DLC 코팅과 비교된 고온 염소처리에 의한 탄소 막의 Tribological 특성 (Tribological Properties of Carbon Layers Produced by High Temperature Chlorination in Comparison with DLC Coating)

  • 최현주;배흥택;나병철;이전국;임대순
    • 한국세라믹학회지
    • /
    • 제44권7호
    • /
    • pp.375-380
    • /
    • 2007
  • Tribological properties of carbon layers produced by high temperature chlorination of SiC ceramic and DLC (diamond-like carbon) coatings produced by ion plating method were investigated and compared. Carbon coatings were produced by exposure of ball and disc type SiC in chlorine and hydrogen gas mixtures at $1200^{\circ}C$. After treatment for 10 h, dense carbon films up to $180{\mu}m$ in thickness were formed. Tribological behavior of newly developed carbon films were compared with that of DLC films. Wear resistance and frictional coefficient of the surface modified ball and disc type SiC were significantly improved compared to an untreated SiC specimen, and also the modified carbon layer had better performance than DLC coatings. Therefore, in this study, the newly developed carbon films have several advantages over existing carbon coatings such as DLC coatings and showed superior tribological performances.

크롬질화박막형 스트레인 게이지의 특성 (The Characteristics of Chromiun Nitride Thin-Film Strain Gauges)

  • 서정환;김일명;이채봉;김순철;정귀상
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1999년도 하계학술대회 논문집 D
    • /
    • pp.1989-1991
    • /
    • 1999
  • This paper presents characteristics of CrN thin-film strain gauges, which were deposited on glass by DC reactive magnetron sputtering in an argon-nitrogen atmosphere(Ar-$(5{\sim}25%)N_2$). The physical and electrical characteristics of these films investigated with the thickness range $3500{\AA}$ of CrN thin films, annealing temperature $(100{\sim}300^{\circ}C)$ and annealing $(24{\sim}72hr)$. The optimized condition of CrN thin-film strain gauges were thickness range of $3500{\AA}$ and annealing condition($300^{\circ}C$, 48 hr) in Ar-10 %$N_2$ deposition atmosphere. Under optimum conditions, the CrN thin-films for strain gauge is obtained a high resistivity, ${\rho}=1147.65{\mu}{\Omega}cm$, a low temperature coefficient of resistance, TCR=$-186ppm/^{\circ}C$ and a high temporal stability with a good longitudinal, 11.17. And change in resistance after annealing for the CrN thin-films were quitely linear and stable.

  • PDF

고압용 X7R 적층 칩 캐패시터의 Er2O3 및 유리프릿 첨가에 따른 전기적 특성 (The Electrical Properties of High Voltage Mutilayer Chip Capacitor with X7R by addition of Er2O3 and Glass Frit)

  • 윤중락;김민기;정태석;우병철;이석원
    • 한국전기전자재료학회논문지
    • /
    • 제21권5호
    • /
    • pp.440-446
    • /
    • 2008
  • To manufacture the MLCC with X7R for high voltage stability, $BaTiO_3-MgO-MnO_2-Y_2O_3$ with $(Ba_{0.4}Ca_{0.6})SiO_3$ glass frit was formulated. Based on this composition, the addition of $Er_2O_3$ showed that TCC(Temperature Coefficient Capacitance) at $85^{\circ}C$ was improved from 5 % to ${\sim}0\;%$, but the dielectric constant and IR (Insulation Resistance) were decreased. The glass frit improved the dielectric constant and IR, so the appropriate contents of $Er_2O_3$ and glass frit were 0.6 mol% and 1 wt%, respectively. It showed that the dielectric constant and RC constant were 2,550 and 2,000 (${\Omega}F$), respectively in the sintering condition at $1250^{\circ}C$ in PO2 $10^{-7}$ Mpa. The MLCC with $3.2{\times}1.6$ (mm) size and $1\;{\mu}F$ was also suited for X7R with the above composition.

Improved Responsivity of an a-Si-based Micro-bolometer Focal Plane Array with a SiNx Membrane Layer

  • Joontaek, Jung;Minsik, Kim;Chae-Hwan, Kim;Tae Hyun, Kim;Sang Hyun, Park;Kwanghee, Kim;Hui Jae, Cho;Youngju, Kim;Hee Yeoun, Kim;Jae Sub, Oh
    • 센서학회지
    • /
    • 제31권6호
    • /
    • pp.366-370
    • /
    • 2022
  • A 12 ㎛ pixel-sized 360 × 240 microbolometer focal plane array (MBFPA) was fabricated using a complementary metaloxide-semiconductor (CMOS)-compatible process. To release the MBFPA membrane, an amorphous carbon layer (ACL) processed at a low temperature (<400 ℃) was deposited as a sacrificial layer. The thermal time constant of the MBFPA was improved by using serpentine legs and controlling the thickness of the SiNx layers at 110, 130, and 150 nm on the membrane, with response times of 6.13, 6.28, and 7.48 msec, respectively. Boron-doped amorphous Si (a-Si), which exhibits a high-temperature coefficient of resistance (TCR) and CMOS compatibility, was deposited on top of the membrane as an IR absorption layer to provide heat energy transformation. The structural stability of the thin SiNx membrane and serpentine legs was observed using field-emission scanning electron microscopy (FE-SEM). The fabrication yield was evaluated by measuring the resistance of a representative pixel in the array, which was in the range of 0.8-1.2 Mohm (as designed). The yields for SiNx thicknesses of SiNx at 110, 130, and 150 nm were 75, 86, and 86%, respectively.

디젤엔진 실린더 라이너-피스톤 링 소재의 연삭 마멸 특성 (Abrasive Wear Characteristics of Materials for Diesel Engine Cylinder Liner and Piston Ring)

  • 장정환;김정훈;김창희;문영훈
    • 열처리공학회지
    • /
    • 제20권2호
    • /
    • pp.72-77
    • /
    • 2007
  • Abrasive wear between piston ring face and cylinder liner is an extremely unpredictable and hard-to-reproduce phenomenon that significantly decreases engine performance. Wear by abrasion are forms of wear caused by contact between a particle and solid material. Abrasive wear is the loss of material by the passage of hard particles over a surface. From the pin-on-disk test, particle dent test and scuffing test, abrasive wear characteristics of diesel engine cylinder liner-piston ring have been investigated. Pin-on-disk test results indicate that abrasive wear resistance is not simply related to the hardness of materials, but is influenced also by the microstructure, temperature, lubricity and micro- fracture properties. In particle dent test, dent resistance stress decreases with increasing temperature. From the scuffing test by using pin-on-disk tester, scuffing mechanisms for the soft coating and hard coating were proposed and experimentally confirmed.

PTFE-폴리이미드 복합 재료의 마찰과 마모 특성 (Friction and Wear Characteristics of PTFE-Polyimide Composite)

  • 심현해;권오관
    • Tribology and Lubricants
    • /
    • 제11권4호
    • /
    • pp.28-34
    • /
    • 1995
  • PTFE has good mechanical and chemical stability at wide temperature range, and more over, shows a low value of friction coefficient. On the other hand, it shows cold flow and high wear rate. However, these short comings can be overcome by adding various fillers. In this experiment, PTFE and polyimide powder were mixed into composite and its tribological characteristics was investigated. 100% polyimide was also tested for comparison. The countefface material was a stainless steel (SUS304). Friction and wear tester of ring-on-block type was used at room temperature and under atmosphere. After the wear test, the worn surfaces were examined by optical microscope. The test results show that PTFE-polyimide composite generates. the wear transfer film on both sides of the friction surfaces, and, the friction coefficient and the wear rates are relatively low. 100% polyimide generated little wear transfer films, showed high friction and wear rates, and also showed some problems of vibration and noise. It even damaged the stainless steel countefface. It was concluded that 100% polyimide does not generate transfer film well because its shear resistanbe is high and it stickslips, thus, friction coefficients and wear rates are high. In case of PTFE-polyimide composite, on the other hand, transfer film containing sufficient PTFE adheres and remains on both wear surfaces well enough because PTFE has low shear resistance. Polyimide particles in the composite were proved to be able to bear normal load and does not show stick-slip because they are covered with transfer film containing much PTFE.

SL 온도특성을 가지는 적층 칩 세라믹 캐패시터용 유전체의 유전 및 전기적 특성 (Dielectric and Electric Properties of Mutilayer Ceramic Capacitor with SL Temperature Characteristics)

  • 윤중락;이상원;김민기;이경민
    • 한국전기전자재료학회논문지
    • /
    • 제21권7호
    • /
    • pp.645-651
    • /
    • 2008
  • To reduce noise in high frequency and distortion of signal, the composition of $(Ca_{0.7}Sr_{0.3})(Zr_{0.97}Ti_{0.03})O_3$ and $(Ba_{0.2}Ca_{0.4}Sr_{0.4})TiO_3$ was developed. The composition was not solid solution, but mixtures of various phases composed of Ca, Sr, Zr, Ti and Ba oxides. The dielectric constant increased, the quality factor and the insulation resistance decreased with $(Ba_{0.2}Ca_{0.4}Sr_{0.4})TiO_3$ content. The composition of $0.4(Ba_{0.2}Ca_{0.4}Sr_{0.4})TiO_3$ satisfied the electric characteristics and the temperature coefficient of dielectric constant (TCC). In addition, the glass frit and $MnO_2$ also affected the electric characteristics. From the result of the best fit simulation, $MnO_2$ 0.3 mol%, the glass frit 0.6 wt% showed the insulation resistance $906{\Omega}{\cdot}F$, the quality factor 821, and the dielectric constant 92. With the selected composition, MLCC capacitors sized $4.5{\times}3.2{\times}2.5mm$ were manufactured with 105 layered of the dielectric thickness $16{\mu}m$ using Ni inner electrode, They represented the capacitance $98{\sim}102$ nF, the quality factor 1,200 and the insulation resistance $1,500{\Omega}{\cdot}F$. Also, they had high break-down voltage with $107{\sim}115V/{\mu}m$, and satisfied the SL TCC characteristics.

Characteristics of tantalum nitride thin film resistors deposited on $SiO_2/Si$ substrate using D.C-magnetron sputtering

  • Cuong, Nguyen Duy;Phuong, Nguyen Mai;Kim, Dong-Jin;Kang, Byoung-Don;Kim, Chang-Soo;Yoon, Soon-Gil
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 하계학술대회 논문집 Vol.6
    • /
    • pp.64-65
    • /
    • 2005
  • The structural and electrical properties of the films are investigated as a function of nitrogen/argon ratio at room temperature and at various deposition temperatures. The phase changes as $Ta_2N$ or TaN in the films were observed as nitrogen/argon ratio increases from 3% to 25%. The phase changes were associated with a change in the resistivity and TCR (temperature coefficient of resistance) of the films. TCR values of the films deposited at room temperature and different nitrogen contents were negative, and strongly decreased with the increase in nitrogen/argon ratio. The Ta2N films deposited at nitrogen/argon ratio of 3% show improved TCR values and thermal stability with increasing deposition temperature. The $Ta_2N$ films grown at nitrogen/argon ratio of 3% and the temperature of $200^{\circ}C$ showed a TCR value of -47 $ppm/^{\circ}C$, which is close to near-zero TCR in the range of deposition temperature.

  • PDF

PTCR Characteristics of BaTiO$_3$Thin Films made by rf/dc Magnetron Sputter Technique

  • Song, Min-Jong;So, Byung-Moom;Kim, Tae-Wan
    • Transactions on Electrical and Electronic Materials
    • /
    • 제1권2호
    • /
    • pp.28-31
    • /
    • 2000
  • BaTiO$_3$cerameic thin films doped with Mn were manufactured by rf/dc magnetron sputter technique. We have investigated crystal structure, surface morphology and PRCR(positive-temperature coefficient of resistance) characteristics of the specimen depending on second heat-treatment temperature. Second heat treatment of the specimen were performed in the temperature range of 400 to 1350$\^{C}$ X-ray diffraction patterns of BaTiO$_3$ thin films show that the specimen heat treated below 600$\^{C}$ is an amorphous phase and the one heat treated above 1100$\^{C}$ forms a poly-crystallization . In this specimen heat-treated at 1300$\^{C}$, a lattice constant ratio(c/a) was 1.188. Scanning electron microscope(SEM) image of BaTiO$_3$ thin films of the specimen heat treated in between 900 and 1100$\^{C}$ shows a grain growth. At 1100$\^{C}$, the specimen stops grain-growing and becomes a poly-crystallization . A resistivity-temperature characteristics of the specimen depends on the doping concentrations of Mn. A resistivity ratio between the value at room temperature and the one above Curie temperature was 10$^4$ for pure BaTiO$_3$ thin films and 10$\^$5/ fo BaTiO$_3$ : additive 0.127mol% MnO

  • PDF

Ni-Mn 산화물 NTC 서미스터의 미세구조와 전기적 특성에 미치는 CuO 첨가의 효과 (Effect of CuO Addition on the Microstructural and Electrical Properties of Ni-Mn Oxide NTC Thermistor)

  • 김경민;이성갑;이동진;박미리
    • 한국전기전자재료학회논문지
    • /
    • 제29권6호
    • /
    • pp.337-341
    • /
    • 2016
  • In this study, $ Ni_{0.79}(Mn_{2.21-x}Cu_x)O_4$ (x=0~0.25) specimens were prepared by using a conventional mixed oxide method. All specimens were sintered in air at $1,200^{\circ}C$ for 12 h and cooled at a rate of $2^{\circ}C/min$ to $800^{\circ}C$, subsequently quenching to room temperature. We investigated the structural and electrical properties of $ Ni_{0.79}(Mn_{2.21-x}Cu_x)O_4$ specimens with variation of CuO amount for the application of NTC thermistors. As results of X-ray diffraction patterns, all specimens showed the formation of a complete solid solution with cubic spinel phase. The relationship between ln ${\rho}$ and the reciprocal of absolute temperature(1/T) for the NTC thermistors was shown linearity, which exhibited the typical NTC thermistor properties. With increasing the amount of CuO, resistivity at room temperature, B-value, and temperature coefficient resistance decreased.