Combination of MCA and SHS for Material Synthesis

  • Soh, Dea-Wha;N., Korobova
    • 동굴
    • /
    • 제78호
    • /
    • pp.1-8
    • /
    • 2007
  • The combination of mechano-chemical activation (MCA)and Self-propagating High-temperature Synthesis (SHS) has widened the technical possibilities for both methods. For YBCO systems the investigation showed that a short-term MCA of initial powders before SHS leads to single-phase and ultra-fine products. A new technique for preparation ultra-fine high-temperature superconductors (HTS) of YBCO composition with a grain size d <1m is developed using combination of MCA and SHS. The specific feature of the technique is formation of the $YBa_2Cu_3O_7-$ crystalline lattice directly from an X-ray amorphous state arising as a result of mechanical activation of the original oxide mixture. The technique allows the stage of formation of any intermediate reaction products to be ruled out. X-ray and magnetic studies of ultra-fine high temperature superconductors are carried out. Dimension effects associated with the microstructure peculiarities are revealed. A considerable enhancement of inter-grain critical currents is found to take place in the ultra-fine samples.

Ultra-fine Grained Aluminum Alloy Sheets fabricated by Roll Bonding Process

  • 김형욱
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2009년도 춘계학술발표대회
    • /
    • pp.6.2-6.2
    • /
    • 2009
  • Ultra-fine grained (UFG) Al alloys, which have submicron grain structures, are expected to show outstanding high strength at ambient temperature and excellent superplastic deformation at elevated temperatures and high strain rate. In order to get the UFG microstructure, various kind of severe plastic deformation (SPD) processes have been developed. Among these processes, accumulative roll bonding (ARB) process is a promising process to make bulky Al sheets with ultrafine grained structure continuously. The purpose of the present study is to clarify the grain refinement mechanism during the ARB process and to investigate on the effects of ultra-fine grained structure on the mechanical properties. In addition, UFG AA8011 alloy (Al-0.72wt%Fe-0.63wt%Si) manufactured by the ARB had fairly large tensile elongation, keeping on the strength. In order to clarify the reason for the increase of elongation in the UFG AA8011 alloy, detailed microstructural and crystallographic analysis was performed by TEM/Kikuchi-line and SEM/EBSP method. The unique tensile properties of the UFG AA8011 alloy could be explained by enhanced dynamic recovery at ambient temperature, owing to the large number of high angle boundaries and the Al matrix with high purity.

  • PDF

누적압연접합에 의한 6061 Al 합금의 결정립 미세화와 마멸 특성 연구 (An Investigation of Sliding Wear and Microstructural Evolution of Ultra-Eine Grained 6061 Al Alloy Fabricated by ARB)

  • 이태오;김용석
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2001년도 춘계학술대회 논문집
    • /
    • pp.147-150
    • /
    • 2001
  • The ARB (Accumulative Rolling Bonding) Process was applied to a 6061 Al alloy to obtain ultra-fine grains. After 4 ARB cycles at $315^{\circ}C$, original equilibrium large grains were transformed to ultra-fine grains of several hundred nano-meter size with nonequilibrium grain boundaries. At lower number of cycles, microsutcture of highly-tangled dislocation cells were observed. Large grains and coarsened precipitates filled the microstructure of specimens experienced ARB cycles more than 5. Sliding wear tests using a pin-on-disk type wear tester were conducted on the ARB processed 6061 Al alloy plate. Wear rates of the 6061 Al alloy increased with the increase of ARB cycle number as well as the applied load. Worn surfaces and debris, cross-sections of the worn specimen were examined with scanning electron microscopy (SEM) to investigate the wear mechanism of the ultra-fine grained 6061 Al Tensile properties of the 6061 Al alloy were also studied and used to correlate the wear test results with the microstructures, which evolved continuously with the number of ARB cycles.

  • PDF

Fabrication of Pure Refractory Metals by Resistance Sintering under Ultra High Pressure

  • Zhou, Zhang-Jian;Du, Juan;Song, Shu-Xiang;Ge, Chang-Chun
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.1323-1324
    • /
    • 2006
  • Refractory materials, such as W and Mo, are very useful elements for use in high-temperature applications. But it is not easy to fabricat pure W and Mo with very high density and retaining very fine grain size because of their high melting point. In this paper, a newly developed method named as resistance sintering under ultra high pressure was use to fabricate pure fine-grained W and Mo. The microstructure was analysis by SEM. The sintering mechanism is primary analyzed. Basic physical property of these sintered pure W and Mo, such as hardness, bend strength, are tested.

  • PDF

ECAP가공된 7010 Al 합금의 초소성 변형 특성 (Superplastic Deformation Behavior of ECA dressed 7010 Al Alloy)

  • 김지식
    • 소성∙가공
    • /
    • 제11권3호
    • /
    • pp.255-261
    • /
    • 2002
  • The grain size of 7010 Al alloy was refined to submicrometer level by using equal channel angular pressing (ECAP) and additional warm rolling. The mechanisms of grain refinement in ECAP process were fragmentation of coarse grain to ultra fine subgrains after a few passes and continuous recrystallization of the subgrains with the increase o( passes. Because of ultrafine grain size, essentially low temperature and high strain rate superplasticity was observed after ECAP process and warm rolling to form a sheet metal. The maximum elongation of 700% was obtained for an ECA pressed specimen after IS passes without warm rolling at $450^{\circ}C$ with strain rate of 5x$10^{-3}$/sec.

초미세 결정립을 가지는 몰리브덴의 제조 및 기계적 특성 (Fabrication of Ultra Fine Grained Molybdenum and Mechanical Properties)

  • 김세훈;서영익;김대건;석명진;김영도
    • 한국분말재료학회지
    • /
    • 제17권3호
    • /
    • pp.235-241
    • /
    • 2010
  • Mo nanopowder was synthesized by ball-milling and subsequent hydrogen-reduction of $MoO_3$ powder. To fabricate ultra fine grained molybdenum, two-step sintering and spark plasma sintering process were employed. The grain size of specimen by two-step sintering and spark plasma sintering was around $0.6\;{\mu}m$ and $0.4\;{\mu}m$, respectively. Mechanical properties of ultra fine grained Mo with relative density of above 90% were significantly improved at room and high temperatures comparing to commercial bulk Mo of 99% relative density. This result was mainly explained by the grain size refinement due to diffusion-controlled sintering.

초미세립 순-타이타늄의 미세조직과 인장물성 (Microstructure and Tensile Properties of Ultrafine Grain Pure-Titanium)

  • 고영건;안정용;신동혁;이종수
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2006년도 춘계학술대회 논문집
    • /
    • pp.215-218
    • /
    • 2006
  • A study was made to investigate microstructural evolution and mechanical properties of ultra-fine grained (UFG) pure-Ti produced by equal channel angular (ECA) pressings. The deformed structures were analyzed by finite element method and transmission electron microscopy with the increment of straining. After 4 isothermal ECA pressings, initial coarse grains ($30{\mu}m$) were significantly refined to ${\sim}0.3{\mu}m$ with homogeneous distribution of microstructure which was resulted from $180^{\circ}$ rotation of the sample between pressings. UFG pure-Ti exhibited the considerable improvement in yield strength while losing strain hardening capacity as compared to coarse grained microstructure at ambient temperature, which was mainly attributed to ultra-fine grain microstructure with non-equilibrium grain boundaries.

  • PDF

ECAP으로 제조된 초미세림 Al-Mg 합금의 동적 변형거동 (High-Strain Rate Deformation of Ultra-Fine Grained Al-Mg Alloys Fabricated by Equal-Channel Angular Pressing)

  • 김양곤;고영건;신동혁;이성학
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2009년도 춘계학술대회 논문집
    • /
    • pp.306-309
    • /
    • 2009
  • The influence of equal-channel angular pressing (ECAP) route on dynamic deformation behavior of ultra-fine grained Al-4.4%Mg alloys was investigated in this study. The 8-pass ECAPed specimens consisted of ultra-fine grains of $0.5{\mu}m$ in size, and contained the considerable amount of second phase particles, which were fragmented and distributed homogeneously in the matrix. The result of dynamic torsional tests indicated that the maximum shear stress and fracture shear strain were lowest in the specimen deformed by ECAP via route A among the 8-pass ECAPed specimens. The formation of adiabatic shear bands was addressed by concepts of critical shear strain, deformation energy required for void initiation, and microstructural homogeneity related to ECAP routes.

  • PDF

DEVELOPMENT OF HYPER INTERFACIAL BONDING TECHNIQUE FOR ULTRA-FONE GRAINED STEELS

  • Kazutoshi Nishimoto;Kazuyoshi Saida;Jeong, Bo-young;Kohriyama, Shin-ichi
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.776-780
    • /
    • 2002
  • This paper describes the concept and the characteristics of hyper interfacial bonding developed as a new concept joining process for UFG (ultra-fine grained) steel. Hyper interfacial bonding process is characterized by instantaneous surface melting bonding which involves a series of steps, namely, surface heating by high frequency induction, the rapid removing of heating coil and joining by pressing specimens. UFG steels used in this study have the average grain size of 1.25 ${\mu}{\textrm}{m}$. The surface of specimen can be rapidly heated up and melted within 0.2s. Temperature gradient near heated surface is relatively steep, and peak temperature drastically fell down to about 1100K at the depth of 2~3mm away from the heated surface of specimen. Bainite is observed near bond interface, and also M-A (martensite-austenite) islands are observed in HAZ. Grain size increases with increasing heating power, however, the grain size in bonded zone can be restrained under 11 ${\mu}{\textrm}{m}$. Hardened zone is limited to near bond interface, and the maximum hardness is Hv350~Hv390.

  • PDF

ECAP가공한 P/M 6061 Al 합금의 미세조직과 기계적 성질 (Microstructural and Mechanical Characteristics of the ECAPed P/M 6061 Al Alloy)

  • 장시영
    • 한국분말재료학회지
    • /
    • 제9권1호
    • /
    • pp.43-49
    • /
    • 2002
  • Microstructural and mechanical characteristics of P/M 6061 Al alloy subjected to equal channel angular pressing (ECAP) were investigated. The P/M 6061 Al alloy had an intial grain size of approximately $20\mutextrm{m}$. An equiaxed ultra-fine grained structure with the mean grain size of $~50 \mutextrm{m}$ was obtained by four repetitive ECAP at 473 K. The microhardness of P/M 6061 Al alloy was drastically increased from about 40 Hv to 80 Hv by two repetitive ECAP at 373 K. However, the microhardness decreased with increasing ECAP temperature. The tensile stength of as-hot-pressed P/M 6061 Al alloy before ECAP was 95 MPa, whereas it increased to both 248 MPa after two repetitive ECAP at 373 K and 130 MPa after four repetitive ECAP at 473 K. The tensile properties of the ECAPed sample were compared with those of commercial cast 6061-O and 6061-T4 Al alloys.