• Title/Summary/Keyword: Temperature activation

Search Result 2,253, Processing Time 0.032 seconds

Low temperature activation of dopants by metal induced crystallization (금속 유도 결정화에 의한 저온 불순물 활성화)

  • 인태형;신진욱;이병일;주승기
    • Journal of the Korean Institute of Telematics and Electronics D
    • /
    • v.34D no.5
    • /
    • pp.45-51
    • /
    • 1997
  • Low temperature activation of dopants which were doped using ion mass doping system in amorphous silicon(a-Si) thin films was investigated. With a 20.angs.-thick Ni film on top of the a-Si thin film, the activation temperature of dopants lowered to 500.deg. C. When the doping was performaed after the deposition of Ni thin film on the a-Si thin films (post-doping), the activation time was shorter than that of dopants mass, the activation time of the dopants doped by pre-doping method increased. It turned NiSi2 formation, while the decrease of activation time was mainly due to the enhancement of the NiSi2 formation by mixing of Ni and a-Si at the interface of Ni and a -Si thin during the ion doping process.

  • PDF

In Vitro Development of Mouse Parthenogenetic Embryos: Effect of Temperature before Oocyte Activation

  • Roh Sangho;Won Cheolhee;Min Byung-Moo
    • Reproductive and Developmental Biology
    • /
    • v.29 no.2
    • /
    • pp.117-120
    • /
    • 2005
  • This study was conducted to establish the optimal temperature condition before oocyte activation in B6m F1 mouse. In experiment 1, two embryo culture media (CZB vs KSOM) were evaluated for the development of activated mouse oocytes. Parthenogenetic embryos cultured in KSOM showed better blastocyst development than ones cultured in CZB $(56.2\%\;vs\;81.0\%\;p<0.01)$. Two-hour of pre-incubation before activation significantly reduced the number of hatched blastocysts in KSOM $(22.0\%\;versus\;8.8\%\;p<0.05)$. In experiment 2, recovered oocytes were pre-incubated at different temperature conditions before activation. The experimental groups were divided by 5 as follows. Group A: pre-incubation for 120 min at $37^{\circ}C$, Group B: pre-incubation at $37^{\circ}C$ for 90 min then at $25^{\circ}C$ for 30 min, Group C: pre-incubation at $37^{\circ}C$ for 60 min then at $25^{\circ}C$for 60 min, Group D: pre-incubation at $37^{\circ}C$ for 30 min then at $25^{\circ}C$ for 90 min, and Group E: pre-incubation at $25^{\circ}C$ for 120 min before activation. Group A $(67.6\%)$ and B $(66.7\%)$ showed better development to the blastocyst stage than other groups $(Group\;C:\;50.0\%\;Group \;D:\;49.2\%\;Group\;E:\;33.3\%,\;p<0.05)$. The present study indicates that the temperature before activation affects the development of B6D2 F1 mouse parthenogenetic oocytes and exposure to room temperature should be limited to 30-min when the oocytes are left in HEPES-buffered medium for micromanipulation.

Low temperature solid phase crystallization of amorphous silicon thin film by crystalline activation

  • Kim, Hyung-Taek;Kim, Young-Kwan
    • Journal of Korean Vacuum Science & Technology
    • /
    • v.2 no.2
    • /
    • pp.97-100
    • /
    • 1998
  • We have investigated the effects of crystalline activation on solid phase crystallization (SPC) of amorphous silicon (a-Si) thin films. Wet blasting and self ion implantation were employed as the activation treatments to induce macro or micro crystalline damages on deposited a-Si films. Low temperature and larger grain crystallization were obtained by the applied two-step activation. High degree of crystallinity was also observed on both furnace and rapid SPC. crystalline activations showed the promotion of nucleation on the activated regions and the retardation of growth in an amorphous matrix in SPC. The observed behavior of two-step SPC was strongly dependent on the applied activation and annealing processes. It was also found that the diversified effects by macro and micro activations on the SPC were virtually diminished as the annealing temperature increased.

  • PDF

Prediction of Concrete Strength by a Modified Rate Constant Model (수정 반응률 상수 모델에 의한 콘크리트의 강도의 예측)

  • 한상훈;김진근
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1999.10a
    • /
    • pp.155-158
    • /
    • 1999
  • This paper discusses the validity of models to predict the compressive strength of concrete subjected to various temperature histories and the shortcomings of existing rate constant model and apparent activation energy concept. Based on the discussion, a modified rate constant model is proposed. The modified rate constant model, in which apparent activation energy is a nonlinear function of curing temperature and age, accurately estimates the development of the experimental compressive strengths by a few researches. Also, the apparent activation energy of concrete cured with high temperature decreases rapidly with age, but that cured with low temperature decreases gradually with age. Finally a generalized model to predict apparent activation energy and compressive strength is proposed, which is based on the regression results.

  • PDF

A New Method of HTS Material Synthesis by Combination of MCA and SHS

  • Korobova, N.;Soh, Dea-Wha
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2004.07b
    • /
    • pp.1270-1273
    • /
    • 2004
  • The combination of methane-chemical activation and Self-propagating High-temperature synthesis (SHS) has widened the possibilities for both methods. For YBCO systems the investigation showed that a short-term mechano-chemical activation of initial powders before SHS leads to single-phase and ultra-fine products. A new technique for preparation ultra-fine high-temperature superconductors of YBCO composition with a grain size d < $1{\mu}m$ is developed. The specific feature of the technique is formation of the $YBa_2Cu_3O_{7-x}$ crystalline lattice directly from an X-ray amorphous state arising as a result of mechanical activation of the original oxide mixture. The technique allows the stage of formation of any intermediate reaction products to be ruled out. X-ray and magnetic studies of ultra-fine high temperature superconductors (HTS) are carried out. Dimension effects associated with the microstructure peculiarities are revealed. A considerable enhancement of inter-grain critical currents is found to take place in the ultra-fine samples investigated.

  • PDF

Hydrolsis Behaviour of Antheraea pernyi Silk Fiber Treated with HCI (염산처리 작잠견사의 가수분해거동)

  • 권해용;이광길;이용우;여주홍;엄인철
    • Journal of Sericultural and Entomological Science
    • /
    • v.40 no.2
    • /
    • pp.163-168
    • /
    • 1998
  • Hydrolysis rate and activation energy of Antheraea pernyi silk fiber treated with HCI were examined. Thermal decomposition temperature and surface morphology were also investigated by using differential scanning calorimeter and scanning electron microscope. As the concentration of hydrochloric acid and the treatment temperature increased, the hydrolysis occurred more rapidly. The activation energy of Antheraea pernyi, 74.0 kJ/mol, was higher than that of Bombyx mori, 58.1 kJ/mol. As the concentration of hydrochloric acid increases, the activation energy of Antheraea pernyi decreased from 74.0 kJ/mol to 62.0 kJ/mol. The shape of acid-resistance fraction of Antheraea pernyi became more distroyed and was transformed from fiber to powdered form with an increase of hydrolysis rate. The thermal decomposition temperature of Antheraea pernyi was 360.8$^{\circ}C$ until the hydrolysis rate was 81.8 wt%, but ti decreased to 347.0$^{\circ}C$ when the hydrolysis rate was 93.8 wt%.

  • PDF

A Study on the Plastic Deformation and Fracture Behavior of Mg-Zn-Mn-(Ca) Alloys (Mg-Zn-Mn-(Ca)합금의 크리이프 소성변형 및 파단거동에 관한 연구)

  • Kang, D.M.;Park, S.C.;Kang, K.I.
    • Journal of Power System Engineering
    • /
    • v.10 no.3
    • /
    • pp.45-50
    • /
    • 2006
  • In this paper, creep tests of Mg-Zn-Mn and Mg-Zn-Mn-Ca alloy casted by mold under the temperature range of 473.00-573.00K, and the stress range of 23.42-87.00Mpa were done with the equipment of automatic controlled temperature and computer for data acquisition. The activation energies were obtained by relationship between creep rate and temperature, and the stress exponents were obtained by relationship between creep rate and stress. From the experiment results, the activation energies of Mg-Zn-Mn and Mg-Zn-Mn-Ca alloy were 149.87kJ/mol, 147.97kJ/mol, respectively, and the stress exponents of those alloy were 5.13, 5.59, respectively, under the temperature of 473.00-493.00K and the stress range of 62.43-78.00Mpa. And the activation energies of those alloy were 134.41kJ/mol, 129.22kJ/mol, respectively, and the stress exponent of those alloy were 3.48, 3.77, respectively, under the temperature of 553-573Mpa and the stress range of 23.42-39.00Mpa. Also the lifes of Mg-Zn-Mn-Ca alloy were higher than those of Mg-Zn-Mn alloy, and the results of SEM showed fracture surfaces under low temperature had smaller dimples than those under high temperature.

  • PDF

Strength Characteristics of Reduced Activation Ferritic Steel for Fusion Blanket by TIG Welding (핵융합로 블랭킷용 저방사화 철강재료 TIG 용접부의 강도특성)

  • ;;;A. Kohyama
    • Journal of Welding and Joining
    • /
    • v.21 no.1
    • /
    • pp.87-92
    • /
    • 2003
  • JLF-1 steel (Fe-9Cr-2W-V-Ta), reduced activation ferritic steel, is one of the promising candidate materials for fusion reactor applications. Tensile properties of JLF-1 base metal and its TIG weldments has been investigated at the room temperature, $400^{\circ}C$ and $600^{\circ}C$. The tensile strength of base metal (JLF-1) showed the level between those of weld metal and the Heat Affected Zone (HAZ). When the test temperature was increased from room temperature to high temperature ($400^{\circ}C$ and $600^{\circ}C$), both strength and ductility decreased or base metal, weld metal and the HAZ. The longitudinal specimens of base metal represented similar strength and ductility at room temperature and high temperature, compared to those of transverse specimens. Little anisotropy for the rolling direction was observed in the base metal of JLF-1 steel.

Pore Structure Characterization of Poly(vinylidene chloride)-Derived Nanoporous Carbons

  • Jung, Hwan Jung;Kim, Yong-Jung;Lee, Dae Ho;Han, Jong Hun;Yang, Kap Seung;Yang, Cheol-Min
    • Carbon letters
    • /
    • v.13 no.4
    • /
    • pp.236-242
    • /
    • 2012
  • Poly(vinylidene chloride) (PVDC)-derived nanoporous carbons were prepared by various activation methods: heat-treatment under an inert atmosphere, steam activation, and potassium hydroxide (KOH) activation at 873, 1073, and 1273 K. The pore structures of PVDC-derived nanoporous carbons were characterized by the $N_2$ adsorption technique at 77 K. Heat treatment in an inert atmosphere increased the specific surface area and micropore volume with elevating temperature, while the average micropore width near 0.65 nm was not significantly changed, reflecting the characteristic pore structure of ultramicroporous carbon. Steam activation for PVDC at 873 and 1073 K also yielded ultramicroporosity. On the other hand, the steam activated sample at 1273 K had a wider average micropore width of 1.48 nm, correlating with a supermicropore. The KOH activation increased the micropore volume with elevating temperature, which is accompanied by enlargement of the average micropore width from 0.67 to 1.12 nm. The average pore widths of KOH-activated samples were strongly governed by the activation temperature. We expect that these approaches can be utilized to simply control the porosity of PVDC-derived nanoporous carbons.

Surface and Adsorption Properties of Activated Carbon Fabric Prepared from Cellulosic Polymer: Mixed Activation Method

  • Bhati, Surendra;Mahur, J.S.;Dixit, Savita;Choubey, O.N.
    • Bulletin of the Korean Chemical Society
    • /
    • v.34 no.2
    • /
    • pp.569-573
    • /
    • 2013
  • In this study, activated carbon fabric was prepared from a cellulose-based polymer (viscose rayon) via a combination of physical and chemical activation (mixed activation) processes by means of $CO_2$ as a gasifying agent and surface and adsorption properties were evaluated. Experiments were performed to investigate the consequence of activation temperature (750, 800, 850 and $925^{\circ}C$), activation time (15, 30, 45 and 60 minutes) and $CO_2$ flow rate (100, 200, 300 and 400 mL/min) on the surface and adsorption properties of ACF. The nitrogen adsorption isotherm at 77 K was measured and used for the determination of surface area, total pore volume, micropore volume, mesopore volume and pore size distribution using BET, t-plot, DR, BJH and DFT methods, respectively. It was observed that BET surface area and TPV increase with rising activation temperature and time due to the formation of new pores and the alteration of micropores into mesopores. It was also found that activation temperature dominantly affects the surface properties of ACF. The adsorption of iodine and $CCl_4$ onto ACF was investigated and both were found to correlate with surface area.