• 제목/요약/키워드: Time-Hardening

검색결과 466건 처리시간 0.033초

GMA용접에서 콘택트팁의 내마모성에 대한 예측 (Prediction on the Wear Resistance of Contact Tips for GMA Welding)

  • 김남훈;김희진;유회수;고진현
    • Journal of Welding and Joining
    • /
    • 제22권4호
    • /
    • pp.35-42
    • /
    • 2004
  • Contact tips are required to have a higher resistance to wear and thus to have an extended life time under the advanced GMAW welding process. Several requirements have been specified and employed by domestic industries for selecting their tips for such a purpose. However no attempt has been made to justify their requirements based on the experimental data of wear resistance or life time of contact tips. In this study, five different contact tips with three different compositions were employed for actual GMA welding up to 4 hours and were evaluated their wear resistance by measuring in every one hour the area of enlarged hole at the exit side. Experimental results clearly showed that the Cr-containing tips strengthened by precipitation hardening have much better resistance to wear than those made by work hardening. It was further noticed that Cr is an excellent alloying element for improving the wear resistance of contact tips only when it is in an properly aged condition. Initial hardness may play some role in the early stage of wear but not in the later stage of welding because the microstructure of tip changes significantly by the prolonged exposure to welding arc heat. Based on these results, critical review has been made on the current requirements employed by domestic industries. Of importance is that a new guideline has been confirmed to be more reasonable.

경화촉진제 사용량에 따른 콘크리트의 조기강도 특성에 관한 연구 (The Study on the Properties of the Early Strength of the Concrete According to the Usage of Hardening Accelerator)

  • 전우철;이지환;서일;이진우;이재삼;조인성
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2012년도 추계 학술논문 발표대회
    • /
    • pp.221-222
    • /
    • 2012
  • This study is to high early concrete development which reveals 14 MPa within 12 hours in order to reduce the mold time of dismantlement and not do the steam curing of the precast concrete product. About (40~50) min could shorten the final setting time if the coagulation test result cement amount 100 kg/m3 was increased. In the case of the compressive strength, it was exposed to be satisfied the target value with the cement amount 500 kg/m3 combination according to the hardening accelerator addition.

  • PDF

자은도사(慈恩島砂)를 이용(利用)한 N-Process의 주형강도(鑄型强度)에 관(關)한 연구(硏究) (A Study on the sand mold compression strength of the N-process mold mixed with JA-EUN-DO sand.)

  • 이원식
    • 한국주조공학회지
    • /
    • 제4권2호
    • /
    • pp.102-107
    • /
    • 1984
  • The variations of the mold compression strength were studied by varing the contents of the silicon powder and water glass, silion purities, and molecule rates of the water glass, when domestic JA EUN DO sand is mixed with water glass (sodium silicate) and metallic silicon or ferro - silicon powder by the self - hardening N - PROCESS method. The results obtained from this experiment are as follows; 1) The compression strength of the mold used with metalic powder was higher and more stable than to be used ferro - silicon powder. 2) 6% water glass of 2.8 molecule rate and 1.5% of ferro - silicon of 75% purity for the N - PROCESS used with JA EUN DO sand was suitable mixing rate. 3) The compression strength increased with self - hardening time, and the PH values of the mixture of silicon powder and water glass did not change after 2 hours, but the compression strength increased steadily due to the reaction of remained silicon. 4) It is recommended to take 24 hours for self - hardening time at least.

  • PDF

칼슘계 경화촉진제를 사용한 프리캐스트 콘크리트의 수축특성에 관한 연구 (A study on the Shrinkage Properties of precast concrete using Calcium hardening accelerator)

  • 민태범;조인성;이한승
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2014년도 추계 학술논문 발표대회
    • /
    • pp.44-45
    • /
    • 2014
  • On this study, initial crack index was evaluated by performing FEM analysis to crack propagation from hydration heat for development of precast concrete. On the result, as increased the usage of hardening accelerator, initial compressive strength were improved and setting time also was shortened. Additionally, central temperature of concrete was increased, the reaching time for the highest temperature could be shortened. By the result to assess crack index, there was no problem about crack despite of growth of initial high hydration heating. This result guessed because of small size element when analyzed trough FEM, realization for mass concrete's crack index should be performed.

  • PDF

A stability factor for structure-dependent time integration methods

  • Shuenn-Yih Chang;Chiu-Li Huang
    • Structural Engineering and Mechanics
    • /
    • 제87권4호
    • /
    • pp.363-373
    • /
    • 2023
  • Since the first family of structure-dependent methods can simultaneously integrate unconditional stability and explicit formulation in addition to second order accuracy, it is very computationally efficient for solving inertial problems except for adopting auto time-stepping techniques due to no nonlinear iterations. However, an unusual stability property is first found herein since its unconditional stability interval is drastically different for zero and nonzero damping. In fact, instability might occur for solving a damped stiffness hardening system while an accurate result can be obtained for the corresponding undamped stiffness hardening system. A technique of using a stability factor is applied to overcome this difficulty. It can be applied to magnify an unconditional stability interval. After introducing this stability factor, the formulation of this family of structure-dependent methods is changed accordingly and thus its numerical properties must be re-evaluated. In summary, a large stability factor can result in a large unconditional stability interval but also lead to a large relative period error. As a consequence, a stability factor must be appropriately chosen to have a desired unconditional stability interval in addition to an acceptable period distortion.

실시간 출력 제어를 통한 구상흑연 주철의 레이저 표면경화 특성 (Characteristics of Surface Hardening by Laser Power Control in Real Time of Spheroidal Graphite Cast Iron)

  • 김종도;송무근
    • 한국레이저가공학회지
    • /
    • 제18권2호
    • /
    • pp.1-4
    • /
    • 2015
  • This study is related to the surface hardening treatment to spheroidal graphite cast iron for die by using high power diode laser. Laser device used in this experiment is capable of real-time laser power control. This is because the infrared temperature sensor (two color pyrometer) attached to the optical system measures the surface temperature of specimen and adjusts the laser power in real time. The surface treatment was carried out with the change of heat treatment temperature at the beam travel speed 3 mm/sec. Hardened width and depth was measured and hardened zone was analyzed by micro vickers hardness test in order to research the optimum condition of heat treatment. The changes in microstructure of the hardened zone also was examined. As a result of hardness measurement and observations on microstructure of hardened zone, hardness increased over three times as compared with base metal because the martensite was formed on the matrix structure.

마이크로시멘트를 이용한 침하복원용 그라우팅재료의 배합 설계 (Mixed Design of Grouting Materials for Settlement Restoration Using Micro Cement)

  • 이일화;이성진;윤원민;박성기
    • 한국철도학회:학술대회논문집
    • /
    • 한국철도학회 2011년도 춘계학술대회 논문집
    • /
    • pp.1786-1792
    • /
    • 2011
  • If the concrete track is settled excessively, it must be restored or reinforced immediately. Especially, reinforcement/restoration method should be applied without affecting on train operation. To deal with this problem, special equipment, process and material should be prepared. This paper suggest a special mixing ratio to restore the settled concrete track. Materials are classified the quick hardening mortar and the middle hardening mortar. The quick hardening mortar is used to restore the settled track and the middle hardening mortar is used to fill the void. These materials must have the appropriate gel time(1-40sec) and compressive strength($5kg/cm^2$). Various compounds is used and the micro cement is used as a main base.

  • PDF

온도에 따른 수중경화형 에폭시수지의 레올로지 특성 (The Properties of Rheology of Underwater-Hardening Epoxy Resin According to the Temperature)

  • 정은혜;강철;곽은구;배기선;이대경;김진만
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2006년도 춘계학술논문 발표대회 제6권1호
    • /
    • pp.49-52
    • /
    • 2006
  • Epoxy resin has less reaction shrinkage, has better water proofing and thermal resistance than other repairing materials, to it has been applied broadly to repair and finish buildings and infrastructures. Although the ambient temperature constructed is varied with the seasons and epoxy resin has to mix with appropriate hardener due to the non self-hardening, as the real construction of it, the ambient temperature is ignored and the blending ration of epoxy resin and hardener is fixed. Also, because of the hardening time is aimed to temperature condition and the tolerance of blending ratio, we investigated the variation of viscosity according to ambient temperatures and hardener ratios. As a results of study, we can select the economical blending ratio of the epoxy resin and hardener according to site situation.

  • PDF

준설매립된 해성점성토에서 시멘트계 고화재를 이용한 표층개량 (The Improvement of Surface Layer Using Cement-hardening Agents in Dredged and Reclaimed Marine Clay)

  • 남정만;윤중만
    • 한국해양공학회지
    • /
    • 제18권4호
    • /
    • pp.46-51
    • /
    • 2004
  • The surface layer in dredged and reclaimed marine clay is improved by mixing of shallow soils and hardening agents, which is made of cement, containing some other special admixtures. Tests in both laboratory and field settings are performed to investigate the improvement effect and strength properties of cement-stabilized soils. The test results show that the hardening agent sufficiently improves the soil properties of the surface layer, while increasing the load-carrying capacity. The strength of cement-stabilized soils depends, primarily, on water-to-cement ratio and curing temperature. That is, the higher curing temperature and the longer curing time, the higher the strength in cement-stabilized soils. The high ratio of water-ta-cement results in a lower strength.

금형재료용 주철의 다이오드 레이저 표면경화처리에 관한 연구(II) - 표면경화의 적용 부위에 따른 열처리 특성의 차이 - (A Study on the Diode Laser Surface Hardening Treatment of Cast Iron for Die Material(II) -Comparison of Hardening Characteristics by the Parts Applied Heat Treatment-)

  • 김종도;송무근;황현태
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제35권8호
    • /
    • pp.1048-1054
    • /
    • 2011
  • 레이저 표면경화처리는 고밀도 에너지 열원에 의해 레이저 조사부위만 급속 가열한 후 표면의 열이 내부로 전도되어 급속히 자기냉각 됨으로써 표면을 경화시키는 방법이다. 이 표면처리 방법은 열처리에 의한 열변형이 거의 없고, 표면경화처리 이후 다른 공정을 수반하지 않는다. 또한 국부적인 가공이 가능하기 때문에 복잡한 형상을 가지는 금형에는 적합한 표면처리 방법이다. 본 연구에서는 열처리에 적합한 빔 프로파일을 가진 고출력 다이오드 레이저를 이용하여 금형재료용 주철의 표면처리를 실시하였다. 프레스 금형 공정에 따른 금형의 형상이 다르기 때문에 적용부위에 따라 시험편을 평면과 모서리부로 나누어 열처리를 실시하였다. 이때 모서리부의 열처리는 광학헤드를 $10^{\circ}$ 기울인 상태에서 진행하였다. 그 결과, 모서리부의 열처리는 평면부와 비교하여 형상에 따른 열전달 루트가 제한되므로, 입열이 집중되기 쉬워 평면 열처리보다 빠른 이송속도에서 경화가 이루어졌다.