The Optical Properties of SiO2/TiO2/ZrO2 Broadband Anti-reflective Multi-layer Thin Films Prepared by RF-Magnetron Sputtering (SiO2/TiO2/ZrO2 광대역 반사방지막의 제작 및 광학적 특성 분석)

  • Kang, M.I.;Ryu, J.W.;Kim, K.W.;Kim, C.H.;Baek, Y.K.;Lee, D.H.;Lee, S.R.
    • Journal of the Korean Vacuum Society
    • /
    • v.17 no.2
    • /
    • pp.138-147
    • /
    • 2008
  • $SiO_2/TiO_2/ZrO_2$ broadband anti-reflective multi-layer thin films were prepared at room temperature by RF sputtering system. Optical constants and structural properties on each layer of films were analyzed by spectroscopic ellipsometer and transmittance spectra of the films were measured by $UV-V_{is}$ spectrophotometer in the range of 300$\sim$900 nm. To evaluate the films, we compared the measured and analyzed spectra with designed spectra. We investigated influence of discrepancy of thickness and refractive indices of each layer on changes of the transmittance spectra. It was found that refractive indices and shape of dispersion of deposition materials are more contributed to changes of the transmittance spectra than thickness of layer.

THE EFFECTS OF SPURE AND INVENTS ON THE CASTING ACCURACY AND POROSITY OF TI-NI CASTINGS

  • Cho Lee-Ra;Yi Yang-Jin;Park Chan-Jin
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.41 no.3
    • /
    • pp.342-350
    • /
    • 2003
  • Statement of problem. Titanium-Nickel alloy might be used in various prosthetic restorations since it has a unique property such as super-elasticity and high fatigue resistance. However, little is known about the casting ability of this alloy. Purpose. This in vitro study compared the casting accuracy and the porosity made with different investments and various sprue designs to ascertain what casting condition would be better for the fabrication of Ti-Ni cast restorations. Material and methods. A total of 70 Ti-Ni alloy crowns were made and divided into 7 groups of 10 copings on a metal master die. For measuring the effect of the sprue numbers, two groups with one and two 8-gauge sprues were compared. Moreover, the results of the conventional sprue and the double thickness sprues were compared. Three investments were used; carbon free phosphate bonded investment, titanium investment and gypsum bonded investment. The cast restorations were evaluated at 48 points on the entire circumferential margin with a stereomicroscope measuring in micrometers. Each crown was radiographically examined for casting defects and porosity. Data on casting accuracy were analyzed using two-way and Post hoc Scheffe's comparison to determine whether significant differences existed at the 95% confidence level. Student-Newman-Keuls test were performed to identify significant differences in the number of voids. Results. The double sprueing group and double thickness group had significantly less marginal discrepancy than the single sprueing group (P<.05 and P<.01, respectively). The castings with phosphate bonded investment showed the least marginal discrepancy and the smoothest surface. The castings invested in the gypsum bonded investment had the greatest gaps in margin and the largest failure rate. The double sprueing group and phosphate bonded investment group had significantly smaller void numbers and smaller void size than the other groups. Conclusion. Within the limitations of this in vitro study, the casting accuracy of the groups using thicker, double sprue design and the phosphate bonded investment was significantly superior. Moreover, void number and size were less than other groups.

Characterization of Nitrogen-Doped $TiO_2$ Thin Films Prepared by Metalorganic Chemical Vapor Deposition (유기금속 화학 기상증착법으로 실리콘 기판위에 증착된 질소치환 $TiO_2$ 박막의 특성분석)

  • 이동헌;조용수;이월인;이전국;정형진
    • Journal of the Korean Ceramic Society
    • /
    • v.31 no.12
    • /
    • pp.1577-1587
    • /
    • 1994
  • TiO2 thin films with the substitution of oxygen with nitrogen were deposited on silicon substrate by metalorganic chemical vapor deposition (MOCVD) using Ti(OCH(CH3)2)4 (titanium tetraisopropoxide, TTIP) and N2O as source materials. X-ray diffraction (XRD) results indicated that the crystal structure of the deposited thin films was anatase TiO2 with only (101) plane observed at the deposition temperatures of 36$0^{\circ}C$ and 38$0^{\circ}C$, and with (101) and (200) plane at above 40$0^{\circ}C$. Raman spectroscopic results indicated that the crystal structure was anatase TiO2 in accordance with the XRD results without any rutile, fcc TiN, or hcp TiN structure. No fundamental difference was observed with temperature increase, but the peak intensity at 194.5 cm-1 increased with strong intensity at 143.0 cm-1 for all samples. The crystalline size of the films varied from 49.2 nm to 63.9 nm with increasing temperature as determined by slow-scan XRD experiments. The refractive index of the films increased from 2.40 to 2.55 as temperature increased. X-ray photoelectron spectroscopy (XPS) study showed only Ti 2s, Ti 2p, C 1s, O 1s and O 2s peaks at the surface of the film. The composition of the surface was estimated to be TiO1.98 from the quatitative analysis. In the bulk of the film Ti 2s, Ti 2p, O 1s, O 2s, N 1s and N 2s were detected, and Ti-N bonding was observed due to the substitution of oxygen with nitrogen. A satellite structure was observed in the Ti 2p due to the Ti-N bonding, and the composition of titanium nitride was determined to be about TiN1.0 from the position of the binding energy of Ti-N 2p3/2 and the quatitative analysis. The spectrum of Ti 2p energy level could be the sum of a 4, 5, or 6 Gaussian curve reconstruction, and the case of the sum of the 6 Gaussian curve reconstruction was physically most meaningful. From the results of Auger electron spectroscopy (AES), it was known that the composition was not varied significantly throughout the whole thickness of the film, and silicon oxide was not observed at the interface between the film and the substrate. The composition of the film was possible (TiO2)1-x.(TiN)x or TiO2-2xNx and in this experimental condition x was found to be about 0.21-0.16.

  • PDF

ANSYS Simulation of VHF Ceramic Resonator Using Thickness-longitudinal vibration mode (두께 진동모드를 이용한 고주파 세라믹 Resonator의 ANSYS Simulation)

  • 홍재일;윤현상;민석규;윤광희;류주현;김종선;박창엽
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.11a
    • /
    • pp.259-262
    • /
    • 2000
  • In this study, 3.1$\times$3.7$\times$0.365 $\textrm{mm}^2$ model of thickness-longitudinal vibration mode VHF ceramic resonator with (Pb,Ca)(Co,W,Ti)O$_3$ ceramics was simulated by ANSYS according to the electrode size. With the variations of electrode size of the model, fundamental and the third overtone dynamic ratio was investigated. At the ratio of electrode to model thickness(1/t) 2.5, third overtone dynamic ratio was largely increased. That model is suitable for 20 MHz resonator.

  • PDF

Effect of Overlayer Thickness of Hole Transport Material on Photovoltaic Performance in Solid-Sate Dye-Sensitized Solar Cell

  • Kim, Hui-Seon;Lee, Chang-Ryul;Jang, In-Hyuk;Kang, Wee-Kyung;Park, Nam-Gyu
    • Bulletin of the Korean Chemical Society
    • /
    • v.33 no.2
    • /
    • pp.670-674
    • /
    • 2012
  • The photovoltaic performance of solid-state dye-sensitized solar cells employing hole transport material (HTM), 2,2',7,7'-tetrakis-(N,N-di-p-methoxyphenyl-amine)-9,9'-spirobifluorene (spiro-MeOTAD), has been investigated in terms of HTM overlayer thickness. Two important parameters, soak time and spin-coating rate, are varied to control the HTM thickness. Decrease in the period of loading the spiro-MeOTAD solution on $TiO_2$ layer (soak time) leads to decrease in the HTM overlayer thickness, whereas decrease in spin-coating rate increases the HTM overlayer thickness. Photocurrent density and fill factor increase with decreasing the overlayer thickness, whereas open-circuit voltage remains almost unchanged. The improved photocurrent density is mainly ascribed to the enhanced charge transport rate, associated with the improved charge collection efficiency. Among the studied HTM overlayer thicknesses, ca. 230 nm-thick HTM overlayer demonstrates best efficiency of 4.5% at AM 1.5G one sun light intensity.

A Study on the EM Wave Absorber for Eliminating False Images in Collision-Avoidance Radar (충돌방지레이더의 허상방지용 전파흡수제에 관한 연구)

  • Choi, Chang-Mook;Lim, Bong-Taeck;Ahn, Yong-Woon
    • Proceedings of the Korean Institute of Information and Commucation Sciences Conference
    • /
    • 2008.05a
    • /
    • pp.117-120
    • /
    • 2008
  • In this paper, we developed the EM wave absorber for eliminating false images in collision-avoidance radar. First of all, we fabricated some samples in different composition ratio of $TiO_2$ and CPE. And the relative permittivities of samples are calculated from S-parameter of samples by using 1-port method. We designed and fabricated the EM wave absorber by using the calculated relative permittivity. As a result, the EM wave absorber with composition of $TiO_2$:CPE=70:30 wt% has thickness of 1.85 mm and absorption ability higher than 20 dB in the frequency range 76-77 GHz.

  • PDF

Creep Properties of Plasma Carburized and CrN Coated Ti-6Al-4V Alloy (플라즈마 침탄 및 CrN 코팅된 Ti-6Al-4V 합금의 구조 및 Creep특성)

  • Wey Myeong-Yong;Park Yong-Gwon
    • Korean Journal of Materials Research
    • /
    • v.14 no.8
    • /
    • pp.558-564
    • /
    • 2004
  • In order to improve the low hardness and low wear resistance of Ti-6Al-4V alloy, plasma carburization treatment and CrN film coating were carried out. Effects of the plasma carburization and CrN coating were analyzed and compared with the non-treated alloy by mechanical and creep tests. After plasma carburization and CrN coating treatments, the carburized layer was about 150 ${\mu}m$ in depth and CrN coated layer was about 7.5 ${\mu}m$ in thickness. Hardness value of about $H_{v}$ 402 of the non-treated alloy was improved to $H_{v}$ 1600 and 1390 by plasma carburization and CrN thin film coating, respectively. Stress exponent(n) was decreased from 9.10 in CrN coating specimen to 8.95 in carburized specimen. However, the activation energy(Q) was increased from 242 to 250 kJ/mol. It can be concluded that the static creep deformation for Ti-6Al-4V alloy is controlled by the dislocation climb over the ranges of the experimental conditions.

Microstructure of Glass-ceramics Made from Bottom Ash Produced at a Thermal Power Plant (화력발전소 바닥재로 제조된 결정화 유리의 미세구조)

  • Kang, Seung-Gu
    • Korean Journal of Materials Research
    • /
    • v.19 no.2
    • /
    • pp.95-101
    • /
    • 2009
  • Glass ceramics were made from coal bottom ash by adding CaO and $Li_2O$ as glass modifiers and $TiO_2$ as a nucleating agent in a process of melting and quenching followed by a thermal treatment. The surface of the glass ceramics has 1.6 times more $Li_2O$ compared to the inner matrix. When $TiO_2$ was not added or when only 2 wt% was added, the surface parts of the glass ceramics were crystalline with a thickness close to $130{\mu}m$. In addition, the matrixes showed only the glass phase and not the crystalline phase. However, doping of $TiO_2$ from 4 wt% to 10 wt% began to create small crystalline phases in the matrix with an increase in the quantity of the crystalline. The matrix microstructure of glass ceramics containing $TiO_2$ in excess of 8 wt% was a mixture of dark-gray crystalline and white crystalline parts. These two parts had no considerable difference in terms of composition. It was thought that the crystallization mechanism affects the crystal growth, direction and shape and rather than the existence of two types of crystals.

Annealing Effect on the Crystal Structure of $TiO_2$ Thin Film (이산화티타늄 박막의 열처리에 따른 결정구조 분석)

  • Kim, Seon-Hoon;Yang, Myung-Hak;Kim, Tae-Un;Ki, Hyun-Chul;Kim, Doo-Gun;Han, Myung-Soo;Ko, Hang-Ju;Kim, Hyo-Jin;Kim, Hwe-Jong
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2009.06a
    • /
    • pp.213-213
    • /
    • 2009
  • Titanium dioxide ($TiO_2$) thin films were prepared on glass substrates by ion-assisted electron-beam evaporation with 200nm thickness and subsequently crystallized by rapid thermal annealing at the rage of $200{\sim}700^{\circ}C$ in flowing $N_2$ gas. The crystal structure of the films were examined by X-ray diffractometer. As-deposited $TiO_2$ films were amorphous. After annealing, anatase and rutile phase of $TiO_2$ films were observed together.

  • PDF

Nozzle Clogging Mechanism in Continuous Casting for Titanium-Containing Steel (티타늄 첨가강의 연주 노즐막힘 기구)

  • Jung, Woo-Gwang;Kwon, Oh-Duck;Cho, Mun-Kyu
    • Korean Journal of Materials Research
    • /
    • v.19 no.9
    • /
    • pp.473-480
    • /
    • 2009
  • In order to provide the mechanism of nozzle clogging, recovered nozzles for high strength steel grade were examined carefully after continuous casting. The thickness of clogged material in SEN is increased in the following order: from the bottom to the top of the nozzle, upper part of slag line, and the pouring hole. Nozzle clogging material begins to form due the adhesion of metal to nozzle wall, the decarburization, and reduction of oxide in the refractory by Al and Ti in the melt. The reduction of oxide in the refractory by Al and Ti improves the wettability of the melt on the refractory and forms a thin Al-Ti-O layer. Metal containing micro alumina inclusions is solidified on the Al-Ti-O layer, and the solid layer grows due to the heat evolution through the nozzle wall. Thermodynamic calculation has been made for the related reactions. The effect of superheat to the nozzle clogging is discussed on ultra low carbon steel and low carbon steel.