 특성 (Magnetic Properties in Alternating Magnetic Field for the Sintered Ee-l7Cr-2M(M=Si, Nb, Mo) Alloys)

  • 김정곤;김택기;오용수
    • 한국자기학회지
    • /
    • 제10권6호
    • /
    • pp.269-273
    • /
    • 2000
  • Fe-l7Cr-2M(M=Si, Nb, Mo)합금분말을 Electrode Rotating Atomizer로 제조한 후 성형하여 소결한 시편의 첨가원소, 성형 압력 및 소결온도 에 따른 교류자기특성의 변화를 체계적으로 조사하였다 제조된 Fe-l7Cr-2M(M=Si, Nb, Mo) 합금분말의 형상은 구형이며, 포화자화값은 Mo와 Nb을 첨가한 Fe-l7Cr-2Mo과 Fe-l7Cr-Nb의 경우 약 155 emu/g로 Si을 첨가한 경우보다 크다. 성형압력 12 ton/$cm^2$, 소결온도 1200 $^{\circ}C$에서 제조된 Fe-l7Cr-2M(M=Si, Nb, Mo)합금분말 소결체의 진폭비 투자율은 주파수, f=1 kHz에서 3~5 Oe의 인가자장 범위에서 가장 크다. 전력손실은 인가자장 H$_{a}$ =5 Oe, 주파수 f=1 kHz에서 Fe-l7Cr-2Nb 경우 40 mW/cc로 Si이나 Mo를 첨가한 경우 보다 약 1/2값을 나타낸다.

  • PDF

Synthesis and Characterization of Nb, Mo-doped and Nb/Mo-codoped Monoclinic VO2 Nanoparticles and Their Thin Films by Hydrothermal/Post-Thermal Transformation and Wet-Coating Method

  • Kim, Jongmin;Jung, Young Hee;Kwak, Jun Young;Kim, Yeong Il
    • 대한화학회지
    • /
    • 제63권2호
    • /
    • pp.94-101
    • /
    • 2019
  • Nb, Mo-doped and Nb/Mo-codoped $VO_2(M)$ nanocrystallites with various doping levels were synthesized for the first time by a hydrothermal and post thermal transformation method. The reversible phase transition characteristics of those doped $VO_2(M)$ was comparatively investigated. Nb-doping of $VO_2(M)$ by this method resulted in a very efficient lowering of the transition temperature ($T_c$) with a rate of $-16.7^{\circ}C/at.%$ that is comparable to W-doping, while Mo-doping did not give a serious reduction of $T_c$ with only a rate of $-5.1^{\circ}C/at.%$. Nb/Mo-codoping gave a similar result to Nb-doping without a noticeable difference. The thin films of Nb-doped and Nb/Mo-codoped $VO_2(M)$ with a thickness of ca. 120 nm were prepared by a wet-coating of the nanoparticle-dispersed solutions. Those films showed a good thermochromic modulation of near infrared radiation with 30-35% for Nb-doped $VO_2(M)$ and 37-40% for Nb/Mo-codoped ones. Nb/Mo-codoped $VO_2(M)$ film showed slightly enhanced thermochromic performance compared with Nb-doped $VO_2(M)$ film.

다양한 조건의 플라즈마 원자층 증착법으로 증착된 Mo 금속의 전기적 특성 (Electrical Properties of Molybdenum Metal Deposited by Plasma Enhanced - Atomic Layer Deposition of Variation Condition)

  • 임태완;장효식
    • 한국재료학회지
    • /
    • 제29권11호
    • /
    • pp.715-719
    • /
    • 2019
  • Molybdenum is a low-resistivity transition metal that can be applied to silicon devices using Si-metal electrode structures and thin film solar cell electrodes. We investigate the deposition of metal Mo thin film by plasma-enhanced atomic layer deposition (PE-ALD). $Mo(CO)_6$ and $H_2$ plasma are used as precursor. $H_2$ plasma is induced between ALD cycles for reduction of $Mo(CO)_6$ and Mo film is deposited on Si substrate at $300^{\circ}C$. Through variation of PE-ALD conditions such as precursor pulse time, plasma pulse time and plasma power, we find that these conditions result in low resistivity. The resistivity is affected by Mo pulse time. We can find the reason through analyzing XPS data according to Mo pulse time. The thickness uniformity is affected by plasma power. The lowest resistivity is $176{\mu}{\Omega}{\cdot}cm$ at $Mo(CO)_6$ pulse time 3s. The thickness uniformity of metal Mo thin film deposited by PE-ALD shows a value of less than 3% below the plasma power of 200 W.

몰리브덴과 텅스텐 착물을 이용한 카르보닐기의 이온성 수소화 반응 (Ionic Hydrogenation of Carbonyl Groups With Molybdenum and Tungsten Complexes)

  • 송정섭
    • 한국산학기술학회논문지
    • /
    • 제7권4호
    • /
    • pp.715-720
    • /
    • 2006
  • CO와 유사한 분자궤도함수를 갖는 isocyanide 리간드가 포함된$Cp(CO)_{2}(L)MH$ (L = t-butylisocyanide and 2,6-dimethylphenylisocyanide M = Mo and W)를 합성하고, 이 착물과 triflic acid를 사용하여 카르보닐기를 알코올로 전환시키는 실험을 하였다. 또한, 이들 착물을 촉매 전구체로 이용하여 3-pentanone의 수소화 반응을 온화한 조건 ($23^{\circ}C,\;<4.1\;atm H_{2}$)에서 수행하였다. 촉매 활성은 매우 낮았으며, [$Cp(CO)_{2}(ArNC)Mo][BA_{r}^{F}_{4}$]의 경우에 2 turnovers/day의 결과를 나타내었다.

  • PDF

Extension of Shelf Life of Kimchi by Addition of Encapsulated Mustard Oil

  • Kim, Mi-Jeong;Ha, Jee-Yun;Yun, Ye-Rang;Noh, Jeong-Sook;Song, Yeong-Bok;Song, Yeong-Ok
    • Food Science and Biotechnology
    • /
    • 제15권6호
    • /
    • pp.884-888
    • /
    • 2006
  • In this study, we have attempted to characterize the effects of encapsulated mustard oil with regard to the extension of the shelf life of kimchi. The quantity of mustard oil or encapsulated mustard oil added to the brined cabbage in this study was 0.05%(w/w). Overall, the fermentation processes in the encapsulated mustard oil-added kimchi (EMO) and mustard oil-added kimchi (MO) occurred at a slower rate than in the controls. The periods during which the MO and EMO kimchi samples were edible were prolonged for more than two weeks, according to measurements of pH, total acidity, and microbial changes. The overall acceptability of EMO was superior to MO throughout the entirety of the fermentation period. Sensory evaluation verified that EMO yielded a more favorable product than the MO and control varieties. Encapsulated mustard oil can be employed as a natural food additive to prolong the shelf life of kimchi, via an induced delay of the fermentation process.

직접 에탄올 연료전지(DEFC)의 anode용 삼원소 전극촉매[$Pt_5Ru_4M$(M= Ni, Sn, Mo and W)]의 에탄올 전기산화반응에 관한 연구 (A Study on Electro-oxidation of Ethanol with $Pt_5Ru_4M$(M= Ni, Sn, Mo and W) Ternary Electrocatalysts for Anode of Direct Ethanol Fuel Cell(DEFC))

  • 노창수;강대규;손정민
    • 한국수소및신에너지학회논문집
    • /
    • 제19권5호
    • /
    • pp.423-429
    • /
    • 2008
  • This work was carried out to improve the performance of anodic electrocatalysts in direct ethanol fuel cell(DEFC). PtRu and $Pt_5Ru_4M$(M= Ni, Sn, Mo and W) electrocatalysts were prepared by using a $NaBH_4$ reduction method. Alloy crystal structure and particle size of electrocatalysts were characterized by X-ray diffraction(XRD) and transmission electron microscopy(TEM). The XRD analysis of the electrocatalysts revealed that the face-centered cubic(fcc) peaks shifted to slightly higher diffraction angles when third metals were added. Average size of the uniform particles was observed to be approximately $3{\sim}3.5\;nm$ from the TEM image. The electrochemical measurements were carried out in the solution 1M $H_2SO_4$ and 1M $C_2H_5OH$ at room temperature. Cyclic-voltammogram results showed that $Pt_5Ru_4W$ electrocatalyst exhibited much higher current density for ethanol oxidation of $2.73\;mA/cm^2$ than PtRu electrocatalyst of $0.73\;mA/cm^2$.