Enhancement in Piezoelectric Properties of PZT-Based Ceramics by High Energy Ball-Milling Treatment of Solid-State Synthesized Powders

  • Kim, Dae-Uk;Lee, Han-Bok;Hung, Nguyen Viet;Pham, Ky Nam;Han, Hyoung-Su;Lee, Jae-Shin
    • 한국분말재료학회지
    • /
    • 제17권5호
    • /
    • pp.404-408
    • /
    • 2010
  • The effects of high energy ball-milling (HEBM) on the sintering behavior and piezoelectric properties of 0.1 wt% $Li_2CO_3$ doped 0.8Pb($Mg_{1/3}Nb_{2/3}$)$O_3$-0.2Pb($Zr_{0.475}Ti_{0.525}$)$O_3$ (PMN-PZT) ceramics were investigated. It was found that HEBM treatment was quite effective to reduce the average particle size down to 300 nm, leading to increased density as well as enhanced piezoelectric properties of a sintered specimen even though prolonged HEBM resulted in unwanted secondary phases that caused a degradation of piezoelectric properties. The dielectric constant ($\varepsilon_r$), piezoelectric coupling factor ($k_p$) and piezoelectric constant $d_{33}$ of 0.1 wt% $Li_2CO_3$ doped PMN-PZT ceramics prepared via HEBM for 10 h reached 2040, 0.68 and 554 pC/N, respectively.

Effect of metal conditioner on bonding of porcelain to cobalt-chromium alloy

  • Minesaki, Yoshito;Murahara, Sadaaki;Kajihara, Yutaro;Takenouchi, Yoshihisa;Tanaka, Takuo;Suzuki, Shiro;Minami, Hiroyuki
    • The Journal of Advanced Prosthodontics
    • /
    • 제8권1호
    • /
    • pp.1-8
    • /
    • 2016
  • PURPOSE. The purpose of this study was to evaluate the efficacy of two different metal conditioners for non-precious metal alloys for the bonding of porcelain to a cobalt-chromium (Co-Cr) alloy. MATERIALS AND METHODS. Disk-shaped specimens ($2.5{\times}10.0mm$) were cast with Co-Cr alloy and used as adherend materials. The bonding surfaces were polished with a 600-grid silicon carbide paper and airborne-particle abraded using $110{\mu}m$ alumina particles. Bonding specimens were fabricated by applying and firing either of the metal conditioners on the airborne-particle abraded surface, followed by firing porcelain into 5 mm in diameter and 3 mm in height. Specimens without metal conditioner were also fabricated. Shear bond strength for each group (n=8) were measured and compared (${\alpha}=.05$). Sectional view of bonding interface was observed by SEM. EDS analysis was performed to determine the chemical elements of metal conditioners and to determine the failure modes after shear test. RESULTS. There were significant differences among three groups, and two metal conditioner-applied groups showed significantly higher values compared to the non-metal conditioner group. The SEM observation of the sectional view at bonding interface revealed loose contact at porcelain-alloy surface for non-metal conditioner group, however, close contact at both alloy-metal conditioner and metal conditioner-porcelain interfaces for both metal conditioner-applied groups. All the specimens showed mixed failures. EDS analysis showed that one metal conditioner was Si-based material, and another was Ti-based material. Si-based metal conditioner showed higher bond strengths compared to the Ti-based metal conditioner, but exhibited more porous failure surface failure. CONCLUSION. Based on the results of this study, it can be stated that the application of metal conditioner is recommended for the bonding of porcelain to cobalt-chromium alloys.

Characterization of Wintertime Atmospheric Aerosols in Seoul Using PIXE and Supplementary Analyzers

  • Ma, Chang-Jin;Mikio Kasahara;Hwang, Kyung-Chul;Yeo, Hyun-Gu;Park, Kum-Chan
    • Journal of Korean Society for Atmospheric Environment
    • /
    • 제16권E호
    • /
    • pp.19-27
    • /
    • 2000
  • Particle Induced X-ray Emission (PIXE) and Elemental Analysis Syztem (EAS) were applied to the investiga-tion of the Characteristics and sources of wintertime atmospheric aerosols in Seoul. Atmospheric aerosols were collected by both fine and coarse fractions using a two-stage filter pack sampler from Kon-Kuk university during the winter season of 1999. PIXE was applied to the analysis of the middle and heavy elements with atomic numbers greater than 14(Si) and EAS was applied to the measurement of the light elements such as H, C and N. The fact that 64.2% of mass of fine particles in Seoul consists of the light elements (N, C , and H) suggests that the measurement of light elements is extremely important. The average mass concentration is Seoul was 38.6$\mu\textrm{g}$m(sup)-3. Elements such as Ca, Fe, Mg, and Ti appeared to have very low Fine/Coarse ratios(0.1∼0.4), whereas che-mical components related to anthropogenic sources such as Br, V, Pb, and Zn were observed to accumulate in the fine fraction. In the Asian Dust Storm(ADS) event, the concentation of soil components increased dramatically. Reconstruction of the fine mass concentrations estimated by a newly revised simple model was fairly in good agreement with the measured ones. Source identification was attempted using the enrichment factor and Pearsons coefficient of correlation. The typical elements derived from each source could be classified by this method.

  • PDF

Characterization of Size Distribution and Water Solubility of 15 Elements in Atmospheric Aerosols

  • Park, Jeong-Ho;Sun, Jeong-Min;Park, Kum-Chan
    • Journal of Korean Society for Atmospheric Environment
    • /
    • 제17권E1호
    • /
    • pp.1-7
    • /
    • 2001
  • The elemental characteristics of atmospheric aerosols were investigated as a function of particle size and water solubility. The aerosol particles were samples at 12 individual size ranges between 0.01 and 30㎛. Collected aerosol particles were separated into both soluble and insoluble components. The concentrations of 15 elements in both components were determined by a PIXE analysis using a 2.0 MeV-proton beam. In general, the mass size distribution of particulate matter was represented as a bimodal distribution. The maximum rations of S in July and December were 5.5 and 3.8 %, and they appeared in the size range of 0.47∼1.17㎛(stage No. 6 or 7) . The ratios of a S at non-separated size were 3.1 and 2.2 % in July and December, respectively, On the other hand, the maximum rations of Si in July and December were 7.0 and 5.4% and they appeared in the size range of 5.1∼30㎛(stage No. 0∼2). The ratios of Si at the non-separated size were 2.1 and 1.8% in July and December, respectively, The mass diameter of 12 elements ranged between 0.59㎛ of S and 3.20 of Fe. More than 90% of atmospheric aerosols consisted of the light elements such as C, N, O, H and Al. The soluble component was dominant in the smaller size range and the insoluble component in the larger size range. Large portions of Si. Ti and Fe existed in insoluble state. By contrast, S, Cl, Ca, Zn and Br were dissolved in water.

Vapor Permeation Characteristics of TiO2 Composite Membranes Prepared on Porous Stainless Steel Support by Sol-Gel Method

  • Lee, Yoon-Gyu;Lee, Dong-Wook;Kim, Sang-Kyoon;Sea, Bong-Kuk;Youn, Min-Young;Lee, Kwan-Young;Lee, Kew-Ho
    • Bulletin of the Korean Chemical Society
    • /
    • 제25권5호
    • /
    • pp.687-693
    • /
    • 2004
  • Composite membranes with a titania layer were prepared by soaking-rolling method with the titania sol of nanoparticles formed in the sol-gel process and investigated regarding the vapor permeation of various organic mixtures. The support modification was conducted by pressing $SiO_2$ xerogel of 500 nm in particle size under 10 MPa on the surface of a porous stainless steel (SUS) substrate and designed the multi-layered structure by coating the intermediate layer of ${\gamma}-Al_2O_3$. Microstructure of titania membrane was affected by heat-treatment and synthesis conditions of precursor sol, and titania formed at calcination temperature of 300$^{\circ}C$ with sol of [$H^+$]/[TIP]=0.3 possessed surface area of 210 $m^2$/g, average pore size of 1.25 nm. The titania composite membrane showed high $H_2/N_2$ selectivity and water/ethanol selectivity as 25-30 and 50-100, respectively. As a result of vapor permeation for water-alcohol and alcohol-alcohol mixture, titania composite membrane showed water-permselective and molecular-sieve permeation behavior. However, water/methanol selectivity of the membrane was very low because of chemical affinity of permeants for the membrane by similar physicochemical properties of water and methanol.