Extraoral maxillofacial prostheses are essential for restoring facial structures that are lost as a result of congenital missing, injuries from accidents, surgical treatments of head and neck cancer. Recently, silicone is the most useful material for this purpose and is more advantageous than other maxillofacial prosthetic materials. However, there are some problems for long-term usage of silicone prostheses due to tear and color change. These are major contributing environmental factors to those problems that are such as ultraviolet light, cleansing agents, changes in humidity and successive adhesion and removal. The aim of this study is to evaluate the physical properties and color changes of maxillofacial prosthetic silicone material by those environmental factors using A-2186 silicone material (Factor II, USA) and two pigments, cadmium yellow medium and cosmetic red. Aluminium molds were fabricated according to the ASTM No. D412 & D624 specifications and resulted specimens from molds were fabicated and treated as follows. Control group and experimental I group were fabricated with 0.1% wt. pigment mixing in silicone elastomer and II-1 group, II-2 group of experimental II group were fabricated with 0.2%, 0.3% wt. pigment mixing in silicone elastomer, respectively. Control group was kept in darkroom at room temperature, I-1 group was kept under natural sunlight during 1week, I-2 group was soaked in 20% soap water during 1wk. I-3 group was successively adhered and removed 200 times on inner region of arm using Daro adhesive-33. Experimental II groups were kept in darkroom at room temperature. Instron universal testing machine was used to measure the % elongation, tensile strength, tear strength of control, experimental I, II groups and reflectance spectrophotometer(COLOR EYE-3000, Macbeth, USA) was used to measure the color differences between control group and experimental I group. The results were as follows : 1. When compared with control group, natural weathering group and 20% soap-water soaking group had no significant differences in % elongation(p>0.05). 2. 200 times successive adhesion and removal group, 0.2% wt. pigment group and 0.3% wt. pigment group had significant decreases in % elongation(p<0.05). 3. Natural weathering group, 20% soap-water soaking group and 200 times successive adhesion and removal group had no significant differences in tensile strength (p>0.05). 4. 0.2%, 0.3% wt. pigment groups had significant decreases in tensile strength(p<0.05). 5. Values of all experimental groups were decreased in tear strength. and 200 times successive adhesion and removal group had significant decrease in tear strength(p<0.05). 6. Natural weathering group and 20% soap-water soaking group had significant color differences(${\Delta}E$) and it could be detectable to naked eye(p<0.05). 7. Color differences between control group and 200 times adhesion and removal group were not detectable to the naked eye (${\Delta}E<1.0$).
This study was carried out to examine the effects of adding 0.3at.%Hf in Fe-30at.%Al-5at.%Cr alloy on the variation of microstructures and hot workability. The effect of hot rolling on mechanical properties was estimated by measuring the elongation and tensile strength after rolling at 800 and 1000 respectively. Microstructure of Fe-30at.%Al-5at.%Cr alloy was consisted of large equiaxed grains and it was changed to quasi-equiaxed or columnar structures by adding 0.3at.%Hf to Fe-30at.%Al-5at.%Cr alloy. Every specimens showed a decreased tensile strength after hot rolling compared to that of before rolling. The elongation was increased by hot rolling. Remarkable changes in elongation by hot rollong was observed such as from 1.4% to 4.5% elongation at the specimen of 0.3at.%Hf added to Fe-30at.%Al-5at.%Cr. Fe-30at.%Al-5at.%Cr alloy showed typical cleavage fracture on tensile failure and hot rolling has negligible effects on fracture mode in this alloy. However at the alloy containing Hf fracture mode was changed by hot rolling from intergranular to mixed intergranular and transgranular fracture mode.
The effect of aging treatment on the microstructure and mechanical properties of super duplex stainless steel with W was investigated. The phase was precipitated mainly at the early stage of aging and a lower aging temperature under $750^{\circ}C$, but the phase was formed after long-term aging treatment between $600^{\circ}C$ and $900^{\circ}C$. The volume fraction of the phase increased with aging temperature up to $750^{\circ}C$ and then decreased up to $900^{\circ}C$. With an increase in the aging time, the volume fraction phase at the early stage of aging increased slightly, and then increased rapidly beyond a certain time. The rapid increase in the tensile strength and hardness and decrease in the elongation and impact toughness were measured with aging temperatures up to $750^{\circ}C$. On the other hand, the tensile strength and hardness decreased slightly, and the elongation and Charpy impact toughness were unchanged with aging temperatures over $750^{\circ}C$. The tensile strength and hardness increased rapidly at the early stage of aging, and then increased slowly beyond a certain time. The elongation and Charpy impact toughness decreased rapidly at the early stage of aging, and then remained unchanged beyond a certain time. The phase that formed at the early stage of aging and the lower aging temperature had a considerable effect on the elongation and Charpy impact toughness of the super duplex stainless steel with W.
The effect of shield gas on the weldability, mechanical properties and formability of CO2 laser weld joint in 600MPa grade high strength steel was investigated. Bead on plate welds were made under various welding speed and shield gas. Tensile test was carried out under the load of perpendicular and parallel direction to the weld line, Formability of the joint was evaluated by Erichsen test. As the welding speed increases, the porosity fraction decreases. The porosity fraction in the joint used Ar-$50\%He$ mixed gas as a shield gas was lower than that of the joint used Ar gas. Hardness at the weld metal of full penetrated joint was nearly equal to that of water quenched raw metal. In a tensile test under a perpendicular load to the weld axis, strength and elongation of joint produced by optimum condition were nearly equal to those of base metal. However, the strength of joint in a tensile test under a parallel load to weld axis was higher than that of raw metal, but the elongation of joint was lower than that of raw metal. Elongation and formability were further increased by the method of using Ar+He mixed gas as a shield gas as compared with Ar gas. Formabilities of joints were recorded ranging from $58\%\;to\;70\%$ of that of base metal with different shield gases.
Journal of the Korean Applied Science and Technology
/
v.39
no.2
/
pp.161-168
/
2022
Unmodified castor oil (CO) was used to obtain a castor-based aqueous polyurethane (CPUD) and isophorone diisocyanate (IPDI) was used to obtain a transparent film. The mixing effect of polypropyleneglycole (PPG) was analyzed to increase flexibility. In addition, ethylenediamine (EDA) was used as a chain extender. Tensile strength, elongation, and abrasion resistance were measured according to the change according to the castor oil content and the change in the chain extender, respectively. The tensile strength of the sample containing a lot of castor oil was 1.112 kgf/㎟, and the elongation was 88%. The tensile strength of the sample containing a lot of chain extender was 3.33kgf/㎟, and the elongation was 99%. The surface strength was visually confirmed through SEM. The surface strength was visually confirmed through SEM.
The effect of carbides on the tensile properties in 0.5C-17Cr-0.5Ni martensitic stainless steel was studied. With the increase of austenitizing temperature, the volume fraction of residual carbide was decreased rapidly. In tempered specimens after quenching, the volume fraction of total carbide was decreased with the increase of austenitizing temperature. In tempered specimens after quenching, strength was decrease and elongation was increased with the increase of austenitizing temperature. Tensile strength was increase and elongation was decreased with the increase of volume fraction of residual and total carbides. With the increase of austenitizing temperature, the tensile properties of mod. 0.5C-17Cr-0.5Ni martensitic stainless was affected greatly by residual carbide than tempered carbide.
Effect of Fe and Mn contents on the tensile properties has been studied in Al-9wt%Si-0.3wt%Mg alloy. As Fe content of Al-9wt%Si-0.3wt%Mg-0.5wt%Mn alloy increased from 0.15wt% to 0.45wt%, tensile strength of as-cast alloy decreased from 192 MPa to 174 MPa, and elongation of the alloy also decreased from 4.8% to 4.2%. Decrease of these properties can be explained as the formation of plate shape, ${\beta}-Al_5FeSi$ phase with high Fe/Mn ratio of the alloy. However when Mn content of Al-9wt%Si-0.3wt%Mg-0.45wt%Fe alloy increased from 0.3wt% to 0.5wt%, tensile strength of T6 aged alloy increased from 265 MPa to 275 MPa, and elongation of the alloy increased from 2.3% to 3.6%. These improvements attribute to chinese script, ${\alpha}-Al_{15}(Mn,Fe)_3Si_2$ phase shape-modified from ${\beta}-Al_5FeSi$ phase with low Fe/Mn ratio of the alloy.
Proceedings of the Korean Powder Metallurgy Institute Conference
/
2006.09b
/
pp.1269-1270
/
2006
Mg-Zn-RE alloys had a novel lond period stacking ordered (LPO) structure. Their rapidly solidified powder metallurgy (RS P/M) alloys exhibited a combination of high strength and god ductility (tensile yield strength above 550 MPa and elongation above 5%). The LPO Mg-Zn-RE RS P/M alloys had high elevated temperature strength (tensile yield strength above 380 MPa at 473 K) and exhibited a high-strain-rate superplasticity at higher temperatures. In Japan, a national project for developing high strength LPO Mg-Zn-RE RS P/M alloys has started at 2003 for 5 years, which is founded by the Ministry of Economy, Trade and Industry (METI) of Japan. In the national project, project targets in materials performances have been achieved. The developed LPO Mg-Zn-RE RS P/M alloys exhibited higher tensile yield strength, fatigue strength and corrosion resistance than high strength aluminum alloys of extra-super-duralumin (7075-T6).
This study was carried out to investigate the effect of hot forging ratio and solution treatment temperature on the mechanical properties of incoloy 825 alloy. With an increasing of the hot forging ratio, grain size and range of grain size was decreased. With an increasing of the solution treatment temperature after 90% forging, grain size and range of grain size was increased. Cr carbides and Ti nitrides was precipitated at below $900^{\circ}C$ and volume fraction of precipitate was increased with an decreasing of the solution treatment temperature. With an increasing of the hot forging ratio, hardness, tensile strength and elongation, toughness was increased. With an increasing of the solution treatment temperature after 90% forging, hardness and strength was increased, elongation and toughness was decreased by grain refinement. With an increasing of the forging ratio, effect of solution treatment temperature on the hardness, strength and elongation was small, but on the toughness was large.
With the increasing interest in the expression of individuality and appearance of modern people, it is time to conduct research and development of novel hair coloring from various angles. Therefore, taking into account the order of discoloration of hair pigments, we selected a creative and novel emulsion as a novel material for hair coloring, rather than a cosmetic material such as hot water extract using natural products dealt with in previous studies, commercially available hair manicure, and oxidation hair dye for hair. Thus, the change in tensile strength and elongation of hair samples by color was studied. As a result of the study, hair with green emulsion paint had a significantly higher maximum load, maximum stress, maximum elongation and breaking load, breaking stress, breaking elongation values are shown. Maximum in terms of modulus, green emulsion applied hair and the control group were higher in the 0-15s strain and 15-145s sections, respectively, and the tangential modulus value was much higher in the control group than the experimental group hairs in all the 0-145s sections. This study, which analyzes the dynamic changes of hair samples that extend the daily color gamut, will greatly contribute to the development of innovative hair coloring materials in the research and production of hair beauty works, and it is judged that it will also contribute to the development of the beauty industry.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.