  • Adhesion strength of electroless-plated Ni, Ni-P and Cu deposites on alumina substrate has been studied. Grain boundary spaces produced on the substrate surface by etching treatment provided anchoring sites for enhancing the adhesion strength. Adhesion strengths of Ni-P and Ni deposit were higher than that of Cu deposit, because of higher initial nucleation rates than the latter. The electroless-plated Ni-P and Ni underlayer improved the adhesion strength of the Cu deposit. In could be attributed to the enhanced adhesion between the substrate and those underlayers as well as the satisfactory adhesion between Cu deposits and those underlayers. Heat treatment was also conducted in order to enhance the adhesion strength of Cu layer. The strength was enhanced by about 19% when the treatment was conducted at $150^{\circ}C$ for 2 hours. The enhancement was attributed to relief of internal stress and release of hydrogen.

  • PDF

주조용 티타늄 신합금 개발 (Development of New Titanium Alloys for Castings)

  • 김승언;정희원;현용택;김성준;이용태
    • 연구논문집
    • /
    • 통권29호
    • /
    • pp.163-171
    • /
    • 1999
  • A new titanium alloy system. Ti-xFe-ySi (x,y=0-4 wt%). was designed and characterized with the point at low cost and high strength for casting applications. Fe improved room and elevated temperature mechanical properties owing to solid solution hardening and beta phase stabilization. Si yielded titanium silicides and Si addition over 1 wt% resulted in poor ductility due to coarse silicide chains at prior beta boundaries. The optimum composition was found to be Ti-4Fe-(0.5-1)Si in the viewpoint of tensile strength and ductility which are comparable to the Ti-6Al-4V. The metal-mould reaction was also examined for Ti-xFe and Ti-xSi binary alloy system. The thickness of surface reaction layer w as not affected significantly with Fe content, while it was decreased with Si content. In the Ti-4Si alloy, no reaction layer was found. The depth of surface hardening layer was about $200\mum$ regardless of the mould materials.

  • PDF

징케이트 공정 변화에 따른 무전해 니켈 도금 막의 접착력향상 (Adhesion improvement of electroless plated Ni layer by modifying zincating process)

  • 이성기;진정기;김영호
    • 한국마이크로전자및패키징학회:학술대회논문집
    • /
    • 한국마이크로전자및패키징학회 2002년도 춘계 기술심포지움 논문집
    • /
    • pp.109-114
    • /
    • 2002
  • The adhesion of electroless plated Ni layer on Al/Si substrates has been investigated. The zincating treatment was conducted with a conventional method and a modified method. In a modified method, ultrasonic agitation was applied during zincating. Adhesion strength was evaluated by a pull-off test. The ultrasonic agitation during zincating increased the nucleation density of Zn particles and refined Zn particle size. the adhesion strength of electroless Ni layer deposited on the modified zincated surface was higher than that on the conventionally zincated surface. the improvement of adhesion was attributed to the fine and dense Zn particles.

  • PDF

Ni계 합금분말 용사 코팅기술을 적용한 롤 제조기술 연구 (A Study on the Roll Manufacturing Technology Applying Powder Flame Spray Coating Technology of Ni-Based Alloy Powder)

  • 박지웅;김순국;반계범
    • 한국분말재료학회지
    • /
    • 제29권2호
    • /
    • pp.123-131
    • /
    • 2022
  • The purpose of this study is to improve the mechanical properties and develop manufacturing technology through self-soluble alloy powder flame spray coating on the surface of a run-out table roller for hot rolling. The roller surface of the run-out table should maintain high hardness at high temperatures and possess high wear, corrosion, and heat resistances. In addition, sufficient bonding strength between the thermal spray coating layer and base material, which would prevent the peel-off of the coating layer, is also an important factor. In this study, the most suitable powder and process for roll manufacturing technology are determined through the initial selection of commercial alloy powder for roll manufacturing, hardness, component analysis, and bond strength analysis of the powder and thermal spray coating layer according to the powder.

가스용사에 의한 Ni-Cr 기 자용성합금 용사 의 특성에 미치는 용사조건의 영향 (Effect of Spraying Conditions in Flame Spraying of Ni-Cr Base Self Fluxing Alloy on Mild Steel)

  • 배종규;박경채;정인상
    • 한국표면공학회지
    • /
    • 제22권1호
    • /
    • pp.26-42
    • /
    • 1989
  • It has between investigated that the optimum spaying conditions, such as, spraying distance, fusing temperature and fusing time, ect, in a Ni-cr base self fluxing alloy sprayed on the mild steel substrate by oxygen-acetylenc flame spraying. Sprayed specimens on various conditions were fuused in a vacuum furnace and the results were as follows. The optimum spraying condition for excellent coating layer are obtained under spraying distances, fusing temperature and fusing and time ; 180~240mm,1050~110$0^{\circ}C$and 15~30min, respectively. The adhesive strength and surface hurface hardness of the as sprayed specimens were very low by mechanical bonding becaus of the diffusion layer during process. The carbides and borides and formed in the sprayed coating layer and densification of the layer was resulted from the elimination of pores and oxides. The hardness of sprayed coating layer, particularly in the high temperature, was superior to ordinary tool steels.

  • PDF

용융아연도금한 강판의 기술적 성질에 관한 연구 (A Study on Mechanical Properties of Galvanized Steel Plate)

  • 정동원;곽창섭;최종술
    • 한국표면공학회지
    • /
    • 제16권4호
    • /
    • pp.153-159
    • /
    • 1983
  • The growth rate equation of Fe-Zn alloy layer was represented by x = Kt, and hence the growth of alloy layer was considered to be controlled by diffusion process. The constituent of alloy layer formed on the steel surface was identified to be intermetallic compound of Fe3Zn10 and FeZn10. The ultimate tensile strength and elongation of galvanized steel showed a nearly constant value at the thickness below about 30$\mu\textrm{m}$, and both properties decreased with increasing thickness above about 30$\mu\textrm{m}$. In the case of galvanied steel with a great thickness of alloy layer, crack was formed below yield point of base metal, which is considered to be attributed to the alloy layer failure.

  • PDF

암석과 토층 경계면의 전단강도 특성연구 (A Study on Characteristics of Shear Strength in Rock-soil Contacts)

  • 이수곤
    • 한국환경복원기술학회지
    • /
    • 제4권3호
    • /
    • pp.49-54
    • /
    • 2001
  • It is common that the soil layer is a few meters below the earth's surface and the rock mass is below the soil layer in the view of geological characteristics in Korea. And the boundary between rock and soil is clearly divided. When dealing with the stability of rock masses, as in the case of rock slopes or dam foundations, the majority of the collapses is not within the soil layer, but within the soil-rock boundary. Therefore it is important to identify the shear strength characteristics between soil-rock boundary. And then in the method of reinforcement on landslide this chose a cut slope near Daemo elementary school in Seoul, surveyed shear strength between soil-rock contacts and considered a large scale collapse using a limit equilibrium method.

  • PDF

코로나 방전처리에 의한 반도전-절연 실리콘 고무의 표면특성 및 접착특성 (Surface Properties and Adhesion of Semiconducting and Insulating Silicone Rubber by Corona Discharge Treatment)

  • 이기택;황선묵;홍주일;허창수
    • 한국전기전자재료학회논문지
    • /
    • 제19권9호
    • /
    • pp.868-872
    • /
    • 2006
  • In this work, the effects of the corona treatment on surface properties of semiconducting silicone rubber were investigated in terms of contact angles, ATR-FTIR(Attenuated total reflection fourier transform infrared spectroscopy) and XPS(X-ray photoelectron spectroscopy). And the adhesive characteristics were studied by measuring the T-peel strengths. Based on chemical analysis, the surface modification can be mainly ascribed to the creation of chemically active functional groups such as C-O, C=O and C-OH on semiconducting silicone surface. This oxidized rubber layer is inorganic silica-like structure of Si bound with three to four oxygen atoms ($SiOx,\;x=3{\sim}4$. The Corona treatment produces an increase in joint strength that is maximum for 10 min treatment. However, due to brittle property of this oxidized layer, the highly oxidized layer from too much extended treatment could be act as a weak point, decreasing the adhesion strength.

치과용 지르코니아 이장재 처리에 따른 지르코니아와 도재의 전단결합강도 비교 (Shear bond strength of a layered zirconia and porcelain according to treatment of zirconia liner)

  • 서정일;박원욱;김양근
    • 대한치과기공학회지
    • /
    • 제39권1호
    • /
    • pp.43-52
    • /
    • 2017
  • Purpose: Physical and chemical properties of gold is most suitable to be restored of teeth to its original state. Recently zirconia was used instead of gold because of esthetical and intimacy of human body. Because of high strength and high abrasion resistance of zirconia, all zirconia artificial tooth lead to wear the original tooth of opposite site. To preserve this original tooth, zirconia artificial tooth covered with dental ceramic glass was used. When joining the zirconia core and dental ceramic glass, difference of their thermal expansion coefficient and wetting ability is generated the residual stress at interface lead to crack. In order to solve this problem, intermediate layer what is called zir-liner was imported to decrease the residual stress and increase the bonding strength. Methods: In this study, to identify the optimum conditions for manufacturing process, various methods to rough the surface of zirconia core were adopted, and vary the thickness of interlayer, and analyzed bond strength. Results: Bond strength of sanding specimens group showed higher than that of non-sanding specimens group, and once applied intermediate layer with sanding specimens showed highest bond strength with 28 MPa. SEM photomicrographs of zirconia cores fired at $1500^{\circ}C$ showed parallel straight lines in sanding and pockmarked surface in blasting surfaces as abrasion traces. Observation of the destruction section after shear test by SEM were carried out. Liner applied non-sanding group and non-liner applied sanding group all showed interfacial crack. Sandblasting group with non-liner showed remained dental ceramic glass on the surface of zirconia. Sandblasting group with once applied liner showed partially remained liner and dental ceramic glass on the surface of zirconia. XRD analysis revealed that sandblasting group showed higher monoclinic peaks than other specimens group and this result was due to the high collision energy for stress induced phase transformation. Conclusions: A study on the improvement of bonding strength between zirconia and dental ceramic glass steadily carried out for the future to practical use.

Zircaloy-4에서 산화가 기계적 성질에 미치는 영향에 대한 연구 (A Study of the Effect of Oxidation on the Mechanical Properties of Zircaloy-4)

  • 고진현;김상호;황용화
    • 한국표면공학회지
    • /
    • 제35권5호
    • /
    • pp.312-318
    • /
    • 2002
  • A study on the change of mechanical properties and oxidation behavior of Zircaloy-4 fuel cladding after exposing at 90$0^{\circ}C$ and $1000^{\circ}C$ for various periods of exposure time under the steam atmosphere was carried out. The growth of the $ZrO_2$ layer combined with an oxygen-rich-phase layer into the Zircaloy tube material can be described by an expression, E = 1.1√Dt + $2 $\times$ 10^{-4}$ . The tensile strength of Zircaloy tubes increased for a short period of exposure time and decreased rapidly with further exposure while the hoop strength was not decreased greatly. In the meantime, the axial and circumferential elongations of oxidized Zircaloy tubes were decreased drastically with increasing exposure time as a result of embrittlement phenomena.