• Title/Summary/Keyword: Titanium surface coating

Search Result 212, Processing Time 0.026 seconds

Preparation of Nanocrystalline TiO2 Coated Coal Fly Ash by Dropping Method of Coating Agent and Photocatalytic Characterization (페복제 적하법에 의한 나노 결정 TiO2 피복 석탄회의 제조와 광촉매 특성)

  • Yu, Yeon-Tae;Choe, Yeong-Yun;Kim, Byeong-Gyu
    • Korean Journal of Materials Research
    • /
    • v.12 no.5
    • /
    • pp.334-340
    • /
    • 2002
  • $TiO_2$-coated fly ash was synthesized by dropping method of coating agent in order to get $TiO_2$ coating layer with high photocatalytic activity on the surface of coal fly ash. The properties of the $TiO_2$ coating layer such as morphology, crystal structure, crystal size and photocatalytic activity were compared with those of the $TiO_2$-coated fly ash prepared by the traditional method of precipitation. $TiCl_4$ aqueous solution was used as a titanium stock solution and $NH_4HCO_3$ was used as a precipitant. The $TiO_2$ coating layer obtained by dropping method of coating agent was more uniform than that coated by precipitation. However, the crystal of $TiO_2$ coated by dropping method of coating agent was easy to grow by heat treatment because of the small primary particle size and bulky morphology, and its photocatalytic activity was consequently lower than that of the $TiO_2$ coated by precipitation. The $TiO_2$ coating layer obtained by both methods had a crystal structure of anatase, and the temperature of phase transformation into rutile was 90$0^{\circ}C$. The minimum crystal size of $TiO_2$ for the highest photocatalytic activity was found to be about 10nm.

Ti(CN) coating on aluminum alloy formed by MO-PACVD (Al 합금에 MO-PACVD법으로 증착시킨 Ti(CN) 코팅 층의 물성에 관한 연구)

  • ;;J. Woehle;K.-T. Rie
    • Journal of Surface Science and Engineering
    • /
    • v.33 no.1
    • /
    • pp.38-47
    • /
    • 2000
  • A Ti(CN) layer was formed on aluminum alloy by using diethylamino titanium, hydrogen and nitrogen with the pulsed DC PACVD process. Effect of process parameters such as precursor evaporation temperature, duty ratio, frequency, voltage, $H_2$/$N_2$gas ratio on the properties of Ti(CN) layer were investigated. The layer thus obtained had high hardness and low friction coefficient. Detailed results on the hardness, surface morphology, XRD, WDS analysis, wear test and scratch test of this layer are presented.

  • PDF

Study on blood compatibility of diamond-like carbon and titanium nitride films (Diamond-like carbon 및 titanium nitride 박막의 혈액적합성 연구)

  • Yun Ju-Young;Bae Jin-Woo;Park Ki-Dong;Goo Hyun-Chul;Park Hyung-Dal;Chung Kwang-Wha
    • Journal of the Korean Vacuum Society
    • /
    • v.14 no.3
    • /
    • pp.165-170
    • /
    • 2005
  • There is an increasing interest in developing novel coating to improve the blood compatibility of medical implants. Diamond-like carbon(DLC) and titanium nitride(TiN) films have been proposed as potential biomedical coatings due to their chemical k physical properties and moderate biocompatibility. To study the correlation between blood compatibility and physical properties of the films, the fibrinogen adsorption on the surface as well as morphology & wettability were investigated. The quantity of fibrinogen adsorption are Tower for TiN than DLC, which correlates with a higher hydrophilicity of TiN film. To reduce the quantity of fibrinogen adsorption on the film, plasma treatment and furnace annealing were performed, respectively. With the use of oxygen plasma and furnace annealing, the amount of fibrinogen adsorption on TiN film was remarkably reduced, while there was no decrease of the quantity with DLC.

EFFECT OF VARIOUS INODIZING CHARACTERISTICS ON BONE INTEGRATION OF TITANIUM IMPLANT SURFACE DESIGN (다양한 양극산화막 처리방법이 임프란트 골유착에 미치는 영향)

  • Cha, Soo-Ryun;Lee, Jun;Min, Seung-Ki
    • Maxillofacial Plastic and Reconstructive Surgery
    • /
    • v.30 no.5
    • /
    • pp.417-427
    • /
    • 2008
  • The aim of this study is to investigate the effect of anodizing surface to osseointegration of implant by using of resonance frequency analysis (RFA), quantitative and qualitative assessment of an anodically modified implant type with regard to osseous healing qualities. A total of 96 screw-shaped implants were prepared for this study. 72 implants were prepared by electrochemical oxidation with different ways. 24 (group 1 SP) were prepared at galvanostatic mode in 0.25M sulfuric acid and phosphoric acid. 24 (group 2GC) were prepared at galvanostatic mode in calcium glycerophosphate and calcium acetate and 24 (group 3 CMP (Calcium Metaphosphate) Coating were prepared at galvanostatic mode in 0.25M sulfuric acid and phosphoric acid followed by CMP coating. Rest of 24 (control group were as a control group of RBM surface. Bone tissue responses were evaluated by resonance frequency analysis (RFA) that were undertaken at 2, 4 and 6 weeks after implant placement in the mandible of mini-pig. Group 1 SP (anodized with sulfuric acid and phosphoric acid implants) demonstrated slightly stronger bone responses than control Group RBM. Group 2 GC (anodized surface with calcium glycerophosphate and calcium acetate implants) demonstrated no difference which were compared with control group. Group 3 GMP (anodized and CMP coated implants) demonstrated slightly stronger and faster bone responses than any other implants. But, all observation result of RF A showed no significant differences between experimental groups with various surface type. Histomorphometric evaluation demonstrated significantly higher bone-to-implant contact for group 2 GC. Significantly more bone formation was found inside threaded area for group 2 GC. It was concluded that group 2 GC (anodized surface with calcium glycerophosphate and calcium acetate implants) showed more effects on the bone tissue responses than RBM surface in initial period of implantation. In addition, CMP showed a tendency to promote bone tissue responses.

Effect of $Li_4Ti_5O_{12}$ coating layer on capacity retention of $LiMn_2O_4$ as cathode materials of lithium ion secondary batteries for HEV application (HEV용 리튬 이차전지 양극물질 $LiMn_2O_4$$Li_4Ti_5O_{12}$ 코팅에 따른 영향)

  • Wai, Yin-Loo;Choi, Byung-Hyun;Jee, Mi-Jung;Lee, Dae-Jin;Shin, Jae-Su;Song, Kwang-Ho
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 2007.11a
    • /
    • pp.125-128
    • /
    • 2007
  • In these recent years, low cost and stable battery electrode materials have been studied for HV/HEV application. Spinel cathode material $LiMn_2O_4$ is widely studied as a promising cathode material of lithium ion secondary batteries because of it is low cost, easily to be prepared and capable to be operated in high voltage range. In this study, $LiMn_2O_4$ was undergoing surface modification with spinel lithium titanium oxide by sol-gel method in order to enhance its capacity retention. Properties of both unmodified and surface-modified $LiMn_2O_4$ were characterized by XRD, SEM, particle size analyzer while their cycling performance was tested with charge and discharge tester.

  • PDF

Anti-Reflective Coating with Hydrophilic/Abraion-Resistant Properties using TiO2/SiOxCy Double-Layer Thin Film (TiO2/SiOxCy 이중 박막을 이용한 투명 친수성/내마모성 반사방지 코팅)

  • Lee, Sung-jun;Lee, Min-kyo;Park, Young-chun
    • Journal of Surface Science and Engineering
    • /
    • v.50 no.5
    • /
    • pp.345-351
    • /
    • 2017
  • A double-layered anti-reflective coating with hydrophilic/abrasion-resistant properties was studied using anatase titanium dioxide($TiO_2$) and silicon oxycarbide($SiO_xC_y$) thin film. $TiO_2$ and $SiO_xC_y$ thin films were sequentially deposited on a glass substrate by DC sputtering and PECVD, respectively. The optical properties were measured by UV-Vis-NIR spectrophotometer. The abrasion-resistance and the hydrophilicity were observed by a taber abrasion tester and a contact angle analyzer, respectively. The $TiO_2/SiO_xC_y$ double-layer thin film had an average transmittance of 91.3%, which was improved by 10% in the visible light region (400 to 800 nm) than that of the $TiO_2$ single-layer thin film. The contact angle of $TiO_2/SiO_xC_y$ film was $6.9^{\circ}$ right after UV exposure. After 9 days from the exposure, the contact angle was $10.2^{\circ}$, which was $33^{\circ}$ lower than that of the $TiO_2$ single-layer film. By the abrasion test, $SiO_xC_y$ film showed a superior abrasion-resistance to the $TiO_2$ film. Consequently, the $TiO_2/SiO_xC_y$ double-layer film has achieved superior anti-reflection, hydrophilicity, and abrasion resistance over the $TiO_2$ or $SiO_xC_y$ single-layer film.

Anisotropic TiSrYZrO Thin Films Induced by One-step Brush Coating for Liquid Crystal Molecular Orientation (액정분자 배향용 원스텝 브러시 코팅으로 유도된 이방성 TiSrYZrO 박막)

  • Byeong-Yun Oh
    • The Journal of Korea Institute of Information, Electronics, and Communication Technology
    • /
    • v.17 no.3
    • /
    • pp.146-154
    • /
    • 2024
  • In this paper, we present a convenient liquid crystal (LC) molecular alignment method using brush hairs as an alternative to the rubbing process in the LC display industry. Titanium strontium yttrium zirconium oxide (TiSrYZrO) solution was prepared using a sol-gel process, and the TiSrYZrO alignment film production and LC molecular alignment were integrated through a one-step brush coating process. As the curing temperature increased, the LC molecule alignment of the LC cell improved, and the formation of a physical surface anisotropic structure due to the shear stress caused by the movement of the brush hairs on the coating surface led to uniform alignment of the LC molecules. Uniform and homogeneous LC molecular alignment was confirmed through polarizing optical microscopy and pretilt angle measurement. Through thermal oxidation using X-ray photoelectron spectroscopy, the TiSrYZrO thin film well formed of metal oxide was confirmed and verified to have excellent optical transparency. From these results, it is expected that a convenient LC molecular alignment method using brush hairs as an alternative to the rubbing process will be a viable next-generation technology.

Abrasion of abutment screw coated with TiN

  • Jung, Seok-Won;Son, Mee-Kyoung;Chung, Chae-Heon;Kim, Hee-Jung
    • The Journal of Advanced Prosthodontics
    • /
    • v.1 no.2
    • /
    • pp.102-106
    • /
    • 2009
  • STATEMENT OF PROBLEM. Screw loosening has been a common complication and still reported frequently. PURPOSE. The purpose of this study was to evaluate abrasion of the implant fixture and TiN coated abutment screw after repeated delivery and removal with universal measuring microscope. MATERIAL AND METHODS. Implant systems used for this study were Osstem and 3i. Seven pairs of implant fixtures, abutments and abutment screws for each system were selected and all the fixtures were perpendicularly mounted in liquid unsaturated poly-esther with dental surveyor. After 20 times of repeated closing and opening test, the evaluation for the change of inner surface of implant and TiN-coated abutment screw, and weight loss were measured. Mann-Whitney test with SPSS statistical software for Window was applied to analyze the measurement of weight loss. RESULTS. TiN-coated abutment screws of Osstem and 3i showed lesser loss of weight than non-coated those of Osstem and 3i (P < .05, Mann-Whitney test). CONCLUSION. Conclusively, TiN coating of abutment screw showed better resistance to abrasion than titanium abutment screw. It was concluded that TiN coating of abutment screw would reduce the loss of preload with good abrasion resistance and low coefficient of friction, and help to maintain screw joint stability.

An Antireflection and Antistatic Coatings for CRTs using PEDOT (PEDOT를 이용한 CRT용 반사방지 및 대전방지 코팅)

  • 김태영;김종은;이보현;서광석;김진열
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.15 no.1
    • /
    • pp.61-66
    • /
    • 2002
  • A method for designing antireflection (AR) and antistatic (AS) coating layer by the use of conducting polymer as an electrically conductive transparent layer is proposed. The conducting AR coating is composed of four-layer with alternating high and low refractive index layer: silicon dioxide (n=1.44) and titanium dioxide (n=2.02) prepared at low temperature by sol-gel method are used as the low and high refractive index layer, respectively. The poly(3,4-ethylenedioxythiophene) which has the surface resistivity of 10$^4$Ω/$\square$ is used as a conductive layer. Optical constant of each ARAS coating layers such as refractive index and optical thickness were measured by 7he spectroscopic ellipsometer and from the measured optical constants the spectral properties such as reflectance and transmittance were simulated in the risible region. The reflectance of ARAS films on glass substrate was below 1 %R and the transmittance was higher than 95 % in the visible wavelength (400-700 nm). The measured AR spectral properties was very similar to its simulated results.

BONE RESPONSE OF TWO DIFFERENT SURFACE TITANIUM SUBPERIOSTEAL IMPLANTS - ANODIZED SURFACE, IBAD HA COATING SURFACE (티타늄 임플랜트의 두 가지 표면처리방식에 대한 골반응 - 양극 산화표면, IBAD HA 코팅 표면)

  • Lee, In-Ku;Suh, Kyu-Won;Choi, Joon-Eon;Jung, Sung-Min;Ryu, Jae-Jun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.45 no.1
    • /
    • pp.131-143
    • /
    • 2007
  • Statement of the problem: In case of poor bone quality or immediately loaded implant, various strategies have been developed focusing on the surface of materials to improve direct implant fixation to the bone. The microscopic properties of implant surfaces play a major role in the osseous healing of dental implant. Purpose of study: This study was undertaken to evaluate bone response of ion beam-assisted deposition(IBAD) of hydroxyapatite(HA) on the anodized surface of subperiosteal titanium implants. Material and methods: Two half doughnut shape subperiosteal titanium implants were made. The control group was treated with Anodized surface treatment and the test group was treated with IBAD of HA on control surface. Then two implants inserted together into the subperiosteum of the skull of 30 rats and histological response around implant was observed under LM(light microscope) and TEM(transmission electron microscope) on 4th, 6th and 8th week. Results: Many subperiosteal implants were fixed with fibrous connective tissue not with bony tissue because of weak primary stability. The control group observed poor bone response and there was no significant change at any observation time. However the test group showed advanced bone formation and showed direct bone to implant contact under LM on 8th week. The test group observed much rER in the cell of osteoblast but the control group showed little rER under TEM. Conclusions: The test group showed better bone formation than the control group at the condition of weak primary stability. With these results IBAD surface treatment method on Anodized surface, may be good effect at the condition of weak primary stability.