• 제목/요약/키워드: Tensile strain hardening

검색결과 258건 처리시간 0.025초

고인성 내화보수모르터(FR-ECC)를 활용한 RC 구조물 보수공법의 내구성능 및 내하력에 관한 실험적 연구 (An Experimental Study on the Durability and Load Carrying Capacity of RC Structure Repair System Using FR-ECC)

  • 김정희;임승찬;김재환;권영진
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제16권2호
    • /
    • pp.75-86
    • /
    • 2012
  • 본 논문에서는 FR-ECC의 수축특성과 균열도입 전후의 내동해성을 평가하였으며, FR-ECC를 활용한 다층복공구조의 지수성능과 박리박락저항성, 또한 FR-ECC로 단면복구 된 보부재의 휨성능을 평가하였다. 그 결과, FR-ECC는 소성수축에 의한 균열 및 건조수축에 의한 길이변화율이 기존의 보수모르터에 비해 크게 저감되었으며, 구속상태에서의 건조수축에 대한 균열저항성이 개선됨을 알 수 있었다. 또한, FR-ECC는 내동해성이 매우 우수하였으며, 균열도입 후에도 동결융해작용에 의한 인장성능의 저하는 확인되지 않았다. 한편, FR-ECC로 보수된 휨부재는 초기균열모멘트, 항복모멘트 및 극한모멘트 등의 휨성능이 증대되었으며, 멀티플크랙 특성에 의해 휨파괴시까지 균열폭을 안정적으로 제어할 수 있었다.

Experimental and analytical study on RC beam reinforced with SFCB of different fiber volume ratios under flexural loading

  • Lin, Jia-Xiang;Cai, Yong-Jian;Yang, Ze-Ming;Xiao, Shu-Hua;Chen, Zhan-Biao;Li, Li-Juan;Guo, Yong-Chang;Wei, Fei-Fei
    • Steel and Composite Structures
    • /
    • 제45권1호
    • /
    • pp.133-145
    • /
    • 2022
  • Steel fiber composite bar (SFCB) is a novel type of reinforcement, which has good ductility and durability performance. Due to the unique pseudo strain hardening tensile behavior of SFCB, different flexural behavior is expected of SFCB reinforced concrete (SFCB-RC) beams from traditional steel bar reinforced concrete (S-RC) beams and FRP bar reinforced concrete (F-RC) beams. To investigate the flexural behavior of SFCB-RC beam, four points bending tests were carried out and different flexural behaviors between S/F/SFCB-RC beams were discussed. An flexural analytical model of SFCB-RC beams is proposed and proved by the current and existing experimental results. Based on the proposed model, the influence of the fiber volume ratio R of the SFCB on the flexural behavior of SFCB-RC beams is discussed. The results show that the proposed model is effective for all S/F/SFCB-RC flexural members. Fiber volume ratio R is a key parameter affecting the flexural behavior of SFCB-RC. By controlling the fiber volume ratio of SFCB reinforcements, the flexural behavior of the SFCB-RC flexural members such as bearing capacity, bending stiffness, ductility and repairability of SFCB-RC structures can be designed.

원전 1차 계통수 모사환경에서 Type 304 스테인리스강의 응력부식균열개시 민감도 (Susceptibility of Stress Corrosion Crack Initiation of Type 304 SS in Simulated Primary Water Environment of PWR)

  • 조성환;김성우;이종연
    • 한국압력기기공학회 논문집
    • /
    • 제20권1호
    • /
    • pp.25-31
    • /
    • 2024
  • The core shroud of rector vessel internals (RVI) of OPR1000 and ARP1400 is made of Type 304 stainless steel (SS) by bending and welding process that may induce high deformation and residual stress in manufacturing. This work aims to evaluate the susceptibility of stress corrosion crack (SCC) initiation of bent parts of RVI in high temperature primary water environment. For SCC initiation test, tensile specimens were fabricated from the 90 degree bent plate of Type 304 SS (DT specimen), that is an archived part of a Korean APR1400. After the SCC initiation test, the specimen surface was thoroughly examined by optical and scanning electron microscopy, and compared to the specimen fabricated from the as-received plate of Type 304 SS (AR specimen). The surface observation revealed that SCC initiated on the AR specimen surface in typical intergranular (IG) mode, while SCC on the DT specimen occurred in transgrannular mode as well as IG mode. It was also found that the size and number of SCC on the DT specimen were larger than that on the AR specimen. This was attributable to a strain-hardening during the bending process. To compare the susceptibility of SCC initiation, total crack density (TCD) was calculated from the total crack length divided by the measured area of AR and DT specimens. TCD of DT specimen was 4.6 times higher than AR specimen in average, indicating that higher possibility of degradation of bent parts of RVI for a long-term operation.

에폭시 수지 모르터의 특성에 관한 실험적 연구 (Experimental Studies on the Properties of Epoxy Resin Mortars)

  • 연규석;강신업
    • 한국농공학회지
    • /
    • 제26권1호
    • /
    • pp.52-72
    • /
    • 1984
  • This study was performed to obtain the basic data which can be applied to the use of epoxy resin mortars. The data was based on the properties of epoxy resin mortars depending upon various mixing ratios to compare those of cement mortar. The resin which was used at this experiment was Epi-Bis type epoxy resin which is extensively being used as concrete structures. In the case of epoxy resin mortar, mixing ratios of resin to fine aggregate were 1: 2, 1: 4, 1: 6, 1: 8, 1:10, 1 :12 and 1:14, but the ratio of cement to fine aggregate in cement mortar was 1 : 2.5. The results obtained are summarized as follows; 1.When the mixing ratio was 1: 6, the highest density was 2.01 g/cm$^3$, being lower than 2.13 g/cm$^3$ of that of cement mortar. 2.According to the water absorption and water permeability test, the watertightness was shown very high at the mixing ratios of 1: 2, 1: 4 and 1: 6. But then the mixing ratio was less than 1 : 6, the watertightness considerably decreased. By this result, it was regarded that optimum mixing ratio of epoxy resin mortar for watertight structures should be richer mixing ratio than 1: 6. 3.The hardening shrinkage was large as the mixing ratio became leaner, but the values were remarkably small as compared with cement mortar. And the influence of dryness and moisture was exerted little at richer mixing ratio than 1: 6, but its effect was obvious at the lean mixing ratio, 1: 8, 1:10,1:12 and 1:14. It was confirmed that the optimum mixing ratio for concrete structures which would be influenced by the repeated dryness and moisture should be rich mixing ratio higher than 1: 6. 4.The compressive, bending and splitting tensile strenghs were observed very high, even the value at the mixing ratio of 1:14 was higher than that of cement mortar. It showed that epoxy resin mortar especially was to have high strength in bending and splitting tensile strength. Also, the initial strength within 24 hours gave rise to high value. Thus it was clear that epoxy resin was rapid hardening material. The multiple regression equations of strength were computed depending on a function of mixing ratios and curing times. 5.The elastic moduli derived from the compressive stress-strain curve were slightly smaller than the value of cement mortar, and the toughness of epoxy resin mortar was larger than that of cement mortar. 6.The impact resistance was strong compared with cement mortar at all mixing ratios. Especially, bending impact strength by the square pillar specimens was higher than the impact resistance of flat specimens or cylinderic specimens. 7.The Brinell hardness was relatively larger than that of cement mortar, but it gradually decreased with the decline of mixing ratio, and Brinell hardness at mixing ratio of 1 :14 was much the same as cement mortar. 8.The abrasion rate of epoxy resin mortar at all mixing ratio, when Losangeles abation testing machine revolved 500 times, was very low. Even mixing ratio of 1 :14 was no more than 31.41%, which was less than critical abrasion rate 40% of coarse aggregate for cement concrete. Consequently, the abrasion rate of epoxy resin mortar was superior to cement mortar, and the relation between abrasion rate and Brinell hardness was highly significant as exponential curve. 9.The highest bond strength of epoxy resin mortar was 12.9 kg/cm$^2$ at the mixing ratio of 1:2. The failure of bonded flat steel specimens occurred on the part of epoxy resin mortar at the mixing ratio of 1: 2 and 1: 4, and that of bonded cement concrete specimens was fond on the part of combained concrete at the mixing ratio of 1 : 2 ,1: 4 and 1: 6. It was confirmed that the optimum mixing ratio for bonding of steel plate, and of cement concrete should be rich mixing ratio above 1 : 4 and 1 : 6 respectively. 10.The variations of color tone by heating began to take place at about 60˚C, and the ultimate change occurred at 120˚C. The compressive, bending and splitting tensile strengths increased with rising temperature up to 80˚ C, but these rapidly decreased when temperature was above 800 C. Accordingly, it was evident that the resistance temperature of epoxy resin mortar was about 80˚C which was generally considered lower than that of the other concrete materials. But it is likely that there is no problem in epoxy resin mortar when used for unnecessary materials of high temperature resistance. The multiple regression equations of strength were computed depending on a function of mixing ratios and heating temperatures. 11.The susceptibility to chemical attack of cement mortar was easily affected by inorganic and organic acid. and that of epoxy resin mortar with mixing ratio of 1: 4 was of great resistance. On the other hand, when mixing ratio was lower than 1 : 8 epoxy resin mortar had very poor resistance, especially being poor resistant to organicacid. Therefore, for the structures requiring chemical resistance optimum mixing of epoxy resin mortar should be rich mixing ratio higher than 1: 4.

  • PDF

상온과 316℃에서 SA508 Gr.1a 저합금강 배관과 TP316 스테인리스강 배관의 변형거동에 미치는 하중속도의 영향 (Effect of Loading Rate on the Deformation Behavior of SA508 Gr.1a Low Alloy Steel and TP316 Stainless Steel Pipe Materials at RT and 316℃)

  • 김진원;최명락
    • 대한기계학회논문집A
    • /
    • 제39권4호
    • /
    • pp.383-390
    • /
    • 2015
  • 본 논문에서는 원전 배관 재료의 변형거동에 미치는 하중속도의 영향을 파악하기 위해서, SA508 Gr.1a 저합금강과 SA312 TP316 스테인리스강 배관재를 대상으로 상온과 원전 운전온도인 $316^{\circ}C$에서 다양한 변형률 속도로 인장시험을 수행하였다. 시험 결과, 상온에서는 두 배관재의 변형거동이 일반적인 하중속도 의존성을 보였다. 즉, 하중속도가 증가함에 따라 강도는 증가하고 연성은 감소하는 경향을 보였다. 그러나, $316^{\circ}C$에서는 하중속도가 증가함에 따라 SA508 Gr.1a 저합금강의 강도와 연신률이 모두 감소하였고 단면수축률은 감소 후 증가하는 비선형 거동을 보였다. SA312 TP316 스테인리스강의 강도, 연신률, 그리고 단면수축률은 하중속도에 관계없이 거의 일정한 값을 보였다. 시험 온도에 관계없이 SA508 Gr.1a 저합금강의 가공경화능력은 하중속도에 거의 영향을 받지 않았으나, SA312 TP316 스테인리스강에서는 하중속도가 증가함에 따라 가공경화능력이 감소하였다.

GFRP로 구속된 원형단면 콘크리트 단주의 강도 및 변형 능력 (Strength and Deformation Capacities of Short Concrete Columns with Circular Section Confined by GFRP)

  • 조순호
    • 콘크리트학회논문집
    • /
    • 제19권1호
    • /
    • pp.121-130
    • /
    • 2007
  • 본 연구에서는 FRP(fiber reinforced polymer) 합성재료에 의하여 콘크리트를 구속할 시 예상되는 콘크리트의 강도 및 변형 능력의 향상 효과를 알아보기 위하여 섬유 량 혹은 방향, 단부하중조건에 따른 wrap 혹은 튜브형의 구속형태, 반원형 쉘 및 수직 이음부의 유무에 따른 연속 및 불연속 구속 형태 등을 주요 변수로 한 총 36개의 원형단주 시험체에 대하여 단조가력 실험을 수행하였다. 여러 구속 방법에 따른 FRP의 파단변형률에 대하여서도 주의를 가지고 조사하였다. 구속된 콘크리트의 최대 강도 및 변형률을 산정하기 위하여 기존에 제시된 다양한 배경의 예측 식들에 대하여 검토하였으며, 이들에 의한 예측치와 실험치를 비교, 분석하였다. 구속되지 알은 콘크리트와 비교하여, CW 및 CF형은 매우 큰 강도 및 변형능력의 증가를 나타냈으며, 수직 이음부를 갖는 CP형은 폭발적으로 파괴하였으며, 보다 작은 강도 및 변형능력의 증가가 관측되었다. 대체로, 모든 시험체는 2선 선형관계의 응력-변형률 거동을 나타냈으며, 후반부의 변형경화 정도는 구속매체의 강성에 따라 결정되었다. 모든 시험체에서 관측된 FRP의 파단변형률은 인장시험편으로부터 획득한 극한변형률보다 정도에 따라서는 매우 작았다. 대체로, 기존 예측식들은 본 실험의 최대 강도 및 변형률을 과대평가 하였으며, 변형률 예측은 매우 산란된 분포를 나타냈다. 또한, 본 연구의 실험 결과에 근거하여 구속 콘크리트의 최대 강도 및 변형률을 보다 정확하게 예측할 수 있는 설계 목적의 단순식을 제안하였다. 강도식은 모어-쿨롱 파괴 기준을 사용하여 유도하였으며, 변형률식은 비구속 콘크리트를 주요 영향 요소로 포함하여 실험 결과를 fitting하였다./TEX> = 분광광도법으로 측정한 점토함량(%); $x_2$ = 유기물 함량($g{\cdot}kg^{-1})$)이었으며, 상관계수는 $0.984^{**}$로 두 방법사이에 높은 상관관계가 있는 것으로 조사되었다. 여기서 유도된 회귀방정식을 프로그램화하여 컴퓨터나 분석기기에 입력시 시간과 공간을 절약하고 신속하고 정확하게 점토함량을 분석할 수 있을 것으로 판단된다.119>잠118>잠107>잠117>잠113 순이었고, 웅견층중에서는 잠114>잠108>잠120>잠117>잠118>잠107>잠119>잠119>잠113 순이었다. 자견층 비율에서는 광의의 귀전력이 협의의 귀전력보다 컸고, 웅견층 비율에서는 같았다, 견층 비율에서는 일반조합 능력은 크게 나타났으나, 특정조합 능력과 상반조직 능력은 나타나지 않았다. 자견층 비율에서 교배친의 우성효과는 컸다. 자견층 비율에서는 교배친의 우성효과는 적었다. 자웅견층 비율의 잡종 강세는 적게 나타났다. 환경변이와 상가적 작계는 자웅견층 비율에서는 크게 나타났다. 우성의 방향은 자견층 비율에서는 정의 방향으로 우성 귀전자가 크게 작용하였으며, 자견층 비율에서는 정의 방향으로 우성 귀전자가 부분적으로 작용하였다. 교배친의 자견층 비율의 우성순서는 잠117>잠114>잠108>잠120>잠118>잠119>잠107>잠113 순이었고, 자견층 비율에서는 잠114>잠117>잠108>잠118>잠107>잠119>잠113>잠120의 순이었다.지방산의 조성이 많은 차이를 보였다.{2+}$ 26 및 $Na^+$ 26 mg $L^{-1}$이었다. 양액 재배 후 버려지는 폐양액 중의 무기성분 함량은

고로슬래그 미분말이 혼입된 자기충전 및 숏크리트용 ECC의 개발을 위한 시멘트풀 레올로지 제어 (Rheology Control of Cement Paste for Applying ECC Produced with Slag Particles to Self-Consolidating and Shotcreting Process)

  • 박승범;김정수;김윤용
    • 콘크리트학회논문집
    • /
    • 제20권1호
    • /
    • pp.67-75
    • /
    • 2008
  • 마이크로역학을 기초로 하여 Slag-ECC (고로슬래그 미분말이 혼입된 ECC)가 개발되었으며, 기존의 연구에서는 Slag-ECC가 높은 연성을 나타내도록 마이크로역학을 도입하여 재료의 배합비가 제시되었다. 이 연구에서는 Slag-ECC의 자기충전과 숏크리트 시공성을 구현하기 위하여, Slag-ECC의 기본 배합에 혼화재료의 투입 순서에 상관없이 혼화재료를 한번에 투입하여 유동 특성을 제어하는 레올로지 개념을 도입하였으며, 이는 현장에서 시공성을 높이기 위하여 모든 재료를 분말의 형태로 사용하는 프리팩키지화를 위한 기초 자료로 사용될 것이다. 그리고 자기충전과 숏크리트의 서로 상반되는 레올로지 특성을 구현하기 위하여, 시멘트풀 레올로지 경시 변화 연구를 통해 대략적인 혼화재료의 첨가량을 선정하였고, 자기충전 및 숏크리트의 시공성 검증을 통해 재료의 배합비를 최적화 하였다. 개발된 Slag-ECC의 자기충전성과 숏크리트 적합성은 실험을 통하여 입증되었으며, 자기충전 및 숏크리트의 시공 방법에 의하여 타설된 재료가 굳은 이후에도 Slag-ECC의 역학적 특성인 고인성 특성을 유지하는 것으로 나타났다. 따라서 시멘트풀의 레올로지 특성을 조절하여 개발된 자기충전용 Slag-ECC와 숏크리트용 Slag-ECC는 재료의 고인성 특성을 유지하면서 다양한 현장 적용이 가능할 것으로 판단된다.

고강도 강재보의 비탄성 횡-비틀림좌굴 제어를 위한 횡지지 거리 (Laterally Unbraced Length for Preventing Inelastic Lateral-Torsional Buckling of High-Strength Steel Beams)

  • 박창희;이철호;한규홍;김진호;이승은;하태휴;김진원
    • 한국강구조학회 논문집
    • /
    • 제25권2호
    • /
    • pp.115-130
    • /
    • 2013
  • 본 연구에서는 공칭인장강도 800MPa를 지니는 고강도 강재로 조립된 H형강보의 횡지지거리에 따른 횡비틀림 좌굴강도를 현행 강구조설계기준(KBC 2009, AISC-LRFD 2010)을 바탕으로 평가하였다. 현행 기준은 고강도 강재와 응력도-변형도 특성이 확연히 다른 항복강도 350MPa 이하의 일반강을 전제로 정립된 것으로서, 고강도 강재에 대한 현행 기준의 적합성 여부가 우선 검토되어야 한다. 본 연구의 실험체는 모두 컴팩트 단면으로서 춤-폭비(H/B) 1.7을 갖는 실험군 A(상대적 뒤틀림 강성을 통한 모멘트전달이 작은 경우)와 2.7을 갖는 실험군 B(상대적으로 모멘트전달에 뒤틀림 강성 크게 기여하는 경우)로 구성하였다. 항복 이후의 응력도-변형도 특성의 영향을 받는 비탄성 횡좌굴 거동이 유발되도록 횡지지거리를 제어하면서 횡지지 구간 내에 균등모멘트가 작용하도록 가력하였다. 두 실험군 모두 현행 기준에 요구하는 강도를 충분히 상회하였고, 특히 뒤틀림 거동을 통한 모멘트전달이 크지 않은 실험군 A의 일부실험체는 소성설계에서 요구하는 수준의 회전능력까지 발휘하였다. 이들 실험결과는 현행 기준을 고강도 강재에 보수적으로 확대하여 적용할 수 있음을 보여준다. 실험결과를 좀더 심층적으로 분석하기 위해 일반강 및 고강도강의 응력도-변형도 특성을 고려한 H형강보의 횡지지거리에 따른 비탄성 횡좌굴강도 산정식을 유효접선계수를 반영하여 해석적으로 유도하였다. 이를 통해 소재의 항복강도와 탄성계수만을 고려하여 산정되는 현행 기준의 소성횡지지거리($L_p$) 제한식은, 항복참(yield plateau)없이 즉시 변형경화하는 고강도 강재에 적용하는 경우 보수적인 결과로 귀결됨을 입증하였다. 비탄성 횡좌굴 제어를 위한 횡지지거리는 소재의 항복강도 뿐만 아니라 항복 이후의 변형경화특성까지 반영하여 정의되는 타당하므로 이에 대한 개선의 필요성이 있다.