• Title/Summary/Keyword: Tensile strength test

Search Result 2,693, Processing Time 0.026 seconds

Tensile strain-hardening behaviors and crack patterns of slag-based fiber-reinforced composites

  • Kwon, Seung-Jun;Choi, Jeong-Il;Nguyen, Huy Hoang;Lee, Bang Yeon
    • Computers and Concrete
    • /
    • v.21 no.3
    • /
    • pp.231-237
    • /
    • 2018
  • A strain-hardening highly ductile composite based on an alkali-activated slag binder and synthetic fibers is a promising construction material due to its excellent tensile behavior and owing to the ecofriendly characteristics of its binder. This study investigated the effect of different types of synthetic fibers and water-to-binder ratios on the compressive strength and tensile behavior of slag-based cementless composites. Alkali-activated slag was used as a binder and water-to-binder ratios of 0.35, 0.45, and 0.55 were considered. Three types of fibers, polypropylene fiber, polyethylene (PE) fiber, and polyparaphenylene-benzobisethiazole (PBO) fiber, were used as reinforcing fibers, and compression and uniaxial tension tests were performed. The test results showed that the PE fiber series composites exhibited superior tensile behavior in terms of the tensile strain capacity and crack patterns while PBO fiber series composites had high tensile strength levels and tight crack widths and spacing distances.

A Study on the Estimation of Tensile Properties of High Performance Fiber Reinforced Cementitious Composites (고인성 시멘트복합체의 인장성능평가에 관한 연구)

  • Han, Byung-Chan;Kim, Jae-Hwan;Lim, Seung-Chan;Joen, Yong-Jae;Chung, Yun-Suk;Kwon, Young-Jin
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2006.05b
    • /
    • pp.357-360
    • /
    • 2006
  • In this study, it was proposed a direct tensile testing machine(DTTM) to be simple and to be applied to High Performance Fiber Reinforced Cementitious Composites(HPFRCCs), and it was examined the tensile properties of HPFRCCs by this machine. As a results, it was confirmed that a direct tensile test of HPFRCCs could be certainly carried out DTTM to be developed in this study. Also, tensile strength and yield strength of HPFRCCs were similar regardless of specimens thickness. And, all specimens revealed the stable strain-hardening behavior and multiple cracking in flexible and tensile loads. But, deviation of strain at ultimate tensile strength increased with the increase of specimen thickness.

  • PDF

Flexural Strengthening with Multi-Layer GFRP Sheets on Full-Scale RC Beams (유리섬유쉬트에 의한 실물모형 RC보의 보강매수별 휨 보강효과)

  • You, Young-Chan;Choi, Ki-Sun;Kim, Keung-Hwan
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2005.11a
    • /
    • pp.177-180
    • /
    • 2005
  • The specified tensile strength provided by the manufacturer is determined on the basis of the reliable lower limit ($X-3{\sigma}$ : X=average tensile strength, $\sigma$=standard deviation) obtained from the material test results. Most of these data, however, are based on the test results of 1 layer of FRP sheet. Also, the partial strength reduction factor for strengthening RC members with FRP is based on the small-scale model tests. But, the failure mechanisms of small-scale model tests are reported to be different from those of the full-scale tests. This paper present the test results of full-scale RC beams strengthened with multi-layer GFRP sheets up to 3 layer as well as the material tests. From the material tests, it was observed that the average tensile strengths of GFRP sheets are decreased as the number of layer are increased. Also the premature debonding failure of RC beams strengthened with multi-layer GFRP sheets are observed in inverse proportion to the number of GFRP sheets

  • PDF

On the material properties of shell plate formed by line heating

  • Lim, Hyung Kyun;Lee, Joo-Sung
    • International Journal of Naval Architecture and Ocean Engineering
    • /
    • v.9 no.1
    • /
    • pp.66-76
    • /
    • 2017
  • This paper is concerned with investigating the plastic material properties of steel plate formed by line heating method, and is aimed at implementing more rational design considering the accidental limit states such as collision or grounding. For the present study, line heating test for marine grade steel plate has been carried out with varying plate thickness and heating speed, and then microscopic examination and tensile test have been carried out. From the microscopic, it is found that the grain refined zones like ferrite and pearlite are formed all around the heat affected zone. From the tensile test results, it is seen that yield strength, tensile strength, fracture strain, hardening exponent and strength coefficient vary with plate thickness and heat input quantity. The formulae relating the material properties and heat input parameter should be, therefore, derived for the design purpose considering the accidental impact loading. This paper ends with describing the extension of the present study.

Comparison of Tensile Strengths in Granite Using Brazilian Tests and Hollow Cylinder Tests for Hydraulic Fracturing Test Interpretation (수압파쇄시험 해석을 위한 중공원통 인장시험과 압열인장시험 화강암 인장강도 비교)

  • Jo, Yeonguk;Chang, Chandong;Lee, Tae Jong;Kim, Kwang-Yeom
    • Tunnel and Underground Space
    • /
    • v.23 no.5
    • /
    • pp.362-371
    • /
    • 2013
  • We conducted hollow cylinder tensile strength tests and Brazilian tests in Seokmo granite to measure tensile strength necessary for estimating the magnitude of the maximum horizontal principal stress in hydraulic fracturing stress measurements. Two different pressurization rates were used in hollow cylinder tests. Tensile strengths were determined to be higher at higher pressurization rate, which suggests that tensile strength should be measurement at the same rate used in actual in situ hydraulic fracturing tests. Considering the effect of pressurization rate and specimen size on tensile strength, the hollow cylinder tests and Brazilian tests yield similar results each other. This demonstrates that Brazilian tests can be utilized to produce representative tensile strengths for interpretation of hydraulic fracturing test results.

Study of tensile behavior of Y shape non-persistent joint using experimental test and numerical simulation

  • Sarfarazi, V.;Hajiloo, M.;Ghalam, E. Zarrin;Ebneabbasi, P.
    • Computers and Concrete
    • /
    • v.26 no.6
    • /
    • pp.565-576
    • /
    • 2020
  • Experimental and discrete element methods were used to investigate the effects of angle of Y shape non-persistent joint on the tensile behaviour of joint's bridge area under brazilian test. concrete samples with diameter of 100 mm and thikness of 40 mm were prepared. Within the specimen, two Y shape non-persistent notches were provided. The large notch lengths were 6 cm, 4 cm and 2 cm. the small notch lengths were 3 cm, 2 cm and 1 cm. The angle of larger notch related to horizontal axis was 0°, 30°, 60°, 90°. Totally, 12 different configuration systems were prepared for Y shape non-persistent joints. Also, 18 models with different Y shape non-persistent notch angle and notch length were prepared in numerical model. The large notch lengths were 6 cm, 4 cm and 2 cm. the small notch lengths were 3 cm, 2 cm and 1 cm. The angle of larger notch related to horizontal axis was 0, 30, 60, 90, 120 and 150. Tensile strength of model materil was 1 MPa. The axial load was applied to the model by rate of 0.02 mm/sec. This testing showed that the failure process was mostly governed by the Y shape non-persistent joint angle and joint length. The tensile strengths of the specimens were related to the fracture pattern and failure mechanism of the discontinuities. It was shown that the tensile behaviour of discontinuities is related to the number of the induced tensile cracks which are increased by increasing the joint length and joint angle. The minimum tensile strength occurs when the angle of larger joint related to horizontal axis was 60°. Also, the maximum compressive strength occurs when the angle of larger joint related to horizontal axis was 90°. The tensile strength was decreased by increasing the notch length. The failure pattern and failure strength are similar in both methods i.e. the experimental testing and the numerical simulation methods.

Evaluation of High Temperature Tensile Properties in GTD-111DS (GTD-111DS 소재의 고온 인장 특성 평가)

  • Park H.S.;Kim H.I.;Lee Y.M.;Seok C.S.;Kim M.Y.
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2005.06a
    • /
    • pp.1358-1362
    • /
    • 2005
  • The Ni-base superalloy GTD-111DS was designed in the 1970s and is widely used as the material of the first stage blade under a severe combination of temperature and pressure in gas turbines. But because GTD-111DS is distributed in the shape of blade and blade has a unique figure and many cooling channels, it is hard to manufacture the test specimen. In this reason, there are little data on the microstructure and mechanical properties of the alloy. Therefore through the microstructure analysis, present paper observed that the shape of $\gamma{'}$ did not change even if aging time was increased but the amount and volume of the deposition of secondary $\gamma{'}\;rose\;and\;secondary\;\gamma{'}\;grew\;among\;primary\;\gamma{'}$. Also, by tensile test for different temperature, there was difference between yield strength and tensile strength in room temperature on heat treatment and extracting region but the more increasing temperature, the more decreasing difference between yield strength and tensile strength.

  • PDF

Effects of the Glass Fiber Characteristics on the Mechanical Properties of Thermoplastic Composite (유리섬유의 특성이 열가소성 복합재료의 기계적 성질에 미치는 영향)

  • Lee, Jung-Hui;Lee, Jeong-Gwon;Lee, Gyeong-Yeop
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.24 no.7 s.178
    • /
    • pp.1697-1702
    • /
    • 2000
  • This study has been performed to investigate the effects of glass fiber characteristics on the mechanical properties of thermoplastic composite. The surface of glass fiber was coated with the silan e to enhance the bonding strength between fiber and matrix. A micro-droplet pull-off test was performed to investigate the influence of the silane concentration on the bonding strength. The maximum bonding strength was observed around 10.8% silane concentration. In order to examine the influence of the fiber length and fiber content on the properties of the composite, the composite materials involving tile fiber lengths of 5mm, 10mm, 15mm 20mm, and 25mm were tested. The composites used contain 20%, 30%, and 40% by weight of glass fibers. Tension and flexural tests were performed to investigate their mechanical properties of the composites. The tensile strength and tensile modulus of the composite increase with increasing the glass fiber content. The tensile modulus increases slightly with increasing the fiber length. The maximum tensile strength is observed around the fiber length of 15-20mm. The flexural modulus and strength also increase slightly with increasing the fiber length.

Evaluation of tensile properties of SFRC for TBM tunnel segment (TBM 터널 세그먼트용 강섬유보강 콘크리트의 인장특성 평가)

  • Moon, Do-Young;Chang, Soo-Ho;Bae, Gyu-Jin;Lee, Gyu-Pil
    • Journal of Korean Tunnelling and Underground Space Association
    • /
    • v.14 no.3
    • /
    • pp.247-260
    • /
    • 2012
  • In order to reduce the amount of steel reinforcements in TBM tunnel segments, the use of Steel Fiber Reinforced Concrete(SFRC) is being tried. The steel fibers with higher aspect ratio than that used in tunnel shotcrete are preferred to compensate the deficiency in tensile strength of the segments. In this study, the tensile properties of SFRC with aspect ratio of steel fibers equal to 80 were evaluated through flexural test and Double Punch Test. In the results of flexural test, flexural strengths of the SFRC were increased about 30%~150% thanks to bond of steel fibers used to concrete and could be properly predicted by the equation proposed by Oh(2008). There was a great difference in the estimated direct tensile strengths of the SFRC by the equations presented in ACI and RILEM. It was found that the Double Punch Test could be suitable methodology to estimate the direct tensile strength presented in RILEM of the SFRC.

Formula to identify the Influence of steel fibres on the mechanical properties of HPC

  • Philip, Nivin;Anil, Sarah
    • Computers and Concrete
    • /
    • v.25 no.5
    • /
    • pp.479-484
    • /
    • 2020
  • This work performed to analyses the impact of hooked end steel fibres on the mechanical properties of high performance concrete. The mechanical properties considered incorporate compressive strength, split tensile strength and flexural strength. Taking in to thought parameters, such as, volume fraction of fibres, fibre aspect ratio and grade of concrete, a logical strategy called Taguchi technique was utilized to discover the ideal blend of factors. L9 Orthogonal Array (OA) of Taguchi network comprising of three variables and three dimensions is utilized in this work. The evaluations of concrete considered were M60, M80 and M100. M60 contained 15% of metakaolin as bond swap though for M80 it was 5% of metakaolin and for M100 it was 10% metakaolin and 10% of silica smolder. The volume portion of fiber was fluctuated by 0.5%; 1% and 1.5% and the viewpoints proportions considered were 50, 60 and 80. The test outcomes demonstrate that incorporation of steel fibres enhance significantly the the strength characteristics of concrete, predominantly the splitting tensile strength and flexural strength. In light of relapse investigation of the test information scientific models were produced for compressive strength, split tensile strength and flexural strength of the steel fibre-reinforced high performance concrete.