• Title/Summary/Keyword: Ultrasonic-milling

Search Result 27, Processing Time 0.028 seconds

Synthesis of Nanocomposite Powder for Tungsten Heavy Alloy by Hydrogen Reduction of Ultrasonic-milled Oxide Nanopowders

  • Lee, Chang-Woo;Lee, Seung-Chul;Lee, Jai-Sung
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.422-423
    • /
    • 2006
  • Ultrasonic-milling of metal oxide nanopowders for the preparation of tungsten heavy alloys was investigated. Milling time was selected as a process variable. XRD results of metal oxide nanopowders ultrasonic-milled for 50 and 100h showed that mean crystallite size reduced with increasing milling time and there was no evidence of contamination or change of composition by impurities. It was found that nanocomposite powders reduced at $800^{\circ}C$ in $H_2$ atmosphere had a composition of 93.1W-4.9Ni-2.0Fe by EDX analysis. Hardness of sintered samples of 50 and 100h was 390 and 463 Hv, respectively, which corresponds to the hardness of commercial products.

  • PDF

Synthesis of Tungsten Heavy alloy Nanocomposite Powder by Ultrasonic-milling Process (초음파 밀링 공정을 이용한 텅스텐 중합금 나노복합분말의 제조)

  • Lee, Seung-Chul;Lee, Chang-Woo;Jung, Sung-Soo;Cha, Berm-Ha;Lee, Jai-Sung
    • Journal of Powder Materials
    • /
    • v.14 no.2 s.61
    • /
    • pp.101-107
    • /
    • 2007
  • Ultrasonic-milling of metal oxide nanopowders for the preparation of tungsten heavy alloys was investigated. Milling time was selected as a major process variable. XRD results of metal oxide nanopowders ultrasonic-milled for 50 h and 100 h showed that agglomerate size reduced with increasing milling time and there was no evidence of contamination or change of composition by impurities. It was found that nanocomposite powders reduced at $800^{\circ}C$ in a hydrogen atmosphere showed a chemical composition of 93.1W-4.9Ni-2.0Fe from EDS analysis. Hardness of sintered part using 50 h and 100 h powder samples was 399 Hv and 463 Hv, respectively, which is higher than the that of commercial products (330-340 Hv).

Effect of Dispersion Method on Formation of Electroless Ni-CNT Coatings (분산법이 무전해 Ni-CNT 복합도금막 형성에 미치는 영향)

  • Bae, KyooSik
    • Journal of the Semiconductor & Display Technology
    • /
    • v.13 no.3
    • /
    • pp.51-55
    • /
    • 2014
  • Ni-CNT(Carbon Nanotubes) composite coating is often used for the surface treatment of mechanical/electronic devices to improve the properties of the Ni coating. For the Ni-CNT coating, the dispersion of CNT fibers is a critical process. In this study, ultrasonic treatment instead of the conventional ball milling was attempted as a dispersion method for the electroless Ni-CNT coating. SEM-EDX analysis was performed and contact angle, sheet resistance, and micro-hardness were measured. Results showed that the ultrasonic treatment was comparable to the ball milling, as a dispersion method, but the difference was negligible. However, combined ball milling and ultrasonic treatment(double treatment) showed much improved micro-hardness value, above 350Hv(close to the value obtained by the Ni-CNT electroplating). In addition, electroless Ni-CNT(double-treated) coatings formed on the thin Ni film deposited by the electroless plating(double coating) showed better mechanical properties. Thus, double treatment and double coating are suggested as an improved electroless Ni-CNT coating method.

Investigation on Size Distribution of Tungsten-based Alloy Particles with Solvent Viscosity During Ultrasonic Ball Milling Process (초음파 볼밀링 공정에 의한 용매 점도 특성에 따른 텅스텐계 합금 분쇄 거동)

  • Ryu, KeunHyuk;So, HyeongSub;Yun, JiSeok;Kim, InHo;Lee, Kun-Jae
    • Journal of Powder Materials
    • /
    • v.26 no.3
    • /
    • pp.201-207
    • /
    • 2019
  • Tungsten heavy alloys (W-Ni-Fe) play an important role in various industries because of their excellent mechanical properties, such as the excellent hardness of tungsten, low thermal expansion, corrosion resistance of nickel, and ductility of iron. In tungsten heavy alloys, tungsten nanoparticles allow the relatively low-temperature molding of high-melting-point tungsten and can improve densification. In this study, to improve the densification of tungsten heavy alloy, nanoparticles are manufactured by ultrasonic milling of metal oxide. The physical properties of the metal oxide and the solvent viscosity are selected as the main parameters. When the density is low and the Mohs hardness is high, the particle size distribution is relatively high. When the density is high and the Mohs hardness is low, the particle size distribution is relatively low. Additionally, the average particle size tends to decrease with increasing viscosity. Metal oxides prepared by ultrasonic milling in high-viscosity solvent show an average particle size of less than 300 nm based on the dynamic light scattering and scanning electron microscopy analysis. The effects of the physical properties of the metal oxide and the solvent viscosity on the pulverization are analyzed experimentally.

Fabrication of Sn and SnO2 Nanopowders by Low-Temperature Phase Transformation Method (저온상변태법을 이용한 주석 및 산화주석 나노말의 제조)

  • Lee Kun-Jae;Joo Yeon-Jun;So Yong-Dae;Kim Nam-Hoon;Lee Jai-Sung;Choa Yong-Ho
    • Journal of Powder Materials
    • /
    • v.13 no.1 s.54
    • /
    • pp.46-51
    • /
    • 2006
  • Through the volume change of Sn in a low-temperature phase transformation, the Sn nanopowder with high, purity, was fabricated by an economic and eco-friendly process. The fine cracks were spontaneously generated. in, Sn ingot, which was reduced to powders in the repetition of phase transformation. The Sn nanopowder with 50 run in size was obtained by the 24th repetitions of phase transformation by low-temperature and ultrasonic treatments. Also, the $SnO_2$ powder was fabricated by the oxidation of the produced Sn powder to the ingot and milled by the ultrasonic milling method. The $SnO_2$ nanopowder of 20 nm in size was fabricated after the milling for 180 h.

The Hydrogen Reduction Behavior of Ultrasonic Ball-milled WO3-CuO Nanopowder (초음파 밀링한 WO3-CuO 나노혼합분말의 수소환원 거동)

  • Jung, Sung-Soo;Yoon, Eui-Sik;Lee, Jai-Sung
    • Korean Journal of Metals and Materials
    • /
    • v.47 no.9
    • /
    • pp.597-603
    • /
    • 2009
  • The hydrogen reduction behavior of ultrasonic ball-milled $WO_3-CuO$ nanopowder, which is highly related with micro-pore structure, was investigated by thermogravimetry(TG) and hygrometry system. EDS and TEM results represented that the ultrasonic ball-milled $WO_3-CuO$ nanopowder consisted of the agglomerates which was confirmed as a homogeneous mixture of $WO_3$ and CuO particles. It was found that the reduction reaction of CuO was retarded by initial micro-pores which are smaller than 40 nm in the ultrasonic ball-milled $WO_3-CuO$ nanopowder. The earlier agglomeration of Cu particles at comparably low temperature decreased the volume of micro-pores in the $WO_3-CuO$ nanopowder which caused the retardation of $WO_3$ reduction reaction. These results clearly explain that the micro-pore structure significantly affected the reduction reaction of $WO_3$ and CuO in the $WO_3-CuO$ nanopowder.

Effect of Ultrasonic Vibration on Micro-EDM Channel (Micro-EDM 채널가공에서 초음파 가진의 영향)

  • Lim, Heesung;Hong, Minsung
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.25 no.6
    • /
    • pp.421-425
    • /
    • 2016
  • Micro-EDM is one of the recent fine-machining technologies. Micro-EDM is widely used in precision processes because products manufactured via EDM are free from workpiece hardness. However, the debris produced during the process cause many problems such as reduced precision of the process. The first solution of this problem involves using the milling hole process. Micro-EDM hole process involves an electrode moving rapidly in the vertical direction via a servo system to disperse debris. However, this process can cause reduced work efficiency owing to contact between the electrode and workpiece. In this study, ultrasonic vibration is added to micro-EDM channel machining. Ultrasonic vibration removes the debris during machining and enables precision machining. Consequently, a clean work environment for the subsequent processes is maintained.

The effect of ultrasonic vibration on bond strength of cemented crown according to margin types and cements (초음파 진동이 주조금관의 변연형태와 시멘트의 결합강도에 미치는 영향)

  • Lee, Yun-Kyung;Bang, Mong-Sook;Park, Ha-Ok
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.18 no.3
    • /
    • pp.225-233
    • /
    • 2002
  • This study was aimed to evaluate the effects of ultrasonic vibration on margin types and cements by comparing bond strength of cemented crown. In this study, margins of each metal die, which were chamfer, shoulder and shoulder with bevel, were prepared using computer milling machine. Specimens were cemented with zinc phosphate cement or resin cement. The specimens were divided by the finish line and cement used, ultrasonic vibration. I made total 84 specimens. All specimens were divided into two groups. One group was not vibrated, the other group was subjected to ultrasonic vibration for 12 minutes. Tensile bond strength was measured using Universial testing machine. The changes of bond strength in groups were statistically analyzed by t-test or One-way ANOVA. The results were as follows : 1. Ultrasonic instrumentation diminished the bond strength of crown cemented with zinc phosphate cement and resin cement after 12 minutes application. 2. In case of zinc phosphate cement, the bond strength of a vibrated group was showed significantly decreased(p<0.05). In vibrated groups with zinc phosphate cement, shoulder with bevel exhibit a significant difference to chamfer and shoulder(p<0.05) 3. Resin cement was more resistant to ultrasonic vibration than zinc phosphate cement and showed no significant differences according to ultrasonic vibration and margin type. In conclusion, These results revealed that zinc phosphate cement was most affected and resin cement was the least affected by ultrasonic vibration. Especially shoulder with bevel design was most affected in zinc phosphate cement groups. we should consider these results and be taken in the application of ultrasonic vibration to any teeth restored with crowns.

Elastic Modulus of Magnetic Fluids Evaluated by Ultrasonic Test (초음파 시험에 의한 자기유체의 탄성율 산정)

  • Kim, Jong-Hee;Kim, Kun-Woo;Kim, Cheol-Gi;Lee, Seung-Goo;Koo, Man-Hoi
    • Korean Journal of Materials Research
    • /
    • v.22 no.3
    • /
    • pp.136-139
    • /
    • 2012
  • Magnetic nanoparticles for ferromagnetic fluids and magnetorheological fluids were prepared by chemical coprecipitation and mechanical milling, respectively. The surface-treated particles were dispersed at various weight ratios into a medium of polyethylene glycol. In order to evaluate the elastic modulus of the fluids, ultrasonic pulse velocities were measured with an ultrasonic test using transducers of 5MHz and 2.25MHz. The ultrasonic signals were only available with a transducer of 2.25 MHz at fluid concentrations of 5 mg/ml and lower. In the case of applying transducers over 2.25 MHz and concentrations over 5 mg/ml to the fluids, it was impossible to observe effective ultrasonic signals due to an excessive scattering of the pulses by the dispersed particles. Elastic moduli of the magnetorheological fluids were 5.44 GPa and 6.13 GPa with concentrations of 25 mg/ml and 50 mg/ml, respectively; these values were higher by 40% than the values of 4.04 GPa and 4.28 GPa of ferromagnetic fluids at the same concentrations. As for the effect of an external magnetic field on these dilute fluids, the ultrasonic signals were positioned in a very similar way, which was probably due to insufficient arrangement of the particles even though the reflection energy of the ultrasonic waves apparently increased.

Effect of exfoliated graphite nanoplatelets on the fracture surface morphology and the electrical resistivity of phenylethynyl-terminated polyimide

  • Cho, Dong-Hwan;Fukushima, Hiroyuki;Drzal, Lawrence T.
    • Carbon letters
    • /
    • v.13 no.2
    • /
    • pp.121-125
    • /
    • 2012
  • In the present work, exfoliated graphite nanoplatelets (EGN) of 1 ${\mu}m$ in average particle size, which were prepared by heating at $900^{\circ}C$ and then subjected to ultrasonic, ball-milling, and vibratory ball-milling techniques, were uniformly incorporated into phenylethynyl-terminated polyimide (PETI-5) resin. The fracture surface morphology and the electrical resistivity of the EGN/PETI-5 composites were investigated. The results showed that the fracture surfaces and the electrical resistivity strongly depended on the EGN content. The fracture surfaces became more ductile and roughened with increasing EGN and the electrical resistivity was gradually decreased with increased EGN loading, indicating the percolation threshold at 5 wt% EGN.