• 제목/요약/키워드: Vickers hardness number

검색결과 58건 처리시간 0.023초

복합산화물이 형성된 API X80 라인파이프강의 용접열영향부 미세조직과 기계적 특성의 상관관계 연구 (Correlation Study of Microstructure and Mechanical Properties in Heat Affected Zones of API X80 Pipeline Steels containing Complex Oxides)

  • 신상용;오경식;이성학
    • 대한금속재료학회지
    • /
    • 제47권2호
    • /
    • pp.59-70
    • /
    • 2009
  • This study is concerned with the correlation between microstructure and mechanical properties in heat affected zones (HAZs) of API X80 pipeline steels containing complex oxides. Three kinds of specimens were fabricated by varying alloying elements of Ti, Al, and Mg to form complex oxides, and their microstructures, Vickers hardness, Charpy impact properties were investigated. The number of complex oxides increased as the excess amount of Ti, Al, and Mg was included in the steels. The simulated HAZs containing a number of oxides showed a high volume fraction of acicular ferrite region because oxides acted as nucleation sites for acicular ferrite. According to the correlation study between thermal input, volume fraction of acicular ferrite region, and Charpy impact properties, the ductile fracture occurred predominantly when the volume fraction of acicular ferrite region was 65% or higher, and the Charpy absorbed energy was excellent over 200 J. When the volume fraction of acicular ferrite region was 35% or lower, the Charpy absorbed energy was poor below 50 J as the brittle cleavage fracture occurred. These findings suggested that the active nucleation of acicular ferrite in the oxide-containing steel HAZs was associated with the great improvement of Charpy impact properties of the HAZs.

칼슘보강음료가 법랑질 재광화 효과에 미치는 영향 (Influence of soft drinks supplemented calcium to enamel remineralization)

  • 김민영;이혜진
    • 한국치위생학회지
    • /
    • 제8권3호
    • /
    • pp.13-22
    • /
    • 2008
  • Objectives: The purpose of this study was to identify the correlation between calcium in soft drinks and enamel remineralization. Method: Six soft drinks were used in this study. These were calcium milk, normal milk, calcium yoghurt, normal yoghurt, calcium orange juice, and orange juice. Enamel specimens which 300- 400Vickers Hardness Number (VHN) were selected. These samples were immersed in each soft drink for 12 hours in an in vitro remineralization model. All specimens were processed for SEM image of the enamel surface. Results were analyzed by SPSS 13.0 package program. Results: Calcium milk was the most influential and normal yoghurt was the least to enamel surface. There was not significant difference according to calcium supplement in milk although the difference of enamel hardness was ${\Delta}f13.4$ in calcium milk, and ${\Delta}f4.7$ in normal milk (P>0.05). Other soft drinks showed a little change about calcium but they were insignificant. Demineralization effect was remarkably observed in calcium yoghurt ($-{\Delta}f269.1$) and this effect was confirmed by SEM images. In conclusion, calcium supplemented soft drinks had little influences to hardness of enamel surface.

  • PDF

기후 변화에 따른 자기 애자의 시멘트 경도 변화 (Hardness Profiles of Porcelain Insulators by Climate Changes)

  • 이주현;김홍식;김준동;최인혁
    • 한국전기전자재료학회논문지
    • /
    • 제31권1호
    • /
    • pp.24-28
    • /
    • 2018
  • Insulators used in overhead transmission lines are continuously exposed to a number of mechanical and electrical stresses owing to external environmental factors, resulting in corrosion, reduction in durability, and deterioration. Widely used porcelain insulators are fabricated with cement and porcelain and are especially common in Korea. Changes in the hardness and chemical reactivity of the cement increase the leakage and fault currents and increase the possibility of flashover due to insulation breakdown. Therefore, it is important to evaluate the durability and defects of porcelain insulators. Studies on the reliability of various evaluation methods are needed to prevent accidents by accurately determining the replacement timing and potential defects in porcelain insulators. In this study, the hardness of the cement part of the porcelain insulator was measured using the Vickers hardness test and its composition was analyzed by energy dispersive spectroscopy and X-ray diffraction analysis. The performance of the insulators was compared in two different regions with varying climatic conditions. This study presents an evaluation method of the defects in porcelain insulators by measuring humidity, which can also be used to assess the reliability of the insulators.

유한요소해에 기초한 취성재료의 압입파괴인성평가 (Evaluation of Indentation Fracture Toughens in Brittle Materials Based on FEA Solutions)

  • 현홍철;이진행;;이형일
    • 대한기계학회논문집A
    • /
    • 제37권12호
    • /
    • pp.1503-1512
    • /
    • 2013
  • 본 논문에서는 cohesive zone 모델을 이용한 유한요소해석에 기초해 압입 파괴인성 평가식을 제시한다. 먼저 Vickers 압입균열해석에 기초해 다양한 물성변수(항복변형률 ${\varepsilon}_o$, 푸아송비 ${\nu}$, 영률 E)의 들이 균열크기에 미치는 영향을 분석하고, 파괴인성을 압입 시 측정되는 최대하중과 균열길이로 나타낼 수 있는 수식을 회귀로 얻었다. 아울러 접촉길이 a, E/H (H: 경도) 등을 추가 압입변수로 선정해 다양한 형태의 파괴인성평가법을 제시했다. 이후 동일 압입하중에서 압입자각 및 압입자 형태와 균열 크기의 관계를 분석해 Vickers 압입 파괴인성평가법을 다양한 압입자 형태로 확장했다. 본 연구에서 제안된 평가식을 이용하면 압입시험으로 얻어지는 데이터로부터 바로 취성재료의 파괴인성을 예측할 수 있다.

수종 복합레진에 있어서 효소 역할에 의한 표면 경도와 조도 변화에 관한 연구 (THE STUDY OF CHANGE IN SURFACE HARDNESS AND TEXTURES OF COMPOSITE RESIN DUE TO ENZYMATIC ACTION)

  • 김미리;이명종
    • Restorative Dentistry and Endodontics
    • /
    • 제20권1호
    • /
    • pp.193-213
    • /
    • 1995
  • The purpose of this study is to investigate a possible contribution of nonspecific esterases, which occur in the oral cavity, to the degradation of ester bonds in polymethacrylates. One of the problems connected with the use of composite resins for restorations is their inadequate resistance to wear. It has been shown that methacrylate hydrolysis can be catalyzed by enzymes and that a carboxylic hydrolase (porcine liver esterase) catalyzed the hydrolysis of several mono - and dimethacrylates. The softening effect on a BISGMA/TEGDMA polymer induced by hydrolase will accelerate the in vivo wear of the polymer. Porcine liver esterase (EC 3.1.1.1) 3.2 mol/L $(NH_4)_2$ $SO_4$ was obtained from Sigma Chemical Company. The esterase activity of one unit is defined as the amount of enzyme capable of hydrolyzing $l{\mu}mol$ ethyl butyrate per min at pH 8.0 AT $25^{\circ}C$. Phosphate buffer, 10mmol/L, pH 7.0, was made by adjustment of a solution of $Na_2HPO_4$ with $H_3PO_4$. Composite resins used in this study are Silux Plus, Z-100, Durafil VS, and Prisma APH. Cylindrical specimens, 14mm in diameter and 3mm thick, of Silux Plus, Z-100, Durafil VS, Prisma APH were polymerized under the celluloid strip. 60 specimens were divided into 2 groups. One group was emersed only in buffer solution, the other group was emersed in buffer and enzyme solution. Silux Plus and Z-100 were divided into 2 subgroups, one subgroup was cured only Visilux 2. And the other subgroup was cured Visilux 2 and Triaid II. Thereafter, specimens were polished to its best achievable surface according to manufacture's directions. The Vickers hardness of the specimens was measured after 1, 2, 4, 7, 9, 15, 50 days. The solutions were changed after each measurement. Composite resin surfaces were evaluated for the surface roughness with profilometer (${\alpha}$-step 200, Tencor instruments, USA) after 1 and 50 days. And then surfaces of specimens were pictured with stereosopy after 1 and 50 days. The results were as follows. 1. The surface hardness of Silux plus, durafil VS, and Prisma APH were decreased with time. But, the surface hardness of Z-100 was not decreased. 2. The surface hardness of all composite resins was decreased by esterase. 3. Composite resins, which were light-cured by Visilux 2 and concomitantly baked by oven, showed more hardened surface than light-cured by Visilux 2 only. 4. Significant surface changes were occured in Silux plus after esterase treatment.

  • PDF

철계 복합 분말로 제조된 오버레이 용접층의 미세조직 및 특성 (Microstructure and Characterization of Overlay Welding Layer using Fe-based Composite Powders)

  • 민홍;이종재;이진규
    • 한국분말재료학회지
    • /
    • 제26권3호
    • /
    • pp.214-219
    • /
    • 2019
  • In this study, the microstructure and characterization of an overlay welding layer using Fe-based composite powders are reported. The effects of the number of passes and composition of powders on the microstructure and mechanical properties are investigated in detail. The welding wire and powders are deposited twice on a stainless-steel rod using a laser overlay welding process. The microstructure and structural characterization are performed by scanning electron microscopy and X-ray diffraction. The mechanical properties of the first and second overlay layers are analyzed through the micro-Vickers-hardness tester and abrasion wear tester. In the second overlay layer, the hardness and specific wear are approximately 840 Hv and $2.0{\times}10^{-5}mm^3/Nm$, respectively. It is suggested that the increase of the volume fractions of $(Cr,Fe)_7C_3$ and NbC phases in the second welding layer enhances the hardness and wear resistance.

The effect of thermocycling on the degree of conversion and mechanical properties of a microhybrid dental resin composite

  • Ghavami-Lahiji, Mehrsima;Firouzmanesh, Melika;Bagheri, Hossein;Jafarzadeh Kashi, Tahereh S.;Razazpour, Fateme;Behroozibakhsh, Marjan
    • Restorative Dentistry and Endodontics
    • /
    • 제43권2호
    • /
    • pp.26.1-26.12
    • /
    • 2018
  • Objective: The purpose of this study was to investigate the degree of conversion (DC) and mechanical properties of a microhybrid Filtek Z250 (3M ESPE) resin composite after aging. Method: The specimens were fabricated using circular molds to investigate Vickers microhardness (Vickers hardness number [VHN]) and DC, and were prepared according to ISO 4049 for flexural strength testing. The initial DC (%) of discs was recorded using attenuated total reflectance-Fourier transforming infrared spectroscopy. The initial VHN of the specimens was measured using a microhardness tester under a load of 300 g for 15 seconds and the flexural strength test was carried out with a universal testing machine (crosshead speed, 0.5 mm/min). The specimens were then subjected to thermocycling in $5^{\circ}C$ and $55^{\circ}C$ water baths. Properties were assessed after 1,000-10,000 cycles of thermocycling. The surfaces were evaluated using scanning electron microscopy (SEM). Data were analyzed using 1-way analysis of variance followed by the Tukey honest significant difference post hoc test. Results: Statistical analysis showed that DC tended to increase up to 4,000 cycles, with no significant changes. VHN and flexural strength values significantly decreased upon thermal cycling when compared to baseline (p < 0.05). However, there was no significant difference between initial and post-thermocycling VHN results at 1,000 cycles. SEM images after aging showed deteriorative changes in the resin composite surfaces. Conclusions: The Z250 microhybrid resin composite showed reduced surface microhardness and flexural strength and increased DC after thermocycling.

Effect of Ultra-Soft and Soft Toothbrushes on the Removal of Plaque and Tooth Abrasion

  • Jeong, Moon-Jin;Cho, Han-A;Kim, Su-Yeon;Kang, Ka-Rim;Lee, Eun-Bin;Lee, Ye-Ji;Choi, Jung-Hyeon;Kil, Ki-Sung;Lee, Myoung-Hwa;Jeong, Soon-Jeong;Lim, Do-Seon
    • 치위생과학회지
    • /
    • 제18권3호
    • /
    • pp.164-171
    • /
    • 2018
  • To improve the oral health status of Korean people, it is necessary to encourage proper oral hygiene management habits, such as toothbrushing, through appropriate health promotion techniques. Therefore, the purpose of this study was to evaluate the removal of plaque and tooth abrasion using ultra-soft (filament 0.11~0.12 mm) and soft toothbrushes for toothbrushing. The plaque removal was performed using a dentiform and Arti-spray, and the Patient Hygiene Performance (PHP) index was calculated as the sum total score divided by the total number of surfaces. In the abrasivity experiment, according to the number of brushings, a micro Vickers hardness tester was used, and a sample in the range of 280~380 Vickers hardness number was selected. The number of toothbrushing stroke were 1,800 (2 months), 5,400 (6 months), 10,800 (12 months), and 21,600 (24 months). The tooth abrasion was measured using a scanning electron microscope. Statistical analysis was performed using IBM SPSS Statistics 22.0 and a p-value <0.05 was considered significant. According to the results, there was no statistically significant difference in the degree of plaque removal between ultra-soft and soft toothbrushes. The difference in tooth abrasion between before and after toothbrushing was found to be greater with the soft toothbrushes than with the ultra-soft toothbrushes. Therefore, the ultra-soft toothbrush not only lowers tooth damage by reducing tooth abrasion, but also shows a similar ability to remove plaque as soft toothbrushes.

Goldish Yellow Color인 수종(數種)의 치과용(齒科用) 비귀금속합금(非貴金屬合金) 경도(硬度), 강도(强度) 및 미세조직(微細組織)의 비교(比較)에 관(關)한 연구(硏究) (A Study on the Comparison of hardness, Strength and Microstructure of dental Non-precious Metal Alloys Colored Goldish Yeller)

  • 김재도
    • 대한치과기공학회지
    • /
    • 제14권1호
    • /
    • pp.55-65
    • /
    • 1992
  • The purpose of this study was to investigate the comparison of physical properties of nonprecious metal alloys colored goldish yellow. The experimental groups were copper based dental alloy and control group was Ni-Cr based dental alloy used crown and bridges frameworks. Hardness was tested by vickers hardness tester, tensile strength was tested by universal tension tester. After testing the tensile strength of castings, the microstrucure and the pattern of fracture were investigated by scanning electron microscope and metallurgical microscope. The results were as follows : Hardness of Ni based alloy was higher than Cu based alloys. Hardness number of A group was 200.41$\pm$16.10 Hv, B group was 194.33$\pm$1.69 Hv, C group was 139.29$\pm$2.19 Hv and D group was 293.81$\pm$27.17 Hv, respectively. Tensile strength of D group was 56.42$\pm$6.17 $kg/m^2$, A group was 50.39$\pm$5.68 $kg/m^2$, C group was 45.13$\pm$4.53 $kg/m^2$, B group was 45.25$\pm$9.25 $kg/m^2$, in order, and D group was maximum tensile strength. The fractured surfaces of tensile specimens in the all groups showed the tendency to form large voids in the center of specimens. Thus the ductile fracture was changed into the brittle fracture with the fine grain size.

  • PDF

Relationship between battery level and irradiance of light-curing units and their effects on the hardness of a bulk-fill composite resin

  • Fernanda Harumi Oku Prochnow ;Patricia Valeria Manozzo Kunz;Gisele Maria Correr;Marina da Rosa Kaizer;Carla Castiglia Gonzaga
    • Restorative Dentistry and Endodontics
    • /
    • 제47권4호
    • /
    • pp.45.1-45.10
    • /
    • 2022
  • Objectives: This study evaluated the relationship between the battery charge level and irradiance of light-emitting diode (LED) light-curing units (LCUs) and how these variables influence the Vickers hardness number (VHN) of a bulk-fill resin. Materials and Methods: Four LCUs were evaluated: Radii Plus (SDI), Radii-cal (SDI), Elipar Deep Cure (Filtek Bulk Fill, 3M Oral Care), and Poly Wireless (Kavo Kerr). Irradiance was measured using a radiometer every ten 20-second activations until the battery was discharged. Disks (4 mm thick) of a bulk-fill resin (Filtek Bulk Fill, 3M Oral Care) were prepared, and the VHN was determined on the top and bottom surfaces when light-cured with the LCUs with battery levels at 100%, 50% and 10%. Data were analyzed by 2-way analysis of variance, the Tukey's test, and Pearson correlations (α = 5%). Results: Elipar Deep Cure and Poly Wireless showed significant differences between the irradiance when the battery was fully charged versus discharged (10% battery level). Significant differences in irradiance were detected among all LCUs, within each battery condition tested. Hardness ratios below 80% were obtained for Radii-cal (10% battery level) and for Poly Wireless (50% and 10% battery levels). The battery level showed moderate and strong, but non-significant, positive correlations with the VHN and irradiance. Conclusions: Although the irradiance was different among LCUs, it decreased in half of the devices along with a reduction in battery level. In addition, the composite resin effectiveness of curing, measured by the hardness ratio, was reduced when the LCUs' battery was discharged.