Mechanical strengths of self compacting concrete containing sawdust-ash and naphthalene sulfonate

  • Elinwa, Augustine U.;Mamuda, Mamuda;Ahmed, M.
    • Advances in concrete construction
    • /
    • v.2 no.4
    • /
    • pp.301-308
    • /
    • 2014
  • The present research work is on the effect of sawdust ash (SDA) on the mechanical strengths of self compacting concrete (SCC) using naphthalene sulfonate (NS) as a plasticizer. Experiments on compressive, flexural and splitting tensile strengths are conducted and the data analyzed using the Minitab 15 software. The results showed that SDA can defer the reaction of cement hydration and prolong the setting times of cement paste. This was very much pronounced on the flexural and splitting tensile strengths at 90 days of curing which are 36 % and 33 % higher than the control strengths, respectively. The study has proposed strength relations of mortar compressive strength with the flexural and splitting tensile strengths and these are, 5 and 7 times respectively. The flexural strength is 1.5 times that of the splitting tensile. Finally, linear models were developed on these relationships.

Measurement of Tensile Strength by Diametral Compression of Ring-type Specimen (원환형 시험편을 이용한 간접인장실험에 관한 연구)

  • 이기락;김종우
    • Tunnel and Underground Space
    • /
    • v.7 no.3
    • /
    • pp.221-229
    • /
    • 1997
  • Disc-type and ring-type specimens of four different materials were tested to investigate the tensile characteristics and their brief results are presented. Materials tested were marble, granite, cement mortar and plaster. Unizxial tensile strengths are compared with Brazilian and ring test strengths. It was found that Brazilian strengths were usually greater than uniaxial tensile strengths and affected by loading rates. In the ring tests, tensile strengths were generally found to be decreased as relative hole radius being increased. Ring test strengths, however, converged to some value in r$\geq$0.45 of marble, r$\geqq$0.29 of cement mortar and r$\leq$0.5 of plaster specimens. In such range of r, furthermore, transverse cracking of specimens were observed.

  • PDF

Investigations on the tensile strength of high-performance fiber reinforced concrete using statistical methods

  • Ramadoss, P.;Nagamani, K.
    • Computers and Concrete
    • /
    • v.3 no.6
    • /
    • pp.389-400
    • /
    • 2006
  • This paper presents the investigations towards developing a better understanding on the contribution of steel fibers on the tensile strength of high-performance fiber reinforced concrete (HPFRC). An extensive experimentation was carried out with w/cm ratios ranging from 0.25 to 0.40 and fiber content ranging from zero to 1.5 percent with an aspect ratio of 80. For 32 concrete mixes, flexural and splitting tensile strengths were determined at 28 days. The influence of fiber content in terms of fiber reinforcing index on the flexural and splitting tensile strengths of HPFRC is presented. Based on the test results, mathematical models were developed using statistical methods to predict 28-day flexural and splitting tensile strengths of HPFRC for a wide range of w/cm ratios. The expressions, being developed with strength ratios and not with absolute values of strengths and are applicable to wide range of w/cm ratio and different sizes/shapes of specimens. Relationship between flexural and splitting tensile strengths has been developed using regression analysis and absolute variation of strength values obtained was within 3.85 percent. To examine the validity of the proposed model, the experimental results of previous researchers were compared with the values predicted by the model.

The Strength Properties of Jumchi-Hanji Papers Dyed with Persimmon Juice (감물염색가공에 따른 줌치한지 종이소재의 강도 변화 -감물염색가공 여부와 감물농도 차이에 따른 변화-)

  • Hong, Heesook;Kim, Gi-Eok
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.42 no.2
    • /
    • pp.224-236
    • /
    • 2018
  • This study analyzed differences between Jumchi-Hanji papers not dyed and dyed with persimmon juice (50% concentration) in five strength properties (tensile, wet tensile, tearing, bursting, and folding strengths). For the analysis, the undyed and the dyed Jumchi-Hanji papers were made by Jumchichigi during 40 minutes and made with the Dakji of different layer (a layer, two layers) and Choji method (Oebal-teugi, Ssangbal-teugi). Differences between Jumchi-Hanji papers dyed with the different concentration of persimmon juice (20% vs 70%) in the five strengths were also identified. For this examination, Jumchi-Hanji papers were made with two layer Dakji (Oebal-teugi Choji method) and by Jumchichigi during 60 minutes. Jumchi-Hanji papers made in this study were used as test samples. As a result, Jumchi-Hanji papers dyed with persimmon juice had higher tensile strength (CD), wet tensile strength (MD, CD), and bursting strength than those of undyed Jumchi-Hanji papers. However, tearing strengths (MD, CD) of dyed Jumchi-Hanji papers were lower than undyed Jumchi-Hanji papers. Folding strengths (CD) of dyed Jumchi-Hanji papers were low but the folding strengths (MD) of them were high compared to undyed Jumchi-Hanji papers. In addition, the concentration of persimmon juice influenced the five strength properties of Jumchi-Hanji. The tensile, wet tensile, and bursting strengths of Jumchi-Hanji papers dyed with a 70% concentration were higher than those one of Jumchi-Hanji papers dyed with a 30% concentration while the tearing and folding strengths of Jumchi-Hanji papers dyed with a 70% concentration were lower than Jumchi-Hanji papers dyed with a 30% concentration.

Effect of Persimmon Juice Dyeing on Strength Properties of Jumchi-Hanjis Mixed with Korean and Thai Mulberry Fibers and Wood Pulp (국내산과 태국산 닥섬유 및 목재펄프가 혼합된 줌치한지의 감물염색에 따른 강도 특성)

  • Hong, Heesook;Kim, Gi-Eok;Koh, Jungnye
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.45 no.6
    • /
    • pp.1035-1051
    • /
    • 2021
  • This study compares the strength properties of Jumchi-Hanjis dyed with 70% and 100% persimmon juice concentrations and undyed Jumchi-Hanjis. The Juumchi-Hanjis were made from Dakjis (mulberry papers), which were mixed with different ratios of fibers from paper mulberries originating in Korea and Thailand, including wood pulp from Canada. Research results showed that tensile, wet tensile, and bursting strengths of Jumchi-Hanjis dyed with 70% concentration were higher than those of undyed Jumchi-Hanjis. However, the tearing strengths of the dyed Jumchi-Hanjis were lower than those of undyed Jumchi-Hanjis. The wet tensile strengths of Jumchi-Hanjis dyed with 100% concentration were higher than those of dyed with 70% concentration. The increase and decrease of tensile, tearing, and bursting strengths depending on persimmon juice dyeing differed as per the mixing ratio of the raw materials of Jumchi-Hanjis. Dyeing with 100% persimmon juice concentration tends to be more useful than 70% to increase the tensile (MD) and wet tensile strengths of Jumchi-Hanjis containing only Korean mulberry fibers (90%) and wood pulp (10%) as raw materials. Dyeing with 100% concentration tends to be less useful than 70% to increase the tensile, tearing and bursting strengths of Jumchi-Hanjis with high proportions (90% or 60%) of mulberry fibers from Thailand.

Application of the full factorial design to modelling of Al2O3/SiC particle reinforced al-matrix composites

  • Altinkok, Necat
    • Steel and Composite Structures
    • /
    • v.21 no.6
    • /
    • pp.1327-1345
    • /
    • 2016
  • $Al_2O_3$/SiC particulate reinforced (Metal Matrix Composites) MMCs which were produced by using stir casting process, bending strength and hardening behaviour were obtained using an analysis of variance (ANOVA) technique that uses full factorial design. Factor variables and their ranges were: particle size $2-60{\mu}m$; the stirring speed 450 rpm, 500 rpm and the stirring temperature $620^{\circ}C$, $650^{\circ}C$. An empirical equation was derived from test results to describe the relationship between the test parameters. This model for the tensile strength of the hybrid composite materials with $R^2$ adj = 80% for the bending strength $R^2$ adj = 89% were generated from the data. The regression coefficients of this model quantify the tensile strength and bending strengths of the effects of each of the factors. The interactions of all three factors do not present significant percentage contributions on the tensile strength and bending strengths of hybrid composite materials. Analysis of the residuals versus was predicted the tensile strength and bending strengths show a normalized distribution and thereby confirms the suitability of this model. Particle size was found to have the strongest influence on the tensile strength and bending strength.

Establishment of the design stress intensity value for the plate-type fuel assembly using a tensile test

  • Kim, Hyun-Jung;Tahk, Young-Wook;Jun, Hyunwoo;Kong, Eui-Hyun;Oh, Jae-Yong;Yim, Jeong-Sik
    • Nuclear Engineering and Technology
    • /
    • v.53 no.3
    • /
    • pp.911-919
    • /
    • 2021
  • In this paper, the design stress intensity values for the plate-type fuel assembly for research reactor are presented. Through a tensile test, the material properties of the cladding (aluminum alloy 6061) and structural material (aluminum alloy 6061-T6), in this case the yield and ultimate tensile strengths, Young's modulus and the elongation, are measured with the temperatures. The empirical equations of the material properties with respect to the temperature are presented. The cladding undergoes several heat treatments and hardening processes during the fabrication process. Cladding strengths are reduced compared to those of the raw material during annealing. Up to a temperature of 150 ℃, the strengths of the cladding do not significantly decrease due to the dislocations generated from the cold work. However, over 150 ℃, the mechanical strengths begin to decrease, mainly due to recrystallization, dislocation recovery and precipitate growth. Taking into account the uncertainty of the 95% probability and 95% confidence level, the design stress intensities of the cladding and structural materials are established. The presented design stress intensity values become the basis of the stress design criteria for a safety analysis of plate-type fuels.

Development of Model Equations for Strength Properties with Age in Concrete Pavement (재령에 따른 포장용 콘크리트의 강도특성 예측식 개발)

  • Yang, Sung-Chul;Kwon, Su-Ahn;Lim, Yu-Jin
    • Journal of the Korean Society of Hazard Mitigation
    • /
    • v.10 no.6
    • /
    • pp.35-43
    • /
    • 2010
  • This study was carried out to find reliable relations between various concrete strength properties which are used as input data in concrete pavement design program. Concretes were made from different sources of coarse grained(granite, limestone and sandstone) and fine grained aggregates such as natural sand, washed sand and crushed sand. From strength test results, model equations were obtained based on the relation between strengths. For each coarse grained aggregate, models for compression-flexural strengths, compression-split tensile strengths, compressive strength-modulus and flexural-split tensile strengths with age were obtained. For concrete mixed with gneiss granite aggregates, concrete strengths were obtained from numerical mean values of concrete strengths mixed with fine grained aggregates. In addition models for concrete split tensile strengths and modulus values were provide by averaging numerically the estimated values obtained from the derived relationship and the experimental values. This is due to more scattered values of split tensile strengths and modulus values than other strength properties. Finally criteria for drying shrinkage strain as well as Poisson's ratio for concrete used in pavement were presented for all mixes with differed coarse grained aggregates.

The Effect of Penetrating Agent and Fluorosilane on High Temperature Teflon Coating (침투제와 불소화실란이 고온용 테프론 코팅에 미치는 영향)

  • Lee, Soo;Seong, Eun-Suk
    • Journal of the Korean Applied Science and Technology
    • /
    • v.30 no.4
    • /
    • pp.672-678
    • /
    • 2013
  • Although the basalt fiber has superior fire-resistance and chemical resistance, it has many disadvantages in its applications. Generally, the tensile and loop strengths of basalt fiber were decreased with generated frictional heat during industial appplications. To solve this problem, polytetrafluoroethylene (PTFE) coating system was introduced and a sutable coating condition was evaluated. The basalt fiber was pre-treated with triethoxytrifluoropropylsilane (TMTFPS) at various pHs and then coated with PTFE dispersions with penetrating agent sodium bis(2-ethylhexyl)sulfo succinate (DOS-Na) to increase the tensile and loop strengths as well as to reduce the fibril during working. A universial testing machine (Instron Model 3366) was used to measure tensile and loop strengths. When the PTFE dispersion with 0.25 wt% of DOS-Na was coated on the surface of basalt fiber after pre-treating with 5 wt% of PTFE, the highest tensile and loop strengths were reached to 3.5 gf/D and 2.4 gf/D, respectively.

Effect of Scrap Content on the Hot Tearing Property and Tensile Property of AC2BS Alloy (AC2BS합금의 열간 균열강도 및 인장특성에 미치는 스크랩 함량의 영향)

  • Kwon, Yong-Ho;Kim, Heon-Joo
    • Journal of Korea Foundry Society
    • /
    • v.36 no.2
    • /
    • pp.67-74
    • /
    • 2016
  • The effects of scrap content on the hot tearing property and tensile property were investigated in AC2BS alloy. The hot tearing strengths were $16.4kgf/cm^2$, $15.2kgf/cm^2$, $14.9kgf/cm^2$ and $13.3kgf/cm^2$, respectively, under the constant solid fraction of 29.3% when the scrap contents of the specimens were 0%, 20%, 35% and 50%. In the same way, tensile strengths of the as-cast condition were $24.5kgf/mm^2$, $23.7kgf/mm^2$, $17.3kgf/mm^2$ and $16.0kgf/mm^2$, respectively, and the corresponding tensile strengths of the T6 heat treatment condition were $27.2kgf/mm^2$, $26.7kgf/mm^2$, $24.2kgf/mm^2$ and $23.9kgf/mm^2$. Hot tearing strength and tensile strength decreased as scrap content of the specimen increased. According to the evaluation of the quantitative hot tearing and tensile test results, the decrease of these strengths is due to the presence of oxide films which act as crack initiation site of the specimens. Therefore, elimination of oxide films of aluminum melt to maintain melt cleanliness is required.