• Title/Summary/Keyword: Titanium alloys

Search Result 288, Processing Time 0.025 seconds

Effect of Fe Content on Mechanical and Electrochemical Properties of Ti-Mo-Fe Alloys (Ti-Mo-Fe 합금의 Fe 함량에 따른 기계적 특성과 전기화학적 특성 비교·분석)

  • Ji-Won Kim;Jeong-Yeon Park;Min Gang;Ji-Hwan Park;Dong-Geun Lee
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.36 no.3
    • /
    • pp.145-152
    • /
    • 2023
  • β titanium alloys containing β stabilizing elements such as V, Nb, Ta, Mo and Fe are widely used etc, due to their excellent specific strength, corrosion resistance, fatigue strength and easy formability. New metastable β titanium alloys are developed containing low-cost elements (Mo and Fe) in this study. Fe element is a strong β-stabilizer which can affect the mechanical and electrochemical properties of Ti-5Mo-xFe (x = 1, 4 wt%) alloys. These properties were analyzed in connection with microstructure and phase distribution. Ti-5Mo-4Fe alloy showed higher compression yield stress and maximum stress than Ti-5Mo-1Fe alloy due to solid-solution hardening and grain refinement hardening effect. As Fe element increased, Fe oxide formation and reduction of ${\bar{Bo}}$ (bond order) value affect the decrease of corrosion resistance. Ti-5Mo-xFe alloys were more excellent than Ti-6Al-4V ELI alloy.

Wear Properties of Cast Titanium Alloys for Dental Use (치과용 Titanium 주조합금의 마멸특성)

  • Choi, Seok-Kyu;Kim, Hyung-Il;Park, Ik-Min
    • Journal of Korea Foundry Society
    • /
    • v.11 no.6
    • /
    • pp.482-490
    • /
    • 1991
  • This study presents the wear characteristics of Ti alloys (Pure Ti, Ti-6Al-4V, Ti-5Al-2.5Sn) fabricated by centrifugal precision casting in an Ohara dental titanium casting machine. It was found that the hardness of the surface region is higher than that of the interior region. It is considered that the oxygen adsorption in the surface region during casting, leads to the interstitial solid solution hardening. Wear resistance incerases in the order of pure Ti, Ti-6Al-4V, Ti-5Al-2.5Sn alloys. The interior hardness value increases in the same order. The specific wear rate increases with applied load and increases monotonously with sliding speed. The Fe transfer from the counterpart material was observed on the worn surface of the Ti-5Al-2.5Sn alloy. Oxidative wear occurs at low sliding speeds and mechanical fracture wear occurs at high sliding speeds.

  • PDF

High performance ultrafine-grained Ti-Fe-based alloys with multiple length-scale phases

  • Zhang, Lai-Chang
    • Advances in materials Research
    • /
    • v.1 no.1
    • /
    • pp.13-29
    • /
    • 2012
  • In order to simultaneously enhance the strength and plasticity in nanostructured / ultrafine-grained alloys, a strategy of introducing multiple length scales into microstructure (or called bimodal composite microstructure) has been developed recently. This paper presents a brief overview of the alloy developement and the mechanical behavior of ultrafine-grained Ti-Fe-based alloys with different length-scale phases, i.e., micrometer-sized primary phases (dendrites or eutectic) embedded in an ultrafine-grained eutectic matrix. These ultrafine-grained titanium bimodal composites could be directly obtained through a simple single-step solidification process. The as-prepared composites exhibit superior mechanical properties, including high strength of 2000-2700 MPa, large plasticity up to 15-20% and high specific strength. Plastic deformation of the ultrafine-grained titanium bimodal composites occurs through a combination of dislocation-based slip in the nano-/ultrafine scale matrix and constraint multiple shear banding around the micrometer-sized primary phase. The microstructural charactersitcs associated to the mechanical behaivor have been detailed discussed.

Titanium alloy bolt hot forging process analysis through plastic working analysis (소성 가공 해석을 통한 티타늄 합금 볼트 열간 단조 공정 분석)

  • Choi, Doo-Sun;Kim, Tae-Min;Han, Bong-Seok;Han, Yu-Jin;Ko, Kang-Ho;Park, Jung-Rae;Park, Kyu-Bag;Lee, Jung-Woo;Kim, Do-Un
    • Design & Manufacturing
    • /
    • v.14 no.1
    • /
    • pp.42-48
    • /
    • 2020
  • Titanium alloy has been in the spotlight as a core material in high-tech industries that require high strength and light weight because it has excellent strength and corrosion resistance and strength is higher than that of steel. Therefore, in various industries, existing steel products are intended to be replaced with titanium alloys. Titanium alloys can cause cutting tool breakage during cutting, and heat generated during cutting does not dissipate, accumulates in tools and workpieces, resulting in large wear and tear on thin workpieces. In addition, since titanium alloy is a metal with high chemical activity, the wear of the tool becomes more severe when the cutting speed is high, so machining of titanium bolt through cutting is very disadvantageous in terms of productivity. Therefore, the production of bolts using titanium alloys is being produced through a forging process to improve productivity and product quality. In this paper, hot forging molding analysis was performed on bolts used for fastening automobile parts using Ti-6Al-4V alloy, which is the most commonly used titanium alloy.

Effect of Boron on the Manufacturing Properties of Ti-2Al-9.2Mo-2Fe Alloy (Ti-2Al-9.2Mo-2Fe 합금의 후공정 특성에 미치는 보론의 영향)

  • Kim, Tae-Yong;Lim, Ka-Ram;Lee, Yong-Tai;Cho, Kyung-Mok;Lee, Dong-Geun
    • Korean Journal of Materials Research
    • /
    • v.25 no.11
    • /
    • pp.636-641
    • /
    • 2015
  • Titanium has many special characteristics such as specific high strength, low elastic modulus, excellent corrosion and oxidation resistance, etc. Beta titanium alloys, because of their good formability and strength, are used for jet engines, and as turbine blades in the automobile and aerospace industries. Low cost beta titanium alloys were developed to take economic advantage of the use of low-cost beta stabilizers such as Mo, Fe, and Cr. Generally, adding a trace of boron leads to grain refinement in casted titanium alloys due to the pinning effect of the TiB phases. This study analyzed and evaluated the microstructural and mechanical properties after plastic deformation and heat treatment in boron-modified Ti-2Al-9.2Mo-2Fe alloy. The results indicate that a trace of boron addition made grains finer; this refinement effect was found to be maintained after subsequent processes such as hot forging and solution treatment. This can effectively reduce the number of required manufacturing process steps and lead to savings in the overall cost as well as low-cost beta elements.

High-Temperature Oxidation of Ti Containing Stainless Steel in O2-N2 Atmosphere

  • Onishi, Hidenori;Saeki, Isao;Furuichi, Ryusaburo;Okayama, Toru;Hanamatsu, Kenko;Shibayama, Tamaki;Takahashi, Heishichiro;Kikkawa, Shinichi
    • Corrosion Science and Technology
    • /
    • v.3 no.4
    • /
    • pp.140-147
    • /
    • 2004
  • High temperature oxidation of Fe-19Cr and Fe-19Cr-0.2Ti alloys is studied at 1173-1373 K in 16.5 kPa $O_2$ - balances $N_2$ atmosphere aimed at clarifying the effect of titanium addition. Oxidation rate of Fe-19Cr alloy was accelerated with titanium. For both alloys chromium rich $(Fe,\;Cr)_2O_3$ was formed as a major oxidation product. On Fe-19Cr-0.2Ti alloy, a thin layer composed of spinel type oxide and titanium oxide was also formed and an internal oxidation of titanium was observed. Titanium was concentrated at the oxide surface and internal oxidation zone but a small amount of titanium was also found in the intermediate corundum type $(Fe,\;Cr)_2O_3$ layer. Crystals of corundum type $(Fe,\;Cr)_2O_3$ formed on Fe-19Cr alloy are coarse but that formed on Fe-19Cr -0.2Ti alloys were fine and columnar. Reason for the difference in oxidation kinetics and crystal structure will be discussed relating to the distribution of aliovalent titanium in corundum type $(Fe,\;Cr)_2O_3$ oxide layer.

Corrosion Behaviour of Some Alloys in Tropical Urban and Marine Atmospheres

  • Dang, Vu Ngoan;Bui, Ba Xuan;Nguyen, Nhi Tru
    • Corrosion Science and Technology
    • /
    • v.7 no.2
    • /
    • pp.125-129
    • /
    • 2008
  • Results of corrosion testing for different grades of titanium, copper, zinc, alluminium alloys and steels after two years of outdoor exposure under humid tropical urban and marine conditions have been presented and discussed. Mass loss and corrosion product characteristics for the exposed specimens at Hanoi testing site with high humidity and Nhatrang marine stations (at 100 and 1,000 meters distances from sea) with different airborne salinities (35.9 and $90.0mg/m^2.d$ respectively) have been selected for investigation. From time dependence of the specimen mass loss and corrosion product characteristics, the strong influence of environmental parameters upon durability for the investigated metals and alloys has been demonstrated. Only titanium alloys show high resistance to the marine conditions. All the other specimens (copper, zinc, alluminium alloys and steels) have been underwent strong deterioration under influence of aerosol salinity. Results of corrosion products analysis have been also presented for characterization of environmental impact on the metal degradation processes.

Evaluation of Pess Formability for Ti-6Al-4V Sheet at Elevated Temperature (Ti-합금판재(Ti-6Al-4V)의 고온 성형성 평가)

  • Park, J.G.;Park, N.K.;Kim, Y.S.
    • Transactions of Materials Processing
    • /
    • v.19 no.4
    • /
    • pp.230-235
    • /
    • 2010
  • Titanium alloy sheets have excellent specific strength and corrosion resistance as well as good performance at high temperature. Recently, titanium alloys are widely employed not only for aerospace parts but also for bio prothesis and motorcycle. However, the database is insufficient in the titanium alloy for press forming process. In this study, the effect of temperature on the forming limit diagram was investigated for Ti-6Al-4V titanium alloy sheet through the Hecker‘s punch stretching test at elevated temperature. Experimental results obtained in this study can provide a database for the development of press forming process at elevated temperature of Ti-6Al-4V titanium alloy sheet. From the experimental studies it can be concluded that the formability of Ti-6Al-4V titanium alloy sheet is governed by the ductile failure for the testing temperature. The formability of Ti-6Al-4V titanium alloy sheet at $700^{\circ}C$ increases about 7 times compared with that at room temperature.

Evaluation of press formability for Ti-6Al-4V sheet at elevated temperature (티타늄 합금판재(Ti-6Al-4V)의 고온 성형성 평가)

  • Bae, M.K.;Park, J.G.;Kim, J.H.;Park, N.K.;Kim, Y.S.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2009.05a
    • /
    • pp.152-157
    • /
    • 2009
  • Titanium alloy sheets have excellent specific strength and corrosion resistance as well as good performance at high temperature. Recently, titanium alloys are widely employed not only aerospace parts but also bio prothesis and motorcycle. But the database is insufficient of the titanium alloy for press forming process. In this study, the effect of temperature on the forming limit diagram was investigated for Ti-6Al-4V titanium alloy sheet through the Hocker's punch stretching test at elevated temperature. Experimental results obtained in this study can provide a database for development of press forming process at elevated temperature of Ti-6Al-4V titanium alloy sheet. From the experimental studies it can be concluded that the formability of Ti-6Al-4V titanium alloy sheet is governed by the ductile failure for the testing temperature below and vice versa neck-induced failure above the recrystalization temperature $0.5T_m$. The formability of Ti-6Al-4V titanium alloy sheet at $750^{\circ}C$ increases about 7 times compared with that at room temperature.

  • PDF

A TISSUE RESPONSE TO THE TITANIUM ALLOY (Ti-13Zr-6Nb) IN VIVO

  • Kim Chang-Su;Lee Seok-Hyung;Shin Sang-Wan;Suh Kyu-Won;Ryu Jae-Jun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.42 no.6
    • /
    • pp.619-627
    • /
    • 2004
  • Statement of problem. Mechanisms of tissue-implant interaction and the effect of the implant surface on the behavior of cells has not yet been clarified. Purpose. This study was performed to investigate the tissue reaction to the titanium alloy submerged into rat peritoneum in vivo. Materials and methods. Titanium alloys (titanium-13Zirconium-6Niobium) were inserted inside the peritoneal cavity of Sprague Dawley rats. After 3 months, the tissue formed around the inserted titanium alloys were examined with a light-microscope. Tissue reaction around the material was analyzed by confocal microscopy to evaluate their biocompatibility in a living body. Results. In in vivo study, foreign body type multinucleated giant cells were found in the fibrous tissue formed as a reaction to the foreign material (4 in 20 cases), but the inflammatory reaction was very weak. After experiment, the contaminants of biomaterials was removed from living tissue. In confocal microscopy, we observed that the staining of vinculin and actin showed mixed appearance. In a few cases, we found that the staining of vinculin and beta-catenin showed the prominent appearance. Conclusion. We found that titanium-13Zirconium-6Niobium alloy was an excellent biomaterial.