  • The effect of deformation induced martensite transformation on the mechanical properties in austenitic stainless steel with high Mn was studied. ${\alpha}$'-martensite was formed by deformation in austenitic stainless steel with high Mn. Deformation induced ${\alpha}$'-martensite was formed with surface relief by cold rolling. With the increase of deformation degree, volume fraction of deformation induced martensite was increased rapidly in early stage of deformation and then, increased slowly. With the increase of deformation degree, hardness and tensile strength were rapidly increased with linear relations, while elongation was rapidly decreased and then slowly decreased. Hardness, tensile strengths and elongation were influenced strongly by deformation induced martensite.

현대 패션디자인에 표현된 새 이미지 연구 (A Study on the Bird Image Expressed in Modern Fashion Design)

  • 안세라;금기숙
    • 복식문화연구
    • /
    • 제19권6호
    • /
    • pp.1177-1192
    • /
    • 2011
  • As a free creature that can fly in the sky, the bird has been an object of admiration and mystery and a mediator between human beings and the heavens. This study aims to clarify the aesthetic value of birds through study of the various expressions of the bird image on clothing and by the formative will of designers. Based on the general examination of the bird image through the study of documents, this study is composed of a case analysis, which reveals on modern fashion designs. Additionally, the forms of expression of the bird image are organized according to the stereoscopic expression of shaping, the relief expression of handicraft decoration, the flat expression of surface design, and the characteristic expression of wings and feathers. The aesthetic characteristics revealed by the expression patterns are metaphorical symbolism, surrealistic humor, lyrical naturalness, and fantastical femininity. Since antiquity, the bird image continuously recreated by artists has offered aesthetic value in terms of formativeness in the external form and symbolism in the internal form. This study would help to understand the diversity of creation in contemporary fashion design.

Femtosecond laser induced photo-expansion of organic thin films

  • 채상민;이명수;최지연;이현휘;김효정
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2015년도 제49회 하계 정기학술대회 초록집
    • /
    • pp.120.2-120.2
    • /
    • 2015
  • We propose a novel direct writing technique with a femtosecond laser enabling selective modification of not only the morphology of conducting polymer thin films but also the orientation and alignment of the polymer crystal. Surface relief gratings resulting from photoexpansion on P3HT:PCBM and PEDOT:PSS thin films were fabricated by femtosecond laser direct writing. The photoexpansion was induced at laser fluence below the ablation threshold of the thin film. The morphology (size and shape) of photoexpansion could be quantitatively controlled by laser writing parameters such as focused beam size, writing speed, and laser fluence. GIWAX results showed that face-on P3HT crystals were largely increased in the photoexpansion in comparison with pristine region of the thin film. In addition, the face-on P3HTs in the photoexpansion were aligned with their orientation along the polarization of the laser. The micro-RAMAN spectra confirmed that neither chemical composition change nor the polymer chain breaking was observable after femtosecond laser irradiation. We believe that this laser direct writing technique opens a new door to the fabrication of more efficient OPVs via non-contact, toxic-free approach.

  • PDF

Fe-26Mn-4Co-2Al 제진합금의 감쇠능에 미치는 결정립 크기의 영향 (Effect of Grain Size on the Damping Capacity of Fe-26Mn-4Co-2Al Damping Alloy)

  • 정규성;김도훈;권순두;강창룡
    • 한국재료학회지
    • /
    • 제28권3호
    • /
    • pp.129-134
    • /
    • 2018
  • This study was carried out to investigate the effect of grain size on the damping capacity of the Fe-26Mn-4Co-2Al damping alloy. ${\alpha}^{\prime}$ and ${\varepsilon}-martensite$ were formed by cold working, and these martensites were formed with a specific direction and surface relief. With an increase in grain size, the volume fraction of ${\alpha}^{\prime}$ and ${\varepsilon}-martensite$ increased by decrement the austenite phase stability. This volume fraction more rapidly increased in cold-rolled specimen than in the specimen that was not cold-rolled. The damping capacity also increased more with the augmentation an increased grain size and more rapidly increased in cold-rolled specimen than in the specimen that was not cold rolled. The effect of grain size on the damping capacity was larger in the cold-rolled specimen than the specimen that was not cold-rolled. Damping capacity linearly increased with an increase in volume fraction of ${\varepsilon}-martensite$. Thus, the damping capacity was affected by the ${\varepsilon}-martensite$.

Fe-26Mn-4Co-2Al 합금의 감쇠능에 미치는 가공 유기 마르텐사이트의 영향 (Effect of Deformation Induced Martensite on the Damping Capacity of Fe-26Mn-4Co-2Al Alloy)

  • 정규성;강창룡
    • 한국재료학회지
    • /
    • 제26권9호
    • /
    • pp.493-497
    • /
    • 2016
  • This study was carried out to investigate the effect of deformation induced martensite on the damping capacity of Fe-26Mn-4Co-2Al damping alloy. ${\alpha}^{\prime}$ and ${\varepsilon}$-martensite were formed by cold working, and; deformation induced martensite was formed with according to the specific direction and the surface relief. With an increasing degree of cold rolling, the volume fraction of ${\alpha}^{\prime}$-martensite increased rapidly, while the volume fraction of ${\varepsilon}$-martensite decreased after rising to a maximum value at a specific level of cold rolling. Damping capacity was increased, and then decreased with an increasing of the degree of cold rolling. Damping capacity was influenced greatly by the volume fraction of ${\varepsilon}$-martensite formed by cold working, but the effect of the volume fraction of ${\alpha}^{\prime}$-martensite have a actually on effect on the damping capacity.

냉간압연한 고 Mn 오스테나이트계 스테인리스강의 기계적 성질에 미치는 서브제로처리의 영향 (Effect of Subzero Treatment on the Mechanical Properties of Cold-Rolled High Manganese Austenitic Stainless Steel)

  • 황태현;정목환;이종영;이향백;강창룡
    • 열처리공학회지
    • /
    • 제25권5호
    • /
    • pp.233-238
    • /
    • 2012
  • The effect of subzero treatment on the mechanical properties of cold rolled high manganese austenitic stainless steel was investagated. ${\alpha}$'-martensite was formed by cold rolling, and it was formed with surface relief and specific direction or crossing each other. The volume fraction of martensite increased by subzero treatment, and it was increased with longer time of subzero treatment and higher temperature of subzero treatment. The hardness and strength increased by subzero treatment, while the elongation decreased. With the increase of volume fraction of martensite, the hardness and strength was increased steeply with proportional relationship, elongation was decreased slowly. The results show that the hardness and strength was strongly controlled by the volume fraction of martensite, and the elongation was affected by transformation behavior of deformation induced martensite in the initial stage of deformation.

Fe-26Mn-4Co-2Al 제진합금의 인장강도에 미치는 냉간가공의 영향 (Effect of Cold Working on the Tensile Strength of Fe-26Mn-4Co-2Al Damping Alloy)

  • 강창룡;김성휘;정규성
    • 동력기계공학회지
    • /
    • 제20권6호
    • /
    • pp.46-50
    • /
    • 2016
  • This study was carried out to investigate the effect of cold working on the tensile strength of Fe-26Mn-4Co-2Al damping alloy. ${\alpha}^{\prime}$ and ${\varepsilon}$-martensite were formed by cold working, and martensite was formed with the specific direction and surface relief. With the increasing degree of cold rolling, volume fraction of ${\alpha}^{\prime}$-martensite was increased, whereas the volume fraction of ${\varepsilon}$-martensite was decreased after rising to maximum value at specific lever of cold rolling. Tensile strength was linearly increased with an increasing of degree of cold rolling. Tensile strength was strongly affected to the volume fraction of ${\varepsilon}$-martensite formed by cold working, but the effect of volume fraction of ${\varepsilon}$-martensite on the tensile strength was not observed.

Epitaxial Overlayers vs Alloy Formation at Aluminum-Transition Metal Interfaces

  • Smith, R.J.
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 1999년도 제17회 학술발표회 논문개요집
    • /
    • pp.29-29
    • /
    • 1999
  • The synthesis of layered structures on the nanometer scale has become essential for continued improvements in the operation of various electronic and magnetic devices. Abrupt metal-metal interfaces are desired for applications ranging from metallization in semiconductor devices to fabrication of magnetoresistive tunnel junctions for read heads on magnetic disk drives. In particular, characterizing the interface structure between various transition metals (TM) and aluminum is desirable. We have used the techniques of MeV ion backscattering and channeling (HEIS), x-ray photoemission (ZPS), x-ray photoelectron diffraction(XPD), low-energy ion scattering (LEIS), and low-energy electron diffraction(LEED), together with computer simulations using embedded atom potentials, to study solid-solid interface structure for thin films of Ni, Fe, Co, Pd, Ti, and Ag on Al(001), Al(110) and Al(111) surfaces. Considerations of lattice matching, surface energies, or compound formation energies alone do not adequately predict our result, We find that those metals with metallic radii smaller than Al(e.g. Ni, Fe, Co, Pd) tend to form alloys at the TM-Al interface, while those atoms with larger atomic radii(e.g. Ti, Ag) form epitaxial overlayers. Thus we are led to consider models in which the strain energy associated with alloy formation becomes a kinetic barrier to alloying. Furthermore, we observe the formation of metastable fcc Ti up to a critical thickness of 5 monolayers on Al(001) and Al(110). For Ag films we observe arbitrarily thick epitaxial growth exceeding 30 monolayers with some Al alloying at the interface, possible driven by interface strain relief. Typical examples of these interface structures will be discussed.

  • PDF

이종금속용접부 온도 및 잔류응력의 라운드로빈 해석 (A Round-Robin Analysis of Temperature and Residual Stresses in Dissimilar Metal Weld)

  • 송민섭;강선예;박준수;손갑헌
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2008년도 추계학술대회A
    • /
    • pp.85-87
    • /
    • 2008
  • DMWs are common feature of the PWR in the welded connections between carbon steel and stainless steel piping. The nickel-based weld metal, Alloy 82/182, is used for welding the dissimilar metals and is known to be susceptible to PWSCC. A round-robin program has been implemented to benchmark the numerical simulation of the transient temperature and weld residual stresses in the DMWs. To solve the round-robin problem related to Pressurizer Safety & Relief nozzle, the thermal elasto-plastic analysis is performed in the DMW by using the FEM. The welding includes both the DMW of the nozzle to safe-end and the SMW of the safe-end and piping. Major results of the analyses are discussed: The axial and circumferential residual stresses are found to be -88MPa(225MPa) and -38MPa(293MPa) on the inner surface of the DMW; where the values in parenthesis are the residual stresses after the DMW. Thermo-mechanical interaction by the SMW has a significant effect on the residual stress fields in the DMW.

  • PDF

고 Mn 오스테나이트계 스테인리스강의 감쇠능에 미치는 역변태의 영향 (Effect of Reverse Transformation on the Damping Capacity of High Manganease Austenitic Stainless Steel)

  • 강창룡
    • 동력기계공학회지
    • /
    • 제16권4호
    • /
    • pp.60-65
    • /
    • 2012
  • This study was carried out to investigate the effect of reverse transformation on the damping capacity in high manganese austenitic stainless steel. ${\alpha}^{\prime}$-martensite was formed with the specific direction and surface relief by deformation. Over 95% of the austenite phase was transformed to deformation-induced ${\alpha}^{\prime}$-martensite by 70% cold rolling. Reverse transformation became rapid above an annealing temperature of $550^{\circ}C$, but there was no significant transformation above $700^{\circ}C$. In addition, with increasing annealing time at $700^{\circ}C$, reverse transformation was induced rapidly, but the transformation was almost completed at 10 min. Damping capacity was increased up to $700^{\circ}C$, and than unchanged with the increasing annealing temperature. Damping capacity increased steeply with an increasing reverse treatment time up to 10min, whereas there were no significant change with a treatment time of more than 10 min. Damping capacity increased with an increasing the reversed austenite and was strongly affected by reversed austenite.